100 resultados para SiC substrate
Resumo:
Doubly periodic arrays of strip conductors printed on a composite ferrite-dielectric substrate have been investigated at oblique incidence of linear polarized plane waves. The simulation results revealed strong non-reciprocity of wave reflectance and transmittance at positive and negative angles of incidence. It is also shown that the non-reciprocity is further enhanced by the strip conductor pattern.
Resumo:
Electroless nickel composite coatings with silicon carbide, SiC, as reinforcing particles deposited with Ni–P onto aluminium alloy, LM24, having zincating as under layer were subjected to heat treatment using air furnace. The changes at the interface were investigated using scanning electron microscope (SEM) and energy dispersive X-ray (EDX) to probe the chemistry changes upon heat treatment. Microhardness tester with various loads using both Knoop and Vickers indenters was used to study the load effect clubbed with the influence of second phase particles on the coating at the vicinity of the interface. It was observed that zinc was absent at the interface after elevated temperature heat treatment at 400–500 °C. Precipitation of copper and nickel with a distinct demarcation (copper rich belt) along the coating interface was seen with irregular thickness of the order of 1 μm. Migration of copper from the bulk aluminium alloy could have been the factor. Brittleness of the coating was confirmed on heat treatment when indented with Vickers. However, in composite coating the propagation of the microcrack was stopped by the embedded particles but the microcracks continue in the matrix when not interrupted by second phase particles (SiC).
Resumo:
Surface behaviour is of paramount importance as failure and degradation tend to initiate from the surface. Electroless composite coating (NiP/SiC) was developed using SiC as reinforcing particles. As heat treatment plays a vital role in electroless nickel coating owing to the changes in microstructure, phase structure and mechanical properties, an insight at the interface changes in chemistry and micromechanical behaviour was investigated using scanning electron microscopy (SEM) and energy dispersive X-ray (EDX) and microindentation techniques. Corrosion performance was analysed using electrochemical impedance spectroscopy (EIS). Absence of zinc and migration of copper at the interface was detected. Brittleness and microcracks was seen long the interface when indenting at load of 500 gf (Vickers). Corrosion performance is weaker than particles free coating. However, a thin blanket of NiP could enhance the resistance to corrosive medium.
Resumo:
The paper reports on the mm-wave characterization of a low temperature co-fired ceramic (LTCC) substrate. A substrate integrated resonator (SIW) method is presented for robust extraction of both permittivity and loss tangent of the substrate. The data obtained allow full characterization of the substrate in the 71 GHz – 95 GHz frequency range suitable for accurate modelling of E-and W-band printed circuits.
Resumo:
Hepatocyte growth factor-regulated tyrosine kinase substrate (Hrs) is a prominent substrate for activated tyrosine kinase receptors that has been proposed to play a role in endosomal membrane trafficking. The protein contains a FYVE domain, which specifically binds to the lipid phosphatidylinositol (PI) 3-phosphate (PI 3-P). We show that this interaction is required both for correct localization of the protein to endosomes that only partially coincides with early endosomal autoantigen 1 and for efficient tyrosine phosphorylation of the protein in response to epidermal growth factor stimulation. Treatment with wortmannin reveals that Hrs phosphorylation also requires PI 3-kinase activity, which is necessary to generate the PI 3-P required for localization. We have used both hypertonic media and expression of a dominant-negative form of dynamin (K44A) to inhibit endocytosis; under which conditions, receptor stimulation fails to elicit phosphorylation of Hrs. Our results provide a clear example of the coupling of a signal transduction pathway to endocytosis, from which we propose that activated receptor (or associated factor) must be delivered to the appropriate endocytic compartment in order for Hrs phosphorylation to occur.
Resumo:
The second harmonic generation (SHG) intensity spectrum of SiC, ZnO, GaN two-dimensional hexagonal crystals is calculated by using a real-time first-principles approach based on Green's function theory [Attaccalite et al., Phys. Rev. B: Condens. Matter Mater. Phys. 2013 88, 235113]. This approach allows one to go beyond the independent particle description used in standard first-principles nonlinear optics calculations by including quasiparticle corrections (by means of the GW approximation), crystal local field effects and excitonic effects. Our results show that the SHG spectra obtained using the latter approach differ significantly from their independent particle counterparts. In particular they show strong excitonic resonances at which the SHG intensity is about two times stronger than within the independent particle approximation. All the systems studied (whose stabilities have been predicted theoretically) are transparent and at the same time exhibit a remarkable SHG intensity in the range of frequencies at which Ti:sapphire and Nd:YAG lasers operate; thus they can be of interest for nanoscale nonlinear frequency conversion devices. Specifically the SHG intensity at 800 nm (1.55 eV) ranges from about 40-80 pm V(-1) in ZnO and GaN to 0.6 nm V(-1) in SiC. The latter value in particular is 1 order of magnitude larger than values in standard nonlinear crystals.
Resumo:
With increasing excitation wavelength from 514 to 782 nm, a significant difference in the Raman spectra of SiC nanorods was observed as compared to bulk material. The intensity ratio of the LO mode to that of the IF mode increases with the excitation wavelength increasing. This has been identified as resonant Raman scattering caused by Fröhlich interaction.
Resumo:
Biological colonization of stone is a major concern in the preservation and presentation of cultural heritage. Colonization is typically associated with unpleasant soiling, and varying degrees of biodeterioration. A better understanding of why organisms grow where they do, will aid in
developing preventative, and treatment methods for biosoiling of cultural heritage. Sandstone exposure trials were set up at nine different locations across Northern Ireland to investigate the influences of local climate, local environmental,and micro-climatic factors on the early stages (up to 21 months) of biological colonization.
Results showed that, green and yellow soiling occurred on tooled stone surfaces, whereas darkening occurred preferentially on smooth surfaces. It is likely that different populations of organisms occur on these surfaces with green algae occurring on tooled surfaces due to slower drying rates (i.e. prolonged moisture retention), and cyanobacteria and fungi thriving on smooth surfaces due to their ability to withstand moisture fluctuation.
Resumo:
The investigation is focused on the wear behaviour at elevated test temperature of composite Ni–P/SiC deposit, with varying concentration of the reinforcing SiC particles. The phase evolution measured by X-ray diffraction suggests slight crystallisation during wear testing at 200 °C. In coating without reinforcing particles, adhesive wear is accompanied by microcracks. The thermal heat generated and the cyclic loading could have induced sub-surface microcracks. Owing to the effective matrix-ceramics system in composite coatings, fine grooves, abrasive polishing and uniform wearing are observed. Reinforcing particles in the matrix hinder microcrack formation and significantly reduce the wear rate. Triboxidation is confirmed from energy dispersive X-ray spectrometry.