159 resultados para MULTILAYERED POLYELECTROLYTE FILMS
Resumo:
In this paper, the initial stage of films assembled by energetic C36 fullerenes on diamond (001)–(2 × 1) surface at low-temperature was investigated by molecular dynamics simulation using the Brenner potential. The incident energy was first uniformly distributed within an energy interval 20–50 eV, which was known to be the optimum energy range for chemisorption of single C36 on diamond (001) surface. More than one hundred C36 cages were impacted one after the other onto the diamond surface by randomly selecting their orientation as well as the impact position relative to the surface. The growth of films was found to be in three-dimensional island mode, where the deposited C36 acted as building blocks. The study of film morphology shows that it retains the structure of a free C36 cage, which is consistent with Low Energy Cluster Beam Deposition (LECBD) experiments. The adlayer is composed of many C36-monomers as well as the covalently bonded C36 dimers and trimers which is quite different from that of C20 fullerene-assembled film, where a big polymerlike chain was observed due to the stronger interaction between C20 cages. In addition, the chemisorption probability of C36 fullerenes is decreased with increasing coverage because the interaction between these clusters is weaker than that between the cluster and the surface. When the incident energy is increased to 40–65 eV, the chemisorption probability is found to increased and more dimers and trimers as well as polymerlike-C36 were observed on the deposited films. Furthermore, C36 film also showed high thermal stability even when the temperature was raised to 1500 K.
Resumo:
This paper presents a methodology for determining the vertical hydraulic conductivity (Kv) of an aquitard, in a multilayered leaky system, based on the harmonic analysis of arbitrary water-level fluctuations in aquifers. As a result, Kv of the aquitard is expressed as a function of the phase-shift of water-level signals measured in the two adjacent aquifers. Based on this expression, we propose a robust method to calculate Kv by employing linear regression analysis of logarithm transformed frequencies and phases. The frequencies, where the Kv are calculated, are identified by coherence analysis. The proposed methods are validated by a synthetic case study and are then applied to the Westbourne and Birkhead aquitards, which form part of a five-layered leaky system in the Eromanga Basin, Australia.
Resumo:
One limitation of electrospinning stems from the charge build-up that occurs during processing, preventing further fibre deposition and limiting the scaffold overall thickness and hence their end-use in tissue engineering applications targeting large tissue defect repair. To overcome this, we have developed a technique in which thermally induced phase separation (TIPS) and electrospinning are combined. Thick three-dimensional, multilayered composite scaffolds were produced by simply stacking individual polycaprolactone (PCL) microfibrous electrospun discs into a cylindrical holder that was filled with a 3% poly(lactic-co-glycolic acid) (PLGA) solution in dimethylsulfoxide (a good solvent for PLGA but a poor one for PCL). The construct was quenched in liquid nitrogen and the solvent removed by leaching out in cold water. This technique enables the fabrication of scaffolds composed principally of electrospun membranes that have no limit to their thickness. The mechanical properties of these scaffolds were assessed under both quasi-static and dynamic conditions. The multilayered composite scaffolds had similar compressive properties to 5% PCL scaffolds fabricated solely by the TIPS methodology. However, tensile tests demonstrated that the multilayered construct outperformed a scaffold made purely by TIPS, highlighting the contribution of the electrospun component of the composite scaffold to enhancing the overall mechanical property slate. Cell studies revealed cell infiltration principally from the scaffold edges under static seeding conditions. This fabrication methodology permits the rapid construction of thick, strong scaffolds from a range of biodegradable polymers often used in tissue engineering, and will be particularly useful when large dimension electrospun scaffolds are required.
Resumo:
We present an electrochemical exfoliation method to produce controlled thickness graphene flakes by ultrasound assistance. Bilayer graphene flakes are dominant in the final product by using sonication during the electrochemical exfoliation process, while without sonication the product contains a larger percentage of four-layer graphene flakes. Graphene sheets prepared by using the two procedures are processed into films to measure their respective sheet resistance and optical transmittance. Solid-state electrolyte supercapacitors are made using the two types of graphene films. Our study reveals that films with a higher content of multilayer graphene flakes are more conductive, and their resistance is more easily reduced by thermal annealing, making them suitable as transparent conducting films. The film with higher content of bilayer graphene flakes shows instead higher capacitance when used as electrode in a supercapacitor.
Resumo:
Laser deposition was used to deposit YBaCuO thin films on Yttria-stabilized Zirconia substrates, at substrate holder temperatures of 710-765 °C. We observed a transition from singlecrystalline to polycrystalline growth at a temperature of ∼750 °C. All films were highly c-axis oriented and had critical temperatures between 89.5 and 92 K. In the twinned singlecrystalline films, the lowest measured microwave surface resistance was 0.37 mΩ at 4.2 K and 21.5 GHz, and the highest critical current 5×106 A/cm2 at 77 K. The polycrystalline films had up to a factor of 50 higher surface resistance and a factor of 10 lower critical current. A meander line resonator made of a film on a LaAlO3 substrate, showed a microwave surface resistance of 5μΩ at 4.2 K and 2.5 GHz. © 1991.
Resumo:
High-quality YBa2Cu3O7-δ films grown on (001) single-crystal Y-ZrO2 substrates by pulsed laser deposition have been studied as a function of substrate temperature using transmission electron microscopy. A transition from epitaxial films to c-axis oriented polycrystalline films was observed at 740°C. An intermediate, polycrystalline, BaZrO3 layer was formed from a reaction between the film and the substrate. A dominant orientation relationship of [001] YBCO//[001]int. layer//[001]YSZ and [110] YBCO//[110]int. layer//[100]YSZ was observed. The formation of grain boundaries in the films resulted in an increased microwave surface resistance and a decreased critical-current density. The superconducting transition temperature remained fairly constant at about 90 K.
Resumo:
The early stages of growth of high quality YBa2Cu 3O7-δ (YBCO) films grown on (001) Y-ZrO2 (YSZ) substrates by pulsed laser deposition have been studied using a combination of atomic force microscopy and transmission electron microscopy. A one unit cell thick YBCO layer and relatively large CuO particles formed in the initial stages. Additional YBCO grew on top of the first layer in the form of one or a few unit cell high c-axis oriented islands about 30 nm in diameter. The rounded islands subsequently coalesced into faceted domains. Elongated Y 2BaCuO5 particles nucleated after the first layer of YBCO. A highly textured BaZrO3 layer formed between the YSZ and the YBCO with a cube-on-cube dominant orientation relationship with respect to the YBCO film.
Resumo:
The microstructure of artificial grain boundaries in YBa2Cu3O7-δ (YBCO) thin films grown on [001] tilt YZrO2 (YSZ) bicrystal substrates has been characterized using transmission electron microscopy and atomic force microscopy. Despite a relatively straight morphology of the substrate boundaries, the film boundaries were wavy. The waviness was a result of the combined effects of grooving at the substrate boundaries prior to the film deposition and an island-growth mechanism for YBCO on YSZ substrates. The dihedral angle of the groove walls varied with the misorientation angle and depended on the symmetry of the substrate boundary. The amplitudes of the film boundary waviness compared well with the widths of the grooves. In addition, the grooves induced local bending of the YBCO lattice planes and additional tilt components perpendicular to the c-axis close to the film boundaries. © 1995.
Resumo:
YBCO thin films were fabricated by laser deposition, in situ on MgO substrates, using both O2 and N2O as process gas. Films with Tc above 90 K and jc of 106 A/cm2 at 77 K were grown in oxygen at a substrate temperature of 765 °C. Using N2O, the optimum substrate temperature was 745 °C, giving a Tc of 87 K. At lower temperatures, the films made in N2O had higher Tc (79 K) than the films made in oxygen (66 K). SEM and STM investigations of the film surfaces showed the films to consist of a comparatively smooth background surface and a distribution of larger particles. Both the particle size and the distribution density depended on the substrate temperature.
Resumo:
c-axis-oriented YBa2Cu3O7-x (YBCO) thin films were laser deposited on (001) yttria-stabilized ZrO2 (YSZ) substrates with different surface morphologies. The in-plane orientation of the films on smooth substrates was sensitive to the deposition conditions, often resulting in mixed orientations. However, a strongly dominating [110] YBCO//[110]YSZ orientation was obtained at a deposition temperature of 770°C. Films on substrates with surface steps, induced by depositing a homoepitaxial buffer layer or by thermally annealing the substrate, had a [110]YBCO//[100]YSZ orientation when deposited at the same temperature. It was concluded that the [110]YBCO//[100] YSZ orientation was promoted by a graphoepitaxial mechanism. Films prepared under identical conditions on smooth and stepped substrates grew with extended c axes on the former. It is proposed that the extension can be induced by disorder, invoked by a low oxygen pressure and a low density of adsorption sites. The disorder may be eliminated by either an increase of the oxygen pressure or an increase of the density of adsorption sites in the form of steps. The film microstructure influenced the microwave surface resistance, which was similar for films with one exclusive in-plane orientation and higher for films with mixed orientations. The films on the stepped surfaces had superior superconducting properties; inductive measurements gave a Tc onset of 88 K, a ΔT(90%-10%) c of 0.2 K, and the transport jc was 1.5×106 A/cm2 at 83 K, for films on substrates with homoepitaxial buffer layers.
Resumo:
Y Ba Cu oxide thin films were grown epitaxially on single cryst. yttria-stabilized zirconia substrates by laser deposition. [on SciFinder(R)]
Resumo:
The microstructures of the grain boundaries in epitaxial YBa2Cu3O7-δ thin films grown on [001]-tilt yttria-stabilized ZrO2 bicrystal substrates were characterized by TEM and at. force microscopy. The exact boundary plane geometries of the bicrystal substrates were not transferred to the films which instead had wiggling grain boundaries. [on SciFinder(R)]
Resumo:
Superconducting YBa2Cu3O7 thin films with various thicknesses from 100 Å to 5000 Å were deposited on (100) SrTiO3 substrates with std. BaF2 coevaporation process. The films had crit. temps. of up to 93 K. The best crit. currents were 1 × 106 A/cm2 at 77 K and 3 × 107 A/cm2 at 4.2 K. The crit. current was generally higher for thinner films. Two different etching methods were used to pattern the films for jc measurements: Ar ion etching and EDTA wet etching. The wet etching was found to work well for thicker films (>1000 Å). For the thinner films, the ion etching process was preferred because of the reduced film surface degrdn. [on SciFinder(R)]