Resumo:
This paper shows the results of an experimental investigation carried out on a connection element of glulam and concrete composite structures, through double-sided push-out shear tests. The connection system was composed of perforated steel plates glued with epoxy adhesive. Five specimens were made and tested under shear forces. This innovative connection system showed an average initial slip modulus equivalent to 339.4 kN/mm. In addition, the connection system was evaluated by means of numerical simulations and the software ANSYS was used for this purpose. The numerical simulations demonstrated good agreement with the experimental data, especially in the regime of elastic-linear behavior of materials. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
Masonry spandrels together with shear walls are structural components of a masonry building subjected to lateral loads. Shear walls are the main components of this structural system, even if masonry spandrels are the elements that ensure the connection of shear wall panels and the distribution of stresses through the masonry piers. The use of prefabricated truss type bars in the transversal and longitudinal directions is usually considered a challenge, even if the simplicity of the applications suggested here alleviate some of the possible difficulties. This paper focus on the experimental behavior of masonry spandrels reinforced with prefabricated trusses, considering different possibilities for the arrangement of reinforcement and blocks. Reinforced spandrels with three and two hollow cell concrete blocks and with different reinforcement ratios have been built and tested using a four and three point loading test configuration. Horizontal bed joint reinforcement increased the capacity of deformation as well as the ultimate load, leading to ductile responses. Vertical reinforcement increased the shear strength of the masonry spandrels and its distribution play a central role on the shear behavior. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
This article presents the results of a combined experimental and theoretical study of fracture and resistance-curve behavior of hybrid natural fiber- and synthetic polymer fiber-reinforced composites that are being developed for potential applications in affordable housing. Fracture and resistance-curve behavior are studied using single-edge notched bend specimens. The sisal fibers used were examined using atomic force microscopy for fiber bundle structures. The underlying crack/microstructure interactions and fracture mechanisms are elucidated via in situ optical microscopy and ex-situ environmental scanning microscopy techniques. The observed crack bridging mechanisms are modeled using small and large scale bridging concepts. The implications of the results are then discussed for the design of eco-friendly building materials that are reinforced with natural and polypropylene fibers.
Resumo:
O trabalho analisa a história da produção do edifício da Faculdade de Arquitetura e Urbanismo da Universidade de São Paulo, projetado por João Batista Vilanova Artigas (1915-1985) em 1961 e concluído em 1969. Mais especificamente, o artigo se volta aos materiais do edifício, oferecendo insumos para uma discussão sobre o papel do chamado “brutalismo paulista” na década de 1960. O edifício da FAUUSP, como se sabe, é um marco na arquitetura moderna brasileira. Seu caráter paradigmático consiste na síntese das posições programáticas de Artigas, tanto em relação ao ensino de arquitetura como em relação à poética moderna, que ultrapassa o limite autoral e constitui uma escola. São características dessa escola – por vezes chamada de “paulista”, “brutalista” ou “artiguista” – alguns princípios como a continuidade espacial, o elogio das formas estruturais, a verdade dos materiais e o desenvolvimento das forças produtivas através da superação tecnológica. Esses princípios respondiam a algumas das questões mais urgentes da arquitetura moderna brasileira naquele período, deslocando a nova monumentalidade para uma dimensão construtiva. A nova poética, claramente exposta no projeto da FAUUSP, coincide com o surgimento de uma estética que atribuiu um novo valor político e crítico à produção. Passam a ser frequentes, por exemplo, interpretações do concreto armado brasileiro como síntese do subdesenvolvimento, por suas marcas de feitura artesanal e seus recordes tecnológicos. O objetivo deste artigo é contribuir com esse debate caracterizando em detalhe a produção do edifício em seus materiais: o concreto armado, a esquadria, os materiais de acabamento e os componentes industriais. O exame de aspectos históricos da produção do edifício, recolhidos em documentos originais e depoimentos, permite verificarmos de que modo a poética arquitetônica participa das decisões da obra e qual o seu impacto na economia do edifício e em sua forma de produção. Aprendemos, por exemplo, que o concreto armado apresenta manifestações visuais distintas e independentes de seu modo de produção (que foram pelo menos três: moldado in loco, protendido, e com agregados leves, sem função estrutural); que a empena da fachada exigiu uma fundação própria para seu cimbramento; que a modulação dos caixilhos não correspondia à modulação da estrutura; que a resina epóxi foi usada de modo pioneiro e experimental; que as fôrmas foram produzidas por um hábil carpinteiro português, mas as relações de trabalho eram precárias; que a contratação do projeto básico previa o detalhamento durante a obra pelo Escritório Técnico do Fundo para a Construção da Cidade Universitária. Essa noção ampla de material, entendida como a matéria mais o trabalho social que a define historicamente, nos permite tratar, simultaneamente, de aspectos técnicos, econômicos e artísticos da obra e assim compreender com maior exatidão dos termos do debate acerca da produção na arquitetura “brutalista” e seu papel político.
Resumo:
Purpose: To investigate the periapical tissue response of 4 different retrograde root-filling materials, ie, intermediate restorative material, thermoplasticized gutta-percha, reinforced zinc oxide cement (Super-EBA), and mineral trioxide aggregate (MTA), in conjunction with an ultrasonic root-end preparation technique in an animal model. Materials and Methods: Vital roots of the third and fourth right mandibular premolars in 6 healthy mongrel dogs were apicectomized and sealed with 1 of the materials using a standardized surgical procedure. After 120 days, the animals were sacrificed and the specimens were analyzed radiologically, histologically, and scanning electron microscopically. The Fisher exact test was performed on the 2 outcome values. Results: Twenty-three sections were analyzed histologically. Evaluation showed better re-establishment of the periapical tissues and generally lower inflammatory infiltration in the sections from teeth treated with the intermediate restorative material and the MTA. New root cement on the resected dentin surfaces was seen on all sections regardless of the used material. New hard tissue formation, directly on the surface of the material, was seen only in the MTA sections. There was no statistical difference in outcome among the tested materials. Conclusions: The results from this dog model favor the intermediate restorative material and MTA as retrograde fillings when evaluating the bone defect regeneration. MTA has the most favorable periapical tissue response when comparing the biocompatibility of the materials tested. (C) 2012 American Association of Oral and Maxillofacial Surgeons J Oral Maxillofac Surg 70:2041-2047, 2012
Resumo:
The construction industry is one of the greatest sources of pollution because of the high level of energy consumption during its life cycle. In addition to using energy while constructing a building, several systems also use power while the building is operating, especially the air-conditioning system. Energy consumption for this system is related, among other issues, to external air temperature and the required internal temperature of the building. The facades are elements which present the highest level of ambient heat transfer from the outside to the inside of tall buildings. Thus, the type of facade has an influence on energy consumption during the building life cycle and, consequently, contributes to buildings' CO2 emissions, because these emissions are directly connected to energy consumption. Therefore, the aim is to help develop a methodology for evaluating CO2 emissions generated during the life cycle of office building facades. The results, based on the parameters used in this study, show that facades using structural glazing and uncolored glass emit the most CO2 throughout their life cycle, followed by brick facades covered with compound aluminum panels or ACM (Aluminum Composite Material), facades using structural glazing and reflective glass and brick facades with plaster coating. On the other hand, the typology of facade that emits less CO2 is brickwork and mortar because its thermal barrier is better than structural glazing facade and materials used to produce this facade are better than brickwork and ACM. Finally, an uncertainty analysis was conducted to verify the accuracy of the results attained. (C) 2011 Elsevier Inc. All rights reserved.
Resumo:
Introduction: The aim of this study was to evaluate the pH, calcium ion release, setting time, and solubility of white mineral trioxide aggregate (WMTA) and white Portland cement (WPC) combined with the following radiopacifying agents: bismuth oxide (BO), calcium tungstate (CT), and zirconium oxide (ZO). Methods: Fifty acrylic teeth with root-end filling material were immersed in ultrapure water for measurement of pH and calcium release (atomic absorption spectrophotometry) at 3, 24, 72, and 168 hours. For evaluation of setting time, each material was analyzed according to the American Society for Testing and Materials guidelines 266/08. The solubility test was performed according to American National Standards Institute/American Dental Association specification no. 57/2000. Solubility, setting time, and pH values were compared by using analysis of variance and Tukey test, and the values of calcium release were compared by the Kruskal-Wallis and Miller tests. The significance level was set at 5%. Results: The pH and calcium release were higher at 3 and 24 hours. WPC was the material with the higher values for both properties. WMTA had the greatest solubility among all materials (P < .05). All radiopacifiers increased the setting time of WPC, and WMTA had the shortest setting time among all materials (P < .05). Conclusions: All materials released calcium ions. Except for WPC/CT at 168 hours, all materials promoted an alkaline pH. On the basis of the obtained results, ZO and CT can be considered as potential radiopacifying agents to be used in combination with Portland cement. (J Endod 2012;38:394-397)
Resumo:
Duarte MAH, Alves de Aguiar K, Zeferino MA, Vivan RR, Ordinola-Zapata R, Tanomaru-Filho M, Weckwerth PH, Kuga MC. Evaluation of the propylene glycol association on some physical and chemical properties of mineral trioxide aggregate. International Endodontic Journal, 45, 565570, 2012. Abstract Aim To evaluate the influence of propylene glycol (PG) on the flowability, setting time, pH and calcium ion release of mineral trioxide aggregate (MTA). Methodology Mineral trioxide aggregate was mixed with different proportions of PG, as follows: group 1: MTA + 100% distilled water (DW); group 2: MTA + 80% DW and 20% PG; group 3: MTA + 50% DW and 50% PG; group 4: MTA + 20% DW and 80% PG; group 5: MTA + 100% PG. The ANSI/ADA No. 57 was followed for evaluating the flowability and the setting time was measured by using ASTM C266-08. For pH and calcium release analyses, 50 acrylic teeth with root-end cavities were filled with the materials (n = 10) and individually immersed in flasks containing 10 mL deionized water. After 3 h, 24 h, 72 h and 168 h, teeth were placed in new flasks and the water in which each specimen was immersed had its pH determined by a pH metre and the calcium release measured by an atomic absorption spectrophotometer with a calcium-specific hollow cathode lamp. Data were analysed by using one-way anova test for global comparison and by using Tukeys test for individual comparisons. Results The highest value of flowability was observed with MTA + 20% DW and 80% PG and the lowest values were found with MTA + 100% DW. They were significantly different compared to the other groups (P < 0.05). The presence of PG did not affect the pH and calcium release. The MTA + 100% PG favoured the highest (P < 0.05) pH and calcium release after 3 h. Increasing the PG proportion interfered (P < 0.05) with the setting time; when used at the volume of 100% setting did not occur. Conclusion The addition of PG to MTA-Angelus increased its setting time, improved flowability and increased the pH and calcium ion release during the initial post-mixing periods. The ratio of 80% DW 20% PG is recommended.
Resumo:
This study aimed to evaluate, ex vivo, the nanoleakage in dentinal tubules, the linear infiltration of silver nitrate in the dentin wall/root-end filling material interface, and the presence of gaps in this interface in root-end cavities filled with 4 filling materials. Forty-eight disto-buccal root canals of maxillary molars were instrumented and filled. Retrograde cavities were prepared with ultrasonic points (apical 2 mm). The samples were divided into 2 control groups (n = 4) and 4 experimental groups (n = 10): Group I white mineral trioxide aggregate (MTA); Group II Super EBA; Group III Portland cement; and Group IV Sealer 26. After 1 week, the specimens were subjected to silver nitrate and prepared for SEM (backscattered electrons). In the apical-apical segment, an area with significantly higher leakage was observed for Super EBA, followed by Portland cement, MTA, and Sealer 26 (P = 0.0054). In the medium and cervical segments, all materials showed the same leakage behavior (P = 0.1815 and P = 0.1723, respectively). The linear infiltration at the dentin wall/root-end filling material interface was higher with Super EBA than the other groups. No differences in the percentage of gaps along the 3 mm of dentin wall/root-end filling material interface between the 4 materials were evident (P > 0.05). Nanoleakage occurred mainly in the apical segment of the samples, and Super EBA showed the highest values. The area and linear leakage were lower in the middle and coronal segments, regardless of the root-end filling material. No material perfectly sealed the root-end cavities, which allowed for the leakage occurrence. Microsc. Res. Tech. 75:796800, 2012. (C) 2011 Wiley Periodicals, Inc.
Resumo:
Aim To compare the changes in the surface structure and elemental distribution, as well as the percentage of ion release, of four calcium silicate-containing endodontic materials with a well-established epoxy resin-based sealer, submitted to a solubility test. Methodology Solubility of AH Plus, iRoot SP, MTA Fillapex, Sealapex and MTA-Angelus (MTA-A) was tested according to ANSI/ADA Specification 57. The deionized water used in the solubility test was submitted to atomic absorption spectrophotometry to determine and quantify Ca2+, Na+, K+, Zn2+, Ni2+ and Pb2+ ions release. In addition, the outer and inner surfaces of nonsubmitted and submitted samples of each material to the solubility test were analysed by means of scanning electron microscopy and energy-dispersive spectroscopy (SEM/EDX). Statistical analysis was performed by using one-way anova and Tukeys post hoc tests (a = 0.05). Results Solubility results, in percentage, sorted in an increasing order were -1.24 +/- 0.19 (MTA-A), 0.28 +/- 0.08 (AH Plus), 5.65 +/- 0.80 (Sealapex), 14.89 +/- 0.73 (MTA Fillapex) and 20.64 +/- 1.42 (iRoot SP). AH Plus and MTA-A were statistically similar (P > 0.05), but different from the other materials (P < 0.05). High levels of Ca2+ ion release were observed in all groups except AH Plus sealer. MTA-A also had the highest release of Na2+ and K+ ions. Zn+2 ion release was observed only with AH Plus and Sealapex sealers. After the solubility test, all surfaces had morphological changes. The loss of matrix was evident and the filler particles were more distinguishable. EDX analysis displayed high levels of calcium and carbon at the surface of Sealapex, MTA Fillapex and iRoot SP. Conclusions AH Plus and MTA-A were in accordance with ANSI/ADAs requirements regarding solubility whilst iRoot SP, MTA Fillapex and Sealapex did not fulfil ANSI/ADAs protocols. High levels of Ca2+ ion release were observed in all materials except AH Plus. SEM/EDX analysis revealed that all samples had morphological changes in both outer and inner surfaces after the solubility test. High levels of calcium and carbon were also observed at the surface of all materials except AH Plus and MTA-A.
Resumo:
The electronic interactions between the [Cu(opba)]2- anions (where opba is orthophenylenebis (oxamato)) and single-wall carbon nanotubes (SWCNTs) were investigated by resonance Raman spectroscopy. The opba can form molecular magnets, and the interactions of opba with SWCNTs can produce materials with very different magnetic/electronic properties. It is observed that the electronic interaction shows a dependence on the SWCNT diameter independent of whether they are metallic or semiconducting, although the interaction is stronger for metallic tubes. The interaction also is dependent on the amount of complex that is probably adsorbed on the carbon surface of the SWCNTs. Some charge transfer can be also occurring between the metallic complex and the SWCNTs. Copyright (c) 2012 John Wiley & Sons, Ltd.
Resumo:
Aim: To compare the clinical, radiographic and histological responses of the pulp to mineral trioxide aggregate (MTA), calcium hydroxide (CH) and Portland cement (PC) when used as a pulpotomy agent in human primary teeth. Study design: Forty-five mandibular primary molar teeth were randomly assigned to CH, MTA or PC groups and treated by pulpotomy technique. Methods: The teeth were treated by conventional pulpotomy technique, differing only in the capping material for each group. Clinical and radiographic evaluations were recorded at 6-, 12- and 24-month follow-up. Teeth in the regular exfoliation period were further processed for histologic analysis. Statistics: The teeth were treated by conventional pulpotomy technique, differing only in the capping material for each group. Clinical and radiographic evaluations were recorded at 6-, 12- and 24-month follow-up. Teeth in the regular exfoliation period were further processed for histologic analysis. Statistics: Clinically and radiographically, the MTA and PC groups showed 100 % success rates at 6, 12 and 24 months. In CH group, several teeth presented clinical and radiographic failures detected throughout the follow-up period, and internal resorption was a frequent radiographic finding. Histologic analysis revealed the presence of dentine-like mineralised material deposition obliterating the root canal in the PC and MTA groups. CH group presented, in most of the sections, necrotic areas in the root canals. Conclusions: MTA and PC may serve as effective materials for pulpotomies of primary teeth as compared to CH. Although our results are very encouraging, further studies and longer follow-up assessments are needed in order to determine the safe clinical indication of Portland cement.
Resumo:
Root perforation represents an undesirable complication that may lead to an unfavorable prognosis. The aims of this study were to characterize and to compare the presence of calcium oxide (CaO) on the chemical composition of materials used for root perforation therapy: gray and white mineral trioxide aggregate (MTA) and Portland cement (PC), gray MTA+5%CaO and gray MTA+10%CaO. The last two materials were analyzed to evaluate the increase of CaO in the final sample. CaO alone was used as a standard. Eighteen polyethylene tubes with an internal diameter of 3 mm and 3 mm in length were prepared, filled and then transferred to a chamber with 95% relative humidity and a temperature of 37ºC. The chemical compounds (particularly CaO) and the main components were analyzed by energy-dispersive X-ray microanalysis (EDX). EDX revealed the following concentrations of CaO: gray MTA: 59.28%, white MTA: 63.09%; PC: 72.51%; gray MTA+5%CaO: 63.48% and gray MTA+10%CaO: 67.55%. The tested materials presented different concentrations of CaO. Even with an increase of 5 and 10% CaO in gray MTA, the CaO levels found in the MTA samples were lower than those found in PC.
Resumo:
The aim of this paper is to verify the influence of composition variability of recycled aggregates (RA) of construction and demolition wastes (CDW) on the performance of concretes. Performance was evaluated building mathematical models for compressive strength, modulus of elasticity and drying shrinkage. To obtain such models, an experimental program comprising 50 concrete mixtures was carried out. Specimens were casted, tested and results for compressive strength, modulus of elasticity and drying shrinkage were statistically analyzed. Models inputs are CDW composition observed at seven Brazilian cities. Results confirm that using RA from CDW for concrete building is quite feasible, independently of its composition, once compressive strength and modulus of elasticity still reached considerable values. We concluded the variability presented by recycled aggregates of CDW does not compromise their use for concrete building. However, this information must be used with caution, and experimental tests should always be performed to certify concrete properties.
Resumo:
In many countries buildings are responsible for a substantial part of the energy consumption, nd it varies according to their energetic and environmental performances. The potential for major reductions in buildings consumption have bee well documented in Brazil. Opportunities have been identified throughout the life cycle of the buildings, due of projects in diverse locations without the proper adjustments. This article offers a reflection about project processes and how its understanding can be conducted in an integrated way, favoring the use of natural resources and lowering energy consumption. It concludes by indicating that the longest phase in the life cycle of a building is also the phase responsible for its largest energy consumption, not only because of its duration but also for the interaction with the end user. Therefore, in order to harvest the energy cost reduction potential from future buildings designers need a holistic view of the surrounding, end users, materials and methodologies.