22 resultados para FT-IR spectroscopy

em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo


Relevância:

100.00% 100.00%

Publicador:

Resumo:

The purpose of this study was to compare the inorganic content and morphology of one nanofilled and one nanohybrid composite with one universal microhybrid composite. The Vickers hardness, degree of conversion and scanning electron microscope of the materials light-cured using LED unit were also investigated. One nanofilled (Filtek (TM) Supreme XT), one nanohybrid (TPH (R) 3) and one universal microhybrid (Filtek (TM) Z-250) composite resins at color A2 were used in this study. The samples were made in a metallic mould (4 mm in diameter and 2 mm in thickness). Their filler weight content was measured by thermogravimetric analysis (TG). The morphology of the filler particles was determined using scanning electron microscope equipped with a field emission gun (SEM-FEG). Vickers hardness and degree of conversion using FT-IR spectroscopy were measured. Filtek (TM) Z-250 (microhybrid) composite resin shows higher degree of conversion and hardness than those of Filtek (TM) Supreme XT (nanofilled) and TPH (R) 3 (nanohybrid) composites, respectively. The TPH3 (R) (nanohybrid) composite exhibits by far the lowest mechanical property. Nanofilled composite resins show mechanical properties at least as good as those of universal hybrids and could thus be used for the same clinical indications as well as for anterior restorations due to their high aesthetic properties. Microsc. Res. Tech. 75:758765, 2012. (C) 2011 Wiley Periodicals, Inc

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work, barium zirconate (BaZrO3) ceramics synthesized by solid state reaction method and sintered at 1670 degrees C for 4 h were characterized by X-ray diffraction (XRD), Rietveld refinement, and Fourier transform infrared (FT-IR) spectroscopy. XRD patterns, Rietveld refinement data and FT-IR spectra which confirmed that BaZrO3 ceramics have a perovskite-type cubic structure. Optical properties were investigated by ultraviolet-visible (UV-vis) absorption and photoluminescence (PL) measurements. UV-vis absorption spectra suggested an indirect allowed transition with the existence of intermediary energy levels within the band gap. Intense visible green PL emission was observed in BaZrO3 ceramics upon excitation with a 350 nm wavelength. This behavior is due to a majority of deep defects within the band gap caused by symmetry breaking in octahedral [ZrO6] clusters in the lattice. The microwave dielectric constant and quality factor were measured using the method proposed by Hakki-Coleman. The dielectric resonator antenna (DRA) was investigated experimentally and numerically using a monopole antenna through an infinite ground plane and Ansoft's high frequency structure simulator software, respectively. The required resonance frequency and bandwidth of DRA were investigated by adjusting the dimension of the same material. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Binary and ternary systems of Ni2+, Zn2+, and Pb2+ were investigated at initial metal concentrations of 0.5, 1.0 and 2.0 mM as competitive adsorbates using Arthrospira platensis and Chlorella vulgaris as biosorbents. The experimental results were evaluated in terms of equilibrium sorption capacity and metal removal efficiency and fitted to the multi-component Langmuir and Freundlich isotherms. The pseudo second order model of Ho and McKay described well the adsorption kinetics, and the FT-IR spectroscopy confirmed metal binding to both biomasses. Ni2+ and Zn2+ interference on Pb2+ sorption was lower than the contrary, likely due to biosorbent preference to Pb. In general, the higher the total initial metal concentration, the lower the adsorption capacity. The results of this study demonstrated that dry biomass of C. vulgaris behaved as better biosorbent than A. platensis and suggest its use as an effective alternative sorbent for metal removal from wastewater. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Magnetic iron oxide nanoparticles (magnetite) (MNPs) were prepared using different organic and inorganic bases. Strong inorganic base (KOH) and organic bases (NH4OH and 1,4-diazabicyclo[2.2.2]octane (DABCO)) were used in the syntheses of the MNPs. The MNPs were characterized by X-ray diffraction (XRD), scanning electron microscope (SEM). Fourier transform infrared spectroscopy (FT-IR) and magnetization measurements. MNPs prepared with strong inorganic base yielded an average size of 100 nm, whereas the average size of the MNPs prepared with the organic bases was 150 nm. The main competitive phase for MNPs prepared with the strong inorganic and organic bases was maghemite; however, syntheses with KOH yielded a pure magnetite phase. The transfection study performed with the MNPs revealed that the highest transfection rate was obtained with the MNPs prepared with KOH (74%). The correlation between the magnetic parameters and the transfection ratio without transfection agents indicated that MNPs prepared with KOH were a better vector for possible applications of these MNPs in biomedicine. HeLa cells incubated with MNP-KOH at 10 mu g/mL for 24 and 48 h exhibited a decrease in population in comparison with the control cells and it was presumably related to the toxicity of the MNPs. However, the cells incubated with MNP-KOH at 50 and 100 mu g/mL presented a very small difference in the viability between the cell populations studied at 24 and 48 h. These data illustrate the viability of HeLa cells treated with MNP-KOH and suggest the potential use of these MNPs in biomedical applications. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In this paper, we report our initial research to obtain hexagonal rod-like elongated silver tungstate (alpha-Ag2WO4) microcrystals by different methods [sonochemistry (SC), coprecipitation (CP), and conventional hydrothermal (CH)] and to study their cluster coordination and optical properties. These microcrystals were structurally characterized by X-ray diffraction (XRD), Rietveld refinements, Fourier transform infrared (FT-IR), X-ray absorption near-edge structure (XANES), and extended X-ray absorption fine structure (EXAFS) spectroscopies. The shape and average size of these alpha-Ag2WO4 microcrystals were observed by field-emission scanning electron microscopy (FE-SEM). The optical properties of these microcrystals were investigated by ultraviolet-visible (UV-vis) spectroscopy and photoluminescence (PL) measurements. XRD patterns and Rietveld refinement data confirmed that alpha-Ag2WO4 microcrystals have an orthorhombic structure. FT-IR spectra exhibited four IR-active modes in a range from 250 to 1000 cm(-1). XANES spectra at the W L-3-edge showed distorted octahedral [WO6] clusters in the lattice, while EXAFS analyses confirmed that W atoms are coordinated by six O atoms. FE-SEM images suggest that the alpha-Ag2WO4 microcrystals grow by aggregation and the Ostwald ripening process. PL properties of alpha-Ag2WO4 microcrystals decrease with an increase in the optical band-gap values (3.19-3.23 eV). Finally, we observed that large hexagonal rod-like alpha-Ag2WO4 microcrystals prepared by the SC method exhibited a major PL emission intensity relative to alpha-Ag2WO4 microcrystals prepared by the CP and CH methods.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

A comprehensive structural and vibrational study of the potential metal-protein attenuating compound 8-hydroxyquinoline-2-carboxaldehyde isonicotinoyl hydrazone is reported. X-ray diffraction data, as well as FT-IR and Raman frequencies, were compared with the respective theoretical values obtained from DFT calculations. Theory agrees well with experiment. In this context, an attempt of total assignment concerning the FT-IR and Raman spectra of the title compound was performed, shedding new light on previous partial assignments published elsewhere.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Although electrochemical oxidation of simple organic molecules on metal catalysts is the basic ingredient of fuel cells, which have great technological potential as a renewable source of electrical energy, the detailed reaction mechanisms are in most cases not completely understood. Here, we investigate the ethanol-platinum interface in acidic aqueous solution using infrared-visible sum frequency generation (SFG) spectroscopy and theoretical calculations of vibrational spectra in order to identify the intermediates present during the electro-oxidation of ethanol. The complex vibrational spectrum in the fingerprint region imply on the coexistence of several adsorbates. Based on spectra in ultra-high-vacuum (UHV) and electrochemical environment from the literature and our density functional theory (DFT) calculations of vibrational spectra, new adsorbed intermediates, never before observed with conventional infrared (IR) spectroscopy, are proposed here: g2-acetaldehyde, g2-acetyl, ethylidyne, monodentate acetate, methoxy, tertiary methanol derivative, COH residue, g2-formaldehyde, mono and bidentate formate, CH3 and CH2 residues. In addition, we present new evidences for an ethoxy intermediate, a secondary ethanol derivative and an acetyl species, and we confirm the presence of previously observed adsorbates: a tertiary ethanol derivative, bidentate acetate, and COad. These results indicate that the platinum surface is much more reactive, and the reaction mechanism for ethanol electro-oxidation is considerably more complex than previously considered. This might be also true for many other molecule-catalyst systems.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Organic-inorganic hybrids containing methacrylic acid (McOH, CH(2)= C(CH(3))COOH)) modified zirconium tetrapropoxide, Zr(OPr(n))(4), classed as di-ureasil-zirconium oxo-cluster hybrids, have been prepared and structurally characterized by X-ray diffraction (XRD), small-angle X-ray scattering (SAXS), Fourier transform infrared (FT-IR) and Raman (FT-Raman) spectroscopies, Si and C nuclear magnetic resonance (NMR), and atomic force microscopy (AFM). XRD and SAXS results have pointed out the presence of Si- and Zr-based nanobuilding blocks (NBBs) dispersed into the organic phase. Inter-NBBs correlation distances have been estimated for the pure di-ureasil and a model compound obtained. by hydrolysis/condensation of Zr(OPr(n))(4):McOH (molar ratio 1: 1): d(Si) approximate to 26 +/- 1 angstrom and d(Zr) approximate to 16 +/- 1 angstrom, respectively. In the case of the di-ureasil-zirconium oxo-cluster hybrids, these distances depend on the Zr relative molar percentage (rel. mol. Zr %) (d(Si) ranges from 18 to 25 angstrom and d(Zr) from 14 to 23 angstrom, as the rel. mol. Zr % increases from 5 to 75), suggesting that the Si- and Zr-based clusters are interconstrained. Complementary data from FT-IR, FT-Raman, (29)Si and (13)C NMR, and AFM support to a structural model where McOH-modified Zr-based NBBs (Zr-OMc) are present over the whole range of composition. At low Zr-OMc contents (rel. mol. Zr % <30) the clusters are well-dispersed within the di-ureasil host, whereas segregation occurs at the 0.1 mu m scale at high Zr-OMc concentration (rel. mol. Zr % = 50). No Zr-O-Si heterocondensation has been discerned. Monomode waveguides, diffractions gratings, and Fabry-Perot cavities have been written through the exposure of the hybrid monoliths to UV light. FT-Raman has shown that the chemical process that takes place under illumination is the polymerization of the methacrylate groups of the Zr-OMc NBBs. The guidance region in patterned channels is a Gaussian section located below the exposed surface with typical dimensions of 320 mu m wide and 88 mu m deep. The effective refractive index is 1.5162 (maximum index contrast on the order of 1 x 10(-4)) and the reflection coeficient of the Fabry-Perot cavity (formed by a grating patterned into a 0.278 cm channel) is 0.042 with a free spectral range value of 35.6 GHz.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

By means of in situ IR spectroscopy we investigate the effect of dissolved alkali cations on the electro-oxidation of ethylene glycol on platinum in alkaline media. The results revealed that the increase in the oxidation currents (Li(+) < Na(+) < K(+)) is reflected in the increase in the ratio between carbonate and oxalate produced.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The hydrolysis of pyridoxalrhodanine in a basic medium containing the dimethylthallium(III) cation afforded the compound [TlMe2(L)]center dot H2O (1.H2O) [HL = 5-(hydroxymethyl)-8-methyl-3-thiol-7-azacoumarin]. This compound was characterized in solid state by IR spectroscopy and in solution by H-1 and C-13{H-1} NMR spectrometry. X-ray diffraction showed that the crystal consists of associated TlMe2(L) units and hydrogen bonded water molecules. The L- anion is bound to the metal mainly by a bridging S atom [Tl-S = 2.9458(18) angstrom; 2.9616(16) angstrom], although secondary interactions through O atoms (Tl-O: 2.861(5); 2.900(5) angstrom)] are also present. The longer Tl-O interaction and the hydrogen bonds of the water molecules give rise to a tridimensional polymeric structure. (C) 2012 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The worldwide production of bamboo generates large volumes of leaf wastes, which are deposited in landfills or burned in an uncontrolled manner, with negative effects in the environment. The ash obtained by calcining of the bamboo leaf waste, shows good qualities as supplementary cementing material for the production of blended cements. The current paper shows a detailed scientific study of a Brazilian bamboo leaf ash (BLA) calcined at 600 degrees C in small scale condition, by using different techniques (XRF, XRD, SEM/EDX, FT-IR, TG/DTG) and technical study in order. to analyse the behaviour of this ash in blended cements elaborated with 10% and 20% by mass of BLA. The results stated that this ash shows a very high pozzolanic activity, with a reaction rate constant K of the order of 10(-1)/h and type I CSH gel was the main hydrated phase obtained from pozzolanic reaction. The BLA blended cements (10% and 20%) complied with the physical and mechanical requirements of the existing European standards. (c) 2012 Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Carbon-supported Pt-based electrocatalysts were synthesized by Pechini method for the ethanol oxidation (EOR). Physicochemical characterizations were helpful to estimate the diameters of the obtained materials ranging from 2 nm to 5 nm. Main electrochemical experiments were carried out at 90 degrees C i.e. under the working conditions of performing the single 5 cm(2) direct ethanol fuel cell (DEFC). Pt(80)Sn(20)/C was the anode catalyst which has given the highest power density of 37 mW cm(-2). Importantly, the IR spectroscopy measurements associated with the qualitative analysis done at the output of the anodic compartment of the fuel cell have shown that ethanol oxidation on Pt(80)Sn(20)/C was mainly a two-electron sustainable process. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Synthesis, characterization, DFT simulation and biological assays of two new metal complexes of 2-(2-thienyl)benzothiazole - BTT are reported. The complexes [Ag(BTT)(2)NO3] - AgBTT2 and [Au(BTT)Cl]center dot 1/2H(2)O - AuBTT were obtained by mixing the ligand with silver (I) nitrate or gold(I) chloride in methanolic solution. Characterization of the complexes were based on elemental (C, H, N and S), thermal (TG-DTA) analysis, C-13 and H-1 NMR, FT-IR and UV-Vis spectroscopic measurements, as well as the X-ray structure determination for AgBTT2. Spectroscopic data predicted by DFT calculations were in agreement with the experimental data for both complexes. The ligand BTT was synthesized by the condensation of 2-thiophenecarboxaldehyde and 2-aminothiophenol in a microwave furnace. AgBTT2 has a monomeric structure. Both complexes show a good activity against Mycobacterium tuberculosis. Free BIT shows low antitubercular activity. (C) 2012 Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Information on the solvation in mixtures of water, W, and the ionic liquids, ILs, 1-allyl-3-R-imidazolium chlorides; R = methyl, 1-butyl, and 1-hexyl, has been obtained from the responses of the following solvatochromic probes: 2,6-dibromo-4-[(E)-2-(1-R-pyridinium-4-yl)ethenyl] phenolate, R = methyl, MePMBr2; 1-octyl, OcPMBr(2), and the corresponding quinolinium derivative, MeQMBr(2). A model developed for solvation in binary mixtures of W and molecular solvents has been extended to the present mixtures. Our objective is to assess the relevance to solvation of hydrogen-bonding and the hydrophobic character of the IL and the solvatochromic probe. Plots of the medium empirical polarity, E-T(probe) versus its composition revealed non-ideal behavior, attributed to preferential solvation by the IL and, more efficiently, by the IL-W hydrogen-bonded complex. The deviation from linearity increases as a function of increasing number of carbon atoms in the alkyl group of the IL, and is larger than that observed for solvation by W plus molecular solvents (1-propanol and 2-(1-butoxy)ethanol) that are more hydrophobic than the ILs investigated. This enhanced deviation is attributed to the more organized structure of the ILs proper, which persists in their aqueous solutions. MeQMBr(2) is more susceptible to solvent lipophilicity than OcPMBr(2), although the former probe is less lipophilic. This enhanced susceptibility agrees with the important effect of annelation on the contributions of the quinonoid and zwitterionic limiting structures to the ground and excited states of the probe, hence on its response to both medium composition and lipophilicity of the IL.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Witzkeite, ideally Na4K4Ca(NO3)(2)(SO4)(4)center dot 2H(2)O, is a new mineral found in the oxidation zone of the guano mining field at Punta de Lobos, Tarapaca region, Chile. It occurs as colorless, tabular crystals up to 140 mu m in length, associated with dittmanite and nitratine. Witzkeite is colorless and transparent, with a white streak and a vitreous luster. It is brittle, with Molts hardness 2 and distinct cleavage on {001}. Measured density is 2.40(2) g/cm(3), calculated density is 2.403 g/cm(3). Witzkeite is biaxial (-) with refractive indexes alpha = 1.470(5), beta = 1.495(5), gamma = 1.510(5), measured 2V = 50-70 degrees. The empirical composition is (electron microprobe, mean of five analyses, H2O, CO2, and N2O5 by gas chromatography; wt%): Na2O 12.83, K2O 22.64, CaO 7.57, FeO 0.44, SO3 39.96, N2O5 12.7, H2O 4.5, total 100.64; CO2 was not detected. The chemical formula, calculated based on 24 O, is: Na3.40K3.95Ca1.11Fe0.05(NO3)(1.93)(SO4)(4.10)(H4.10O1.81). Witzkeite is monoclinic, space group C2/c, with unit-cell parameters: a = 24.902(2), b = 5.3323(4), c = 17.246(1) angstrom, beta = 94.281(7)degrees, V = 2283.6(3) angstrom(3) (Z = 4). The crystal structure was solved using single-crystal X-ray diffraction data and refined to R-1(F) = 0.043. Witzkeite belongs to a new structure type and is noteworthy for the very rare simultaneous presence of sulfate and nitrate groups. The eight strongest X-ray powder-diffraction lines [d in angstrom (I in %) (h k l)] are: 12.38 (100) (2 0 0), 4.13 (19) (6 0 0), 3.10 (24) (8 0 0), 2.99 (7) ((8) over bar 02), 2.85 (6) (8 02), 2.69 (9) ((7) over bar 1 3), 2.48 (12) (10 0 0), and 2.07 (54) (12 0 0). The IR spectrum of witzkeite was collected in the range 390-4000 cm(-1). The spectrum shows the typical bands of SO42- ions (1192, 1154, 1116, 1101, 1084, 993, 634, and 617 cm(-1)) and of NO3- ions (1385, 1354, 830, 716, and 2775 cm(-1)). Moreover, a complex pattern of bands related to H2O is visible (bands at 3565, 3419, 3260, 2405, 2110, 1638, and 499 cm(-1)). The IR spectrum is discussed in detail.