Resumo:
The standard free energies of formation of Zn2Ti04 and ZnTi03 have been determined in the temperature range 930° to i ioo'x from electromotive force measurements on reversible solid oxide galvanic cells;Ag-5at%znll I Pt, + CaO-Zr02 ZnO I II Ag-5at%Zn Y20r Th02 CaO-Zr02 + ,Pt Zn2Ti04+ ZnTi03 and II Ag-5at%Zn CaO-Zr02 + ,Pt ZnTi03+ Ti02 The values may be expressed by the equations,2ZnO (wurtz) + Ti02(rut) -> Zn2Ti04(sp), f:!:.Go = -750-2-46T (±75)cal;ZnO(wurtz) +Ti02(rut) -> ZnTi03(ilmen) ,f:!:.Co = -]600-0·]99T(±50)cal.Combination of the free energy values with the calorimetric heat of formation, and low-temperature and high-temperature heat capacity of Zn2Ti04 reported in literature, suggests a residual entropy of ],9 (±0·6) cal K-1 mol ? for the cubic spinel. Ideal mixing of Zn2+ and Ti4+ ions on the octahedral sites would result in a configurational contribution to the entropy of 2· 75 cal K-1 rnol ".The difference is indicative of short-range ordering of cations on octahedral sites.
Resumo:
The solubility of oxygen in liquid gallium in the temperature range 775 –1125 °C and in liquid gallium-copper alloys at 1100 °C, in equilibrium with β-Ga2O3, has been measured by an isopiestic equilibrium technique. The solubility of oxygen in pure gallium is given by the equation log (at.% O) = −7380/T + 4.264 (±0.03) Using recently measured values for the standard free energy of formation of β-Ga2O3 and assuming that oxygen obeys Sievert's law up to the saturation limit, the standard free energy of solution of oxygen in liquid gallium may be calculated : View the MathML sourceΔ°298 = −52 680 + 6.53T (±200) cal where the standard state for dissolved oxygen is an infinitely dilute solution in which the activity is equal to atomic per cent. The effect of copper on the activity of oxygen dissolved in liquid gallium is found to be in good agreement with that predicted by a recent quasichemical model in which it was assumed that each oxygen is interstitially coordinated to four metal atoms and that the nearest neighbour metal atoms lose approximately half their metallic cohesive energies.
Resumo:
Scanning tunneling microscopy was used to study the surface nanostructure of the epitaxial film Nd2/3Sr1/3MnO3 that shows giant magnetoresistance. The surface morphology of the film consists of a number of overlapping platelets of about 30–35 Å diameter that grow at an angle of 35°–45° to the surface normal. The peak to peak height of the platelets are multiples of the c‐axis lattice parameter of 7.85 Å showing that the growth of the platelets takes place by the layer by layer addition of one formula unit. The mean surface roughness is about 10 Å. In the range of a few microns the film exhibits no defects or dislocations. The film is unstable in ambient atmosphere and tends to get covered by an adsorbate layer. Tip‐surface interactions cause the adsorbate to be dislodged exposing the surface nanostructure. The degradation of the film in real time when imaged in air was recorded. The adsorbates increase the surface roughness of the film.
Resumo:
An optimal composition of La0.67Cd0.33MnO3 was synthesized by ceramic route. The compound crystallized in a rhombohedral structure with lattice parameters a = 5.473(4) Å and α = 60°37′. Resistivity measurement showed an insulator-to-metal transition coupled with a ferromagnetic transition of around 255 K. Epitaxial thin films were fabricated on the LaAlO3 (100) substrate by a pulsed laser deposition technique. The psuedocubic lattice parameter a of the film is 3.873(4) Å. The insulator-to-metal transition of the film was observed at 250 K which is comparable with the bulk value. The film was ferromagnetic below this temperature. Magnetoresistance defined as ΔR/R0 = (RH−R0)/R0 was over −86% near the insulator-to-metal transition temperature of 240 K at 6 T magnetic field and over-30% at relatively low fields of 1 T. No magnetoresistance was observed at low temperatures in the film unlike in the polycrystalline sample, where about a 40% decrease in resistance was observed on applying 6 T magnetic field due to the spin dependent scattering at the grain boundaries.
Resumo:
This letter investigates the influence of a corrugated gate on the transfer characteristics of thin-film transistors. Corrugations that run parallel to the length of the channel from source to drain are patterned on the gate. The author finds that these corrugations result in higher currents as compared to conventional planar-gate transistors.
Resumo:
We have synthesized La0.83Na0.11MnO2.93 by heating La2O3 and MnCO3 in NaCl melt at 900 °C. The exact composition was arrived by analyzing each ion by an independent chemical method. The compound crystallized in a rhombohedral structure and showed an insulator-to-metal transition at 290 K. Epitaxial thin films were fabricated on LaAlO3 (100) using a pulsed laser deposition technique. The film also showed an insulator-to-metal transition at 290 K. Magnetoresistance [ΔR/R0 = (RH−R0)/R0] was −71% near the insulator-to-metal transition temperature of 290 K at 6 T magnetic field.
Resumo:
In this paper we report a systematic study of low-frequency 1/fα resistance fluctuation in a metal film at different stages of electromigration. The resistance fluctuation (noise) measurement was carried out in presence of a dc electromigration stressing current. We observe that in addition to the increase in the spectral power SV(f), the frequency dependence of the spectral power changes as the electromigration process progresses and the exponent α starts to change from 1 to higher value closer to 1.5. We interpret this change in α as arising due to an additional contribution to the spectral power with a 1/f3/2 component, which starts to contribute as the electromigration process progresses. This additional component SV(f) ∼ 1/f3/2 has been suggested to originate from long range diffusion that would accompany any electromigration process. The experimental observation finds support in a model simulation, where we also find that the enhancement of noise during electromigration stressing is accompanied by a change in spectral power frequency dependence.
Resumo:
A highly transparent all ZnO thin film transistor (ZnO-TFT) with a transmittance of above 80% in the visible part of the spectrum, was fabricated by direct current magnetron sputtering, with a bottom gate configuration. The ZnO-TFT with undoped ZnO channel layers deposited on 300 nm Zn0.7Mg0.3O gate dielectric layers attains an on/off ratio of 104 and mobility of 20 cm2/V s. The capacitance-voltage (C−V) characteristics of the ZnO-TFT exhibited a transition from depletion to accumulation with a small hysteresis indicating the presence of oxide traps. The trap density was also computed from the Levinson’s plot. The use of Zn0.7Mg0.3O as a dielectric layer adds additional dimension to its applications. The room temperature processing of the device depicts the possibility of the use of flexible substrates such as polymer substrates. The results provide the realization of transparent electronics for next-generation optoelectronics.
Resumo:
Homogeneous thin films of Sr(0.6)Ca(0.4)TiO(3) (SCT40) and asymmetric multilayer of SrTiO(3) (STO) and CaTiO(3) (CTO) were fabricated on Pt/Ti/SiO(2)/Si substrates by using pulsed laser deposition technique. The electrical behavior of films was observed within a temperature range of 153 K-373 K. A feeble dielectric peak of SCT40 thin film at 273 K is justified as paraelectric to antiferroelectric phase transition. Moreover, the Curie-Weiss temperature, determined from the epsilon'(T) data above the transition temperature is found to be negative. Using Landau theory, the negative Curie-Weiss temperature is interpreted in terms of an antiferroelectric transition. The asymmetric multilayer exhibits a broad dielectric peak at 273 K. and is attributed to interdiffusion at several interfaces of multilayer. The average dielectric constants for homogeneous Sr(0.6)Ca(0.4)TiO(3) films (similar to 650) and asymmetric multilayered films (similar to 350) at room temperature are recognized as a consequence of grain size effect. Small frequency dispersion in the real part of the dielectric constants and relatively low dielectric losses for both cases ensure high quality of the films applicable for next generation integrated devices. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Ga and In co-doped ZnO (GIZO) thin films together with ZnO, In-doped ZnO (IZO), Ga-doped ZnO (GZO), and IZO/GZO multilayer for comparison, were grown on corning glass and boron doped Si substrates by PLD. The photoluminescence spectra of GIZO showed a strong white light emission and the current-voltage characteristics showed relatively lower turn-on voltage and larger forward current. The CIE coordinates for GIZO were observed to be (0.31, 0.33) with a correlated colour temperature of 6650 K, indicating a cool white light, and establishing a possibility of white light emitting diodes. (C) 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Resumo:
Protein nanoparticles (NPs) have found significant applications in drug delivery due to their inherent biocompatibility, which is attributed to their natural origin. In this study, bovine serum abumin (BSA) nanoparticles were introduced in multilayer thin film via layer-by-layer self-assembly for localized delivery of the anticancer drug Doxorubicin (Dox). BSA nanoparticles (similar to 100 nm) show a high negative zeta potential in aqueous medium (-55 mV) and form a stable dispersion in water without agglomeration for a long period. Hence, BSA NPs can be assembled on a substrate via layer-by-layer approach using a positively charged polyelectrolyte (chitosan in acidic medium). The protein nature of these BSA nanoparticles ensures the biocompatibility of the film, whereas the availability of functional groups on this protein allows one to tune the property of the self-assembly to have a pH-dependent drug release profile. The growth of multilayer thin film was monitored by UV-visible spectroscopy, and the films were further characterized by atomic force microscopy (AFM) and field emission scanning electron microscopy (FESEM). The drug release kinetics of these BSA nanoparticles and their self-assembled thin film has been compared at a physiological pH of 7.4 and an acidic pH of 6.4.
Resumo:
We report the synthesis of a novel class of low band gap copolymers based on anacenaphtho[1,2-b]quinoxaline core and oligothiophene derivatives acting as the acceptor and the donor moieties, respectively. The optical properties of the copolymers were characterized by ultraviolet-visible spectroscopy while the electrochemical properties were determined by cyclic voltammetry. The band gap of these polymers was found to be in the range 1.8-2.0 eV as calculated from the optical absorption band edge. X-ray diffraction measurements show weak pi-pi stacking interactions between the polymer chains. The hole mobility of the copolymers was evaluated using field-effect transistor measurements yielding values in the range 10(-5)-10(-3) cm(2)/Vs.
Resumo:
Photoresponse of n-type indium-doped ZnO and a p-type polymer (PEDOT:PSS) heterojunction devices are studied, juxtaposed with the photoluminescence of the In-ZnO samples. In addition to the expected photoresponse in the ultraviolet, the heterojunctions exhibit significant photoresponse to the visible (532 nm). However, neither the doped ZnO nor PEDOT: PSS individually show any photoresponse to visible light. The sub-bandgap photoresponse of the heterojunction originates from visible photon mediated e-h generation between the In-ZnO valence band and localized states lying within the band gap. Though increased doping of In-ZnO has limited effect on the photoluminescence, it significantly diminishes the photoresponse. The study indicates that optimally doped devices are promising for the detection of wavelengths in selected windows in the visible. (C) 2012 American Institute of Physics. http://dx.doi.org/10.1063/1.4704655]