33 resultados para Die-casting.

em Indian Institute of Science - Bangalore - Índia


Relevância:

100.00% 100.00%

Publicador:

Resumo:

The present work discusses the findings obtained from simulations of semi solid die filling of a steering knuckle, prior to actual component development using in-house developed rheo pressure die casting system. Die filling capability of A356 Al alloy at semi-solid state has been investigated using commercial software Flow-3Dcast to optimise the pouring temperature of semi-solid slurry into the die cavity, while all other variables such as gating design, die preheat temperature and injection velocity are kept constant based on the prior knowledge obtained from trial numerical simulations and experimentation. Efforts have been made to nullify the essence of costly, time consuming experiments towards obtaining high-quality castings out of the findings obtained from numerical simulations. The optimum pouring temperature identified in the present study is 610 A degrees C, which facilitates smoother slurry flow, minimum surface defect concentration, uniform temperature field and solid fraction distribution within the component cavity.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The relationship between the as-cast microstructure and creep behaviour of the heat-resistant MRI230D Mg alloy produced by two different casting technologies is investigated. The alloy in both ingot-casting (IC) and high pressure die-casting (HPDC) conditions consists of alpha-Mg, 06 ((Mg,AI)(2)Ca), Al-Mn and Sn-Mg-Ca rich phases. However, the HPDC alloy resulted in relatively finer grain size and higher volume fraction of finer, denser network of eutectic C36 phase in the as-cast microstructure as compared to that of the IC alloy. The superior creep resistance exhibited by the HPDC alloy at all the stress levels and temperatures employed in the present investigation was attributed to the more effective dispersion strengthening effect caused by the presence of finer and denser network of the C36 phase. The increased amount of the eutectic C36 phase was the only change observed in the microstructures of both alloys following creep tests. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A conventional magnesium alloy, AZ91D, and two creep resistant magnesium alloys, developed for powertrain applications, MRI 153M and MRI 230D, are prepared by high pressure die casting. These alloys are tested for their creep behaviour in the continuous manner, as is the Current practice, and in the interrupted manner, which represents the real life Situation more closely. It is observed that the interrupted creep tests give rise to a primary creep appearing at the beginning of each cycle resulting in a higher average strain rate than that encountered in the continuous creep tests. Further, the shorter the cycle time, higher is the average strain rate in the interrupted creep tests. A higher average strain rate will give rise to a higher strain over the same period. This is attributed to the recovery taking place during the cooling and heating between two cycles. The effect of additional precipitation during interrupted creep tests depends on the nature of the precipitates. The additional precipitation of beta phase during the cooling and heating between two cycles increases the steady state strain rate in the AZ91D and MRI 153M alloys. whereas the additional precipitation of C36 phase during the cooling and heating between two cycles decreases the steady state strain rate in the MRI 230D alloy. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The development work for producing an automobile component by thixocasting using A356.2 alloy was introduced. As the first step, the alloy was electromagnetically stirred and solidified to produce a billet with non-dendritic microstructure. The microstructure depended on several process parameters such as stirring intensity, stirring frequency, cooling rate, and melt initial superheat. Through a series of computational studies and controlled experiments, a set of process parameters were identified to produce the best microstructures. Reheating of a billet with non-dendritic microstructure to a semisolid temperature was the next step for thixo-casting of the components. The reheating process was characterized for various reheating cycles using a vertical-type reheating machine. The induction heating cycle was optimized to obtain a near-uniform temperature distribution in radial as well as axial direction of the billet, and the heating was continued until the liquid fraction reached about 50%. These parameters were determined with the help of a computational fluid dynamics (CFD) model of die filling and solidification of the semisolid alloy. The heated billets were subsequently thixo-cast into automobile components using a real-time controlled die casting machine. The results show that the castings are near net shape, free from porosity, good surface finish and have superior mechanical properties compared to those produced by conventional die casting processes using the same alloy.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Cooling slope (CS) has been used in this study to prepare semi-solid slurry of A356 Al alloy, keeping in view of slurry generation on demand for Rheo-pressure die casting process. Understanding the physics of microstructure evolution during cooling slope slurry formation is important to satisfy the need of semi-sold slurry with desired shape, size and morphology of primary Al phase. Mixture of spherical and rosette shaped primary Al phase has been observed in the samples collected during melt flow through the slope as well as in the cast (mould) samples compared to that of dendritic shape, observed in case of conventionally cast A356 alloy. The liquid melt has been poured into the slope at 650 A degrees C temperature and during flow it falls below the liquidus temperature of the said alloy, which facilitates crystallization of alpha-Al crystals on the cooling slope wall. Crystal separation due to melt flow is found responsible for nearly spherical morphology of the primary Al phase.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report a circuit technique to measure the on-chip delay of an individual logic gate (both inverting and non-inverting) in its unmodified form using digitally reconfigurable ring oscillator (RO). Solving a system of linear equations with different configuration setting of the RO gives delay of an individual gate. Experimental results from a test chip in 65nm process node show the feasibility of measuring the delay of an individual inverter to within 1pS accuracy. Delay measurements of different nominally identical inverters in close physical proximity show variations of up to 26% indicating the large impact of local or within-die variations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The work studies the extent of asymmetric flow in water models of continuous casting molds of two different configurations. In the molds where fluid is discharged through multiple holes at the bottom, the flow pattern in the lower portion depends on the size of the lower two recirculating domains. If they reach the mold bottom, the flow pattern in the lower portion is symmetrical about the central plane; otherwise, it is asymmetrical. On the other hand, in the molds where the fluid is discharged through the entire mold cross section, the flow pattern is always asymmetrical if the aspect ratio is 1:6.25 or more. The fluid jet swirls while emerging through the nozzle. The interaction of the swirling Jets with the wide sidewalls of the mold gives rise to asymmetrical flow inside the mold. In the molds with lower aspect ratios, where the jets do not touch the wide side walls, the flow pattern is symmetrical about the central plane.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A numerical model of the entire casting process starting from the mould filling stage to complete solidification is presented. The model takes into consideration any phase change taking place during the filling process. A volume of fluid method is used for tracking the metal–air interface during filling and an enthalpy based macro-scale solidification model is used for the phase change process. The model is demonstrated for the case of filling and solidification of Pb–15 wt%Sn alloy in a side-cooled two-dimensional rectangular cavity, and the resulting evolution of a mushy region and macrosegregation are studied. The effects of process parameters related to filling, namely degree of melt superheat and filling velocity on macrosegregation in the cavity, are also investigated. Results show significant differences in the progress of the mushy zone and macrosegregation pattern between this analysis and conventional analysis without the filling effect.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In closed-die forging the flash geometry should be such as to ensure that the cavity is completely filled just as the two dies come into contact at the parting plane. If metal is caused to extrude through the flash gap as the dies approach the point of contact — a practice generally resorted to as a means of ensuring complete filling — dies are unnecessarily stressed in a high-stress regime (as the flash is quite thin and possibly cooled by then), which reduces the die life and unnecessarily increases the energy requirement of the operation. It is therefore necessary to carefully determine the dimensions of the flash land and flash thickness — the two parameters, apart from friction at the land, which control the lateral flow. The dimensions should be such that the flow into the longitudinal cavity is controlled throughout the operation, ensuring complete filling just as the dies touch at the parting plane. The design of the flash must be related to the shape and size of the forging cavity as the control of flow has to be exercised throughout the operation: it is possible to do this if the mechanics of how the lateral extrusion into the flash takes place is understood for specific cavity shapes and sizes. The work reported here is part of an ongoing programme investigating flow in closed-die forging. A simple closed shape (no longitudinal flow) which may correspond to the last stages of a real forging operation is analysed using the stress equilibrium approach. Metal from the cavity (flange) flows into the flash by shearing in the cavity in one of the three modes considered here: for a given cavity the mode with the least energy requirement is assumed to be the most realistic. On this basis a map has been developed which, given the depth and width of the cavity as well as the flash thickness, will tell the designer of the most likely mode (of the three modes considered) in which metal in the cavity will shear and then flow into the flash gap. The results of limited set of experiments, reported herein, validate this method of selecting the optimum model of flow into the flash gap.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the design and characterization of a circuit technique to measure the on-chip delay of an individual logic gate (both inverting and noninverting) in its unmodified form. The test circuit comprises of digitally reconfigurable ring oscillator (RO). The gate under test is embedded in each stage of the ring oscillator. A system of linear equations is then formed with different configuration settings of the RO, relating the individual gate delay to the measured period of the RO, whose solution gives the delay of the individual gates. Experimental results from a test chip in 65-nm process node show the feasibility of measuring the delay of an individual inverter to within 1 ps accuracy. Delay measurements of different nominally identicall inverters in close physical proximity show variations of up to 28% indicating the large impact of local variations. As a demonstration of this technique, we have studied delay variation with poly-pitch, length of diffusion (LOD) and different orientations of layout in silicon. The proposed technique is quite suitable for early process characterization, monitoring mature process in manufacturing and correlating model-to-hardware.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Systems of learning automata have been studied by various researchers to evolve useful strategies for decision making under uncertainity. Considered in this paper are a class of hierarchical systems of learning automata where the system gets responses from its environment at each level of the hierarchy. A classification of such sequential learning tasks based on the complexity of the learning problem is presented. It is shown that none of the existing algorithms can perform in the most general type of hierarchical problem. An algorithm for learning the globally optimal path in this general setting is presented, and its convergence is established. This algorithm needs information transfer from the lower levels to the higher levels. Using the methodology of estimator algorithms, this model can be generalized to accommodate other kinds of hierarchical learning tasks.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A hot billet in contact with relatively cold dies undergoes rapid cooling in the forging operation. This may give rise to unfilled cavities, poor surface finish and stalling of the press. A knowledge of billet-die temperatures as a function of time is therefore essential for process design. A computer code using finite difference method is written to estimate such temperature histories and validated by comparing the predicted cooling of an integral die-billet configuration with that obtained experimentally.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Schwefeltetrafluorid läßt sich in reiner Form in einer CCl3F-Lösung durch direkte Fluorierung von elementarem Schwefel bei -78°C in hoher Ausbeute darstellen.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Wear of dies is a serious problem in the forging industry. The materials used for the dies are generally expensive steel alloys and the dies require costly heat treatment and surface finishing operations. Degeneration of the die profile implies rejection of forged components and necessitates resinking or replacement of the die. Measures which reduce wear of the die can therefore aid in the reduction of production costs. The work reported here is the first phase of a study of the causes of die wear in forging production where the batch size is small and the machine employed is a light hammer. This is a problem characteristic of the medium and small scale area of the forging industry where the cost of dies is a significant proportion of the total capital investment. For the same energy input and under unlubricated conditions, die wear has been found to be sensitive to forging temperature; in cold forging the yield strength of the die material is the prime factor governing the degeneration of the die profile, whilst in hot forging the wear resistance of the die material is the main factor which determines the rate of die wear. At an intermediate temperature, such as that characteristic of warm forging, the die wear is found to be less than that in both cold and hot forging. This preliminary study therefore points to the fact that the forging temperature must be taken into account in the selection of die material. Further, the forging industry must take serious note of the warm forging process, as it not only provides good surface finish, as claimed by many authors, but also has an inherent tendency to minimize die wear.