Resumo:
The inhibition effect of metal-free phthalocyanine (H2Pc), copper phthalocyanine (CuPc) and copper phthalocyanine tetrasulfuric tetrasodium salt (CuPc center dot S(4)center dot Na-4) on mild steel in I mol/l HCl in the concentration range of 1.0 X 10(-5) to 1.0 X 10(-3) mol/l was investigated by electrochemical test, scanning electron microscope with energy dispersive spectrometer (SEM/EDS) and quantum chemical method. The potentiodynamic polarization curves of mild steel in hydrochloric acid containing these compounds showed both cathodic and anodic processes of steel corrosion were suppressed, and the Nyquist plots of impedance expressed mainly as a capacitive loop with different compounds and concentrations. For all these phthalocyanines, the inhibition efficiency increased with the increase in inhibitor concentration, while the inhibition efficiencies for these three phthalocyanines with the same concentration decreased in the order Of CuPc center dot S(4)center dot Na-4 > CuPc > H2Pc according to the electrochemical measurement results. The SEM/EDS analysis indicated that there are more lightly corroded and oxidative steel surface for the specimens after immersion in acid solution containing 1.0 x 10(-3) mol/l phthalocyanines than that in blank. The quantum chemical calculation results showed that the inhibition efficiency of these phthalocyanines increased with decrease in molecule's LUMO energy, which was different from the micro-cyclic compounds. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The inhibiting effect and mechanism of 1-cyclopropyl-6-fluoro-1,4-dihydro-4-oxo-7-(1-piperazinyl)-3-quinoline carboxylicacid(ciprofloxacin), 1-ethyl-6-fluoro-1,4-dihydro-4-oxo-7-(1-piperazinyl)-3-quinoline carboxylic acid (norfloxacin) and (-)-(S)-9-fluoro-2,3-dihydro-3-methyl-10-(4-methyl-1-piperazinyl)-7-oxo-7 H-pyrido(1,2,3-de)-1,4-benzoxazine-6 carboxylic acid (ofloxacin) on the corrosion of mild steel in 1 mol/L HCl have been studied using electrochemical method, quantum chemical method and SEM at 303 K. The potentiodynamic results showed that these compounds suppressed both cathodic and anodic processes of mild steel corrosion in 1 mol/L HCl. The impedance spectroscopy showed that R-p values increased, and C-dl values decreased with the rising of the working concentration. Quantum chemical calculation showed that there was a positive correlation between some inhibitors structure properties and the inhibitory efficiency. The inhibitors function through adsorption followed Langmuir isotherm, and chemisorption made more contribution to the adsorption of the inhibitors on the steel surface compared with physical adsorption. SEM analysis suggested that the metal had been protected from aggressive corrosion because of the addition of the inhibitors.
Resumo:
Protozoan were collected from 16 stations in water system of Changde City (China) using the PFU method. Sampling programs were conduced on a yearly basis, with seasonal frequency at diverse sites in the water system and 488 species of protozoa was identified. At the same time, Water sampling from these stations was conducted and various water chemical parameters, including DO, COD, BOD5, NH3, TP, and Volatile Phenol, were analyzed. The aim of the research was, on one hand, using chemical method to take an investigation to the water pollution status of Changde City; on the other hand, using protozoan to make an evaluation to the water quality. With the chemical water parameters and protozoa data, a biotic index was derived for the investigated region. The species pollution value (SPV) of 469 protozoa species was established, and the community pollution value (CPV) calculated from SPV was used to evaluate water quality. The method of the biotic index was tested and the result showed that CPV calculated from SPV had a close correlation with the degree of water pollution (p < 0.00001). This indicated that the method of the biotic index is reliable. The water quality degrees divided by CPV were suggested. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Mn-doped ZnS nanocrystals of about 3 nm diameter were synthesized by a wet chemical method. X-ray diffraction (XRD) measurements showed that the nanocrystals have the structure of cubic zinc blende. The broadening of the XRD lines is indicative of nanomaterials. Room temperature photoluminescence (PL) spectrum of the undoped sample only exhibited a defected-related blue emission band. But for the doped samples, an orange emission from the Mn2+ T-4(1)-(6)A(1) transition was also observed, apart from the blue emission. The peak position (600 nm) of the Mn2+ emission was shifted to longer wavelength compared to that (584 nm) of bulk ZnS:Mn. With the increase of the Mn2+ concentration, the PL of ZnS:Mn was significantly enhanced. The concentration quenching effect was not observed in our experiments. Such PL phenomena were attributed to the absence of Mn2+ pairs in a single ZnS:Mn nanocrystal, considering the nonradiative energy transfer between Mn2+ ions based on the Poisson approximation. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Using a solution-based chemical method, we have prepared ZnS nanocrystals doped with high concentration of Mn2+. The X-ray diffraction analysis confirmed a zinc blende structure. The average size was about 3 nm. Photoluminescence spectrum showed room temperature emission in the visible spectrum, which consisted of the defect-related emission and the T-4(1)-(6)A(1) emission of Mn2+ ions. Compared with the undoped sample, the luminescence of the ZnS:Mn sample is enhanced by more than an order of magnitude, which indicated that the Mn2+ ions can efficiently boost the luminescence of ZnS nanocrystals.
Resumo:
The room-temperature photoluminescence (PL) of copper doped zinc sulfide (ZnS:Cu) nanoparticles were investigated. These ZnS:Cu nanoparticles were synthesized by a facile wet chemical method, with the copper concentration varying from 0 to 2 mol%. By Gaussian fitting, the PL spectrum of the undoped ZnS nanoparticles was deconvoluted into two blue luminescence peaks (centered at 411 nm and 455 nm, respectively), which both can be attributed to the recombination of the defect sates of ZnS. But for the doped samples, a third peak at about 500 nm was also identified. This green luminescence originates from the recombination between the shallow donor level (sulfur vacancy) and the t(2) level of Cu2+. With the increase of the CU2+ concentration, the green emission peak is systematically shifted to longer wavelength. In addition, it was found that the overall photoluminescence intensity is decreased at the Cu2+ concentration of 2%. The concentration quenching of the luminescence may be caused by the formation of CuS compound. (c) 2005 Elsevier B.V. All rights reserved.
Synthesis and temperature-dependent near-band-edge emission of chain-like Mg-doped ZnO nanoparticles
Resumo:
Chain-like Mg-doped ZnO nanoparticles were prepared using a wet chemical method combined with subsequent heat treatment. The blueshifted near-band-edge emission of the doped ZnO sample with respect to the undoped one was investigated by temperature-dependent photoluminescence. Based on the energy shift of the free-exciton transition, a band gap enlargement of similar to 83 meV was estimated, which seems to result in the equivalent shift of the bound-exciton transition. At 50 K, the transformation from the donor-acceptor-pair to free-to-acceptor emissions was observed for both the undoped and doped samples. The results show that Mg doping leads to the decrease of the acceptor binding energy. (c) 2006 American Institute of Physics.
Resumo:
造纸行业是造成我国水环境有机污染物的重要污染源之一,其水污染的特点是小厂多、草浆多、工艺落后、污染扩散面广、造成废 水排放量大,每年排放的废水量约39亿立方米,占全国工业废水排放量的1/6,其中有机污染物(以BOD5计)160万吨左右,约占全 国工业废水中有机污染物总量的1/4。尤以占全国制浆造纸行业90%以上的碱法草浆造纸厂的蒸煮黑液量大面广,除含有机物外,还 含有木质素、残碱、硫化物、氯化物等污染物,属于PH值高、色度深、难于治理的高浓度有机废水,对水体污染特别严重,各地要 求治理呼声很高,急待研究并尽快找出各种有效的治理途径。对于碱法草浆蒸煮,黑液高浓度废水的治理,有各种方法,根据国内 的研究进展和我们已有试验工作表明,最经济有效,具有实用价值,在生产上可获得成功是厌氧处理法。近10多年来,国外关于高 效厌氧处理技术研究进展迅速,并出现了多种多样的工艺设备,如高效厌氧生物反应器,并在实用化方面取得了很大成绩,建立了 生产性装置,达到了高负荷运行,效果良好。本试验是根据我们已有研究基础,针对我国国情,对小型制浆造纸厂水污染防治除了 开发碱回收及各种综合利用技术外,要特别加强废水(废液)实用技术研究的指导思想,本试验采用改进型的上流式厌氧污泥床反应 器,设计了两种试验方案,通过试验结果如下。1. 试验方案I—碱法草浆黑液酸化和厌氧发酵I号UASB反应器动态模型试验结果表 明:(1). 采用中温35℃±1℃高效厌氧反应器USAB内装有填料(陶粒)和三相分离器,具有保持高浓度生物量和防止污泥流失的特点 ,污泥浓度Vs 可达30%以上,因而具有高效、节能、产能、滞留期短的优点,当进水CODcr在7500-10000mg/l,HRT由7天缩短到3天 ,有机容积负荷在1.22gCODcr/l·d-3.43gCODcr/l·d时,CODcr平均去除率可达55%-45.5%,最高CODcr去除率可达60.2-63.5%, BOD5去除率可达75.9-83.2%,沼气容积产气率可达0.29-0.67l/l·d,每克CODcr转化为沼气产率达0.39-0.48l/gCODcr·d,CH4含量 65.8-75.5%。厌氧发酵出水再用化学法进行后处理脱除难降解的木质素,CODcr总去除率达80%以上。(2). 动态试验结果表明:采 用酸化—厌氧发酵处理黑液工艺合理,技术路线可行。2. 试验方案II—黑液用化学法(Hcl)去除木质素进行厌氧发酵,II号UASB反 应器动态模型试验结果表明:(1). 采用中温35℃±1℃高效厌氧反应器UASB(内有软填料),当进水CODcr7000-13000mg/l左右,HRT 由6天缩短到1天,有机负荷由0.98gCODcr/l·d增加到11gCODcr/l·d时,COD平均去除率均可稳定在70-77%,BOD5去除率为87.3- 93.1%,沼气容积产气率0.21-2.6l/l·d,每克CODcr转化为沼气产率为0.39-0.48l/gCODcr·d,高的可达0.53l/gCODcr·d,转化 率较高,CH4含量63-70%。(2). 试验证明碱法草浆黑液物化预处理—厌氧发酵处理的技术路线也是可行的,工艺合理、效果较好。 在有条件的工厂可采用。3.厌氧发酵阶段几大类群微生物计数表明:(1). 当发酵工艺和运行处于相对稳定状态时,微生物群体的 组成也达到相对的稳定,各类微生物之间保持动态平衡关系。当产乙酸菌的数量为107-108个/ml时,产甲烷菌的数量为105-106 个/ml,当产乙酸菌数量为106-107个/ml时,产甲烷菌的数量为103-105个/ml。(2).稳态运行条件下,黑液预处理为甲烷发酵创造 了有利的生态环境,获得了较好的处理效果和较高的COD转化为沼气的产率0.39-0.48l/g·CODcr·d,反应器中形成较为稳定而数 量较下水污泥中高1-2个数量级的厌氧发酵微生物区系组成。这一结果为黑液厌氧发酵提供了微生物理论依据。Paper industry is one of the important pollution source of water environment in our country. Its character of water pollution is many small factories, much grass pulp, disadvantageous technique, large preading area of pullution. Its effluent makes up 1/6 of whole country's industry wastwater. Its organic pollutant accounts 1/4 of whole country's. Alkaline grass paper pulp effluent with pollutants such as ligoin, remaining alkali sulfide, chloride besides organic material, is a kind of high concentrate organic wastewater which has high PH walug, dark colour and is difficult in treatment. There is urgent require to find ways to treat the wastewater. There are different ways to treat alkaline paper grass pulp effluent. According to the research advances and our experiment work, the most economical and useful way is anaerobic degradation which was advanced quick in last ten years. In the control of waste water of small pulp paper mill, the study of wastewater utilization technology should be emphasized, besides alkaline retrieving and different kinds of comprehensive utilization technology. Our experiment used modified UASB(Upflow Anaerobic Sludge Blanket Reactor). Two kinds of plan were disgned. The results are lined below. 1. The first experiment plant-aciding black pulp effluent and methanogenic digestion. The dynamic model experiment results of I-UASB reactor showed: (1)The mesophilic(35℃±1℃)high effect UASB reactor having haydite and threee state seperation in it had the character of keeping high bioimass concentration and preventing losss of sludge. It had advantages of high effect, energe saving, energe prodcing and short HRT(Hydroulic retention time). When the influent COD was 7500-10000mg, HRT was shortened from 7 days to 3days, organic loading rate was 1.22g-3.43COD/l· d, the average COD removal efficiency was 55%-45%. The highest COD efficiency was 60.2-63.5%, BOD removal of 75.9 -83.4% was achieved. Biogass production rate were up to 0.29-0.67l/l·d. Biogass converted efficiency from every gram of COD could reach 0.39-0.48l/gCOD·d. Methane content was 65.0-75.5%. Chemical method was used to deplate lignin in anaerobic digestion effluent. Total COD removal efficiency could be more than 80%. (2)Using aciding annaerobic digestion to treat the black effluent was reseanable in technique and technology. 2. The second experiment plan-anaerobic digestion was used after the chemical method was used to deplate lignin in the black effluent. The result of dynamic experiment of II-UASB reactor showed: (1)High effect mesophilic (35℃±1℃)UASB reactor having soft slaffing in was used. When influent COD was about 7000-13000mg/l, HRT was shortened from 6 days to 1 day and organic loading rate was increased from 0.90 to 11g COD /l·d, average COD removal efficiency remained stable on 70-77%. BOD, removal efficiency was between 87.3-93.1%. Biogass production rate was 0.2-2.6l/l ·d .Biogass converted efficiency from a gram of COD was 0.39-0.481/gCOD·d with the high value of 0.53l/gCOD·d. Methane content was 63-70%. (2)The way that using physical, chemical Pre-treatment-anaerobic digestion to treat alkaline black effluent is feasible and can be used in some factories when the condition exists. 3. Counting of several class of microoganisms in anaerobic digestion stage showed: (1)As the disgestion was in stable motion, the compositon of microorganic colony could get relative stable. Dynamic balance was remaining among different kinds of microorganism such as methanogenic bacteria, Acidogenic bacteria, sulfate reducing bacteria, and heterotrophic bacteria. (2)Under stable motion, the pre-treatment of black effluent produced favourable eco-enviroment for methanegenic digestion. Good treatment effect and high biogass convertent efficiency from COD(0.39-0.48l/g·COD· d)were gotten. Some stable and high quantity(10-100times more than sewage sludge)microorganism colony were formed in the reactor. This result provided theoretical basis for anaerobic digestion of black effluent.
Resumo:
In this study, varieties of lipid bilayer-protected gold nanoparticles (AuNPs) were synthesized through a simple wet chemical method, and then the effect of freeze-thawing on the as-prepared AuNPs was investigated. The freeze-thawing process induced fusion or fission of lipid bilayers tethered on the AuNPs. The UV-vis spectra and transmission electron microscopy experiments revealed that the disruption of lipid bilayer structures on the nanoparticles led to the fusion or aggregation of AuNPs.
Resumo:
A high-efficiency nanoelectrocatalyst based on high-density Au/Pt hybrid nanoparticles supported on a silica nanosphere (Au-Pt/SiO2) has been prepared by a facile wet chemical method. Scanning electron microscopy, transmission electron microscopy, energy-dispersive X-ray spectroscopy, and X-ray photoelectron spectroscopy are employed to characterize the obtained Au-Pt/SiO2. It was found that each hybrid nanosphere is composed of high-density small Au/Pt hybrid nanoparticles with rough surfaces. These small Au/Pt hybrid nanoparticles interconnect and form a porous nanostructure, which provides highly accessible activity sites, as required for high electrocatalytic activity. We suggest that the particular morphology of the AuPt/SiO2 may be the reason for the high catalytic activity. Thus, this hybrid nanomaterial may find a potential application in fuel cells.
Resumo:
Europium-doped Gd2O3 with an average size of similar to15 nm was coated on the surface of preformed silica nanospheres by the wet chemical method. SEM and TEM photographs showed that SiO2/Gd2O3:Eu core-shell submicrospheres are obtained. XRD patterns indicated that the Gd2O3:Eu shell is crystalline after heat treatment. FTIR and XPS spectra showed that the Gd2O3:Eu shell is linked to the silica surface by forming a Si-O-Gd bond. Photoluminescence studies showed that the luminescent properties are still retained after coating on an inert silica core; additionally, we noted that the emitting peaks are broadened, which results from size effects and interface effects of nanocrystal.
Resumo:
Natural bone is one kind of compounds consisting of hydroxyapatite (HAp) nano-rods, which are embedded in the template of collagen matrix in vivo with the same crystallographic organization. Herein HAp nano-rods precursors were synthesized via wet chemical method. Large-scale HAp nano-wires with the same crystallographic organization as the template of anodic aluminum oxide (AAO) were obtained by the electrophoretic deposition and the technology of the template. It provides a meaningful method to study and understand the information of biological molecules' mineralization process.
Resumo:
CeO2 nanoparticles hydrosol was synthesized by colloidal chemical method. The optimum experiment conditions for the preparation of CeO2 nanoparticles hydrosol were discussed. The effects of pH values, the reactant concentration and temperature on peptization process were studied. TEM photos showed that the CeO2 nanoparticles were spherical in shape and the size was about 3nm. Particle size distribution was in narrow range, and no agglomerates were observed. ED images indicated that the CeO2 nanoparticles were polycrystalline structure, and some of CeO2 were monocrystal particles.
Resumo:
Oxyapatite NaY9Si6O26 was prepared by sol-gel method. By choosing the precursors, a single phase compound was obtained. This soft chemical method lowered the reaction temperature by 100degreesC compared with the solid state method. Its morphology was studied by transmission electron microscopy (TEM). Several rare earth ions (Eu3+, Tb3+, Dy3+) and Pb2+ ion were doped in this compound. The high resolution emission spectrum of Eu3+ showed that rare earth ions occupied two yttrium sites. In spite of the charge imbalance of Pb2+ with the cations in this compound, it was found that Pb2+ could emit in UV range and transfer its excitation energy to Dy3+ ion.