127 resultados para METASTABLE EL2
em Indian Institute of Science - Bangalore - Índia
Resumo:
It is shown that thermally stimulated photocurrent measurements provide a simple and effective method of determining the activation energy of thermal regeneration rate of EL2 from the metastable state to the normal state in undoped semi‐insulating GaAs. The thermal regeneration rate r is found to be 2.5×108 exp(−0.26 eV/kT) s−1.
Resumo:
The photoquenching of EL2 in semi‐insulating gallium arsenide is seen to be a complex process, where at low temperatures the initial slow quenching is followed by a switch to fast quenching. A possible explanation involving lattice strain mediated cooperative structural relaxation arising out of transition to the metastable state is proposed.
Resumo:
Texture evolution in a low cost beta titanium alloy was studied for different modes of rolling and heat treatments. The alloy was cold rolled by unidirectional and multi-step cross rolling. The cold rolled material was either aged directly or recrystallized and then aged. The evolution of texture in alpha and beta phases were studied. The rolling texture of beta phase that is characterized by the gamma fiber is stronger for MSCR than UDR; while the trend is reversed on recrystallization. The mode of rolling affects alpha transformation texture on aging with smaller alpha lath size and stronger alpha texture in UDR than in MSCR. The defect structure in beta phase influences the evolution of a texture on aging. A stronger defect structure in beta phase leads to variant selection with the rolled samples showing fewer variants than the recrystallized samples.
Resumo:
In this paper the results of a detailed investigation on the metastable phase relations in undercooled as well as rapidly solidified Al---Ge alloys containing 2–50 at.% Ge are reported. Data obtained on the structure and morphology of phases enable us to arrive at the phase relations and transformation processes occurring in undercooled and rapidly quenched melts of this system. These results are explained with the help of a metastable phase diagram consisting of a peritectic and eutectic reaction involving metastable phases.
Resumo:
It is conjectured that the hard sphere system has several distinct solid phases, all but one of which are metastable. The bifurcation theory analysis of freezing is extended to the description of the transition between a supercooled liquid and a disordered solid by defining a restricted phase space for the disordered solid. This approach leads to the prediction of a first order transition between a supercooled hard sphere fluid and a disordered metastable hard sphere solid. The results of the calculation are in qualitative agreement with the results of Woodcock's molecular dynamics computer simulations. The Journal of Chemical Physics is copyrighted by The American Institute of Physics.
Resumo:
Pressure dependence of the electrical resistivity of bulk, melt quenched GexTe100−x glasses (15 less-than-or-equals, slant x less-than-or-equals, slant 28) has been studied up to 8GPa pressure. All the glasses exhibit a sharp, discontinuous glass to crystal transition under pressure. The high pressure crystalline phases are identified to have a face centered cubic structure. The value of the cell constant is 0.779nm for 15 less-than-or-equals, slant x less-than-or-equals, slant 17, 0.642nm for x=20 and 0.55lnm for 22 ≤ x ≤ 28 samples respectively. The cell constants of the high pressure crystalline phases suggest the possible existance of a new metastable crystalline compound in the Ge---Te system with F.C.C. structure and cell constant equal to 1.109nm as reported by Moore et al.
Resumo:
We report magnetic trapping of Yb in the excited P-3(2) state. This state, with a lifetime of 15 s, could play an important role in studies ranging from optical clocks and quantum computation to the search for a permanent electric dipole moment. Yb atoms are first cooled and trapped in the ground state in a 399-nm magneto-optic trap. The cold atoms are then pumped into the excited state by driving the S-1(0) -> P-3(1) -> S-3(1) transition. Atoms in the P-3(2) state are magnetically trapped in a spherical quadrupole field with an axial gradient of 110 G/cm. We trap up to 10(6) atoms with a lifetime of 1.5 s.
Resumo:
Attempts are made to measure activities of both components of a binary alloy (A�B) at 650 K using a solid-state galvanic cell incorporating a new composite solid electrolyte. Since the ionic conductivity of the composite solid electrolyte is three orders of magnitude higher than that of pure CaF2, the cell can be operated at lower temperatures. The alloy phase is equilibrated in separate experiments with flourides of each component and fluorine potential is measured. The mixture of the alloy (A�B) and the fluoride of the more reactive component (BF2) is stable, while (A�B) + AF2 mixture is metastable, Factors governing the possible use of metastable equilibria have been elucidated in this study. In the Co�Ni system, where the difference in Gibbs energies of formation of the fluorides is 21.4 kJ/mol, emf of the cell with metastable phases at the electrode is constant for periods ranging from 90 to 160 ks depending on alloy composition. Subsequently, the emf decreases because of the onset of the displacement reaction. In the Ni�Mn system, measurement of the activity of Ni using metastable equilibria is not fully successful at 650 K because of the large driving force for the displacement reaction (208.8 kJ/mol). Critical factors in the application of metastable equilibria are the driving force for displacement reaction and diffusion coefficients in both the alloy and fluoride solid solution.
Resumo:
Pure Y2O3 and Y2O3---ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0–30% ZrO2 and precursors with 0–50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D53). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D53 structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.
Resumo:
Texture evolution in h. c. p. (alpha) phase derived from aging of a differently processed metastable b.c.c. (beta) titanium alloy was investigated. The study was aimed at examining (i) the effect of different b. c. c. cold rolling textures and (ii) the effect of different defect structures on the h. c. p transformation texture. The alloy metastable beta alloy Ti-10V-4.5Fe-1.5Al was rolled at room temperature by unidirectional (UDR) and multi-step cross rolling (MSCR). A piece of the as-rolled materials were subjected to aging in order to derive the h. c. p. (alpha) phase. In the other route, the as-rolled materials were recrystallized and then aged. Textures were measured using X-ray as well as Electron Back Scatter Diffraction. Rolling texture of beta phase, as characterized by the presence of a strong gamma fibre, was found stronger in M S C R compared to UDR, although they were qualitatively similar. The stronger texture of MSCR sample could be attributed to the inhomogeneous deformation taking place in the sample that might contribute to weakening of texture. Upon recrystallization in beta phase field close to beta-transus. the textures qualitatively resembled the corresponding beta deformation textures; however, they got strengthed. The aging of differently beta rolled samples resulted in the product alpha-phase with different textures. The (UDR + Aged) sample had a stronger texture than (MSCR + Aged) sample, which could be due to continuation of defect accumulation in UDR sample, thus providing more potential sites for the nucleation of alpha phase. The trend was reversed in samples recrystallized prior to aging. The (MSCR + Recrystallized + Aged) sample showed stronger texture of alpha phase than the (UDR + Recrystallized + Aged) sample. This could be attributed to extensive defect annihilation in the UDR sample on recrystallization prior to aging. The (MSCR + Aged) sample exhibited more alpha variants when compared to (MSCR + Recrystallized + Aged) sample. This has been attributed to the availability of more potential sites for nucleation of alpha phase in the former. It could be concluded that alpha transformation texture depends mainly on the defect structure of the parent phase.
Resumo:
Pure Y2O3 and Y2O3-ZrO2 solid solutions have been prepared by melt atomization and by pyrolysis of nitrate solutions. Extended solubility is readily achieved in both techniques for the entire composition range investigated: melts with 0-30% ZrO2 and precursors with 0-50% ZrO2. However, solidification of under cooled droplets yields almost exclusively single phase powders with the structure of cubic yttria (D5(3)). In contrast, the pyrolysis route leads to a sequence of metastable microstructures beginning with a nanocrystalline disordered fluorite-based (C1) solid solution. Further heating leads to the evolution of much larger (micron size) flake crystals with a {001} texture, concurrent with partial ordering of the oxygen ions to the sites occupied in the D5(3) structure. The driving force for ordering and the rate of grain growth decrease with increasing ZrO2 addition. Abrupt heating to high temperatures or electron irradiation can induce ordering without substantial grain growth. There is no significant reduction in porosity during the recrystallization, which with the other observations suggests that grain growth is driven by the free energy available for the ordering transformation from fluorite to the yttria structure. This route offers opportunities for single crystal thin film development at relatively low processing temperatures.
Resumo:
In this paper we report the mechanical alloying behaviour of elemental aluminium with diamond cubic elements Ge and Si. A metastable crystalline phase with rhombohedral crystal structure forms in Al-70 Ge-30 and Al-60 Ge-40 alloy compositions. The phase always coexists with elemental constituents and decomposes over a broad temperature range. No such metastable phase could be observed in the Al-Si system. We also report X-ray diffractometry and differential scanning calorimetry results suggestive of amorphization. Finally a comparison was made of the present result with that obtained in rapid solidification.
Resumo:
Wet chemical reaction of hydrated alumina gels, Al2O3.yH(2)O(80
Resumo:
Deintercalation of amines from the layered amine adducts of WO3, MoO3 and W1-xMoxO3 has been employed as a soft chemical route to produce unusual metastable structures of the oxides. After the adducts of WO3, MoO3 and W1-xMoxO3 (x = 0.25, 0.5, 0.75) with amines such as triethylamine (TEA), pyridine, n-butylamine and n-octylamine had been characterized, deintercalation was carried out thermally as well as by acid leaching. Thermal deintercalation yielded novel metastable structures of WO3 and MoO3 that were significantly different from the stable forms, which contain distorted metal-oxygen octahedra. Thus, ReO3-type cubic WO3 was obtained by the thermal deintercalation of WO3 . 0.5 TEA. Acid leaching of the amines gave metastable phases of WO3, MoO3 and W1-xMoxO3, which were different from those obtained thermally. All the metastable phases transformed to the corresponding stable forms at higher temperatures.