20 resultados para INDIUM-OXIDE NANOPARTICLES
Resumo:
In the present work we revisit the size data of CdS microcrystals previously collected in the glassy matrix of Germanium oxide. The CdS clusters analyzed using electron microscopy images have shown a wurtzite structure. The mean average radius, dispersion and volume evaluated from the histograms showed good agreement for t(1/3), t(2/3) and t laws, respectively. We observed that the amount of microcrystals remains constant throughout the heat treatment process, as well as that the radii distribution has a lower limit and increases with heat treatment. The distribution of radii follows a distribution similar to the Lifshitz-Slyozov-Wagner distribution limited in the origin. Discussions led to the conclusion that the growth of CdS is a process that occurs after the fluctuating nucleation and coalescence phases. We then analyze the growth process, assuming that the evaporation is overcome by the precipitation rate, stabilizing all clusters with respect to dissolution back into the matrix. The problem was simplified neglecting anisotropy and the assuming a spherical shape for clusters and particles. The low interface tension was described in terms of an empirical potential barrier in the surface of the cluster. The growth dynamics developed considering that the number of clusters remains constant, and that the minimum size of these clusters grow with time, as the first order approximation showed a good agreement with the flaw. (C) 2012 Elsevier B.V. All rights reserved.
Resumo:
In this work we report studies of the photoluminescence emission in samples based on Si/SiOx films deposited by the Pulsed Electron Beam Ablation (PEBA) technique. The samples were prepared at room temperature using targets with different Si/SiO2 concentrations. The samples were characterized using X-ray Absorption Edge Spectroscopy (XANES) at the Si-K edge, Raman spectroscopy, Photoluminescence (PL) and X-ray Photoelectron Spectroscopy (XPS). The concentration of a-Si and nc-Si in the film was dependent on the silicon concentration in the target. It was also observed that the PL is strongly dependent on the structural amorphous/crystalline arrangement. Crown Copyright (C) 2011 Published by Elsevier B.V. All rights reserved.
Resumo:
The electrochromic behavior of iron complexes derived from tetra-2-pyridyl-1,4-pyrazine (TPPZ) and a hexacyanoferrate species in polyelectrolytic multilayer adsorbed films is described for the first time. This complex macromolecule was deposited onto indium-tin oxide (ITO) substrates via self-assembly, and the morphology of the modified electrodes was studied using atomic force microscopy (AFM), which indicated that the hybrid film containing the polyelectrolyte multilayer and the iron complex was highly homogeneous and was approximately 50 nm thick. The modified electrodes exhibited excellent electrochromic behavior with both intense and persistent coloration as well as a chromatic contrast of approximately 70%. In addition, this system achieved high electrochromic efficiency (over 70 cm(2) C-1 at 630 nm) and a response time that could be measured in milliseconds. The electrode was cycled more than 10(3) times, indicating excellent stability.
Resumo:
We describe the preparation of platinum nanoparticles (PtNPs) using the 3-n-propylpyridinium silsesquioxane chloride (SiPy+Cl-) as a nanoreactor and stabilizer. The formation of PtNPs was monitored by UV-Vis spectroscopy by measuring the decrease in the intensity of the band at 375 nm, which is attributed to the electronic absorption of PtCl62- ions. TEM images of Pt-SiPy+Cl- nanohybrid indicated an average size of 3-40 nm for PtNPs. The Pt-SiPy+Cl- was used as a polycation in the preparation of layer-by-layer films (LbL) on a glass substrate coated with fluorine-doped tin oxide (FTO) alternating with the polyanion poly(vinyl sulfonic acid) (PVS). The films were electrochemically tested in sulfuric acid to confirm the deposition of Pt-SiPy+Cl- onto the LbL films, observing the adsorption and desorption of hydrogen (E-pa = 0.1 V) and by the redox process of formation for PtO with E-pa = 1.3 V and E-pc = 0.65 V. FTIR and Raman spectra confirmed the presence of the PVS and Pt-SiPy+Cl- in the LbL films. A linear increase in the absorbance in the UV-Vis spectra of the Pt-SiPy+Cl- at 258 nm (pi -> pi* transition of the pyridine groups) with a number of Pt-SiPy+Cl-/PVS or PVS/SiPy+Cl- bilayers (R = 0.992) was observed. These LbL films were tested for the determination of dopamine (DA) in the presence of ascorbic acid (AA) with a detection limit (DL) on the order of 2.6 x 10(-6) mol L-1 and a quantification limit (QL) of 8.6 x 10(-6) mol L-1. The films exhibited a good repeatability and reproducibility, providing a potential difference of 550 mV for the oxidation of DA with AA interferent.
Resumo:
Ceria (CeO2) plays a vital role in emerging technologies for environmental and energy-related applications. The catalytic efficiency of ceria nanoparticles depends on its morphology. In this study, CeO2 nanoparticles were synthesized by a microwave-assisted hydrothermal method under different synthesis temperatures. The samples were characterized by X-ray diffraction, transmission electron microscopy, Raman scattering spectroscopy, electron paramagnetic resonance spectroscopy and by the Brunauer-Emmett-Teller method. The X-ray diffraction and Raman scattering results indicated that all the synthesized samples had a pure cubic CeO2 structure. Rietveld analysis and Raman scattering also revealed the presence of structural defects due to an associated reduction in the valence of the Ce4+ ions to Ce3+ ions caused by an increasing molar fraction of oxygen vacancies. The morphology of the samples was controlled by varying the synthesis temperature. The TEM images show that samples synthesized at 80 degrees C consisted of spherical particles of about 5 nm, while those synthesized at 120 degrees C presented a mix of spherical and rod-like nanoparticles and the sample synthesized at 160 degrees C consisted of nanorods with 10 nm average diameter and 70 nm length. The microwave-assisted method proved to be highly efficient for the synthesis of CeO2 nanoparticles with different morphologies.