The influence of sodium (Na) on nucleation and growth of the Al-Si eutectic in a commercial hypoeutectic Al-Si-Cu-Mg foundry alloy has been investigated. The microstructural evolution during eutectic solidification was studied by a quenching technique. By comparing the orientation of the aluminium in the eutectic to that of the surrounding primary aluminium dendrites by EBSD, the eutectic solidification mode could be determined. The results show that the eutectic solidification starts near the mould wall and evolves with front growth opposite the thermal gradient on a macro-scale, and on a micro-scale with independent heterogeneous nucleation of eutectic grains in interdendritic spaces. Na-modified alloys therefore behave significantly differently from those modified by other elemental additions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Yield strength (YS) ageing curves have been modelled for A356 and A357 aluminium casting alloys below the solvus temperature of the main hardening precipitate. Predictions are based on the Shercliff and Ashby methodology (Acta MetaH. Mater. 38 (1990) 1789) for wrought alloys. Differences between strengthening in wrought and cast Al-Si-Mg alloys are considered. A Brinell hardness to YS conversion incorporating strain hardening has been established to enable YS ageing curves to be predicted with reduced experimental effort. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study explores several important aspects of the management of new product development (NPD) in the Chinese steel industry. Specifically it explores NPD success factors, the importance of management functions to new product success and measures of new product success from the perspective of the industry's practitioners. Based on a sample of 190 industrial practitioners from 18 Chinese steel companies, the study provides a mixed picture as China makes the transition from a centrally-controlled to market-based economy. On one hand, respondents ranked understanding users' needs as the most important factor influencing the performance of the new products. Further, formulating new product strategy and strengthening market research are perceived as the most important managerial functions in NPD. However, technical performance measures are regarded as more important and are more widely used in industry than market-based or financial measures of success.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Water wetting is a crucial issue in carbon dioxide (CO.) corrosion of multiphase flow pipelines made from mild steel. This study demonstrates the use of a novel benchtop apparatus, a horizontal rotating cylinder, to study the effect of water wetting on CO2 corrosion of mild steel in two-phase flow. The setup is similar to a standard rotating cylinder except for its horizontal orientation and the presence of two phases-typically water and oil. The apparatus has been tested by using mass-transfer measurements and CO2 corrosion measurements in single-phase water flow. CO2 corrosion measurements were subsequently performed using a water/hexane mixture with water cuts varying between 5% and 50%. While the metal surface was primarily hydrophilic under stagnant. conditions, a variety of dynamic water wetting situations was encountered as the water cut and fluid velocity were altered. Threshold velocities were identified at various water cuts when the surface became oil-wet and corrosion stopped.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A model of iron carbonate (FeCO3) film growth is proposed, which is an extension of the recent mechanistic model of carbon dioxide (CO2) corrosion by Nesic, et al. In the present model, the film growth occurs by precipitation of iron carbonate once saturation is exceeded. The kinetics of precipitation is dependent on temperature and local species concentrations that are calculated by solving the coupled species transport equations. Precipitation tends to build up a layer of FeCO3 on the surface of the steel and reduce the corrosion rate. On the other hand, the corrosion process induces voids under the precipitated film, thus increasing the porosity and leading to a higher corrosion rate. Depending on the environmental parameters such as temperature, pH, CO2 partial pressure, velocity, etc., the balance of the two processes can lead to a variety of outcomes. Very protective films and low corrosion rates are predicted at high pH, temperature, CO2 partial pressure, and Fe2+ ion concentration due to formation of dense protective films as expected. The model has been successfully calibrated against limited experimental data. Parametric testing of the model has been done to gain insight into the effect of various environmental parameters on iron carbonate film formation. The trends shown in the predictions agreed well with the general understanding of the CO2 corrosion process in the presence of iron carbonate films. The present model confirms that the concept of scaling tendency is a good tool for predicting the likelihood of protective iron carbonate film formation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Twenty-one strains of Bacillus (10 B. stearothermophilus, 3 B. cereus, and 8 B. licheniformis strains) were assayed for spore surface hydrophobicity on the basis of three measures: contact angle measurement (CAM), microbial adhesion to hydrocarbons (MATH), and hydrophobic interaction chromatography (HIC). On the basis of the spore surface characteristics obtained from these assays, along with data on the heat resistance of these spores in water, eight strains of Bacillus (three B. stearothermophilus, three B. cereus, and two B. licheniformis strains) either suspended in water or adhering to stainless steel were exposed to sublethal heat treatments at 90 to 110degreesC to determine heat resistance (D-value). Significant increases in heat resistance (ranging from 3 to 400%) were observed for the eight strains adhering to stainless steel. No significant correlation was found between these heat resistance increases and spore surface characteristics as determined by the three hydrophobicity assays. There was a significant positive correlation between the hydrophobicity data obtained by the MATH assay and those obtained by the HIC assay, but these data did not correlate with those obtained by the CAM assay.