516 resultados para QUASI-CRYSTALLINE ALLOY


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-contained Non-Equilibrium Molecular Dynamics (NEMD) simulations using Lennard-Jones potentials were performed to identify the origin and mechanisms of atomic scale interfacial behavior between sliding metals. The mixing sequence and velocity profiles were compared via MD simulations for three cases, viz.: sell-mated, similar and hard-softvcrystal pairs. The results showed shear instability, atomic scale mixing, and generation of eddies at the sliding interface. Vorticity at the interface suggests that atomic flow during sliding is similar to fluid flow under Kelvin-Helmholtz instability and this is supported by velocity profiles from the simulations. The initial step-function velocity profile spreads during sliding. However the velocity profile does not change much at later stages of the simulation and it eventually stops spreading. The steady state friction coefficient during simulation was monitored as a function of sliding velocity. Frictional behavior can be explained on the basis of plastic deformation and adiabatic effects. The mixing layer growth kinetics was also investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By choosing appropriate microemulsion systems, hexagonal cobalt (Co) and cobalt-nickel (1:1) alloy nanoparticles have been obtained with cetyltrimethylammonium bromide as a cationic surfactant at 500 degrees C. This method thus stabilizes the hcp cobalt even at sizes (<10 nm) at which normally fcc cobalt is predicted to be stable. On annealing the hcp cobalt nanoparticles in H-2 at 700 degrees C we could transform them to fcc cobalt nanoparticles. Microscopy studies show the formation of spherical nanoparticles of hexagonal and cubic forms of cobalt and Co-Ni (1:1) alloy nanoparticles with the average size of 4, 8 and 20 nm, respectively. Electrochemical studies show that the catalytic property towards oxygen evolution is dependent on the applied voltage. At low voltage (less than 0.65 V) the Co (hexagonal) nanoparticles are superior to the alloy (Co-Ni) nanoparticles while above this voltage the alloy nanoparticles are more efficient catalysts. The nanoparticles of cobalt (hcp and fcc) and alloy (Co-Ni) nanoparticles show ferromagnetism. The saturation magnetization of Co-Ni nanoparticles is reduced compared to the bulk possibly due to surface oxidation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The creep behaviour of a creep-resistant AE42 magnesium alloy reinforced with Saffil short fibres and SiC particulates in various combinations has been investigated in the transverse direction, i.e., the plane containing random fibre orientation was perpendicular to the loading direction, in the temperature range of 175-300 degrees C at the stress levels ranging from 60 to 140 MPa using impression creep test technique. Normal creep behaviour, i.e., strain rate decreasing with strain and then reaching a steady state, is observed at 175 degrees C at all the stresses employed, and up to 80 MPa stress at 240 degrees C. A reverse creep behaviour, i.e., strain rate increasing with strain, then reaching a steady state and then decreasing, is observed above 80 MPa stress at 240 degrees C and at all the stress levels at 300 degrees C. This pattern remains the same for all the composites employed. The reverse creep behaviour is found to be associated with fibre breakage. The apparent stress exponent is found to be very high for all the composites. However, after taking the threshold stress into account, the true stress exponent is found to range between 4 and 7, which suggests viscous glide and dislocation climb being the dominant creep mechanisms. The apparent activation energy Q(C) was not calculated due to insufficient data at any stress level either for normal or reverse creep behaviour. The creep resistance of the hybrid composites is found to be comparable to that of the composite reinforced with 20% Saffil short fibres alone at all the temperatures and stress levels investigated. The creep rate of the composites in the transverse direction is found to be higher than the creep rate in the longitudinal direction reported in a previous paper.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microstructure of a cast Al---Si alloy-graphite particle composite is examined using optical and analytical scanning electron microscopy. Specimens containing different percentages of graphite were machined by orthogonal planning with 25° and 45° rake angle tools at both 6.5 and 13.2 m min−1. The machining forces are reported and the chip-rake-face friction coefficients and shear flow stresses are calculated. It is shown that the reduction in machining forces with increasing graphite content is due mostly to a decrease in the shear flow stress rather than to lower chip-rake-face friction. Both the polished and the machined surfaces of the composite are rougher than those of the simple alloy, apparently owing to the greater porosity, the tearing out of graphite particles, or the opening of cracks at the graphite particles in the wake of the tool.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Vapour species effusing from a magnesia Knudsen cell containing Mg-Zn alloy at 923 K were condensed on a water cooled copper plate. The equilibrium composition of the vapour phase over the alloy was determined from chemical analysis of the condensate. The activity coefficients of both components in the alloy have been derived from the data using a modified Gibbs-Duhem relation. The ratio of saturation vapour pressures of pure Zn and Mg obtained from the analysis of alloy data agree well with values from the literature, providing an internal check on the accuracy of data obtained in this study. Both components of the alloy exhibit negative deviations from Raoult's law. The concentration-concentration structure factor of Bhatia and Thomton at zero wave vector, evaluated from the measurements, indicate the presence of MgZn2 type complex in the liquid state. The associated regular solution model has been used for the thermodynamic description of liquid Mg-Zn alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Surface segregation of Ge is seen in the Cu-5at%Ge alloy with an activation enthalpy equal to 17 kJ/mol. Oxidation of the alloy in the temperature range 400 to 600 K shows the formation of Cu2O and GeO which on further heating in vacuum at 650 K converts to GeO2 with the reduction of Cu2O to Cu.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A study of the transport properties of layered crystalline semiconductors GeS (undoped and doped with Ag, P impurity) under quasihydrostatic pressure using Bridgman anvil system is made for the first time. Pressure-induced effects in undoped crystals reveal initial rise in resistivity followed by two broad peaks at higher pressures. Silver doping induces only minor changes in the behaviour except removing the second peak. Phosphorous impurity is found to have drastic effect on the transport properties. Temperature dependence of the resistivity exhibits two activation energies having opposite pressure coefficients. Results are discussed in the light of intrinsic features of the layered semiconductors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The discovery of a solid exhibiting m 3 5 point group symmetry by Shechtman et. al. (l) in a rapidly solidified Al-14at%Mn alloy has activated intensive studies of a new class of solids, termed as quasicrystals (2). While the original discovery reported the existence of quasicrystals in AI-Mn. AI-Fe and AI-Cr alloys, subsequent work has revealed their existence in Mg-Zn-Al(3,4), Mg-A]-Cu(5), AI-Mn-Si(6) and Ti-Ni-V(7) alloys (Table l).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tensile experiments on a fine-grained single-phase Mg–Zn–Al alloy (AZ31) at 673 K revealed superplastic behavior with an elongation to failure of 475% at 1 × 10−4 s−1 and non-superplastic behavior with an elongation to failure of 160% at 1 × 10−2 s−1; the corresponding strain rate sensitivities under these conditions were 0.5 and 0.2, respectively. Measurements indicated that the grain boundary sliding (GBS) contribution to strain ξ was 30% under non-superplastic conditions; there was also a significant sharpening in texture during such deformation. Under superplastic conditions, ξ was 50% at both low and high elongations of 20% and 120%; the initial texture became more random under such conditions. In non-superplastic conditions, deformation occurred under steady-state conditions without grain growth before significant flow localization whereas, under superplastic conditions, there was grain growth during the early stages of deformation, leading to strain hardening. The grains retained equiaxed shapes under all experimental conditions. Superplastic deformation is attributed to GBS, while non-superplastic deformation is attributed to intragranular dislocation creep with some contribution from GBS. The retention of equiaxed grain shapes during dislocation creep is consistent with a model based on local recovery related to the disturbance of triple junctions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The optimum conditions for producing cast aluminium alloy-mica particle composites, by stirring mica particles (40 to 120 mgrm) in molten aluminium alloys (above their liquidus temperatures), followed by casting in permanent moulds, are described. Addition of magnesium either as pieces along with mica particles on the surface of the melts or as a previously added alloying element was found to be necessary to disperse appreciable quantities (1.5 to 2 wt.%) of mica particles in the melts and retain them as uniform dispersions in castings under the conditions of present investigation. These castings can be remelted and degassed with nitrogen at least once with the retention of about 80% mica particles in the castings. Electron probe micro-analysis of these cast composites showed that magnesium added to the surface of the melt along with mica has a tendency to segregate around the mica particles, apparently improving the dispersability for mica particles in liquid aluminium alloys. The mechanical properties of the aluminium alloy-mica particle composite decrease with an increase in mica content, however, even at 2.2% the composite has a tensile strength of 14.22 kg mm–2 with 1.1% elongation, a compression strength of 42.61 kg mm–2, and an impact strength of 0.30 kgm cm–2. The properties are adequate for certain bearing applications, and the aluminium-mica composite bearings were found to run under boundary lubrication, semi-dry and dry friction conditions whereas the matrix alloy (without mica) bearings seized or showed stick slip under the same conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The tensile stress–strain response and fracture in a hypereutectic Ti–6Al–4V–1.7B (weight percent) alloy were investigated by employing interrupted tensile tests combined with acoustic emission measurements, with the aim to identify the cause for the observed low ductility in this alloy. These tests were complemented with microscopy. The alloy contains TiB whiskers of different length scales, the majority of which include micro-whiskers ( 5–10 μm length) and a few primary-whiskers ( 200–300 μm length). Although the fracture of both types of whiskers occur during deformation, the former leads to a gradual decrease in the secant modulus whereas initiation of the latter leads to a drastic drop in the modulus along with failure of the specimen, limiting the ductility.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Octahedral Co2+ centers have been connected by mu(3)-OH and mu(2)-OH2 units forming [Co-4] clusters which are linked by pyrazine forming a two-dimensional network. The two-dimensional layers are bridged by oxybisbenzoate (OBA) ligands giving rise to a three-dimensional structure. The [Co-4] clusters bond with the pyrazine and the OBA results in a body-centered arrangement of the clusters, which has been observed for the first time. Magnetic studies reveal a noncollinear frustrated spin structure of the bitriangular cluster, resulting in a net magnetic moment of 1.4 mu B per cluster. For T > 32 K, the correlation length of the cluster moments shows a stretched-exponential temperature dependence typical of a Berezinskii-Kosterlitz-Thouless model, which points to a quasi-2D XY behavior. At lower temperature and down to 14 K, the compound behaves as a soft ferromagnet and a slow relaxation is observed, with an energy barrier of ca. 500 K. Then, on further cooling, a hysteretic behavior takes place with a coercive field that reaches 5 Tat 4 K. The slow relaxation is assigned to the creation/annihilation of vortex-antivortex pairs, which are the elementary excitations of a 2D XY spin system.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report molecular dynamics simulations of bilayers using a united atom model with explicit solvent molecules. The bilayer consists of the single tail cationic surfactant behenyl trimethyl ammonium chloride (BTMAC) with stearyl alcohol (SA) as the cosurfactant. We study the gel to liquid crystalline transitions in the bilayer by varying the amount of water at fixed BTMAC to SA ratio as well as by varying the BTMAC to SA ratio at fixed water content. The bilayer is found to exist in the tilted, Lβ′ phase at low temperatures, and for the compositions investigated in this study, the Lβ′ to Lα melting transition occurred in the temperature range 330−338 K. For the highest BTMAC to SA composition (2:3 molar ratio), a diffuse headgroup−water interface is observed at lower temperatures, and an increase in the d-spacing occurs prior to the melting transition. This pretransition swelling is accompanied by a sharpening in the water density variation across the headgroup region of the bilayer. Signatures of this swelling effect which can be observed in the alkane density distributions, area per headgroup, and membrane thickness are attributed to the hydrophobic effect. At a fixed bilayer composition, the transition temperature (>338 K) from the Lβ′ to Lα transition obtained for the high water content bilayer (80 wt %) is similar to that obtained with low water content (54.3 wt %), confirming that the melting transition at these water contents is dominated by chain melting.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The variation in the tensile properties at 77 K and 300 K in warm-rolled (300 K) Cd-1% Ag alloy with deformation has been studied in longitudinal as well as transverse specimens. The low-temperature yield strength increases with warm rolling without much loss in ductility. The strength at 300 K, however, decreases with heavy warm deformation. From microstructural studies and X-ray investigations, it was observed that changes in grain size and texture occur during warm rolling. Both these changes are found to be important in deciding the tensile properties. The longitudinal and transverse strengths at 77 K vary linearly with l-frac12, where l is the average grain diameter, and thus they obey the Hall-Petch relation. The Hall-Petch slope, k, is lower in specimens with favourable lcub1013rcub texture while the intercept σo is higher when the lcub0002rcub texture is less favourable.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new geometrical method for generating aperiodic lattices forn-fold non-crystallographic axes is described. The method is based on the self-similarity principle. It makes use of the principles of gnomons to divide the basic triangle of a regular polygon of 2n sides to appropriate isosceles triangles and to generate a minimum set of rhombi required to fill that polygon. The method is applicable to anyn-fold noncrystallographic axis. It is first shown how these regular polygons can be obtained and how these can be used to generate aperiodic structures. In particular, the application of this method to the cases of five-fold and seven-fold axes is discussed. The present method indicates that the recursion rule used by others earlier is a restricted one and that several aperiodic lattices with five fold symmetry could be generated. It is also shown how a limited array of approximately square cells with large dimensions could be detected in a quasi lattice and these are compared with the unit cell dimensions of MnAl6 suggested by Pauling. In addition, the recursion rule for sub-dividing the three basic rhombi of seven-fold structure was obtained and the aperiodic lattice thus generated is also shown.