This study focuses on the temperature dependent optical band gap changes in the amorphous Ge2Sb2Te5 (GST) films. The behavior of the amorphous GST thin films at low temperatures has been studied. The band gap increment of around 0.2 eV is observed at low temperature (4.2 K) compared to room temperature (300 K). The band gap changes associated with the temperature are completely reversible. The other optical parameters like Urbach energy and Tauc parameter (B-1/2) are studied for different temperatures and discussed. The observed changes in optical band gap (E-g) are fitting to Fan's one phonon approximation. Phonon energy ((h) over bar omega) corresponding to a frequency of 3.59 THz is derived from Fan's approximation, which is close to the reported value of 3.66 THz. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The performance of reinforced earth structures depends on the mobilization of interfacial shearing resistance between soil and reinforcement. This criterion typically eliminates the use of fine-grained soil as a backfill material in reinforced earth structures. Considering the distribution of induced interfacial shear stress in soil around the surface of the reinforcement, it has been shown that only a thin zone of frictional material around the reinforcement is required to mobilize almost full interfacial shearing resistance of sand. Six series of pullout tests have been conducted, with different types of reinforcement, to study the effect of thickness of sand (frictional material) around the reinforcement on the pullout resistance. Sawdust and kaolin clay have been used as bulk backfill material, providing the soil with negligible friction. With low-friction-strength soil as bulk material, a 15-mm thickness of sand around the reinforcement is required to increase the interfacial shearing resistance to that with sand as the bulk material. With this new technique, low-frictional fine-grained soils can be used as bulk backfill material in reinforced earth constructions.
Resumo:
The dielectric response of pulsed laser ablated Bi-1 Zn-5(1) Nb-0(1) O-5(7) (BZN) thin films are investigated within the temperature range of 300-660 K and frequency range of 100 Hz-100 kHz Thin film exhibited a strong dielectric relaxation behavior A sharp rise in dielectric constant of BZN thin film at high temperatures is related to disorder in canon and anion lattices Observed dielectric relaxation implies a redistribution of charges within the unit cell This phenomenon suggests that the large change in dielectric constant is due to a dynamical rise of dipolar fluctuations in the unit cell XPS spectra of BZN (A(2)B(2)O(6)O') cubic pyrochlore confirm that the relaxation corresponds to the ionic hopping among the A and O' positions of several local potential minima Barrier height for hopping is distributed between 0 and 0 94 eV The O is spectrum confirms presence of two types of oxygen in BZN thin film The disorder in charge neutralized thin film is correlated with XPS spectra (C) 2010 Elsevier Ltd All rights reserved
Resumo:
Polystyrene/multiwall carbon nanotube composite films are prepared with loading up to 7 weight percent (wt%) of multiwall carbon nanotubes by solution processing and casting technique. In the formation of these composite films, iron filled carbon nanotubes with high aspect ratio (similar to 4000) were used. Scanning electron microscopy study shows that the nanotubes are uniformly dispersed within the polymer matrix. At high magnification, bending of carbon nanotubes is noticed which can be attributed to their elastic properties. The electrical conductivity measurements show that the percolation threshold is rather low at 0.21 wt%. Hysteresis loop measurements on the bulk multiwall carbon nanotube and composite samples are done at 10, 150 and 300 K and the coercivity values are found to be largest at all the temperatures, for 1 wt% composite sample. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
An optical microscopy study of stress relief patterns in diamondlike carbon films is presented. Interesting stress relief patterns are observed which include the well known sinusoidal type, branching pattern and string of beads pattern. The last one is shown to relieve stresses under marginal conditions. Two new stress relief patterns are noted in the present study. One of them is of a sinusoidal shape with two extra branches at every peak position. The distribution of different stress relief forms from the outer edge of the films towards the interior is markedly dependent on film thickness. Our new patterns support the approach in which the stress relief forms have been analysed earlier using the theory of plate buckling.
Resumo:
This paper discusses the optical properties of single-layer TiO2 films deposited using an activated reactive evaporation process. The combined effects of substrate temperature (in the range 70–200 °C) and discharge currents (0–400 mA) on refractive index, extinction coefficient and packing density of these films are investigated. Significant changes in refractive index values have been observed with increases in substrate temperature and discharge current. The change in refractive index is correlated with the variation in packing density. The variation in extinction coefficient was reduced using the combined effects of substrate temperature and discharge currents. A comparison with films deposited in neutral oxygen has also been made.
Resumo:
Evidence is presented for the strong interaction of oxygen and nitrogen with solid films of buckminsterfullerene based on core-level spectroscopic studies. Cr, Ni and Cu deposited on C60 films interact strongly giving rise to large changes in the C(Is) and C(2p) binding energies as well as the (2p) binding energies of the transition metals.
Resumo:
Formation of crystalline, monophasic indium selenide (InSe) thin solid films by elemental evaporation on hot glass substrates (400 to 530 K) is reported. The compound formation as well as the composition of the formed films are confirmed by X-ray photoelectron spectroscopy (XPS) analysis. The crystallinity of the rhombohedral InSe films can be improved by post-depositional annealing for t < 30 min at 533 K. The InSe thin films become Se-deficient at higher temperatures of deposition or longer duration of annealing. Optical studies reveal the bandgap to be around 1.29 eV. Under optimum conditions of preparations the lowest resistivity of ≈ 12.8 Ω cm is obtained. Durch Verdampfen aus den Elementen auf heiße Glassubstrate (400 bis 530 k) werden dünne, kristalline, einphasige Indiumselenid (InSe)-Festkörperschichten gebildet. Sowohl die Bildung der Verbindung als auch die Zusammensetzung der Schichten werden durch Röntgen-Photoelektronenspektroskopie (XPS) untersucht. Die Kristallinität der rhomboedrischen InSe-Schichten kann durch eine Temperung bei 533 K für t < 30 min nach der Abscheidung verbessert werden. Die dünnen InSe-Schichten zeigen nach Abscheidung bei höheren Temperaturen oder längerer Temperungsdauer einen Se-Unterschuß. Optische Untersuchungen ergeben, daß die Bandlücke bei etwa 1,29 eV liegt. Unter optimalen Präperationsbedingungen wird ein niedrigster Widerstand von ≈ 12.8 Ω cm erreicht.
Resumo:
This paper deals with the reactive sputtering of titanium in an argon and oxygen mixture. The variation in cathode potential as a function of oxygen partial pressure has been explained in terms of cathode poisoning effects. The titania films deposited during this process have been studied for their structural and optical characteristics. The effect of substrate temperature (from 25 to 400 °C) and annealing (from 250 to 700 °C) on the packing density, refractive index, extinction coefficient, and crystallinity has been investigated. The refractive index varied from 2.24 to 2.46 and extinction coefficient from 2.6 × 10-3 to 10.4× 10-3 at 500 nm as the substrate temperature increased from 25 to 400 °C. The refractive index increased from 2.19 to 2.35 and extinction coefficient changed from 3.2× 10-3 to 11.6 × 10-3 at 500 nm as the annealing temperature was increased from 250 to 700 °C. Anatase and rutile phases have been observed in the films deposited at 400 °C substrate temperature and annealed at 300 °C. The changes in the optical constants at higher substrate temperature have been attributed to an increase in packing density, oxygen content, and crystallinity of the films.
Resumo:
We have studied the hydrodynamics of freely suspended membranes, liquid as well as crystalline, with surface tension. We find that nonlinear coupling to thermally excited undulations gives a singular contribution to the kinetic coefficients of these systems at low frequency and wavenumber. Our results differ in some important respects from those of Katz and Lebedev on this problem, and can be tested in mechanical impedance as well as time-correlation studies.
Resumo:
Studies of ZrO2 films prepared by d.c. reactive magnetron sputtering are described. The effects of substrate temperature on the packing density, refractive index, extinction coefficient and crystallinity phase have been investigated in the temperature range 25–450 °C. The refractive index varied from 1.84 to 1.95 and extinction coefficient from 2 × 10−3 to 9.6 × 10−3. This was explained on the basis of an increase in packing density from 0.686 to 0.813. The change in packing density has been attributed to a decrease in the oxygen condensation at higher temperatures. Annealing results in a decrease in refractive index and increase in extinction coefficient. The films deposited at 150 °C showed a monoclinic phase which transforms to a tetragonal phase at higher substrate temperatures.
Resumo:
The effect of substrate and annealing temperatures on mechanical properties of Ti-rich NiTi films deposited on Si (100) substrates by DC magnetron sputtering was studied by nanoindentation. NiTi films were deposited at two substrate temperatures viz. 300 and 400 degrees C. NiTi films deposited at 300 degrees C were annealed for 4 h at four different temperatures, i.e. 300, 400, 500 and 600 degrees C whereas films deposited at 400 degrees C were annealed for 4 h at three different temperatures, i.e. 400, 500 and 600 degrees C. The elastic modulus and hardness of the films were found to be the same in the as-deposited as well as annealed conditions for both substrate temperatures. For a given substrate temperature, the hardness and elastic modulus were found to remain unchanged as long as the films were amorphous. However, both elastic modulus and hardness showed an increase with increasing annealing temperature as the films become crystalline. The results were explained on the basis of the change in microstructure of the film with change in annealing temperature.
Resumo:
Fine-particle rare-earth-metal zirconates, Ln2Zr2O7, where Ln = La, Ce, Pr, Nd, Sm, Gd and Dy having the pyrochlore structure have been prepared using a novel combustion process. The process employs aqueous solutions of the corresponding rare-earth-metal nitrate, zirconium nitrate and carbohydrazide/urea in the required molar ratio. When the solution is rapidly heated to 350–500 °C it boils, foams and burns autocatalytically to yield voluminous oxides. The formation of single-phase Ln2Zr2O7 has been confirmed by powder X-ray diffraction, infrared and fluorescence spectroscopy. The solid combustion products are fine, having surface areas in the range 6–20 m2 g–1. The cold-pressed Pr2Zr2O7 compact when sintered at 1500 °C, 4 h in air, achieved 99% theoretical density.