175 resultados para phosphors

em Chinese Academy of Sciences Institutional Repositories Grid Portal


Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new kind of rare earth material with high efficient long-persistent phosphors, such as SrAl2O4: Eu, Dy, has been developed in recent years. The PMMA with long-persistent phosphors is typical one of applications for the phosphors. In this work, we try to probe into the affection of the manufacture process on the PMMA with long-persistent phosphors, to analyze its performance, and its luminescence behavior, especially to study the self-excitation of the PMMA with long-persistent phosphors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Compounds of Sr3Al2O6: Eu, Sr4Al14O25: Eu, and BaZnSiO4: Eu were synthesized by high-temperature solid state reactions. The doping Eu3+ ions were partially reduced to Eu2+ in Sr4Al14O25: Eu and BaZnSiO4: Eu prepared in an oxidizing atmosphere, N-2 + O-2. However, such an abnormal reduction process could not be performed in Sr3Al2O6: Eu, which was also prepared in an atmosphere of N-2 + O-2. Moreover, even though Sr3Al2O6: Eu was synthesized in a reducing condition CO, only part of the Eu3+ ions was reduced to Eu2+. The existence of trivalent and divalent europium ions was confirmed by photoluminescent spectra. The different valence-change behaviors of europium ions in the hosts were attributed to the difference in host crystal structures. The higher the crystal structure stiffness, the easier the reduction process from Eu3+ to Eu2+.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

EU3+ -doped Y3Al5O12 (YAG:Eu3+) phosphors were synthesized by a facile sol-gel combustion method. In this process, citric acid traps the constituent cations and reduces the diffusion length of the precursors. YAG phase is obtained through sintering at 900 degrees C for 2h. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed. The charge transfer band of nanocrystalline phosphors shows a shift toward the high-energy side, compared with that of amorphous ones due to lower covalency of Eu-O bond for nanocrystalline phosphors. The higher concentration quenching in YAG:EU3+ nanophosphors may be caused by the confinement effect on resonant energy transfer of nanocrystalline. It also indicates that the sol-gel combustion synthesis method provides a good distribution of Eu3+ activators in YAG host. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The synthesis and optical properties of Y3Al5O12:Tb3+ phosphors are reported in this paper. Y3Al5O12:Tb3+ phosphors were synthesized by a facile solution combustion method. Citric acid traps the constituent cations and also acts as a fuel. Y3Al5O12 (YAG) phase can crystallize through sintering at 900 degrees C for 2 h, and there were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) in the sintering process. The excitation spectra of crystalline Y3Al5O12:Tb3+ are different from that of amorphous one due to the crystal field effect. The emission spectra mainly show D-5(4) -> F-7(6) transition under UV excitation. The higher concentration quenching in Y3Al5O12:Tb3+ nanophosphors may be due to the confinement effect on resonant energy transfer of nanocrystalline. It is also indicated that the solution combustion synthesis method provides a good distribution of Tb3+ activators in Y3Al5O12 host. (c) 2005 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zn2SiO4:Mn2+, Zn2SiO4:Eu3+ and Zn2SiO4:Mn2+ Eu3+ phosphors were prepared by a sol-gel process and their luminescence spectra were investigated. The emission bands from intra-ion transitions of Mn2+ and Eu3+ samples were studied as a function of pressure. The pressure coefficient of Mn2+ emission was found to be -25.3 +/- 0.5 and -28.5 +/- 0.9 meV/GPa for Zn2SiO4:Mn2+ and Zn2SiO4:Mn2+ Eu3+, respectively. The Eu3+ emission shows only weak pressure dependence. The pressure dependences of the Mn2+ and Eu3+ emissions in Zn2SiO4:Mn2+ Eu3+ are slightly different from that in Zn2SiO4:Mn2+ and Zn2SiO4:Eu3+ samples, which can be attributed to the co-doping of Mn2+ and Eu3+ ions. The Mn2+ emission in the two samples, however, exhibits analogous temperature dependence and similar luminescence lifetimes, indicating no energy transfer from Mn2+ to Eu3+ occurs. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The photo- and thermo-stimulated luminescence (PSL and TSL) of BaFCl0.8Br0.2:Sm2+,Sm3+ phosphors were investigated. It is found that the stimulated luminescence intensity of Sm2+ is almost equal to that of Sm3+ even if the content of Sm2+ is much lower than that of Sm3+. Only the stimulated luminescence of Sm2+ is observed in the sample in which the content of Sm2+ is much higher than Sm3+, demonstrating that the PSL or TSL efficiency of Sm2+ is much higher than that of Sm3+. This is attributed to the effective overlap of the e-h emission with the absorption of Sm2+ centers which may make the energy transfer from the electron-hole pairs to Sm2+ effectively. In BaFCl0.8Br0.2:Sm2+,Sm3+ the stimulated luminescence is considered to be occurred via the recombination of photoreleased electrons with the [Sm2+ + h] or [Sm3+ + h] complex and the energy transfer from the electron-hole pairs to the luminescence centers (Sm2+ and Sm3+) is concerned to be the major step to determine the stimulated luminescence efficiency. The X-ray-induced stimulated luminescence is compared and connected to the photon gated hole burning. The net result of the two processes is quite similar and may be comparable. It is suggested from the observations of stimulated luminescence that electron migration between Sm2+ and Sm3+ is not the major process, color centers may play an important role in hole burning. The information from stimulated luminescence is helpful for the understanding of the hole burning mechanism. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Here we report the electron migration by photo- or thermostimulation in BaFCl:Eu2+. Electrons released from F centers may be trapped by other defect sites to form F aggregates or another type of F center and vice versa. This migration reduces the photostimulated luminescence efficiency, lowers the imaging plate sensitivity, and causes the difference between the optical absorption and photostimulation spectra of color centers. (C) 1997 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

After x-irradiation for 10 s, luminescence from BaFBr:Eu2+ phosphors by photostimulation of longer wavelength than F absorption bands was observed and assigned to the surface states or intrinsic defects of the powders. It is found that the luminescence by photostimulation into F bands can be reduced via electron migration from F centers into the surface states or intrinsic defects, thus reducing the x-ray storage or image stability. Surface passivation can lower these defects and improve the phosphors or imaging plate quality. (C) 1996 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The photoluminescence (PL) and photostimulated luminescence (PSL) of BaFBr: Eu phosphors are reported. In the photoluminescence of BaFBr:Eu, the emission of Eu2+, e-h recombination and Eu3+ have been observed, while in the photostimulated luminescence only the emission of Eu2+ was observed. This phenomenon may be explained well by the suggestion of a two-hand model for the host emission in which the host emission energy may transfer to Eu2+ difference of excitation in those two processes results in different transfer rates which makes the PL and PSL emission different.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

With the target to design and develop new functionalized green triplet light emitters that possess distinctive electronic properties for robust and highly efficient phosphorescent organic light-emitting diodes (PHOLEDs), a series of bluish-green to yellow-green phosphorescent tris-cyclometalated homoleptic iridium(III) complexes [Ir(ppy-X)(3)] (X=SiPh3, GePh3, NPh2, POPh2, OPh, SPh, SO2Ph, Hppy=2-phenylpyridine) have been synthesized and fully characterized by spectroscopic, redox, and photophysical methods

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaGaO3:Sm3+, LaGaO3:Tb3+ and LaGaO3: Sm3+, Tb3+ phosphors were prepared through a Pechini-type sol-gel process. X-Ray diffraction, field emission scanning electron microscopy, photoluminescence (PL), and cathodoluminescence (CL) spectroscopy were utilized to characterize the synthesized phosphors. Under excitation with ultraviolet light (250-254 nm), the LaGaO3: Sm3+, LaGaO3: Tb3+ and LaGaO3: Sm3+, Tb3+ phosphors mainly show the characteristic broadband emission (from 300 to 600 nm with a maximum around 430 nm) of the LaGaO3 host lattice, accompanied by the weak emission of Sm3+ ((4)G(5/2) -> H-6(5/2), H-6(7/2), H-6(9/2) transitions) and/or Tb3+ (D-5(3,4) -> F-7(6,5,4,3) transitions). However, under excitation by low-voltage electron beams (1-3 kV), the LaGaO3: Sm3+, LaGaO3: Tb3+ and LaGaO3: Sm3+, Tb3+ phosphors exhibit exclusively the characteristic emissions of Sm3+ and/or Tb3+ with yellow (Sm3+), blue (Tb3+, with low concentrations) and white (Sm3+ + Tb3+) colors, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lu3Ga5O12:Eu3+, Lu3Ga5O12:Tb3+, and Lu3Ga5O12:Pr3+ phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), photoluminescence, and cathodoluminescence spectra were utilized to characterize the synthesized phosphors. The XRD results reveal that the sample begins to crystallize at 800 degrees C and fully crystallined pure Lu3Ga5O12 phase can be obtained at 1000 degrees C. The FESEM image indicates that the phosphor sample is composed of aggregated rice grainlike particles with sizes around 80-120 nm.