83 resultados para Lanthanum manganite (LaMnO3)


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal decomposition of lanthanum biscitrato chromium(III) dihydrate has been studied in static air and dynamic argon atmospheres. The complex decomposes in four steps: dehydration, decomposition of the citrate to an intermediate oxycarbonate, formation of LaCrO4(V) from oxycarbonate, and finally decomposition of LaCrO4(V) to LaCrO3. Formation of LaCrCrO4(V) requires the presence of oxygen The decomposition behaviour of a mechanical mixture of lanthanum citrate hydrate and chromium citrate hydrate was compared with that of the citrato complex. Both the starting material and the intermediates were characterized by X-ray diffraction, IR electronic and ESR spectroscopy, surface area and magnetic susceptibility measurements, as well as by chemical analysis. A scheme is proposed for the decomposition of lanthanum biscitrato chromium(III) dihydrate in air. LaCrO3 can be obtained at temperatures as low as 875 K by isothermal decomposition of the complex.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

La2-xNiO4, La2-xSrxNiO4 and related layered nickelates have been investigated for possible presence of superconductivity. While there is clear onset of diamagnetism around 20 K in many of these nickelates, we do not, however, find any anomaly in the electrical resistivity, magnetoresistance or thermopower around 20 K. High energy spectroscopic studies show Ni to be in the 2+ oxidation state accompanied by a substantial proportion of oxygen holes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report a simple modified polymeric precursor route for the synthesis of highly crystalline and homogenous nanoparticles of lanthanum calcium manganese oxide (LCMO). The LCMO phase formation was studied by thermal analysis, x-ray powder diffraction, and infrared spectroscopy at different stages of heating. These nanocrystallites (average particle size of 30 nm) possess ferromagnetic-paramagnetic transition temperature (T-c) of 300 K, nearly 50 K higher than that of a single crystal. The Rietveld analysis of the powder x-ray diffraction data of the nanopowders reveals significant lattice contraction and reduction in unit cell anisotropy-these structural changes are correlated to the enhancement in T-c.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the rapid solution combustion synthesis and characterization of Ag-substituted LaMnO3 phases at relatively low temperature using oxalyl dihydrazide, as fuel. Structural parameters were refined by the Rietveld method using powder X-ray diffraction data. While the parent LaMnO3 crystallizes in the orthorhombic structure, the Ag-substituted compounds crystallize in the rhombohedral symmetry. On increasing Ag-content, unit cell volume and Mn-O-Mn bond angle decreases. The Fourier transform infra red spectrum shows two absorption bands corresponding to Mn-O stretching vibration (v(s) mode) and Mn-O-Mn deformation vibration (v(b) mode) around 600 cm(-1) and 400 cm(-1) for the compositions x = 0.0, 0.05 and 0.10, respectively. Electrical resistivity measurements reveal that composition-controlled metal to insulator transition, with the maximum metal to insulator being 280 K for the composition La0.75Ag0.25MnO3. Increase in magnetic moment was observed with increase in Ag-content. The maximum magnetic moment of 35 emu/g was observed for the composition La0.80Ag0.20MnO3. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thermal expansion of several compositions of Sr and Mg-doped LaGaO3 including an A-site deficient composition (La0.9Sr0.1)(0.98)(Ga0.8Mg0.2)O-2.821 were measured in the temperature range from 298 to 1273 K. The effect of doping on thermal expansion was studied by varying the composition at one site of the perovskite structure (either A or B), while keeping the composition at the other site invariant. Thermal expansion varied nonlinearly with temperature and exhibited an inflexion between 550 and 620 K, probably related to the change in crystal structure from orthorhombic to rhombohedral. The dependence of average thermal expansion coefficient (alpha (av)) on the dopant concentration on either A or B site of the perovskite structure was found to be linear, when the composition at the other site was kept constant. Mg doping on the B-site had a greater effect on the average thermal expansion coefficient than Sr doping on the A-site. Cation deficiency at the A-site decreases thermal expansion when compositions at both sites are held constant.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new series of substituted perovskites of the type LaCr1−xMxO3−δ, where M=Cu or Mg have been synthesised by the citrate gel process and characterized by means of powder X-ray diffraction, infrared spectroscopy, selected area diffraction and also by electron paramagnetic resonance spectroscopy. The general powder morphology was also observed using scanning electron microscopy. 40 mole percent substitution of Cr3+ by Cu2+ or Mg2+ have shown to result in single phase perovskite structure. Beyond x=0.5, a new phase has been identified in a narrow compositional range. Effect of Cu and Mg substitution on the sinterability of pure LaCrO3 has also been studied. It is possible to get near theoretically dense materials at a temperature as low as 1200°C in air by copper substitution.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaMnO3+? samples with Mn4+ content up to 50% have been prepared by different methods. The structure of LaMnO3+? changes from orthorhombic to cubic (via rhombohedral) with increase in the Mn4+ content. LaMnO3+? samples containing greater than 20% Mn4+ are ferromagnetic and show resistivity maxima at a temperature Tt which is close to the ferromagnetic Curie temperature. The resistivity maximum is due to the occurrence of a metal-insulator transition. In samples heated to the same temperature, the value of Tt increases with % Mn4+. For a given sample, Tt increases with the temperature of heat treatment due to the increase in particle size. The onset of ferromagnetism in LaMnO3+? accompanied by an insulator-metal transition is similar to that found in La1-xCaxMnO3 and La1-xSrxCoO3.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Electron transport and magnetic properties of several compositions of the La1-xSx-zYzMnO3 system have been investigated in order to explore the effect of yttrium substitution on the magnetoresistance and related properties of these manganates. Yttrium substitution lowers the T-c and the insulator-metal transition temperature, while increasing the peak resistivity. A comparison of the properties of La1-xSrx-zYzMnO3 with the corresponding La1-xCax-zYzMnO3 compositions shows that the observed properties can be related to the average size of the A-site cations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Strontium-doped lanthanum chromites, La1−xSrxCrO3, have been synthesised to investigate the effect of strontium doping on the stability and physico-chemical characteristics of the perovskite LaCrO3. Both microscopic and X-ray examinations show that the materials exist as single phase perovskite structure for all compositions up to 50 mole% strontium substitution. The materials have been further characterized by infrared and electron paramagnetic resonance spectra. These materials show a good sinterability even in air at 1773 K. Electrical conductivity of thse perovskites has been measured as a function of temperature. Electrical conductivity has been found to be a maximum at x=0.2. The observed electrical and magnetic properties are consistent with activated polaron transport as the mechanism for electrical conduction in these materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaMnO3 compositions possessing orthorhombic, rhombohedral and cubic structures and containing 12, 24 and 33% Mn4+ respectively have been investigated by X-ray diffraction, electron diffraction and high resolution electron microscopy. The study shows that the defect structure of LaMnO3 is best described in terms of the random distribution of La and Mn vacancies, rather than by anion excess. Density measurements confirm the cation vacancy model involving an equal number of La and Mn vacancies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Anomalous changes in the infrared intensity of the cobalt-oxygen stretching modes in the infrared spectrum of lanthanum cobaltate (LaCoO3) suggest vibronic coupling. This phenomenon has been studied by infrared vibrational spectroscopy both by temperature-induced changes of spin-state occupation and pressure-induced changes of the crystal field splitting 10Dq.