The combination of nanostenciling with pulsed laser deposition (PLD) provides a flexible, fast approach for patterning the growth of Ge on Si. Within each stencilled site, the morphological evolution of the Ge structures with deposition follows a modified Stranski–Krastanov (SK) growth mode. By systematically varying the PLD parameters (laser repetition rate and number of pulses) on two different substrate orientations (111 and 100), we have observed corresponding changes in growth morphology, strain and elemental composition using scanning electron microscopy, atomic force microscopy and μ-Raman spectroscopy. The growth behaviour is well predicted within a classical SK scheme, although the Si(100) growth exhibits significant relaxation and ripening with increasing coverage. Other novel aspects of the growth include the increased thickness of the wetting layer and the kinetic control of Si/Ge intermixing via the PLD repetition rate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Rupture of vulnerable atheromatous plaque in the carotid and coronary arteries often leads to stroke and heart attack respectively. The role of calcium deposition and its contribution to plaque stability is controversial. This study uses both an idealized and a patient-specific model to evaluate the effect of a calcium deposit on the stress distribution within an atheromatous plaque. Methods: Using a finite-element method, structural analysis was performed on an idealized plaque model and the location of a calcium deposit within it was varied. In addition to the idealized model, in vivo high-resolution MR imaging was performed on 3 patients with carotid atheroma and stress distributions were generated. The individual plaques were chosen as they had calcium at varying locations with respect to the lumen and the fibrous cap. Results: The predicted maximum stress was increased by 47.5% when the calcium deposit was located in the thin fibrous cap in the model when compared with that in a model without a deposit. The result of adding a calcium deposit either to the lipid core or remote from the lumen resulted in almost no increase in maximal stress. Conclusion: Calcification at the thin fibrous cap may result in high stress concentrations, ultimately increasing the risk of plaque rupture. Assessing the location of calcification may, in the future, aid in the risk stratification of patients with carotid stenosis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This project provides a steppingstone to comprehend the mechanisms that govern particulate fouling in metal foam heat exchangers. The method is based on development of an advanced Computational Fluid Dynamics model in addition to performing analytical validation. This novel method allows an engineer to better optimize heat exchanger designs, thereby mitigating fouling, reducing energy consumption caused by fouling, economize capital expenditure on heat exchanger maintenance, and reduce operation downtime. The robust model leads to the establishment of an alternative heat exchanger configuration that has lower pressure drop and particulate deposition propensity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The development of novel organic polymer thin films is essential for the advancement of many emerging fields including organic electronics and biomedical coatings. In this study, the effect of synthesis conditions, namely radio frequency (rf) deposition power, on the material properties of polyterpenol thin films derived from nonsynthetic environmentally friendly monomer was investigated. At lower deposition powers, the polyterpenol films preserved more of the original monomer constituents, such as hydroxy functional groups; however, they were also softer and more hydrophilic compared to polymers fabricated at higher power. Enhanced monomer fragmentation and consequent reduction in the presence of the polar groups in the structure of the high-power samples reduced their optical band gap value from 2.95 eV for 10 W to 2.64 eV for 100 W. Regardless of deposition power, all samples were found to be optically transparent with smooth, defect-free, and homogenous surfaces.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Owing to the structural flexibility, uncomplicated processing and manufacturing capabilities, plasma polymers are the subject of active academic as well as industrial research. Polymer thin films prepared from non-synthetic monomers combine desirable optical and physical properties with biocompatibility and environmental sustainability. However, the ultimate expediency and implementation of such materials will dependent on the stability of these properties under varied environmental conditions. Polyterpenol thin films were manufactured at different deposition powers. Under ambient conditions, the bulk of ageing occurred within first 150h after deposition and was attributed to oxidation and volumetric relaxation. Films observed for further 12 months showed no significant changes in thickness or refractive index. Thermal degradation behaviour indicated thermal stability increased for the films manufactured at higher RF powers. Annealing the films to 405°C resulted in full degradation, with retention between 0.29 and 0.99%, indicating films' potential as sacrificial material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We propose the use of solution-processed molybdenum disulfide (MoS2) flakes as hole transport layer (HTL) for metal-organic perovskite solar cells. MoS2 bulk crystals are exfoliated in 2-propanol and deposited on perovskite layers by spray coating. We fabricated cells with glass/FTO/compact-TiO2/mesoporous-TiO2/CH3NH3PbI3/spiro- OMeTAD/Au structure and cells with the same structure but with MoS2 flakes as HTL instead of spiro-OMeTAD, the most widely used HTL. The electrical characterization of the cells with MoS2 as HTL show promising power conversion efficiency -η- of 3.9% with respect to cells with pristine spiro-OMeTAD (η=3.1%). Endurance test on 800-hour shelf life has shown higher stability for the MoS2–based cells (ΔPCE/PCE=-17%) with respect to the doped spiro-OMeTAD-based one (ΔPCE/PCE =-45%). Further improvements are expected with the optimization of the MoS2 deposition process

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The choice of ethanol (C2H5OH) as carbon source in the Chemical Vapor Deposition (CVD) of graphene on copper foils can be considered as an attractive alternative among the commonly used hydrocarbons, such as methane (CH4) [1]. Ethanol, a safe, low cost and easy handling liquid precursor, offers fast and efficient growth kinetics with the synthesis of fullyformed graphene films in just few seconds [2]. In previous studies of graphene growth from ethanol, various research groups explored temperature ranges lower than 1000 °C, usually reported for methane-assisted CVD. In particular, the 650–850 °C and 900 °C ranges were investigated, respectively for 5 and 30 min growth time [3, 4]. Recently, our group reported the growth of highly-crystalline, few-layer graphene by ethanol-CVD in hydrogen flow (1– 100 sccm) at high temperatures (1000–1070 °C) using growth times typical of CH4-assisted synthesis (10–30 min) [5]. Furthermore, a synthesis time between 20 and 60 s in the same conditions was explored too. In such fast growth we demonstrated that fully-formed graphene films can be grown by exposing copper foils to a low partial pressure of ethanol (up to 2 Pa) in just 20 s [6] and we proposed that the rapid growth is related to an increase of the Cu catalyst efficiency due weak oxidizing nature of ethanol. Thus, the employment of such liquid precursor, in small concentrations, together with a reduced time of growth and very low pressure leads to highly efficient graphene synthesis. By this way, the complete coverage of a copper catalyst surface with high spatial uniformity can be obtained in a considerably lower time than when using methane.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ti3Si(Al)C2 films were electrophoretically deposited at 3 V on indium-tin-oxide (ITO) conductive glass from Ti3Si(Al) C2 aqueous suspension with 1 vol% solid loading at pH 9 in the absence of any dispersant. The surface morphology, cross section microstructure, and preferred orientation of the films were investigated by scanning electron microscopy and X-ray diffraction. The as-deposited Ti3Si(Al)C 2 films exhibited (00l) preferred orientation and the thickness can be controlled by the deposition-drying-deposition method. These results demonstrate that electrophoretic deposition is a simple and feasible method to prepare MAX-phases green films at room temperature.