Resumo:
The melting behavior of poly(methyl methacrylate)-grafted nascent polyethylene reactor powder by plasma irradiation was studied by differential scanning calorimetry (DSC). The grafting yield ranged hom 11 to 190%. Grafting was found to lower both melting point and heat of fusion during the first run of DSC determination. The heat of fusion was used to calculate the apparent grafting yield of the samples. There was little strain induced by plasma-irradiated grafting on the surface of the polyethylene crystals. A method to determine the covalent grafting yield in the graft copolymer systems was developed. (C) 1995 John Wiley & Sons, Inc.
Resumo:
Mg65 Cu25 Gdlo bulk metallic glass and its carbon nanotube reinforced composite were prepared. Differential scanning calorimeter (DSC) was used to investigate the kinetics of glass transition and crystallization processes. The influence of CNTs addition to the glass matrix on the glass transition and crystallization kinetics was studied. It is shown that the kinetic effect on glass transition and crystallization are preserved for both the monothetic glass and its glass composite. Adding CNTs in to the glass matrix reduces the influence of the heating rate on the crystallization process. In addition, the CNTs increase the energetic barrier for the glass transition. This results in the decrease of GFA . The mechanism of the GFA decrease was also discussed.
Resumo:
The molar heat capacities of the two biphenyl liquid crystals, 3BmFF and 3BmFFXF3, with a purity of 99.7 mol% have been precisely measured by a fully automated precision adiabatic calorimeter in the temperature range between T = 80 and 350 K. Nematic phase-liquid phase transitions were found between T = 297 K and 300 K with a peak temperature of T-peak = (298.071 +/- 0.089) K for 3BmFF, and between T = 316 and 319 K with a peak temperature of T-peak = (315.543 +/- 0.043) K for 3BmFFXF3. The molar enthalpy (Delta(trs)H(m)) and entropy (Delta(trs)S(m)) corresponding to these phase transitions have been determined by means of the analysis of the heat capacity curves, which are (15.261 +/- 0.023) U mol(-1) and (51.202 +/- 0.076) J K-1 mol(-1) for 3BmFF, (31.624 +/- 0.066) kJ mol(-1) and (100.249 +/- 0.212) J K-1 mol(-1) for 3BmFFXF3, respectively. The real melting points (TI) and the ideal melting points (TO) with no impurities of the two compounds have been obtained from the fractional melting method to be (298.056 +/- 0.018) K and (298.165 +/- 0.038) K for 3BmFF, (315.585 +/- 0.043) K and (315.661 +/- 0.044) K for 3BmFFXF3, respectively. In addition, the transitions of these two biphenyl liquid crystals from nematic phase to liquid phase have further been investigated by differential scanning calorimeter (DSC) technique; the repeatability and reliability for these phase transitions were verified. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Molar heat capacities of ibuprofen were precisely measured with a small sample precision automated adiabatic calorimeter over the temperature range from 80 to 400 K. The polynomial functions of C-p,C-m (J K-1 mol(-1)) versus T were established on the heat capacity measurements by means of the least fitting square method. The functions are as follows: for solid ibuprofen, at the temperature range of 79.105 K less than or equal to T less than or equal to 333.297 K, C-p,C-m = 144.27 + 77.046X + 3.5171X(2) + 10.925X(3) + 11.224X(4), where X = (T - 206.201)/127.096; for liquid ibuprofen, at the temperature range of 353.406 K less than or equal to T less than or equal to 378.785 K, C-p,C-m = 325.79 + 8.9696X - 1.6073X(2) - 1.5145 X-3, where X = (T - 366.095)/12.690. A fusion transition at T = 348.02 K was found from the C-p-T curve. The molar enthalpy and entropy of the fusion transition were determined to be 26.65 kJ mol(-1) and 76.58 J mol(-1) K-1, respectively. The thermodynamic functions on the base of the reference temperature of 298.15 K, (H-T - H-298.15) and (S-T - S-298.15), were derived. Thermal characteristic of ibuprofen was studied by thermo-gravimetric analysis (TG-DTG) and differential scanning calorimeter (DSC). The temperature of fusion, the molar enthalpy and entropy of fusion obtained by DSC were well consistent with those obtained by adiabatic calorimeter. The evaporation process of ibuprofen was investigated further by TG and DTG, and the activation energy of the evaporation process was determined to be 80.3 +/- 1.4 kJ mol(-1). (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The sulphonated phenol novolac (PNBS) which was used as a curing agent of epoxy was synthesised from phenol novolac (PN) and 1,4-butane sultone and confirmed by FTIR and H-1 NMR. The degree of sulphonation (DS) in PNBS was calculated by H-1 NMR. The semi-IPN membranes composed of sulphonated tetramethyl poly(ether ether ketone) (STMPEEK) (the value of ion exchange capacity is 2.01 meq g(-1)), epoxy (TMBP) and PNBS were successfully prepared. The semi-IPN membranes showed high thermal properties which were measured by differential scanning calorimeter (DSC) and thermogravimetric analysis (TGA) With the introduction of the corss-linked TMBP/PNBS, the mechanical properties, dimensional stability, methanol resistance and oxidative stability of the membranes were improve in comparison to the pristine STMPEEK membrane.
Resumo:
The results obtained for poly(butylene succinate) (PBS) after Co-60 gamma-ray irradiation, studied by wide-angle X-ray diffraction (WAXD), differential scanning calorimeter (DSC) and polarizing optical microscopy (POM), revealed that the degree of crystallinity, melting temperature and enthalpy decreased with increasing irradiation dose, but that the crystal structure of PBS did not vary when compared to non-irradiated PBS. By using Scherrer equation, small changes occurred in the crystal sizes of L-020, L-110 and L-111. The spherulitic morphology of PBS was strongly dependent on irradiation dose and changed significantly at higher irradiation dosages. The crystallization kinetics of PBS indicated that the Avrami exponent (n) for irradiated PBS was reduced to 2.3, when compared to non-irradiated PBS (3.3).
Resumo:
The crystallization behavior of crystalline-crystalline diblock copolymer containing poly(ethylene oxide) (PEO) and poly(epsilon-caprolactone) (PCL), in which the weight fraction of PCL is 0.815, has been studied via differential scanning calorimeter (DSC), wide-angle X-ray diffraction (WAXD), and polarized optical microscopy (POM). DSC and WAXD indicated that both PEO and PCL blocks crystallize in the block copolymer. POM revealed a ring-banded spherulite morphology or the PEO-b-PCL diblock copolymer.
Resumo:
Fractionated crystallization behavior of dispersed PA6 phase in PP/PA6 blends compatibilized with PP-g-MAH was investigated by scanning electron microscopy (SEM), differential scanning calorimeter (DSC), polarized light microscopy (PLM), and wide-angle X-ray diffraction (WAXD) in this work. The lack of usual active heterogeneities in the dispersed droplet was the key factor for the fractionated crystallization of PA6. The crystals formed with less efficient nuclei might contain more defects in the crystal structures than those crystallized with the usual active nuclei. The lower the crystallization temperature, the lesser the perfection of the crystals and the lower crystallinity would be. The fractionated crystallization of PP droplets encapsulated by PA6 domains was also observed. The effect of existing PP-g-MAH-g-PA6 copolymer located at the interface on the fractionated crystallization could not be detected in this work.
Resumo:
A series of blue light-emitting poly(aryl ether)s (PAEs) containing ter- or pentafluorenes in the main chain have been synthesized via nucleophilic substitution polycondensation reaction. The energy levels of the polymers were tuned by introducing hole-transporting triaryamine groups in the side chains and/or incorporating electron-transporting oxadiazole segments in the main chain. The optical properties of the polymers are dominantly determined by the well-defined oligofluorene segments, and therefore all polymers show high photoluminescence quantum yield. Differential scanning calorimeter (DSC) characterizations indicate that they are vitrified polymers with high glass transition temperature (up to 156 degrees C). The polymers comprising pentafluorenes exhibit electroluminescent properties equal to or better than fully conjugated fluorene homopolymers. With the device structure of ITO/PEDOT:PSS/polymer/Ca/Al, an external quantum efficiency of 1.4% along with Commission Internationale de L'Eclairage (CIE) coordinates of (0.17, 0.09) has
Resumo:
Mg-20Gd(%, mass fraction) samples were prepared using melt-spinning and copper mold casting techniques. Microstructures and properties of the Mg-20Gd were investigated. Results show that the melt-spun ribbon is mainly composed of supersaturated alpha-Mg solid solution phase and the as-east ingot mainly contains alpha-Mg solid solution and Mg5Gd phase. The differential scanning calorimeter (DSC) curve of the ribbon exhibits a small exothermic peak in the temperature range from 630 to 680 K, which indicates that the ribbon contains a metastable phase (amorphous). Tensile strength at room temperature of the melt-spun ribbon and as-cast specimen are 308 and 254 MPa, respectively. The elongations of the two samples are less than 2%. The fracture surfaces demonstrate that the fracture mode of the as-cast Mg-20Gd is a typical cleavage fracture and that of the melt-spun sample is a combination of brittle fracture and ductile fracture.
Resumo:
Isothermal crystallization, subsequent melting behavior and non-isothermal crystallization of nylon 1212 samples have been investigated in the temperature range of 160-171 degreesC using a differential scanning calorimeter (DSC). Subsequent DSC scans of isothermally crystallized samples exhibited three melting endotherms. The commonly used Avrami equation and that modified by Jeziorny were used, respectively, to fit the primary stage of isothermal and non-isothermal crystallizations of nylon 1212. The Avrami exponent n was evaluated, and was found to be in the range of 1.56-2.03 for isothermal crystallization, and of 2.38-3.05 for non-isothermal crystallization. The activation energies (DeltaE) were determined to be 284.5 KJ/mol and 102.63 KJ/mol, respectively, for the isothermal and non-isothermal crystallization processes by the Arrhenius' and the Kissinger's methods.
Resumo:
Naphthalene-labeled polypropylene (PP) was prepared by melt reaction of maleic anhydride-grafted-polypropylene (PP-g-MA) with 1-aminonaphthalene in a Barabender mixer chamber. The structure of the product was analyzed with fourier transform infrared (FT-IR), ultraviolet (UV) and fluorescence. The results showed that naphthyl groups grafted onto the PP molecular chains through the imide bonds formed between MA and 1-aminonaphthalene. The content of the chromophores was 1.8 X 10(-4) mol g(-1) measured by elemental analysis. Isothermal crystallization behavior was studied by differential scanning calorimeter (DSC). Labeled PP had a higher crystallization rate than PP-g-MA. Wide-angle X-Ray diffraction (WAXD) analysis revealed that labeled PP had higher crystallinity than PP-g-MA.
Resumo:
Differential scanning calorimeter (DSC), wide-angle X-ray diffraction (WAXD), small-angle X-ray scattering (SAXS), and density techniques have been used to investigate the structural parameters of the solid state of Nylon 11 annealed at different temperatures. The equilibrium heat of fusion Delta H-m(0) and equilibrium melting temperature T-m(0) were estimated to be 189.05 J g(-1) and 202.85 degrees C respectively by using the Hoffman-Weeks approach. The degree of crystallinity (W-c,W-x) ranged approximately 24-42% was calculated by WAXD and compared with those by calorimetry (W-c,W-h) and density (W-c,W-d) measurements. The radius of gyration R-g, crystalline thickness L-c, noncrystalline thickness L-a, long period L, semiaxes of the particles (a, b), electron-density difference between the crystalline and noncrystalline regions eta(c) - eta(a), and the invariant Q increased with increasing annealing temperature. The analysis of the SAXS data was based upon the particle characteristic function and the one-dimensional electron-density correlation function. An interphase region existed between the crystalline and noncrystalline region with a clear dimension of about 2 nm for semicrystalline Nylon 11. Instead of the traditional two-phase model, a three-phase model has been proposed to explain these results by means of SAXS.
Resumo:
Poly(ethylene oxide) (PEO) and silica (SiO2) organic-inorganic hybrid materials have been synthesized by sol-gel approach. The crystallization behavior of PEO in silica networks has been investigated by differential scanning calorimeter (DSC) and scanning electron micrograph (SEM). The degree of PEO crystallinity in PEO/SiO2 hybrid networks reduces with the increase of SiO2. PEO is in amorphous state when the concentration of PEO is lower than 50 wt% in the hybrid materials. The melting points of PEO in the networks are lower than that of pure PEG, but the melting point of PEO in the networks almost has the same melting point. WAXD and SEM results show that the crystalline behavior of PEO in PEO/SiO2 hybrid system is sternly confined. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
The miscibility, crystallization behavior and morphological structure of PHB/PMA blends have been studied by the differential scanning calorimeter (DSC) and polarized optical microscopy (POM). The chemical repeat units of the two components of the blend are isomers. The results indicate that PHB and PMA are miscible in the melt. The addition of PMA into PHB results in a depression in the spherulite growth rate of PHB. With increasing PMA content in the blends, the texture of PHB spherulite becomes more open.