343 resultados para Wear mechanism
Resumo:
Aluminium alloy (A356)-SiC composites containing 15 and 25 wt.% silicon carbide particles (average size 43 μm) were tested for sliding wear at different loads using a pin on disc machine. Composites exhibited better wear resistance compared with unreinforced alloy up to a pressure of 26 MPa. Scanning electron microscopy examination of worn surfaces and subsurfaces show that the presence of dispersed SiC particles help in reducing the propensity of material flow at the surface, at the same time leading to the formation of an iron-rich layer on the surface.
Resumo:
In order to depict the mechanism of coalescence in fibrous bed coalescers, a model coalescer was fabricated. Both water/oil and oil/water dispersions were run through this model coalescer to check for coalescence on PTFE and glass surfaces. The equilibrium contact angle and the dynamic contact angle of the dispersed drops were measured on these surfaces in the presence of the continuous phase. Coalescence was monitored using a microscope. Based on these observations a mechanism of coalescence in the model coalescer is proposed. Different modes of coalescence are correlated to the equilibrium contact angle and the dynamic contact angle. Deposition of dirt on the coalescing surface is observed to result in change of wettability, leading to redispersion of the already coalesced dispersed phase into larger droplets.
Resumo:
A novel mechanism is proposed for efficient manipulation of transport forces acting on the droplets during spray pyrolytic deposition of thin films. A ‘‘burst mode’’ technique of spraying is used to adjust the deposition conditions so as to transport the droplets under the new mechanism. Transparent, conducting thin films of undoped tin oxide prepared by this method showed significant improvement in growth rate. The films are found to be of fairly good quality with optical transmission of 82% and sheet resistance of 35 Ω/☒. The films are chemically homogeneous and grow preferentially along 〈200〉 direction.
Resumo:
Spironaphthalenones 1b–g on reaction with hydroxylamine hydrochloride gave the expected pyrrolotropones 2b–g. Furanotropone 6, postulated as an intermediate in the formation of pyrrolotropones, remained unchanged on reaction with hydroxylamine hydrochloride in ethanol. Reaction of unsymmetrical spironaphthalenones 1h–o with NH2OH.HCl gave the rearranged pyrrolotropones 2h–o.
Resumo:
A mechanism involving the intermediacy of nitrene 5, formed from the oxime of spironaphthalenone 1 by acid catalysed dehydration, has been proposed to explain the formation of pyrrolotropones/pyrrolo esters from spironaphthalenones. The initially formed nitrene rearranges to the isopyrrole 6, which either undergoes sigmatropic migration to the pyrrolotropone 2 or adds alcohol to form the pyrrolo ester depending on substitution at 1′ position. The isopyrrole intermediate 6 has been trapped as a Diels-Alder adduct 8.
Resumo:
We demonstrate a robust strategy for obtaining a high dispersion of ultrafine Pt and PtRu nanoparticles on graphene by exploiting the nucleation of a metal precursor phase on graphite oxide surfaces. Our method opens up new possibilities to engineer graphene-based hybrids for applications in multifunctional nanoscale devices.
Resumo:
Failure to repair DNA double-strand breaks (DSBs) can lead to cell death or cancer. Although nonhomologous end joining (NHEJ) has been studied extensively in mammals, little is known about it in primary tissues. Using oligomeric DNA mimicking endogenous DSBs, NHEJ in cell-free extracts of rat tissues were studied. Results show that efficiency of NHEJ is highest in lungs compared to other somatic tissues. DSBs with compatible and blunt ends joined without modifications, while noncompatible ends joined with minimal alterations in lungs and testes. Thymus exhibited elevated joining, followed by brain and spleen, which could be correlated with NHEJ gene expression. However, NHEJ efficiency was poor in terminally differentiated organs like heart, kidney and liver. Strikingly, NHEJ junctions from these tissues also showed extensive deletions and insertions. Hence, for the first time, we show that despite mode of joining being generally comparable, efficiency of NHEJ varies among primary tissues of mammals.
Resumo:
The integrated diffusion coefficient of the phases and the tracer diffusion coefficients of the species are determined in the Nb-Si system by the diffusion couple technique. The diffusion rate of Si is found to be faster than that of Nb in both the NbSi2 and Nb5Si3 phases. The possible atomic mechanism of diffusion is discussed based on the crystal structure and on available details of the defect concentration data. The faster diffusion rate of Si in the Nb5Si3 phase is found to be unusual. The growth mechanism of the phases is also discussed on the basis of the data calculated in this study. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
A compression moulded Kevlar-phenolic resin composite consisting of 30 wt% continuous fibres was slid against a steel disc such that the fibre axis was normal to the sliding plane. The sliding experiments were conducted in a normal pressure range of 0.47–4.27 MPa and at a sliding speed of 0.5 ms–1. The initial sliding interaction is abrasive. With further sliding, as patches of polymer transfer film develop on the polymer pin and counterface, the interaction becomes adhesive and steady-state friction is established. The wear resistance of the polymer was found to be related to the stability of this film.
Resumo:
Polytetrafluoroethylene (PTFE) is an important engineering material. When rubbed or slid against a hard surface, PTFE exhibits a low coefficient of friction but a high rate of wear. These unique properties of the polymer have encouraged many mechanistic and physical examinations of the processes involved in the friction and wear of this polymer. A section of such work carried out over the past 30 years is reviewed here. When rubbed against a hard surface, the PTFE chain undergoes scission, creating active groups which chemically react with the counterface. This results in strong adhesion and a coherent transfer film. Further interaction between the bulk polymer and the transfer film gives rise to anisotropic deformation of the unit cell, which results in closeness of adjacent chains and easy shear between chains. Sliding brings about growth in as well as reorientation of crystallites situated in a very thin subsurface region of the bulk polymer. Such structural rearrangement facilitates the joining of adjacent aligned crystallites to form films and ribbons which emerge as debris.