284 resultados para FILM FORMATION

em Indian Institute of Science - Bangalore - Índia


Relevância:

60.00% 60.00%

Publicador:

Resumo:

The fabrication of hydrogen bonded polymer self-assembly for drug delivery has been accomplished via layer-by-layer sequential assembly from aqueous solution. In this study, the self-assembly was constructed based on hydrogen bonding between DNA base (adenine and thymine) pairs substituted on the backbone of chitosan and hyaluronic acid. Chitosan was modified with adenine, whereas hyaluronic acid was modified with thymine. Subsequently, these two polymers were sequentially absorbed on flat substrate by taking advantage of interactions of DNA base pairs via hydrogen bonding. Interlayer hydrogen bonding of these two polymers produces stable multilayer film without using any cross-linking agent. Thin film formation on quartz substrate has been monitored with UV-vis spectra and an AFM study. Formation of multilayer hydrogen-bonded thin film has been further confirmed with SEM. Encapsulation and release behavior of the therapeutic drug from the multilayer thin film at different conditions has been illustrated using UV-vis spectra. Cell viability of modified polymers using MTT assay confirmed no cytotoxic effect.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Frictional performance of molybdenum disulfide (MoS2) particles sprayed on a substrate is investigated in a ball-on-disc tribometer. The ability of large (similar to 2 mu m) and small (similar to 50 nm) particles to generate low-friction transfer film is investigated with a view to elucidate the requirement for film formation. Particle migration, particle stability in the contact region, oxidation potential, and particle adhesion to the substrate are explored within a span of operating parametersp; normal load, and sliding velocity. It is found that the larger particles are able to migrate to the contact to raise a homogeneous but nonuniform low-friction transfer film that flows plastically to yield large contact areas, which aid in wear protection. Within the present load and speed range, the inability of small particles to stay in the contact region and undergo basal slip militates against the formation of a low-friction transfer film.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The influence of Li+ ions on the corrosion behaviour of the Al-Li alloy 8090-T851 and of commercially pure aluminium in aqueous solutions at pH 12 was studied by weight loss and electrochemical polarisation methods. The inhibiting role of Li+ was concentration dependent, corrosion rate decreasing lineally with log[Li+] in the concentration range 10(-4)-10(-1) mol L(-1). A change from general to pitting corrosion was evident from scanning election microscopy studies. Polarisation studies revealed that Li+ primarily acts as an anodic inhibitor (passivator). Passive film formation and stability also become more feasible with increasing Li+ concentration. Fitting potential was dependent on the Cl- ion concentration in the solution. Both materials were affected similarly by the presence of Li+ ions, the corrosion rate of the alloy being slightly lower. This is attributed to the lithium in the alloy acting as a source of lithium for passive film formation. (C) 1995 The Institute of Materials.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Condensation of water droplets during rapid evaporation of a polymer solution, under humid conditions, has been known to generate uniformly porous polymer films. Similar porous films are also formed when a solution of the polymer in THF containing small amounts of water, is allowed to evaporate rapidly under air flow; this suggests that water droplets may be formed during the final stages of film formation. In the presence of added surfactants, the interface of water droplets could become lined with the surfactants and consequently the internal walls of the pores generated, upon removal of the water, could become decorated with the hydrophilic head groups of the surfactant molecules. In a series of carefully designed experiments, we have examined the effect of added surfactants, both anionic and cationic, on the formation of porous PMMA films; the films were prepared by evaporating a solution of the polymer in THF containing controlled amounts of aqueous surfactant solutions. We observed that the average size of the pores decreases with increasing surfactant concentration, while it increases with increasing amounts of added water. The size of the pores and their distribution were examined using AFM and IR imaging methods. Although IR imaging possessed inadequate resolution to confirm the presence of surfactants at the pore surface, exchange of the inorganic counterion, such as the sodium-ion of SDS, with suitable ionic organic dyes permitted the unequivocal demonstration of the presence of the surfactants at the interface by the use of confocal fluorescence microscopy.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We report, strong ultraviolet (UV) emission from ZnO nanoparticle thin film obtained by a green synthesis, where the film is formed by the microwave irradiation of the alcohol solution of the precursor. The deposition is carried out in non-aqueous medium without the use of any surfactant, and the film formation is quick (5 min). The film is uniform comprising of mono-disperse nanoparticles having a narrow size distribution (15-22 nm), and that cover over an entire area (625 mm(2)) of the substrate. The growth rate is comparatively high (30-70 nm/min). It is possible to tune the morphology of the films and the UV emission by varying the process parameters. The growth mechanism is discussed precisely and schematic of the growth process is provided.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We incorporate various gold nanoparticles (AuNPs) capped with different ligands in two-dimensional films and three-dimensional aggregates derived from N-stearoyl-L-alanine and N-lauroyl-L-alanine, respectively. The assemblies of N-stearoyl-L-alanine afforded stable films at the air-water interface. More compact assemblies were formed upon incorporation of AuNPs in the air-water interface of N-stearoyl-L-alanine. We then examined the effects of incorporation of various AuNPs functionalized with different capping ligands in three-dimensional assemblies of N-lauroyl-L-alanine, a compound that formed a gel in hydrocarbons. The profound influence of nanoparticle incorporation into physical gels was evident from evaluation of various microscopic and bulk properties. The interaction of AuNPs with the gelator assembly was found to depend critically on the capping ligands protecting the Au surface of the gold nanoparticles. Transmission electron microscopy (TEM) showed a long-range directional assembly of certain AuNPs along the gel fibers. Scanning electron microscopy (SEM) images of the freeze-dried gels and nanocomposites indicate that the morphological transformation in the composite microstructures depends significantly on the capping agent of the nanoparticles. Differential scanning calorimetry (DSC) showed that gel formation from sol occurred at a lower temperature upon incorporation of AuNPs having capping ligands that were able to align and noncovalently interact with the gel fibers. Rheological studies indicate that the gel-nanoparticle composites exhibit significantly greater viscoelasticity compared to the native gel alone when the capping ligands are able to interact through interdigitation into the gelator assembly. Thus, it was possible to define a clear relationship between the materials and the molecular-level properties by means of manipulation of the information inscribed on the NP surface.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We report the in situ optical transmission change in the complete visible region of the electromagnetic spectrum to asses the kinetics of photo induced interdiffusion in Sb/As2S3 nanomultilayered film. The interdiffusion of Sb into As2S3 matrix results in the formation of Sb-As2S3 ternary solid solutions which is explained by the change in optical band gap, absorption coefficients and Tauc parameter (B-1/2) with evolution of time. The wavelength dependence of the time constants provides a better description of photo induced effects. The time evolution of the absorption coefficients and optical band gap are significantly faster in this process. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The increase in optical band gap (photo bleaching) due to light illumination was studied at room temperature as well as at low (4.2 K) temperature for Sb/As2S3 multilayered film of 640 nm thickness by Fourier Transform Infrared Technique. The interdiffusion of Sb into As2S3 matrix results the formation of Sb-As2S3 ternary solid solutions which is explained by the change in optical band gap (E-g), absorption coefficient (alpha), Tauc parameter (B-1/2), Urbach edge (E-e). At the same time, photo darkening phenomena was observed in (As2S3)(0.93)Sb-0.07 film of same thickness both at low and room temperatures. From our X-ray Photoelectron Spectroscopy measurements,we are able to show that some of the As-As, S-S and Sb-Sb bonds are converted into As-S and S-Sb bonds in case of multilayers. We found that the energetically favoured heteropolar bond formation take place by a phonon-assisted mechanism using the lone pair pi electrons of S-2(0). But in case of (As2S3)(0.93)Sb-0.02 film, the homopolar bonds are playing a major role. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Microwave switches operating in the X band were designed and fabricated using amorphous chalcogenide semiconductors of composition GexTeyAsz. Threshold devices were shown to operate as microwave modulators at modulation frequencies of up to 100 MHz. No delay time was observed at the highest frequency although the modulation efficiency decreased above 10 MHz owing to the finite recovery time which was approximately 0.3 × 10−8s. The devices can also be used as variolossers, the insertion loss being 0.5 dB in the OFF state and increasing on switching from 5 dB at 1 mA device current to 18 dB at 100 mA.The behaviour of the threshold switches can be explained in terms of the formation of a conducting filament in the ON state with a constant current density of 2 × 104Acm−2 that is shunted by the device capacitance. The OFF state conductivity σ varies as ωn (0.5 < n < 1) which is characteristic of hopping in localized states. However, there was evidence of a decrease in n or a saturation of the conductivity at high frequencies.As a result of phase separation memory switches require no holding current in the ON state and may be used as novel latching semiconductor phase-shifters.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The electrical switching behavior of amorphous Al23Te77 thin film devices, deposited by flash evaporation, has been studied in co-planar geometry. It is found that these samples exhibit memory type electrical switching. Scanning Electron Microscopic studies show the formation of a crystalline filament in the electrode region which is responsible for switching of the device from high resistance OFF state to low resistance ON state. It is also found that the switching behavior of thin film Al-Te samples is similar to that of bulk samples, with the threshold fields of bulk samples being higher. This has been understood on the basis of higher thermal conductance in bulk, which reduces the Joule heating and temperature rise in the electrode region. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A distinctive characteristic of silver in oxygen incorporation of oxide thin films during pulsed laser ablation has been discovered. Optical emission spectroscopy studies of laser-induced plume of Ag-target indicates the presence of AgO species whose concentration increases with an increase in oxygen partial pressure. The formation of AgO in laser-plume has been found to be very useful for the realization of high temperature superconducting YBa2Cu3O7-delta (YBCO) and giant magnetoresistive La0.7MnO3-delta (LMO) thin films with dramatically superior quality if the target materials contained a small amount of silver. The improvement in the quality of these films is brought about by the supply of atomic oxygen to oxide lattices during their formation. This becomes possible due to the fact that Ag, after it is ablated with other constituent materials in the target, gets moderately oxidized in an oxygen atmosphere and the oxidized species dissociate back into Ag and nascent O at the substrate surface. The nascent oxygen is very highly reactive and is easily assimilated into the lattice of these compounds. (C) 1997 Elsevier Science S.A.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Films with Fe–25 at.% Ge composition are deposited by the process of laser ablation on single crystal NaCl and Cu substrates at room temperature. Both the vapor and liquid droplets generated in this process are quenched on the substrate. The microstructures of the embedded droplets show size as well as composition dependence. The hierarchy of phase evolution from amorphous to body-centered cubic (bcc) to DO3 has been observed as a function of size. Some of the medium-sized droplets also show direct formation of ordered DO19 phase from the starting liquid. The evolution of disordered bcc structure in some of the droplets indicates disorder trapping during liquid to solid transformation. The microstructural evolution is analyzed on the basis of heat transfer mechanisms and continuous growth model in the solidifying droplets.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Lead ruthenate is used as a bifunctional electrocatalyst for both oxygen evolution and reduction and as a conducting component in thick-film resistors. It also has potential applications in supercapacitors and solid oxide fuel cells. However, thermodynamic properties of the compound have not been reported in the literature. The standard Gibbs energy of formation has now been determined in the temperature range from 873 to 1123 K using a solid-state cell incorporating yttria-stabilized zirconia (YSZ) as the electrolyte, a mixture of PbO + Pb2Ru2O6.5 + Ru as the measuring electrode, and Ru + RuO2 as the reference. The design of the measuring electrode is based on a study of phase relations in the ternary system Pb–Ru–O at 1123 K. For the reaction,S0884291400095625_eqnU1 the standard enthalpy of formation and standard entropy at 298.15 K are estimated from the high-temperature measurements. An oxygen potential diagram for the system Pb–Ru–O is composed based on data obtained in this study and auxiliary information from the literature

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We report crack formation in alumina films grown on Si(100), caused by annealing in a controlled oxidizing ambient. The films were grown in a low-pressure CVD reactor, using aluminium acetylacetonate as precursor. High purity argon and nitrous oxide were employed as carrier and oxidizing gas, respectively. The films were characterized by optical microscopy and SEM/EDAX. The proportion and chemical nature of the heteroatoms, namely C and H, incorporated into the films from the precursor, were characterized by XPS, and FTIR. As-deposited films do not exhibit any cracks, while post-deposition annealing results in cracks. Apart from the delamination of the films, annealing in nitrous oxide ambient leads to an unusual crack geometry, which we term the “railway-track”. These twin cracks are very straight and run parallel to each other for as much as several millimeters. Often, two such linear tracks meet at exactly 90°. Between some of these tracks lie bullet-like structures with very sharp tips, oriented in a specific direction. As cracks are generally activated by residual stress, both thermal and intrinsic, the origins of the stresses that generate these linear cracks are discussed. The redistribution of stress, arising from the removal of C and H during annealing, will also be discussed. An attempt has been made to correlate the formation of cracks with the crystal structure of the film.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Bilayer thin films of Te/As(2)S(3) were prepared from Te and As(2)S(3) by thermal technique under high vacuum. Optical constants were calculated by analysing the transmission spectrum in the spectral range 400-1100 nm. The optical band gap decreases with the addition of Te to As(2)S(3). The decrease of optical band gap has been explained on the basis of density of states and the increase in disorder in the system. We have irradiated the as-deposited films using a diode pumped solid state laser of 532 nm wavelength to study photo-diffusion of Te into As(2)S(3). The changes were characterised by Fourier Transform Infrared and X-ray Photoelectron Spectroscopy (XPS). The optical band gap is found to be decreased with the light irradiation which is proposed due to homopolar bond formation. The core level peaks in XPS spectra give information about different bond formation. (C) 2011 Elsevier B.V. All rights reserved.