223 resultados para Modified Al-7wt-percent-si Alloy


Relevância:

40.00% 40.00%

Publicador:

Resumo:

The present work discusses the findings obtained from simulations of semi solid die filling of a steering knuckle, prior to actual component development using in-house developed rheo pressure die casting system. Die filling capability of A356 Al alloy at semi-solid state has been investigated using commercial software Flow-3Dcast to optimise the pouring temperature of semi-solid slurry into the die cavity, while all other variables such as gating design, die preheat temperature and injection velocity are kept constant based on the prior knowledge obtained from trial numerical simulations and experimentation. Efforts have been made to nullify the essence of costly, time consuming experiments towards obtaining high-quality castings out of the findings obtained from numerical simulations. The optimum pouring temperature identified in the present study is 610 A degrees C, which facilitates smoother slurry flow, minimum surface defect concentration, uniform temperature field and solid fraction distribution within the component cavity.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The addition of small amount of boron to Ti and it alloys refines the as-cast microstructure and enhances the mechanical properties. In this paper, we employ nanoindentation on each of the constituent phases in the microstructure and `rule-of-mixture' type analysis to examine their relative contributions to the strength enhancement in a Ti-6Al-4V alloy modified with 0.3 wt% B. Our results indicate to two main contributors to the relatively higher flow strength of B-modified alloy vis-a-vis the base alloy: (a) strengthening of alpha phase due to the reduction in the effective slip length that occurs as a result of the microstructural refinement that occurs upon B addition, and (b) composite strengthening caused by the TiB whiskers present in the alloy. (C) 2015 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Designing and fabricating hybrid systems with a visible light active semiconductor as one of its components is an important research area for the development of highly efficient photocatalysts. Herein, we report visible-light driven photocatalytic activity of graphene oxide (GO) and controllably reduced GO (rGO) modified Ag3PO4 composites fabricated by an in situ method. Concentration of graphene derivatives in GO/rGO-Ag3PO4 composites was in the range of 0.13-0.52 wt% which is very minute compared to those reported previously. The optimal concentration of GO in Ag3PO4 with a kinetics (k = 1.23 +/- 0.04 min(-1)) for the degradation of rhodamine B is 0.26 wt%. GO-Ag3PO4 photocatalysts display an improved catalytic activity compared with pristine and rGOs modified Ag3PO4. In line with this, GO/rGO-Ag3PO4 composites show improved photocatalytic activity for the degradation of 2-chlorophenol compared with Degussa P-25. Our experiments with GO reduced to different extents show that, rGO with more polar functional groups exhibits a higher photocatalytic efficiency. The photocatalytic activity in the presence of different scavengers reveals that holes and O-2(-center dot) reactive species play major roles in the degradation phenomenon. In view of our experimental results and reported theoretical studies, a change in conduction band energy level and variation in the contribution of different charge orbitals (C 2p and O 2p) to the conduction band in the composite favours electron flow from graphene derivatives to the semiconductor, enhancing its photocatalytic response.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

We show that the alloy disorder potential can be a possible cause for the valley splitting observed in the Si/Si1-xGex heterostructures at high magnetic fields and low electron densities.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Nine tie-lines between Fe-Ni alloys and FeTiO3-NiTiO3 solid solutions were determined at 1273 K. Samples were equilibrated in evacuated quartz ampoules for periods up to 10 days. Compositions of the alloy and oxide phases at equilibrium were determined by energy-dispersive x-ray spectroscopy. X-ray powder diffraction was used to confirm the results. Attainment of equilibrium was verified by the conventional tie-line rotation technique and by thermodynamic analysis of the results. The tie-lines are skewed toward the FeTiO3 corner. From the tie-line data and activities in the Fe-Ni alloy phase available in the literature, activities of FeTiO3 and NiTiO3 in the ilmenite solid solution were derived using the modified Gibbs-Duhem technique of Jacob and Jeffes [K.T. Jacob and J.H.E. Jeffes, An Improved Method for Calculating Activities from Distribution Equilibria, High Temp. High Press., 1972, 4, p 177-182]. The components of the oxide solid solution exhibit moderate positive deviations from Raoult's law. Within experimental error, excess Gibbs energy of mixing for the FeTiO3-NiTiO3 solid solution at 1273 K is a symmetric function of composition and can be represented as: Delta G(E) = 8590 (+/- 200) X-FeTiO3 X-NiTiO3 J/mol Full spectrum of tie-lines and oxygen potentials for the three-phase equilibrium involving Fe-Ni alloys, FeTiO3-NiTiO3 solid solutions, and TiO2 at 1273 K were computed using results obtained in this study and data available in the literature.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Al-Li-SiCp composites were fabricated by a simple and cost effective stir casting technique. A compound billet technique has been developed to overcome the problems encountered during hot extrusion of these composites. After successful fabrication hardness measurement and room temperature compressive test were carried out on 8090 Al and its composites reinforced with 8, 12 and 18vol.% SiC particles in as extruded and peak aged conditions. The addition of SiC increases the hardness. 0.2% proof stress and compressive strength of Al-Li-8%SiC and Al-Li-12%SiC composites are higher than the unreinforced alloy. in case of the Al-Li-18%SiC composite, the 0.2% proof stress and compressive strength were higher than the unreinforced alloy but lower than those of Al-Li-8%SiC and Al-Li-12%SiC composites. This is attributed to clustering of particles and poor interfacial bonding.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the present investigation, two nozzle configurations are used for spray deposition, convergent nozzle (nozzle-A), and convergent nozzle with 2 mm parallel portion attached at its end (nozzle-C) without changing the exit area. First, the conditions for subambient aspiration pressure, i.e., pressure at the tip of the melt delivery tube, are established by varying the protrusion length of the melt delivery tube at different applied gas pressures for both of the nozzles. Using these conditions, spray deposits in a reproducible manner are successfully obtained for 7075 Al alloy. The effect of applied gas pressure, flight distance, and nozzle configuration on various characteristics of spray deposition, viz., yield, melt flow rate, and gas-to-metal ratio, is examined. The over-spray powder is also characterized with respect to powder size distribution, shape, and microstructure. Some of the results are explained with the help of numerical analysis presented in an earlier article.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Small additions of B to Titanium alloys refine the as-cast microstructure significantly and hence improve their mechanical performance. In this work, tensile, fracture and fatigue properties of the as-cast and HIPed Ti-6Al-4V alloy with hypoeutectic wt.% of B additions have been examined, with particular emphasis on identifying the microstructural length scale that controls the mechanical properties of these alloys.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The effect of deposition of Al +Al2O3 on MRI 153 M Mg alloy processed using a pulsed Nd:YAG laser is presented in this study. A composite coating with metallurgical joint to the substrate was formed. The microstructure and phase constituents were characterized and correlated with the thermal predictions. The laser scan speed had an effect on the average melt depth and the amount of retained and/or reconstituted alumina in the final coating. The coating consisted of alumina particles and highly refined dendrites formed due to the extremely high cooling rates (of the order of 10(8) K/s). The microhardness of the coating was higher and several fold improvement of wear resistance compared to the substrate was observed for the coatings. These microstructural features and physical properties were correlated with the effects predicted by a thermal model.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Vapour species effusing from a magnesia Knudsen cell containing Mg-Zn alloy at 923 K were condensed on a water cooled copper plate. The equilibrium composition of the vapour phase over the alloy was determined from chemical analysis of the condensate. The activity coefficients of both components in the alloy have been derived from the data using a modified Gibbs-Duhem relation. The ratio of saturation vapour pressures of pure Zn and Mg obtained from the analysis of alloy data agree well with values from the literature, providing an internal check on the accuracy of data obtained in this study. Both components of the alloy exhibit negative deviations from Raoult's law. The concentration-concentration structure factor of Bhatia and Thomton at zero wave vector, evaluated from the measurements, indicate the presence of MgZn2 type complex in the liquid state. The associated regular solution model has been used for the thermodynamic description of liquid Mg-Zn alloys.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Electron spectroscopic studies clearly demonstrate that modification of the surfaces of Mn, Fe and Ni metals by chlorine significantly decreases the strength of interaction between the metal and adsorbed molecules such as CO and N2. This is in contrast to the effect of electropositive additives such as Ba and Al which increase the adsorption bond strength significantly.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The tensile stress–strain response and fracture in a hypereutectic Ti–6Al–4V–1.7B (weight percent) alloy were investigated by employing interrupted tensile tests combined with acoustic emission measurements, with the aim to identify the cause for the observed low ductility in this alloy. These tests were complemented with microscopy. The alloy contains TiB whiskers of different length scales, the majority of which include micro-whiskers ( 5–10 μm length) and a few primary-whiskers ( 200–300 μm length). Although the fracture of both types of whiskers occur during deformation, the former leads to a gradual decrease in the secant modulus whereas initiation of the latter leads to a drastic drop in the modulus along with failure of the specimen, limiting the ductility.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Seizure resistance of several cast aluminium base alloys has been examined using a standard Hohman Wear Tester. Disks of aluminium base alloys were run against a standard aluminium 12% silicon base alloy. The seizure resistance of the alloys (as measured by the lowest bearing parameter reached before seizure) increased with hardness, yield and tensile strength. In Al-Si-Ni alloys where silicon and nickel have little solid solubility in α-aluminium and Si and Ni Al3 hard phases are formed, the minimum bearing parameter decreased with the parameter V (The product of vol. % of hard phases in the disk and the shoe). Apparently the silicon and NiAl3 particles provided discontinuities in the matrix and reduced the probability (1 − V) of the α-aluminium phase in the disk coming into contact with the α-aluminium phase in the shoe. The copper and magnesium containing Al-Si-Ni alloys with lesser volumes of hard phases exhibit considerably better seizure resistance indicating that a slight increase in the solute content or the hardness of the primary α-phase leads to a considerable increase in seizure resistance. Deformation during wear and seizure leads to fragmentation of the original hard particles into considerably smaller particles uniformly dispersed in the deformed α-aluminium matrix.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A direct method of preparing cast aluminium alloy-graphite particle composites using uncoated graphite particles is reported. The method consists of introducing and dispersing uncoated but suitably pretreated graphite particles in aluminium alloy melts, and casting the resulting composite melts in suitable permanent moulds. The optical pretreatment required for the dispersion of the uncoated graphite particles in aluminium alloy melts consists of heating the graphite particles to 400° C in air for 1 h just prior to their dispersion in the melts. The effects of alloying elements such as Si, Cu and Mg on the dispersability of pretreated graphite in molten aluminium have also been reported. It was found that additions of about 0.5% Mg or 5% Si significantly improve the dispersability of graphite particles in aluminium alloy melts as indicated by the high recoveries of graphite in the castings of these composites. It was also possible to disperse upto 3% graphite in LM 13 alloy melts and retain the graphite particles in a well distributed fashion in the castings using the pre-heat-treated graphite particles. The observations in this study have been related to the information presently available on wetting between graphite and molten aluminium in the presence of different elements and our own thermogravimetric analysis studies on graphite particles. Physical and mechanical properties of LM 13-3% graphite composite made using pre-heat-treated graphite powder, were found to be adequate for many applications, including pistons which have been successfully used in internal combustion engines.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Some initial results are presented on the formation of the y phase, based on the intermetallic TiA1 (LIo, c/a = 1.02) from the phase, based on the intermetallic TidAl (DOts , c/a = 0.801) in a Ti-31wt. Al-13wt Mo alloy. The study is part of a programme to evaluate microstractures and properties of alloys containing the y phase in the Ti-Mo-AI ternary system.