294 resultados para micro-structure optical device
em Chinese Academy of Sciences Institutional Repositories Grid Portal
Resumo:
We present a detail investigation on the development of a series of gradient index (GRIN) optical glass microlens and polymer microlens and microlens arrays in our laboratory in recent years. The special glass material GRIN lenses have been fabricated mainly by using ion-exchange technology, which are applied to construct micro-optic devices and other applications. On one hand, we demonstrated the light propagation and imaging properties of GRIN lenses and the results analyzed. On the other hand, we have explored a drop-on-demand ink-jet printing method to produce microlens array using nano-scale polymer droplets involved with a uniform ultraviolet light and heat solidifying process. The experimental setup for manufacturing polymer microlens array and the performance of refractive microlens elements are also given in this paper. (C) 2006 Elsevier GmbH. All rights reserved.
Resumo:
A novel terbium complex, Tb(acac)(3)AAP (acac: acetylacetone, AAP: 4-amino-antipyrine), was synthesized and its luminescent properties were studied. When it was used as an emitting center, triple-layer-type device with a structure of glass substrate/ITO (indium-tin oxide)/TPD (N,N'-diphenyl-N,N'-bis(3-methylphenyl)-1,1'-biphenyl-4,4'-diamine)./Tb(acac)(3)AAP/PBD (2-(4-biphenyl)-5-(4-t-butylphenyl)-1,3,4-oxadiazole) or Alq(3) (tris(8-hydroxyquinolinato) aluminum)/Al (aluminum) exhibited bright characteristic emission of terbium ion upon applying d.c. voltage. The maximum luminance of the device is 56 cd/m(2) at 19 V and the maximum luminance efficiency is 0.357 lm/W.
Resumo:
The one-mode analysis method on the pull-in instability of micro-structure under electrostatic loading is presented. Taylor series are used to expand the electrostatic loading term in the one-mode analysis method, which makes analytical solution available. The one-mode analysis is the combination of Galerkin method and Cardan solution of cubic equation. The one-mode analysis offers a direct computation method on the pull-in voltage and displacement. In low axial loading range, it shows little difference with the established multi-mode analysis on predicting the pull-in voltages for three different structures (cantilever, clamped-clamped beams and the plate with four edges simply-supported) studied here. For numerical multi-mode analysis, we also show that using the structural symmetry to select the symmetric mode can greatly reduce both the computation effort and the numerical fluctuation.
Resumo:
TiO2 thin films are prepared on fused silica with conventional electron beam evaporation deposition. After annealed at different temperatures for 4h, the spectra and XRD patterns of the TiO2 thin film are obtained. Weak absorption of coatings is measured by the surface thermal lensing technique, and laser-induced damage threshold (LIDT) is determined. It is found that with the increasing annealing temperature, the transmittance of TiO2 films decreases. Especially when coatings are annealed at high temperature over 1173K, the optical loss is very serious. Weak absorption detection indicates that the absorption of coatings decreases firstly and then increases, and the absorption and defects play major roles in the LIDT of TiO2 thin films.
Resumo:
Ta2O5 films were deposited by conventional electron beam evaporation method and then annealed in air at different temperature from 873 to 1273 K. It was found that the film structure changed from amorphous phase to hexagonal phase when annealed at 1073 K, then transformed to orthorhombic phase after annealed at 1273 K. The transmittance was improved after annealed at 873 K, and it decreased as the annealing temperature increased further. The total integrated scattering (TIS) tests and AFM results showed that both scattering and root mean square (RMS) roughness of films increased with the annealing temperature increasing. X-ray photoelectron spectroscopy (XPS) analysis showed that the film obtained better stoichiometry and the O/Ta ratio increased to 2.50 after annealing. It was found that the laser-induced damage threshold (LIDT) increased to the maximum when annealed at 873 K, while it decreased when the annealing temperature increased further. Detailed damaged models dominated by different parameters during annealing were discussed. (C) 2008 Elsevier B. V. All rights reserved.
Resumo:
AlGa1-xAs/GaAs heterostructures have been grown by two different liquid phase epitaxy (LPE) modes, i.e. the supercooled and melt-etch methods, for the fabrication of highly efficient solar cells. Typical structural characteristics observed under a transmission electron microscope (TEM), an Auger energy spectrometer (AES) and corresponding device parameters were presented. The results indicated that the P+PNN+ configuration grown by the melt-etch method could be used to produce high performance, large area solar cells with effectively reducing the defects of the substrate and improving the minority carrier collection by forming a compositionally graded region in the window layer.
Resumo:
An optical modulator is designed and fabricated based on a Si0.75Ge0.25/Si/Si0.5Ge0.5 asymmetrical superlattice structure. The device comprises a p-i-n diode made on the asymmetrical superlattice integrated with a 920-mu m-long Fabry-Perot (F-P) cavity. Parameters of the rib waveguide are designed to satisfy only the fundamental-TE mode transmission. Here, 65 and 40-pm red shifts of the peak resonant were measured under the applied bias of 2.5 and -32.0 V, respectively. The analysis shows that, besides the thermal-optical and plasma dispersion effects, the Pockels effect also contributes to such a peak shift. The corresponding calculated effective Pockels coefficient is about 0.158 pm/V.
Resumo:
Because of the load transfer effect of interface layer, the stress distribution inside the composite structure of film/substrate can be very different from the Timoshenko's model. In this paper, we give the derivation and analysis of such load transfer effect of shear-lag (S-L) model. The micro-structure size (boundary conditions) effect together with interface load transfer effect becomes more and more important as the microstructure size including the three dimensions of thickness, width and length shrinks. The microstructure size is also responsible for the so-called edge-induced stress. The edge effect and difference of S-L model and Timoshenko model are also demonstrated.
Resumo:
Calculations of the electronic structure and the density of states of GaN with Mn are carried out by means of first-principles plane-wave pesudopotential method based on density functional theory. The results reveal a 100% spin polarized impurity band in band structure of Ga1-xMnxN due to hybridization of Mn 3d and N 2p orbitals. The material is half metallic and suited for spin injectors. In addition, a peak of refractive index can be observed near the energy gap. The absorption coefficient increases in the UV region with the increase of the Mn content.
Resumo:
Size tolerance of a 4X4 general interference tapered multimode interference (MMI) coupler in a silicon-on-insulator (SOI) structure is investigated by means of a 2-D finite difference beam propagation method (2D-FDBPM), together with an effective refractive index method (EIM). The results show that the tapered multimode interference coupler exhibits relatively larger size tolerance when light is launched from the edgeport than from midport, though it has much better output power uniformity when light is launched from midport. Besides that, it can reduce the device length greatly. The 4X4 general interference tapered MMI coupler has a slightly larger size tolerance compared with a conventional straight multimode interference coupler. (C) 2003 Society of Photo-Optical Instrumentation Engineers.
Resumo:
A novel semiconductor optical amplifier (SOA) optical gate with a graded strained bulk-like active structure is proposed. A fiber-to-fiber gain of 10 dB when the coupling loss reaches 7 dB/factet and a polarization insensitivity of less than 0.9 dB for multiwavelength and different power input signals over the whole operation current are obtained. Moreover, for our SOA optical gate, a no-loss current of 50 to 70 mA and an extinction ratio of more than 50 dB are realized when the injection current is more than no-loss current, and the maximum extinction ratio reaches 71 dB, which is critical for crosstalk suppression. (C) 2003 society of Photo-Optical Instrumentation Engineers.
Resumo:
Micro-cavity structure composed of silicon wire with 240nm square cross section and two symmetrical sidewall waveguide Bragg gratings is fabricated and studied for the operation under telecommunication wavelengths. Optical filter of quasi-TE mode was realized based on this cavity. In such micro-cavity, optical quality factor (Q) was measured up to 380 with a 4.8nm free spectral range (FSR) and 12dB fringe contrast (FC). The measured group index of silicon waveguide with only 240nm square cross section was between 3.80 and 5.43. It is the first time group delay of silicon wire waveguide with such small core dimension is studied. Larger group delay can be expected after optimizing the design parameters and the fabrication process.
Resumo:
Nano/microstructure of bis(propyl)triethoxysilane substituted perylenediimide (1) with nanoparticle and twisted microrod morphologies were obtained by reprecipitation method induced by water and petroleum ether, respectively. It is believed that the different nucleation and growth processes involved are responsible for the formation of the nano/micro-structure With different morphologies of 1. UV-vis absorption and photoluminescence measurements show that their UV-vis absorption and photoluminescence properties are different from each other as well as their monomer mid bulk materials due to the different effects on the change transfer (CT) transition energy levels caused by their different aggregation behaviors.
Resumo:
Abstract: In order to investigate the effects of the grain size distribution and the micro-structure of soils on the mechani- cal characteristics, some static triaxial compression tests were carried out, and then the relationship of stress-strain and the strength behavior of silty sand were compared among undisturbed samples with different grain size distribution, undis- turbed and remolded samples with the same grain size distribution, and reconstituted samples (or called mixed samples) with different grain size distribution. The effects of grain size distribution and structure on the mechanic behavior of silty sands were mainly analyzed. It is shown that the obvious differences of the mechanical characteristics between undis- turbed soils and remolded soils are caused by the differences of soil structures. Although the grain size distribution are different between two soil samples, their mechanical characteristics may be close to each other, or may have obvious differences because of the effects of micro-structure.