Effect Of Molybdenum And Silicon On The Electrochemical Corrosion Behavior Of Fenib Metallic Glasses
Resumo:
Molybdenum-doped TiO2 organic-inorganic hybrid nanoparticles were synthesized under mild hydrothermal conditions by in situ surface modification using n-butylamine. This was carried out at 150 degrees C at autogeneous pressure over 18 h. n-Butylamine was selected as a surfactant since it produced nanoparticles of the desired size and shape. The products were characterized using powder X-ray diffraction, Fourier transform infrared spectrometry, dynamic light-scattering spectroscopy, UV-Vis spectroscopy and transmission electron microscopy. Chemical oxygen demand was estimated in order to determine the photodegradation efficiency of the molybdenum-doped TiO2 hybrid nanoparticles in the treatment of pharmaceutical effluents. It was found that molybdenum-doped TiO2 hybrid nanoparticles showed higher photocatalytic efficiency than untreated TiO2 nanoparticles.
Resumo:
This paper reports the variations in impedance with frequency of metal‐oxide‐semiconductor (MOS) structures on polycrystalline silicon. The origin of these impedance‐frequency characteristics are qualitatively explained. These characteristics indicate that the MOS structure on polycrystalline silicon can be exploited to realize voltage controlled filters.
Resumo:
A.C. electrical conductivity of potassium perchlorate (KP) has been measured in the temperature range 25�325°C at frequencies ranging from 50�500 Hz using an automated technique. The results are interpreted in terms of a novel mechanism involving Schottky defects in the anion sublattice and Frenkel defects in the cation sublattice. Theconductivity behavior of KP is compared with literature data on similar low-symmetry systems containing polyatomic ions.
Resumo:
Ga1-xMnxSb crystals are grown with different Mn doping concentrations by the horizontal Bridgman method (x = 0 - 0.04). Optical absorption and photoluminescence studies are carried out in the temperature range 3-300 K. Optical absorption studies reveal that the inter-valence band transition from the spin-orbit split-off band to the light/heavy hole bands is dominant over the fundamental valence band to conduction band absorption. In higher doped crystals, the fundamental absorption peak is merged with the inter-valence band transition and could not be resolved. Photoluminescence measurements in heavily doped crystals reveal the band gap narrowing and band filling effects due to the Fermi level shifting into the valence band.
Resumo:
The current density-voltage (J-V) characteristics of poly(3-methylthiophene) devices show a negative differential resistance (NDR) at room temperature with a large peak to valley current ratio (similar to 507). This NDR can be tuned by two orders of magnitude by controlling the carrier density due to the variation of the space-charge region in the device. The temperature and scan rate dependent J-V measurements infer that the NDR is mainly driven by the trapping and de-trapping of carriers. The photo-generation of carriers is observed to reduce the NDR effect.
Resumo:
Excimer laser irradiation at ambient temperature has been employed to produce nanostructured silicon surfaces. Nanoindentation was used to investigate the nanomechanical properties of the deformed surfaces as a function of laser parameters, such as the angle of incidence and number of laser pulses at a fixed laser fluence of 5 J cm(-2). A single-crystal silicon 311] surface was severely damaged by laser irradiation and became nanocrystalline with an enhanced porosity. The resulting laser-treated surface consisted of nanometer-sized particles. The pore size was controlled by adjusting the angle of incidence and the number of laser pulses, and varied from nanometers to microns. The extent of nanocrystallinity was large for the surfaces irradiated at a small angle of incidence and by a high number of pulses, as confirmed by x-ray diffraction and Raman spectroscopy. The angle of incidence had a stronger effect on the structure and nanomechanical properties than the number of laser pulses.
Resumo:
We investigated the rare-earth transition-metal oxide series, Ln(2)CuTiO(6) (Ln = Y, Dy, Ho, Er, and Yb), crystallizing in the hexagonal structure with noncentrosymmetric P6(3)cm space group for possible occurrences of multiferroic properties. Our results show that while these compounds, except Ln = Y, exhibit a low-temperature antiferromagnetic transition due to the ordering of the rare-earth moments, the expected ferroelectric transition is frustrated by the large size difference between Cu and Ti at the B site. Interestingly, this leads these compounds to attain a rare and unique combination of desirable paraelectric properties with high dielectric constants, low losses, and weak temperature and frequency dependencies. First-principles calculations establish these exceptional properties result from a combination of two effects. A significant difference in the MO5 polyhedral sizes for M = Cu and M = Ti suppress the expected cooperative tilt pattern of these polyhedra, required for the ferroelectric transition, leading to relatively large values of the dielectric constant for every compound investigated in this series. Additionally, it is shown that the majority contribution to the dielectric constant arises from intermediate-frequency polar vibrational modes, making it relatively stable against any temperature variation. Changes in the temperature stability of the dielectric constant among different members of this series are shown to arise from changes in relative contributions from soft polar modes.
Resumo:
The effect of magnesium addition and subsequent heat treatment on mild wear of a cast hypoeutectic aluminium-silicon alloy when slid against EN 24 steel is studied. Morphology and chemistry of worn surface and subsurface are studied with a view to identify wear mechanism. Stability of an iron-aluminium mixed surface layer was found to be the key factor controlling wear resistance.
Resumo:
We show that the characteristic Mn2+ d emission color from Mn2+-doped CdS nanocrystals can be tuned over as much as 40 nm, in contrast to what should be expected from such a nearly localized d-d transition. This is achieved surprisingly by a fine-tuning of the host particle diameter from 1.9 to 2.6 nm, thereby changing the overall emission color from red to yellow. Systematic experiments in conjunction with state-of-the-art ab initio calculations with full geometry optimization establish that Mn2+ ions residing at surface/subsurface regions have a distorted tetrahedral coordination resulting in a larger ligand field splitting. Consequently, these near-surface Mn2+ species exhibit a lower Mn2+ d emission energy, compared to those residing at the core of the nanocrystal with an undisturbed tetrahedral coordination. The origin of the tunability of the observed Mn2+ emission is the variation of emission contributions arising from Mn2+ doped at the core, subsurface, and surface of the host. Our findings provide a unique and easy method to identify the location of an emitting Mn2+ ion in the nanocrystal, which would be otherwise very difficult to decipher.
Resumo:
Aluminium-silicon alloy, an important material used for the construction of internal combustion engines, exhibit pressure induced distinct regimes of wear and friction; ultra-mild and mild. In this work the alloy is slid lubricated against a spherical steel pin at contact pressures characteristic of the two test regimes, at a very low sliding velocity. In both cases, the friction is controlled at the initial stages of sliding by the abrasion of the steel pin by the protruding silicon particles of the disc. The generation of nascent steel chips helps to breakdown the additive in the oil by a cationic exchange that yields chemical products of benefits to the tribology. The friction is initially controlled by abrasion, but the chemical products gain increasing importance in controlling friction with sliding time. After long times, depending on contact pressure, the chemical products determine sliding friction exclusively. In this paper, a host of mechanical and spectroscopic techniques are used to identify and characterize mechanical damage and chemical changes. Although the basic dissipation mechanisms are the same in the two regimes, the matrix remains practically unworn in the low-pressure ultra-mild wear regime. In the higher pressure regime at long sliding times a small but finite wear rate prevails. Incipient plasticity in the subsurface controls the mechanism of wear.
Resumo:
A numerical procedure is presented for calculating high-frequency capacitance variation with bias in amorphous (undoped)/crystalline silicon heterojunction. The results of the model calculations using this procedure have been reported, for different p silicon substrates. These have been compared with the corresponding capacitance variations in the other limiting case, in which the heterostructure acts like an MIS structure. The effect of interface states on the capacitance characteristics has also been studied. In the second part, we report the results of 1 MHz capacitance measurements on various amorphous (undoped)/crystalline silicon heterostructures.
Resumo:
Hypo-eutectic Ti-6.5 wt % Si alloy modified by separate additions of misch metal and low surface tension elements (Na, Sr, Se and Bi) has been examined by microscopic study and thermal analysis. Addition of third element led to modification of microstructure with apparently no significant enhancement of tensile ductility, with the exception of bismuth. Bismuth enhanced the ductility of the alloy by a factor of two and elastic-plastic fracture toughness to 9 MPa m–1/2 from a value of almost zero. The improved ductility of bismuth modified alloy is attributed to the reduced interconnectivity of the eutectic suicide, absence of significant suicide precipitation in the eutectic region and increase in the volume fraction of uniformly distributed dendrites. These changes are accompanied by a decrease in the temperature of eutectic solidification.
Resumo:
Pure silicon tetrafluoride can be prepared in 66% yield from silicon tetrachloride by refluxing with lead fluoride in acetonitrile. The gas can be reduced to pure silane by lithium aluminum hydride in diethyl ether.