384 resultados para Aluminum-silicon Alloys


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The decomposition of the beta phase in rapidly quenched Ti-2.8 at. pet Co, Ti-5.4 at. pet Ni, Ti-4.5 at. pet, and 5.5 at. pet Cu alloys has been investigated by electron microscopy. During rapid quenching, two competitive phase transformations, namely martensitic and eutectoid transformation, have occurred, and the region of eutectoid transformation is extended due to the high cooling rates involved. The beta phase decomposed into nonlamellar eutectoid product (bainite) having a globular morphology in Ti-2.8 pet Co and Ti-4.5 pet Cu (hypoeutectoid) alloys. In the near-eutectoid Ti-5.5 pet Cu alloy, the decomposition occurred by a lamellar (pearlite) type, whereas in Ti-5.4 pct Ni (hypereutectoid), both morphologies were observed. The interfaces between the proeutectoid alpha and the intermetallic compound in the nonlamellar type as well as between the proeutectoid alpha and the pearlite were often found to be partially coherent. These findings are in agreement with the Lee and Aaronson model proposed recently for the evolution of bainite and pearlite structures during the solid-state transformations of some titanium-eutectoid alloys. The evolution of the Ti2Cu phase during rapid quenching involved the formation of a metastable phase closely related to an ''omega-type'' phase before the equilibrium phase formed. Further, the lamellar intermetallic compound Ti2Cu was found to evolve by a sympathetic nucleation process. Evidence is established for the sympathetic nucleation of the proeutectoid alpha crystals formed during rapid quenching.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We present a comprehensive study of magnetoresistance (MR) of the crystalline pseudobinary ?-phase Fe alloy series FexNi80-xCr20 (50?x?66). This alloy series shows exotic magnetic phases as the composition (x) is varied. It has a critical composition for ferromagnetism at x=xc?59�60. MR was measured in the temperature range 1.7�110 K and up to a field of 7 T. The observed MR was small and the change was ?1%. The temperature dependence of MR was found to contain a positive and a negative contribution. The positive term was found to be ?H2 and it dominates at high field and high temperatures. We explain this as a manifestation of Kohler�s rule. The negative MR was found to have a quadratic dependence on magnetization M. The magnitude of the negative MR reaches a maximum as x?xc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanoparticles of Ag-Pd and Gu-Pd alloys with diameters in the 5-40 nm range have been prepared over the entire range of compositions, by employing the heterogeneous reaction of dry methanol or ethanol with intimate mixtures of AgNO3+PdOx and CuOx+PdOx, respectively. The nanoscale alloys have been characterized by energy-dispersive Xray (EDX) analysis, transmission electron microscopy (TEM) and X-ray diffraction (XRD). All the alloy particles possess the fee structure and can be obtained in bulk quantities.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present work deals with an ultrasonic type of wave propagation characteristics of monolayer graphene on silicon (Si) substrate. An atomistic model of a hybrid lattice involving a hexagonal lattice of graphene and surface atoms of diamond lattice of Si is developed to identify the carbon-silicon bond stiffness. Properties of this hybrid lattice model is then mapped into a nonlocal continuum framework. Equivalent force constant due to Si substrate is obtained by minimizing the total potential energy of the system. For this equilibrium configuration, the nonlocal governing equations are derived to analyze the ultrasonic wave dispersion based on spectral analysis. From the present analysis we show that the silicon substrate affects only the flexural wave mode. The frequency band gap of flexural mode is also significantly affected by this substrate. The results also show that, the silicon substrate adds cushioning effect to the graphene and it makes the graphene more stable. The analysis also show that the frequency bang gap relations of in-plane (longitudinal and lateral) and out-of-plane (flexural) wave modes depends not only on the y-direction wavenumber but also on nonlocal scaling parameter. In the nonlocal analysis, at higher values of the y-directional wavenumber, a decrease in the frequency band gap is observed for all the three fundamental wave modes in the graphene-silicon system. The atoms movement in the graphene due to the wave propagation are also captured for all the tree fundamental wave modes. The results presented in this work are qualitatively different from those obtained based on the local analysis and thus, are important for the development of graphene based nanodevices such as strain sensor, mass and pressure sensors, atomic dust detectors and enhancer of surface image resolution that make use of the ultrasonic wave dispersion properties of graphene. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Plate-shaped products resulting from martensitic, diffusional, and mixed mode transformations in zirconium-base alloys are compared. in the present study. These alloys are particularly suitable for the comparison in view of the fact that the lattice correspondence between the parent beta (bcc) and the product alpha (hcp) or gamma-hydride (fct) phases are remarkably similar for different types of transformations. Crystallographic features such as orientation relations, habit planes, and interface structures associated with these transformations have been compared:, with a view toward examining whether the transformation mechanisms have characteristic imprints on these experimental observables. Martensites exhibiting dislocated lath, internally twinned plate, and self-accommodating three-plate cluster morphologies have been encountered in Zr-2.5Nb alloy. Habit planes corresponding to all these morphologies have been found to be consistent with the predictions based on the invariant plane strain (IFS) criterion. Different morphologies have been found to reflect the manner in which the neighboring martensite variants are assembled. Lattice-invariant shears (LISs) for all these cases have been identified to be either {10 (1) over bar 1}(alpha) ((1) over bar 123)(alpha) slip or twinning on (10 (1) over bar 1)(alpha) planes. Widmanstatten alpha precipitates, forming in a step-quenching treatment, have been shown to have a lath morphology, the alpha/beta interface being decorated with a periodic array of (c + a) dislocations at a spacing of 8 to 10 nm. The line vectors of these dislocations are nearly parallel to the invariant lines. The alpha precipitates, forming in the retained beta phase on aging, exhibit an internally twinned structure with a zigzag habit plane. Average habit planes for the morphologies have been found to lie near the {103}(beta) - {113}(beta) poles, which are close to the specific variant of the {112}(beta) plane, which transforms into a prismatic plane of the type {1 (1) over bar 00}(alpha). The crystallography of the formation of the gamma-hydride phase (fct) from both the alpha and beta phases is seen to match the IFS predictions. While the beta-gamma transformation can be treated approximately as a simple shear on the basal plane involving a change in the stacking sequence, the alpha-gamma transformation call be conceptually broken into a alpha --> beta transformation following the Burgers correspondence and the simple beta-gamma shear process. The active eutectoid decomposition in the Zr-Cu system, beta --> alpha + beta', has been described in terms of cooperative growth of the alpha phase from the beta phase through the Burgers correspondence and of the partially ordered beta' (structurally similar to the equilibrium Zr2Cu phase) through an ordering process. Similarities and differences in crystallographic features of these transformations have been discussed. and the importance of the invariant line vector in deciding the geometry of the corresponding habit planes has been pointed out.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The reactivation kinetics of passivated boron accepters in hydrogenated silicon during zero bias annealing in the temperature range of 65-130 degrees C are reported, For large annealing times and high annealing temperatures, the reactivation process follows second-order kinetics and is rate limited by a thermally activated <(H)over tilde (2)> complex formation process, For short annealing times and low annealing temperatures, the reactivation rate is found to be larger than that due to <(H)over tilde (2)> complex formation alone. We conclude that the faster reactivation is caused by the diffusion of the liberated hydrogen atoms into the bulk as well as <(H)over tilde (2)> complex formation. The effective diffusion coefficient of hydrogen is measured and found to obey the Arrhenius relation with an activation energy (1.41 +/- 0.1) eV. (C) 1997 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The formation of the metallic glass and crystalline phases and related microstructures and the decomposition behavior of rapidly solidified Ti75Ni25 alloys obtained under different processing conditions have been investigated in detail. The competition between glass transition and nucleation of beta-Ti during rapid solidification leads to the possibility of synthesizing the nanocomposites of beta-Ti and glass. Additionally, it is shown that the presence of a small amount of Si also promotes simultaneous nucleation of fine Ti2Ni intermetallic compound. Thermodynamic calculation of the metastable phase diagram indicates the presence of a metastable eutectic reaction between alpha-Ti and Ti2Ni. Evidence of this reaction at lower cooling rates has been presented. On heating, the glass decomposes through this reaction. Finally, on the basis of understanding of the microstructural evolution during decomposition, a new approach has been adopted to synthesize a nanodispersed composite of alpha-Ti in the crystalline Ti2Ni matrix with a narrow size distribution by controlling the devitrification heat treatment of the metallic glass.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The synthesis of nanostructured materials is a critical step in the development elf these novel materials. The basic principles involved in the production of nanocrystals and nanocomposites by rapid solidification are dealt with. An analysis of the various factors influencing the final grain size of the nanocrystals achieved during mechanical alloying has been presented. The devitrification of amorphous phase formed during rapid solidification processing and mechanical alloying provides an alternative and attractive route. Examples of the synthesis of nanostructured materials using these three different routes are drawn from our work on titanium alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An attempt was made to study the deep level impurities and defects introduced into thyristor grade silicon under different processing conditions. DLTS, C-V and I-V measurements were carried out. The ideality factors of the diodes is around 1-7. Activation energy, trap density and minority carrier lifetime were measured.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Properties of cast aluminium matrix composites are greatly influenced by the nature of distribution of reinforcing phase in the matrix and matrix microstructural length scales, such as grain size, dendrite arm spacing, size and morphology of secondary matrix phases, etc. Earlier workers have shown that SIC reinforcements can act as heterogeneous nucleation sites for Si during solidification of Al-Si-SiC composites. The present study aims at a quantitative understanding of the effect of SiC reinforcements on secondary matrix phases, namely eutectic Si, during solidification of A356 Al-SiC composites. Effect of volume fraction of SiC particulate on size and shape of eutectic Si has been studied at different cooling rates. Results indicate that an increase in SiC volume fraction leads to a reduction in the size of eutectic Si and also changes its morphology from needle-like to equiaxed. This is attributed to the heterogeneous nucleation of eutectic Si on SiC particles. However, SiC particles are found to have negligible influence on DAS. Under all the solidification conditions studied in the present investigation, SiC particles are found to be rejected by the growing dendrites. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tracer diffusion coefficients are calculated in different phases in the Mo-Si system from diffusion couple experiments using the data available on thermodynamic parameters. Following, possible atomic diffusion mechanism of the species is discussed based on the crystal structure. Unusual diffusion behaviour is found in the Mo(5)Si(3) and Mo(3)Si phases, which indicate the nature of defects present on different sublattices. Further the growth mechanism of the phases is discussed and morphological evolution during interdiffusion is explained. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanoembedded aluminum alloys with bimetallic dispersoids of Sn and Pb of compositions Sn-82-Pb-18,Pb- Sn-64-Pb-36, and Sn-54-Pb-46 were synthesized by rapid solidification. The two phases, face-centered-cubic Pb and tetragonal Sn solid-solution, coexist in all the particles. The crystallographic relation between the two phases and the matrix depends upon the solidification pathways adopted by the particles. For Al-(Sn-82-Pb-18), we report a new orientation relation given by [011]Al//[010]Sn and (011)Al//(101)Sn. Pb exhibits a cube-on-cube orientation with Al in few particles, while in others no orientation relationship could be observed. In contrast, Pb in Sn-64-Pb-36 and Sn-54-Pb-46 particles always exhibits cube-on-cube orientation with the matrix. Sn does not show any orientation relationship with Al or Pb in these cases. Differential scanning calorimetry studies revealed melting at eutectic temperature for all compositions, although solidification pathways are different. Attempts were made to correlate these with the melting and heterogeneous nucleation. characteristics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Formation of silicon carbide in the Acheson process was studied using a mass transfer model which has been developed in this study. The century old Acheson process is still used for the mass production of silicon carbide. A heat resistance furnace is used in the Acheson process which uses sand and petroleum coke as major raw materials.: It is a highly energy intensive process. No mass transfer model is available for this process. Therefore, a mass transfer model has been developed to study the mass transfer aspects of the process along with heat transfer. The reaction kinetics of silicon carbide formation has been taken from the literature. It has been shown that reaction kinetics has a reasonable influence on the process efficiency. The effect of various parameters on the process such as total gas pressure, presence of silicon carbide in the initial charge, etc. has been studied. A graphical user interface has also been developed for the Acheson process to make the computer code user friendly.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cathodic reduction of oxygen in fuel cells is known to be enhanced on platinum alloys in relation to the platinum metal. The higher performance of the platinum alloys is as a result of the improved oxygen-reduction kinetics on the alloys but there is hardly any increase in the electrode platinum-surface-areas for the platinum alloys as compared to the platinum metal, and thus the higher performance is solely due to the enhanced electrocatalytic activity of the alloys as compared to the platinum metal. The present X-ray photoelectron spectroscopic (XPS) study on carbon-supported Pt, Pt–Co and Pt–Co–Cr electrocatalysts suggests the presence of a relatively lower Pt-oxide content on the alloys. The X-ray powder diffraction patterns for these electrocatalysts show that while the carbon-supported platinum electrocatalyst has a face-centered cubic (fcc) phase, carbon-supported Pt–Co and Pt–Co–Cr electrocatalysts exhibit a face-centered tetragonal (fct) phase. But, Pt electrocatalyst has a lower particle-size and, hence, a higher dispersion. Previous studies have shown higher activities on the Pt-alloys than on Pt, and have attributed it to changes in the electronic and structural characteristics of Pt. These changes can be correlated with the lower oxidation-state of Pt sites, as found in this study.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of Fe content (0.2 to 0.6 pct) on the microstructure and mechanical properties of a cast Al-7Si-0.3Mg (LM 25/356) alloy has been investigated. Further, 1 pct mischmetal (MM) additions (a mixture of rare-earth (RE) elements) were made to these alloys, and their mechanical properties at room and at elevated temperatures (up to 200 degreesC) were evaluated. A structure-property correlation on this alloy was attempted using optical microstructure analysis, fractographs, X-ray diffraction, energy-dispersive analysis of X-rays (EDX), and quantitative metallography by image analysis. An increase in Fe content increased the volume percentage of Fe-bearing intermetallic compounds (beta and pi phases), contributing to the lower yield strength (YS), ultimate tensile strength (UTS), percentage elongation, and higher hardness. An addition of 1 pct MM to the alloys containing 0.2 and 0.6 pct Fe was found to refine the microstructure; modify the eutectic silicon and La, Ce, and Nd present in the MM; form different intermetallic compounds with Al, Si, Fe, and Mg; and improve the mechanical properties of the alloys both at room and elevated temperatures.