Resumo:
A noncontacting and noninterferometric depth discrimination technique, which is based on differential confocal microscopy, was used to measure the inverse piezoelectric extension of a piezoelectric ceramic lead zirconate titanate actuator. The response characteristics of the actuator with respect to the applied voltage, including displacement, linearity, and hysteresis, were obtained with nanometer measurement accuracy. Errors of the measurement have been analyzed. (C) 2001 Society of Photo-Optical Instrumentation Engineers.
Resumo:
We demonstrate the broadband optical amplification in bismuth-doped strontium germanate glass with 808 nm and 980 nm laser diodes (LDs) as excitation sources. The net optical gain has been obtained within the wavelength region of 1272 to 1348 nm with 808 nm laser diode under 0.97 W power. The maximum gain and gain coefficients are 1.23 and 1.03 cm(-1) at 1315 nm, respectively. The signal increment at 1300 nm is 2.8 times with 980 nm LD, under 3 W power. The differential thermal analysis measurement reveals the good thermal stability of the studied glass. This glass could be suggested as a promising gain medium for broadband optical amplifiers.
Resumo:
Infrared-to-visible upconversion fluorescence of Er(3+)/Yb(3+) co-doped lithium-strontium-lead-bismuth (LSPB) glasses for developing potential upconversion lasers has been studied under 975-nm excitation. Based on the results of energy transfer efficiency and upconversion spectra, the optimal Yb(3+)-Er(3+) concentration ratio is found to be 5:1. Intense green and red emissions centered at 525, 546, and 657 nm, corresponding to the transitions 2H_(11/2)-->4I_(15/2), 4S_(3/2)-->4I_(15/2), and 4F_(9/2)-->4I_(15/2), respectively, were observed. The quadratic dependence of the 525-, 546-, and 657-nm emissions on excitation power indicates that a two-photon absorption process occurs under 975-nm excitation. The high-populated 4I_(11/2) level is supposed to serve as the intermediate state responsible for the upconversion processes. The intense upconversion luminescence of Er(3+)/Yb(3+) co-doped LSPB glasses may be a potentially useful material for developing upconversion optical devices.
Resumo:
Er3+ -doped strontium lead bismuth glass for developing upconversion lasers has been fabricated and characterized. The Judd-Ofelt intensity parameters Omega(1) (t = 2,4,6), calculated based on the experimental absorption spectrum and Judd-Ofelt theory, were found to be Omega(2) = 2.95 x 10(-20), Omega(4) = 0-91 X 10(-20), and Omega(6) = 0.36 x 10(-20) cm(2). Under 975 nm excitation, intense green and red emissions centered at 525, 546, and 657 nm, corresponding to the transitions H-2(11/2) --> I-4(15/2), S-4(3/2) I-4(15/2), and F-4(9/2) --> I-4(15/2) respectively were observed. The upconversion mechanisms are discussed based oil the energy matching and quadratic dependence on excitation power, and the dominant mechanisms are excited state absorption and energy transfer upconversion for the green and red emissions. The long-lived I-4(11/2) level is supposed to serve as the intermediate state responsible for the upconversion processes. (C) 2004 Published by Elsevier B.V.
Resumo:
Er3+/Yb3+-codoped potassium-barium-strontium-lead-bismuth glasses for developing potential upconversion lasers have been fabricated and characterized. Based on the results of energy transfer efficiency, the optimal Yb3+/Er3+ concentration ratio is found to be 5:1. Intense green and red emissions centered at 525, 546, and 657 run, corresponding to the transitions H-2(11/2) -> I-4(15/2), S-4(3/2) -> I-4(15/2), and F-4(9/2) -> I-4(15/2), respectively, were observed. The quadratic dependence of the 525, 546, and 657 nm emissions on excitation power indicates that a two-photon absorption process occurs under 975 nm excitation. The long-lived I-4(11/2) level is supposed to serve as the intermediate state responsible for the upconversion processes. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
The structure of the titanate glass is destroyed during irradiation by the femtosecond laser pulses, and (TiO6)(8-) and (TiO4)(4-) anion units are exsolved from the network of the titanate glass. These anion units are rearranged to form some crystals such as anatase and Ba2TiO4 crystals. By Raman spectroscopy, it is found that these crystals have a strong dependence on the intensity of the femtosecond laser pulses. The relation between the generation of these crystals and space distribution of the femtosecond laser power intensity is qualitatively explained. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We report on improved electrical properties of lead zirconate titanate (PZT) film deposited on titanium metal foil using nitrogen annealing. After nitrogen annealing of the PZT capacitors, symmetric capacitance-voltage (C-V) characteristics, higher dielectric constant and breakdown field, less change of dielectric constant with frequency, lower dielectric loss and leakage current are obtained. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The influence of gamma-radiation dose rate on the electrical properties of lead zirconate titanate capacitors was investigated. More severe degradations in dielectric constant, coercive field, remanent polarization and capacitance-voltage (C-V) curves occurred with increasing radiation dose at lower dose rates. The electrical properties exhibited distinct radiation dose rate dependence and the worst-case degradation occurred at the lowest dose rate. The radiation-induced degradation of parameters such as the coercive field drift and distortion of the C-V curve can be recovered partly through post-irradiation annealing.
Resumo:
Molecular-dynamics simulations have been carried out to investigate the electric hysteresis of barium titanate nanofilm containing oxygen vacancy ordering array parallel to the {101} crystal plane. The results obtained show a significant weakening of polarization retention from non-zero value to zero as the size of the array was reduced to a critical level, which was attributed to the formation and motion of head-to-head domain wall structure under external field loading process. By comparing with materials containing isolated oxygen vacancies, it was found that the zero retention was due to the oxygen vacancy ordering array rather than to the concentration of oxygen vacancy. Copyright (C) EPLA, 2010