10 resultados para thermal electric cooler (TEC) controller
em Chinese Academy of Sciences Institutional Repositories Grid Portal
Resumo:
In this letter, the power spectrum of a cooled distributed feedback laser module is measured using the self-heterodyne technique. Periodical oscillation peaks have been observed in the measurement. Further investigation shows that the additional modulation signal is coupled from the thermal electric cooler (TEC) controller to the laser driver, and then applied to the laser diode. The additional modulation can be eliminated by properly isolating the laser driving source from the TEC controller.
Resumo:
The thermal expansion coefficient (TEC) of an ideal crystal is derived by using a method of Boltzmann statistics. The Morse potential energy function is adopted to show the dependence of the TEC on the temperature. By taking the effects of the surface relaxation and the surface energy into consideration, the dimensionless TEC of a nanofilm is derived. It is shown that with decreasing thickness, the TEC can increase or decrease, depending on the surface relaxation of the nanofilm.
Resumo:
Lanthanum-zirconium-cerium composite oxide (La-2(Zr0.7Ce0.3)(2)O-7, LZ7C3) as a candidate material for thermal barrier coatings (TBCs) was prepared by electron beam-physical vapor deposition (EB-PVD). The composition, crystal structure, thermophysical properties, surface and cross-sectional morphologies and cyclic oxidation behavior of the LZ7C3 coating were studied. The results indicated that LZ7C3 has a high phase stability between 298 K and 1573 K, and its linear thermal expansion coefficient (TEC) is similar to that of zirconia containing 8 wt% yttria (8YSZ). The thermal conductivity of LZ7C3 is 0.87 W m(-1) K-1 at 1273 K, which is almost 60% lower than that of 8YSZ. The deviation of coating composition from the ingot can be overcome by the addition of excess CeO2 and ZrO2 during ingot preparation or by adjusting the process parameters.
Resumo:
Neodymium-cerium oxide (Nd2Ce2O7) was proposed as a new thermal barrier coating material in this work. Monolithic Nd2Ce2O7 powder was prepared by the solid-state reaction at 1400 degrees C. The phase composition, thermal stability and thermophysical properties of Nd2Ce2O7 were investigated. Nd2Ce2O7 with fluorite structure was thermally stable in the temperature range of interest for TBC applications. The results indicated that the thermal expansion coefficient (TEC) of Nd2Ce2O7 was higher than that of YSZ (6-8 Wt-% Y2O3 + ZrO2) and even more interesting was the TEC change as a function of temperature paralleling that of the superalloy bond coat. Moreover, the thermal conductivity of Nd2Ce2O7 is 30% lower than that of YSZ, which was discussed based on the theory of heat conduction. Thermal barrier coating of Nd2Ce2O7 was produced by atmospheric plasma spraying (APS) using the spray-dried powder. The thermal cycling was performed with a gas burner test facility to examine the thermal stability of the as-prepared coating.
Resumo:
We present a new generation 980 nm submarine pump module that consists of a hermitically sealed 8-pin ceramic MiniDIL package without thermo-electric cooler.
Resumo:
In this work, the microstructure, thermal and electric conductivity properties of near-zero thermal expansion ZrW2O8/ZrO2 and Al2O3 added ZrW2O8/ZrO2 composites were studied. Both the two composites exhibit very low thermal conductivity and the thermal conductivity decreases slightly as the temperature increases. The electric conductivity of the two composites increases with the increasing of the measurement temperature. The Al2O3 added ZrW2O8/ZrO2 composite has higher thermal and electric conductivity than ZrW2O8/ZrO2 composite. The most important factor which causes the difference of the thermal and electric conductivity of the composites is the porosity. (C) 2008 The Ceramic Society of Japan. All rights reserved.
Resumo:
The hole-mediated Curie temperature in Mn-doped wurtzite ZnO nanowires is investigated using the k center dot p method and mean field model. The Curie temperature T-C as a function of the hole density has many peaks for small Mn concentration (x(eff)) due to the density of states of one-dimensional quantum wires. The peaks of T-C are merged by the carriers' thermal distribution when x(eff) is large. High Curie temperature T-C > 400 K is found in (Zn,Mn)O nanowires. A transverse electric field changes the Curie temperature a lot. (Zn,Mn)O nanowires can be tuned from ferromagnetic to paramagnetic by a transverse electric field at room temperature. (c) 2007 American Institute of Physics.
Resumo:
In this paper, we use a pulsed rapid thermal processing (RTP) approach to create an emitter layer of hetero-junction solar cell. The process parameters and crystallization behaviour are studied. The structural, optical and electric properties of the crystallized films are also investigated. Both the depth of PN junction and the conductivity of the emitter layer increase with the number of RTP pulses increasing. Simulation results show that efficiencies of such solar cells can exceed 15% with a lower interface recombination rate, but the highest efficiency is 11.65% in our experiments.
Resumo:
Results are reported of electric-field dependence on thermal emission of electrons from the 0.40 eV level at various temperatures in InGaP by means of deep-level transient spectroscopy. The data are analyzed according to the Poole-Frankel emission from the potentials which are assumed to be Coulombic, square well, and Gaussian, respectively. The emission mte from this level is strongly field dependent. It is found that the Gaussian potential model is more reasonable to describe the phosphorus-vacancy-induced potential in InGaP than the Coulombic and square-well ones.
Resumo:
Electric-field-induced molecular alignments of side-chain liquid-crystalline polyacetylenes [-{HC=C[(CH2)(m)OCO-biph-OC7H15]}-, where biph is 4,4'-biphenylyl and m is 3 (PA3EO7) or 9 (PA9EO7)] were studied with X-ray diffraction and polarized optical microscopy. An orientation as high as 0.84 was obtained for PA9EO7. Furthermore, the molecular orientation of]PA9EO7 was achieved within a temperature range between the isotropic-to-smectic A transition temperature and 115 degreesC, and this suggested that the orientational packing was affected by the thermal fluctuation of the isotropic liquid and the mobility of the mesogenic moieties. The maximum achievable orientation for PA9EO7 was much greater than that for PA3EO7. This was the first time that the electric-field-induced molecular orientation of a side-chain liquid-crystalline polymer with a stiff backbone was studied.