Resumo:
A new biodegradable amphiphilic block copolymer, poly(ethylene glycol)-b-poly(L-factide-co-9-phenyl-2,4,8, 10-tetraoxaspiro[5,5]undecan-3-one) [PEG-b-P(LA-co-PTO)], was successfully prepared by ring-opening polymerization (ROP) Of L-lactide (LA) and functionalized carbonate monomer 9-phenyl-2,4,8,10-tetraozaspiro[5,5]undecan-3-one (PTO) in the presence of monohydroxyl poly(ethylene glycol) as macroinitiator using Sn(Oct)(2) as catalyst. NMR, FT-IR, and GPC studies confirmed the copolymer structure.
Resumo:
A novel biodegradable diblock copolymer, poly(L-cysteine)-b-Poly(L-lactide) (PLC-b-PLLA), was synthesized by ring-opening polymerization (ROP) of N-carboxyanhydride of beta-benzyloxycarbonyl-L-Cysteine (ZLC-NCA) with amino-terminated Poly(L-lactide) (NH2-PLLA) as a macroinitiator in a convenient way. The diblock copolymer and its precursor were characterized by H-1 NMR, Fourier transform infrared (FT-IR), gel permeation chromatography (GPC), and X-ray photoelectron spectroscopy (XPS) measurements. The length of each block polymer could be tailored by molecular design and the ratios of feeding monomers.
Resumo:
The surface modification of hydroxyapatite (HA) nanoparticles by the ring opening polymerization (ROP) of gamma-benzyl-L-glutamate N-carboxyanhydride (BLG-NCA) was proposed to prepare the poly(gamma-benzyl-L-glutamate) (PBLG)-grafted HA nanoparticles (PBLG-g-HA) for the first time. HA nanoparticles were firstly treated by 3-aminopropylthriethoxysilane (APS) and then the terminal amino groups of the modified HA particles initiated the ROP of BLG-NCA to obtain PBLG-g-HA. The process was monitored by XPS and FT-IR. The surface grafting amounts of PBLG on HA ranging from 12.1 to 43.1% were characterized by thermal gravimetric analysis (TGA). The powder X-ray diffraction (XRD) analysis confirmed that the ROP only underwent on the surface of HA nanoparticles without changing its bulk properties. The SEM measurement showed that the PBLG-g-HA hybrid could form an interpenetrating net structure in the self-assembly process.
Resumo:
novel biodegradable Y-shaped copolymer, poly(L-lactide)(2)-b-poly(gamma-benzyl-L-glutamic acid) (PLLA(2)-b-PBLG), was synthesized by the ring-opening polymerization (ROP) of N-carboxyanhydride of gamma-benzyl-L-glutamate (BLG-NCA) with centrally amino-functionalized poly(L-lactide), PLLA(2)-NH2, as a macroinitiator in a convenient way. The Y-shaped copolymer and its precursors were characterized by H-1 NMR, FT-IR, GPC, WAXD and DSC measurements. The self-assembly of the PLLA(2)-b-PBLG copolymer in toluene and benzyl alcohol was examined. It was found that the self-assembly of the copolymer was dependent on solvent and on relative length of the PBLG block. For a copolymer with PLLA blocks of 26 in total degree of polymerization (DP), if the PBLG block was long enough (e.g., DP = 54 or more), the copolymer/toluene solution became a transparent gel at room temperature. In benzyl alcohol Solution, only PLLA(2)-b-PBLG containing ca. 190 BLG residues could form a gel: those with shorter PBLG blocks (e.g., DP = 54) became nano-scale fibrous aggregates and these aggregates were dispersed in benzyl alcohol homogeneously.
Resumo:
This report describes direct formation of giant vesicles from a series of poly(L-lysine)-block-poly(L-phenylalanine) (PLL-b-PPA) block copolymers from their water solution. These polymers are prepared by successive ring-opening polymerization (ROP) of the two alpha-amino acid N-carboxyanhydrides and then removing the side chain protecting groups by acidolysis. The structures of the copolymers are confirmed by nuclear magnetic resonance (NMR), differential scanning calorimetry (DSC), and size exclusion chromatography ( SEC). The vesicles are studied by atomic force microscopy (AFM), field emission scanning electron microscopy (ESEM), and confocal laser scanning microscopy (CLSM). Rhodamine B is used as a fluorescent probe to confirm the existence of the vesicle with an aqueous interior. The vesicle size is in the range 0.55-6 mu m, depending on the absolute and relative lengths of the two blocks, on initial polymer concentration, and on solution pH. The vesicles are still stable in water for 2 months after preparation. Addition of the copolymer to DNA solution results in complex formation with it. The complex assumes the morphology of irregular particles of less than 2 mu m. It is expected to be used in drug and gene delivery.
Resumo:
A novel amphiphilic biodegradable triblock copolymer (PGL-PLA-PGL) with polylactide (PLA) as hydrophobic middle block and poly(glutamic acid) (PGL) as hydrophilic lateral blocks was successfully synthesized by ring-opening polymerization (ROP) Of L-lactide (LA) and N-carboxy anhydride (NCA) consecutively and by subsequent catalytic hydrogenation. The results of cell experiment of PGL-PLA-PGL suggested that PGL could improve biocompatibility of polyester obviously. The copolymer could form micelles of spindly shape easily in aqueous solution. The pendant carboxyl groups of the triblock copolymer were further activated with N-hydroxysuccinimide and combined with a cell-adhesive peptide GRGI)SY Incorporation of the oligopeptide further enhanced the hydrophilicity and led to formation of spherical micelles. PGL-PLAPGL showed better cell adhesion and spreading ability than pure PLA and the GRGDSY-containing copolymer exhibited even further improvement in cell adhesion and spreading ability, indicating that the copolymer could find a promising application in drug delivery or tissue engineering.
Resumo:
Polypeptide/polysaccharide graft copolymers poly(L-lysine)-graft-chitosan (PLL-g-Chi) were prepared by ring-opening polymerization (ROP) of epsilon-benzoxycarbonyl L-lysine N-carboxyanhydrides (Z-L-lysine NCA) in the presence of 6-O-triphenylmethyl chitosan. The PLL-g-Chi copolymers were thoroughly characterized by H-1 NMR, C-13 NMR, Fourier transform infrared (FT-IR), and gel permeation chromatography (GPC). The number-average degree of polymerization of PLL grafted onto the chitosan backbone could be adjusted by controlling the feed ratio of NCA to 6-O-triphenylmethyl chitosan. The particle size of the complexes formed from the copolymer and calf thymus DNA was measured by dynamic light scattering (DLS). It was found in the range of 120 similar to 340 nm. The gel retardation electrophoresis showed that the PLL-g-Chi copolymers possessed better plasmid DNA-binding ability than chitosan. The gene transfection effect in HEK 293T cells of the copolymers was evaluated, and the results showed that the gene transfection ability of the copolymer was better than that of chitosan and was dependent on the PLL grafting ratio. The PLL-g-Chi copolymers could be used as effective gene delivery vectors.
Resumo:
A novel biodegradable triblock copolymer poly(ethylene glycol)-b-poly(L-lactide)-b-poly(L-lysine) (PEG-PLA-PLL) was synthesized by acidolysis of poly(ethylene glycol)-b-poly(L-lactide)-b-poly(F-benzyloxycarbonyl-L-lysine) (PEG-PLA-PZLL) obtained by the ring-opening polymerization (ROP) of epsilon-benzyloxycarbonyl-L-lysine N-carboxyanhydride (ZLys NCA) with amino-terminated PEG-PLA-NH2 as a macro-initiator, and the pendant amino groups of the lysine residues were modified with a peptide known to modulate cellular functions, Gly-Arg-Gly-Asp-Ser-Tyr (GRGDSY, abbreviated as RGD) in the presence of 1,1'-carbonyldiimidazole (CDI). The structures of PEG-PLA-PLL/RGD and its precursors were confirmed by H-1 NMR, FT-IR, amino acid analysis and XPS analysis. The cell adhesion and cell spread on the PEG-PLA-PLL/RGD film were enhanced compared to those on pure PLA film. Therefore, the novel RGD-grafted triblock copolymer is promising for cell or tissue engineering applications. Both copolymers PEG-PLA-PZLL and PEG-PLA-PLL showed an amphiphilic nature and could self-assemble into micelles of homogeneous spherical morphology. The micelles were determined by fluorescence technique, dynamic light scattering (DLS), and field emission scanning electron microscopy (ESEM) and could be expected to find application in drug and gene delivery systems.
Resumo:
An aluminum/Schiff base complex {[2,2-dimethyl-1,3-propylenebis(3,5-di-tert-butylsalicylideneiminato)](isopropanolato)aluminum(III) (2)} based on a bulky ligand and aluminum isopropoxide was prepared and employed for the stereoselective ring-opening polymerization (ROP) of rac-lactide (rac-LA). The initiator was characterized with nuclear magnetic resonance (NMR), crystal structure measurements, and elemental analysis. It contained a five-coordinate aluminum atom that was trigonal bipyramidal in the solid state according to the crystal structure measurements. The two conformational stereoisomers of 2 exchanged quickly on the NMR scale. Compound 2 polymerized rac-LA into a crystalline polymer that was characterized with H-1 NMR, wide-angle X-ray diffraction, electrospray ionization mass spectrometry, and gel permeation chromatography. The kinetics of the polymerization were first-order in both the monomer and initiator, and there was a linear relationship between the rac-LA conversion and the number-average molecular weight of poly(rac-LA) with a narrow molecular distribution (1.04-1.08). These features showed that the polymerization was well controlled. The high melting temperature (196-201 degreesC) and isotacticity of poly(rac-LA) indicated that complex 2 was a highly stereoselective initiator for the ROP of rac-LA.
Resumo:
A novel structural triblock copolymer of poly(gamma-benzyl-L-glutamic acid)-b-poly(ethylene oxide)-b-poly(epsilon-caprolactone) (PBLG-PEO-PCL) was synthesized by a new approach in the following three steps: (1) sequential anionic ring opening polymerization (ROP) of ethylene oxide and epsilon-caprolactone with an acetonitrile/potassium naphthalene initiator system to obtain a diblock copolymer CN-PEO-PCL with a cyano end-group; (2) conversion of the CN end-group into NH2 end-group by hydrogenation to obtain NH2-PEO-PCL; (3) ROP of gamma-benzyl-L-glutamate-N-carboxyanhydrides (Bz-L-GluNCA) with NH2-PEO-PCL as macroinitiator to obtain the target triblock copolymer. The structures from CN-PEO precursor to the triblock copolymers were confirmed by FT-IR and H-1 NMR spectroscopy, and their molecular weights were measured by gel permeation chromatography. The monomer of Bz-L-GluNCA can react almost quantitatively with the amino end-groups of NH2-PEO-PCL macroinitiator by ROP.
Resumo:
An amino isopropoxyl strontium (Sr-PO) initiator, which was prepared by the reaction of propylene oxide with liquid strontium ammoniate solution, was used to carry out the ring-opening polymerization (ROP) of cyclic esters to obtain aliphatic polyesters, such as poly(epsilon-caprolactone) (PCL) and poly(L-lactide) (PLLA). The Sr-PO initiator demonstrated an effective initiating activity for the ROP of epsilon-caprolactone (epsilon-CL) and L-lactide (LLA) under mild conditions and adjusted the molecular weight by the ratio of monomer to Sr-PO initiator. Block copolymer PCL-b-PLLA was prepared by sequential polymerization of epsilon-CL and LLA, which was demonstrated by H-1 NMR, C-13 NMR, and gel permeation chromatography. The chemical structure of Sr-PO initiator was confirmed by elemental analysis of Sr and N, H-1 NMR analysis of the end groups in epsilon-CL oligomer, and Fourier transform infrared (FTIR) spectroscopy. The end groups of PCL were hydroxyl and isopropoxycarbonyl, and FTIR spectroscopy showed the coordination between Sr-PO initiator and model monomer gamma-butyrolactone. These experimental facts indicated that the ROP of cyclic esters followed a coordination-insertion mechanism, and cyclic esters exclusively inserted into the Sr-O bond.
Resumo:
Reaction of YbI2 with two equivalents of cyclopentylindenyl lithium (C5H9C9H6Li) affords ytterbium(II) substituted indenyl complex (C5H9C9H6)(2)Yb(THF)(2) (1) which shows high activity to ring-opening polymerization (ROP) of lactones. The reaction between YbI2 and cyclopentylcyclopentadienyl sodium (C5H9C5H4Na) gives complex [(C5H9C5H4)(2)Yb(THF)](2)O-2 (2) in the presence of a trace amount of O-2, the molecular structure of which comprises two (C5H9C5H4)(2)Yb(THF) bridged by an asymmetric O-2 unit. The O-2 unit and ytterbium atoms define a plane that contains a C-i symmetry center.
Resumo:
Phenolphthalein based polyarylate macrocyclic oligomers were selectively synthesized by an interfacial polycondensation reaction of o-phthaloyl dichloride with phenolphthalein. The high selectivity benefits from the role of phenolphthalein as a color indicator, an efficient phase transfer catalyst, acid a preferred conformation of the starting materials as indicated by analyzing a single-crystal X-ray structure of an analogous macrocycle. The melt ROP of phenolphthalein polyarylate cyclic dimer was studied using nucleophilic initiators, The molecular weight of the resulting polymers builds up very rapidly at the very early stage of polymerization but decreases with time. During the ROP of cyclic dimer, analogous macrocycles with higher degree of polymerization (n greater than or equal to 3) and linear oligomers were produced by backbiting reaction especially at later stage of polymerization. Conversion of cyclic dimer is very fast at the earlier stage of polymerization and then increases slowly with time as analyzed by gel permeation chromatography. However, the total amount of cyclic oligomers in the ROP system increases with time at the later stage of polymerization because of the formation of larger macrocycles. The resulting polymers are amorphous. Glass transition temperatures (T(g)s) of these polymers are influenced by the polymerization time, type of initiator, and initiator concentration.
Resumo:
Two kinds of novel macrocyclic aryl thioether ether oligomers were synthesized by nucleophilic condensation reaction in high yields under pseudo-high-dilution condition. A combination of H-1 NMR, GPC and MALDI-TOF MS analyses unambiguously confirmed the cyclic nature and their distributions, Macrocyclic thioether ether ketone oligomers can undergo facile melt ring opening polymerization(ROP) initiated by thiyl radical to give a high molecular weight polymer.
Resumo:
Novel macrocyclic aryl thioether ester oligomers have been synthesized in high yield from phthaloyl dichloride and 4,4'-thiodiphenol under pseudo high dilution conditions. The cyclic nature was unambiguously confirmed by a combination of MALDI-TOF MS, gel permeation chromatography and NMR analyses. Single-crystal X-ray diffraction of cyclic ester dimer reveals no severe strain on the cyclic structure. The free-radical ring opening polymerization (ROP) of the macrocyclic oligomers was achieved to give high molecular weight polymers via a transthioetherification reaction. The molecular weight of the polymer resulting from ROP decreases as the conversion of cyclic oligomers increases after a polymerization period of 30 min.