Resumo:

Ultrasonic degradation of commercially important polymers, styrene-butadiene (SBR) rubber, acrylonitrile-butadiene (NBR) rubber, styrene-acrylonitrile (SAN), polybutadiene rubber and polystyrene were investigated. The molecular weight distributions were measured using gel permeation chromatography (GPC). A model based on continuous distribution kinetics approach was used to study the time evolution of molecular weight distribution for these polymers during degradation. The effect of solvent properties and ultrasound intensity on the degradation of SBR rubber was investigated using different pure solvents and mixed solvents of varying volatility and different ultrasonic intensities. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

COOH-terminated polybutadiene has been converted into COCl-terminated polybutadiene which was further chemically cross-linked with bisphenol-A and tetrabromobisphenol-A. The flammability characteristics of bisphenol-A and tetrabromobisphenol-A resins have been examined using thermogravimetric, ignition temperature and mass burning rate data. Mass burning rate results support that tetrabromobisphenol-A cross-linked polybutadiene is flame retardant compared to the corresponding non brominated compositions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Measurements have been made of the depolarisation factors \sigma u ,\sigma v ,\sigma h, and the intensity of scattering in the horizontal transverse direction, in the case of solutions of four different samples of chlorinated rubber in carbon tetrachloride. The size, shape and molecular weight of the micelles have been deduced by the application of the light scattering theories of Gans, Vrklajan and Katalinic and Debye. The extent to which the degradation of the rubber molecule occurs on chlorination has also been assessed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

One of the problems associated with outdoor polymeric insulators is tracking and erosion of the weathershed which can directly influence the reliability of the power system. Flame retardants are added to the base material to enhance its tracking and erosion resistance. Hydroxide fillers are regarded as the best flame retardants. This paper deals with studies related to nano - sized magnesium dihydroxide (MDH) and micron-sized Alumina Trihydrate (ATH) fillers as flame retardants in RTV silicone rubber. Tracking and erosion resistance studies were carried out on MDH and ATH silicone rubber composites using an inclined plane tracking and erosion (IPT) resistance tester. The MDH filled (5% by wt) composites performed much better than ATH composites in terms of eroded mass, depth of erosion, width and length of erosion. The eroded mass of MDH composite is 49.8 % that of ATH composite which can be attributed to high surface area and higher thermal stability of MDH nanofillers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

K2Pb[Cu(NO2)6] and [N(CH3)4]2MX4 (M = Mn, Co, Cu or Zn and X = Cl or Br) undergo phase transitions which involve incommensurate phases. The transitions have been investigated by examining the changes in the NO2 and CH3 vibration bands in the i.r. spectra. Splitting and broadening of some of the bands across the incommensurate transitions are discussed in the context of geometrical restrictions in the incommensurate phases. The phase transitions have also been characterized using differential scanning calorimetry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Keeping in view the prospects of biodegradable polymers, a polymer was synthesized by the condensation of carboxy-terminated polybutadiene (CTPB) of Mnsim-5000 with glycerol and tested for its microbial susceptibility. The results of end group estimations and viscosity measurements indicated a quantitative reaction between the two reactants under experimental conditions. The clear-zone method was employed in this investigation to test biodegradability. Two strains of Serratia and three strains of Staphylococcus did show a clear zone surrounding the colony. However, the microbial growth was found to diminish after 4 or 5 days.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Attempts have been made to understand the curing reactions in carboxy-terminated polybutadiene (CTPB), which happens to be the most practical binder in advanced solid composite propellants. The curing of CTPB has been studied for different ratios of curing agents (MAPO and Epoxide) by gel content, molecular weight, crosslink density, and penetration temperature measurements, and the optimum composition of curators for effective curing of CTPB has been determined. Activation energy calculations on the curing of CTPB with 9.5% epoxide and 0.5% MAPO in the temperature range 75100°C gave 14.1 kcal/mol for which a diffusion-controlled or acid-catalyzed epoxide ring opening mechanism has been suggested for the curing process in CTPB.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnS:Cu, Br powder EL phosphors showed 6-line EPR signal at 25°C whose intensity increases with Cu content and on annealing in Zn-vapour. The signal arises from native Mn impurity. The starting material does not show any EPR signal since Mn2+ acts as an affinity potential well for a hole in ZnS, forming Mn3+ - a chemically uncommon situation in sulfides. In doped ZnS, holes are trapped at Cu such that Mn2+ persists. Deterioration of EL brightness is accompanied by the decrease in EPR signal intensity due to field assisted hole transference to Mn2+. Intentional addition of Mn in ZnS:Cu, Br decreases the brightness and shortens life time. Stable phosphors require ZnS with Mn content less than 1014 cmâˆ3.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper describes the experimental and theoretical studies carried out on particulate composites consisting of BaTiO3, graphite, and rubber. It is shown that such composites exhibit a positive voltage coefficient of resistance beyond a certain voltage. A theoretical model developed to explain the observed V-R characteristics and their dependence on parameters of the composite like composition and grain size of the particles is also described. These composites seem to be useful as varistors with positive voltage coefficient of resistance and may find applications as voltage-regulating devices. Journal of Applied Physics is copyrighted by The American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thermal degradation of copolyurethanes based on hydroxyl terminated polybutadiene (HTPB) and poly(12-hydroxy stearic acid-co-TMP) ester polyol (PEP) with varying compositions has been studied by thermo-gravimetric and pyrolysis-GC techniques. The copolyurethanes were found to decompose in multiple stages and the kinetic parameters were found to be dependent on the method of their evaluation. The activation energy for the initial stage of decomposition was found to increase, and for the main stage decreases with the increase in PEP content. The pyrolysis-GC studies on the ammonium perchlorate filled copolyurethanes (solid propellants) showed that the major products during the pyrolysis were C-2, C-3 hydrocarbons and butadiene. The amount of C-2 fraction in the pyrolyslate increased with solid loading, as well as with the HTPB content in the copolyurethanes. A linear relationship apparently exists between the amount of C-2 fraction and the burn rates of the solid propellants. (C) 2000 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report transport and magnetic properties of a different class of highly conducting polyaniline, doped with boron trihalides BX3 (X=F, Cl, and Br). In order to understand the transport mechanism we analyze the temperature dependence of resistivity of a large number of samples, made by pelletizing doped polyaniline powder and by doping films of polyaniline. We find that the charge transport in this class of conducting polyaniline is driven by the charging-energy limited transport of charge carriers, in contrast to the quasi-one-dimensional variable range hopping conduction prevalent in conventional proton-doped polyaniline samples. Magnetic susceptibility provides further insight into the unusually high intrinsic conductivity behavior.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polymeric admixtures to concrete ingredients modify the properties of the processed concrete. Ductility is one such property modification. This investigation deals with the development of a method of incorporating natural rubber latex into concrete ingredients with only marginal effects on the compressive strength of base plain concrete. This retention of the strength has been effected by reducing the water/cement ratio with the aid of a superplasticizer. The quantity of natural rubber latex is expressed as the dry rubber content by percentage of volume of concrete. The compressive and tensile strengths, as well as post peak ductile behaviour have been the basis for comparison with those of unmodified concrete.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In EHV and UHV power transmission lines, corona could occur even on well designed transmission line hardware and insulators especially under wet conditions. Corona if allowed to occur continuously can significantly damage the polymeric insulators used in such lines in the long run. This paper presents the experimental results of corona aging studies conducted on unfilled silicone rubber as well as filled silicone rubber nanocomposites. Corona aging studies were conducted on silicone rubber samples with filler concentrations of 0, 1, 2 and 3 % by wt of nanosilica for 25 h and 50 h. Needle-plane electrode geometry has been used to create the corona on the samples. Different characterization techniques such as Scanning Electron Microscopy, Energy Dispersive X-ray analysis, Hydrophobicity, Fourier Transform Infrared Spectroscopy, and Optical Profilometry have been used to assess the relative performance of the samples with respect to corona aging. Results indicate that at 3 wt %, the performance of the nanocomposite is much better than the unfilled silicon rubber which can be attributed to the modifications in the material caused by the size factor of the filler.