197 resultados para Zinc Purification
em Chinese Academy of Sciences Institutional Repositories Grid Portal
Resumo:
EEnzyme activity of commercial glucose oxidase was enhanced after purification through a strong anionic exchange resin. In order to get a better insight into this phenomenon, surface pressure–area ( –A) isotherms and surface pressure–time ( –t) isotherms was used to study the interaction and the absorption at different pH values of the subphases between octadecylamine and glucose oxidase purified by a styrene system quaternary ammonium type strongly basic anionic exchange resin. Circular dichroism (CD), electrophoresis and enzyme activity measurements were conducted to study these phenomena. A preliminary hypothesis has been suggested to explain why the enzyme activity of purified glucose oxidase was higher than that of the commercial one. © 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Molecular dynamics (MD) simulations and first-principles calculations are carried out to analyze the stability of both newly discovered and previously known phases of ZnO under loading of various triaxialities. The analysis focuses on a graphite-like phase (FIX) and a body-centered-tetragonal phase (BCT-4) that were observed recently in [0 1 (1) over bar 0]- and [0 0 0 1]-oriented nanowires respectively under uniaxial tensile loading as well as the natural state of wurtzite (WZ) and the rocksalt (RS) phase which exists under hydrostatic pressure loading. Equilibrium critical stresses for the transformations are obtained. The WZ -> HX transformation is found to be energetically favorable above a critical tensile stress of 10 GPa in [0 1 (1) over tilde 0] nanowires. The BCT-4 phase can be stabilized at tensile stresses above 7 GPa in [0 0 0 1] nanowires. The RS phase is stable at hydrostatic pressures above 8.2 GPa. The identification and characterization of these phase transformations reveal a more extensive polymorphism of ZnO than previously known. A crystalline structure-load triaxiality map is developed to summarize the new understanding. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
We present an entanglement purification protocol for photonic mixed entangled states based on the two-mode polarization nondemolition parity detectors. Without the use of the controlled-NOT (CNOT) operations, the efficiency of our protocol can nearly approach that of the CNOT protocol. The total successful probability of our protocol can be nearly enhanced to the quantity twice as large as that of the linear-optics-based protocol. Besides, our protocol adopts common photon detectors rather than the sophisticated single-photon detectors required in the linear-optics-based protocol.
Resumo:
We present an entanglement purification scheme for the mixed entangled states of electrons with the aid of charge detections. Our scheme adopts the electronic polarizing beam splitters rather than the controlled-NOT (CNOT) operations, but the total successful probability of our scheme can reach the quantity as large as that of the the CNOT-operation-based protocol and twice as large as that of linear-optics-based protocol for the purification of photonic entangled states. Thus our scheme can achieve a high successful prabability without the usage of CNOT operations.
Resumo:
We analyse further the entanglement purification protocol proposed by Feng et al. (Phys. Lett. A 271 (2000) 44) in the case of imperfect local operations and measurements. It is found that this protocol allows of higher error threshold. Compared with the standard entanglement purification proposed by Bennett et al. [Phys. Rev. Lett. 76 (1996) 722], it turns out that this protocol is remarkably robust against the influences of imperfect local operations and measurements.
Resumo:
The ablation in zinc selenide (ZnSe) crystal is studied by using 150-fs, 800-nm laser system. The images of the ablation pit measured by scanning electronic microscope (SEM) show no thermal stress and melting dynamics. The threshold fluence is measured to be 0.7 J/cm2. The ultrafast ablation dynamics is studied by using pump and probe method. The result suggests that optical breakdown and ultrafast melting take place in ZnSe irradiated under femtosecond laser pulses.
Resumo:
Broadband infrared luminescence covering the optical telecommunication wavelength region of 0, E and S bands was observed from bismuth-doped zinc aluminosilicate glasses and glass-ceramics. The spectroscopic properties of the glasses and glass-ceramics depend on the thermal-treatment history. With the appearance of gahnite (ZnAl2O4) crystalline phase, the fluorescent peak moves to longer wavelength, but the fluorescent intensity decreases. The similar to 1300 nm fluorescence with a FWHM larger than 250 nm and a lifetime longer than 600 mu s possesses these optical materials with potential applications in laser devices and broadband amplifiers. The broad infrared luminescence from the bismuth-doped zinc aluminosilicate glasses and glass-ceramics might be from BiO or bismuth clusters rather than from Bi5+ and Bi3+. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A series of zinc tellurite glasses of 75TeO(2)-20ZnO-(5-x)La2O3-xEr(2)O(3) (x=0.02, 0.05, and 0.1 mol%) with the different hydroxl groups were prepared by the conventional melt-quenching method. Infrared spectra were measured in order to estimate the exact content of OH- groups in samples. The observed increase of the fluorescence lifetime with the oxygen bubbling time has been related to the reduction in the OH- content concentration as evidenced by IR transmission spectra. Various nonradiative decay rates from I-4(13/2) of Er3+ with. the change of OH content were determined from the fluorescence lifetime and radiative decay rates were calculated on the basis of Judd-Ofelt theory. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
this paper is retracted
Resumo:
Polycrystalline Zn1-xNixO diluted magnetic semiconductors have been successfully synthesized by an auto-combustion method. X-ray diffraction measurements indicated that the 5 at% Ni-cloped ZnO had the pure wurtzite structure. Refinements of cell parameters from powder diffraction data revealed that the cell parameters of Zn0.95Ni0.05O were a little bit larger than ZnO. Transmission electron microscopy observation showed that the as-synthesized powders were of the size similar to 60 nm. Magnetic investigations showed that the nanocystalline Zn0.95Ni0.05O possessed room temperature ferromagnetisin with the saturation magnetic moment of 0.1 emu/g (0.29 mu(B)/Ni2+). (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Zinc oxide (ZnO) films with c-oriented were grown on fused quartz glass substrates at room temperature using dc reactive magnetron sputtering. The as-grown films were annealed at 700 degrees C in air and bombarded by ion beam, respectively. The effects of post-treatments on the structural and optical properties of the ZnO films were investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. The XRD spectra indicate that the crystal quality of ZnO films has been improved by both the post-treatments. Compared with the as-grown sample, both annealed and bombarded samples exhibited blueshift in the UV emission peaks, and a strong green emission was found in the annealed ZnO film. In both optical transmittance and absorption spectra, a blueshift of the band-gap edge was observed in the bombarded film, while a redshift was observed in the annealed film. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
CO2 laser irradiation experiments on ZnO thin films are reported. The structural, optical, luminescent and vibrational properties of the samples were investigated by X-ray diffraction (XRD), transmittance, photoluminescence (PL) and Raman measurements. XRD results show that the crystalline of the irradiated films was improved. The (002) peaks of irradiated ZnO films shift to. higher 20 angles due to the stress relaxation in the case of laser beam irradiation. From optical transmittance spectra, all films exhibit high transmittance in the visible range, the optical band edge of irradiated films showed a redshift compared with that of as-grown films. Compared with the as-grown films, the photoluminescence emission (in particular the relative intensities of visible emissions) intensities of irradiated samples enhanced. In the Raman scattering spectral both the A I. and E modes exhibited slight Raman blueshift. (c) 2005 Elsevier B.V. All rights reserved.