Resumo:
Up-converting phosphor technology (UPT)-based lateral-flow immunoassay has been developed for quantitative detection of Yersinia pestis rapidly and specifically. In this assay, 400 nm up-converting phosphor particles were used as the reporter. A sandwich immumoassay was employed by using a polyclonal antibody against F1 antigen of Y. pestis immobilized on the nitrocellulose membrane and the same antibody conjugated to the UPT particles. The signal detection of the strips was performed by the UPT-based biosensor that could provide a 980 nm IR laser to excite the phosphor particles, then collect the visible luminescence emitted by the UPT particles and finally convert it to the voltage as a signal. V-T and V-c stand for the multiplied voltage units for the test and the control line, respectively, and the ratio V-T/V-C is directly proportional to the number of Y pestis in a sample. We observed a good linearity between the ratio and log CFU/ml of Y pestis above the detection limit, which was approximately 10(4) CFU/mI. The precision of the intra- and inter-assay was below 15% (coefficient of variation, CV). Cross-reactivity with related Gram-negative enteric bacteria was not found. The UPT-LF immunoassay system presented here takes less than 30 min to perform from the sample treatment to the data analysis. The current paper includes only preliminary data concerning the biomedical aspects of the assay, but is more concentrated on the technical details of establishing a rapid manual assay using a state-of-the-art label chemistry. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
A novel energy- and time-saving solution combustion method has been developed to prepare Eu:Y2O3 nano-crystal line phosphor. This novel method employs anhydrous ethanol as solvent and fuel. The prepared nano-crystals after heat-treatment own narrow size distribution, well dispersibility and sinterability, confirmed by XRD, TEM and FTIR. The emission spectra of nano-Eu:Y2O3 Samples show clear nano-size related phenomena. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
ZnO:Zn phosphor thin films were prepared by face-to-face annealing at 450 degrees C in air. The effects of the face-to-face annealing on the structural and optical properties of the ZnO films were investigated by X-ray diffraction (XRD), photoluminescence (PL), optical transmittance and absorption measurements. Measurement results showed that the crystal quality of ZnO films was improved by face-to-face annealing. Both UV light emission and visible light emission were enhanced compared to those of open annealing films. The UV emission peak was observed to have a blueshift towards higher energy. The optical band-gap edge of as-annealed films shifted towards longer wavelength. (c) 2005 Elsevier B.V.. All rights reserved.
Resumo:
We fabricated a phosphor-conversion white light using an InGaN laser diode that emits 405 nm near-ultraviolet (n-UV) light and phosphors that emit in the blue and yellow regions when excited by the n-UV and blue light, respectively.The relationship of the luminous flux and the luminous efficacy of the white light with injection current was discussed. The luminous flux increased linearly with increasing current above the threshold of the laser diode, and at 80 mA injection current, the luminous flux and luminous efficacy were estimated to be 5.7 lm and 13 lm/w, respectively. The shift of the Commission International de I'Eclairage coordinates, color temperature, and color rendering index with current are very slight and negligible, which indicates that the blue and the yellow phosphors have an excellent stability and a highly stable white light can be obtained by this way. (c) 2008 American Institute of Physics.
Resumo:
Nanocrystalline Tm3+-doped La2O3 phosphors were prepared through a Pechini-type sol-gel process. X-ray diffraction, field-emission scanning electron microscopy, photoluminescence, and cathodoluminescence spectra were utilized to characterize the synthesized phosphors. Under the excitation of UV light (234 nm) and low-voltage electron beams (1-3 kV), the Tm3+-doped La2O3 phosphors show the characteristic emissions of Tm3+(D-1(2), (1)G(4)-F-3(4), H-3(6) transitions).
Resumo:
By attaching a bulky, inductively electron-with drawing trifluoromethyl (CF3) group on the pyridyl ring of the rigid 2-[3(N-phenylcarbazolyl)]pyridine cyclometalated ligand, we successfully synthesized a new heteroleptic orange-emitting phosphorescent iridium(III) complex [Ir(L-1)(2)(acac)] 1 (HL1=5-trifluoromethyl-2-[3-(N-phenylcarbazolyl)]pyridine, Hacac = acetylacetone) in good yield.