The effect of thermally activated energy on the dislocation emission from a crack tip in BCC metal Mo is simulated in this paper. Based on the correlative reference model on which the flexible displacement boundary scheme is introduced naturally, the simulation shows that as temperature increases the critical stress intensity factor for the first dislocation emission will decrease and the total number of emitted dislocations increase for the same external load. The dislocation velocity and extensive distance among partial dislocations are not sensitive to temperature. After a dislocation emission, two different deformation slates are observed, the stable and unstable deformation states. In the stable deformation slate, the nucleated dislocation will emit from the crack tip and piles up at a distance far away from the crack tip, after that the new dislocation can not be nucleated unless the external loading increases. In the unstable deformation state, a number of dislocations can be emitted from the crack lip continuously under the same external load.
Resumo:
The deformation of alkali metals K, Rb, and Cs under epitaxial deformation is studied via the ab initio pseudopotential plane wave method using the local-density approximation. Under loading from the stable fee phase, metastable stares along directions [001], [111], and [201] are identified. One metastable state, presented at direction [201], has a very low symmetry in contrast to the planes [001] and [201]. Our results show that the softening direction and sequences of growth is significantly affected by the existence of the metastable states and magnitude of the energy barrier. The resulting softening sequences from soft to hard are [201], [110], [001], and [111] under biaxial compression and [001], [111], [201], and [110] under biaxial tension. An orthorhombic deformation path is used to investigate the fact, that the structure of the alkali films K and Cs evolve from the quasihexagonal structure into the (110)-oriented bcc structure, observed by experiments.
Resumo:
This work was supported by the 863 High Technology R&D Program of China (Grant Nos. 2007AA03Z402 and 2007AA03Z451), the Special Funds for Major State Basic Research Project (973 program) of China (Grant No. 2006CB604907), and the National Science Foundation of China (Grant Nos. 60506002 and 60776015). The authors express their appreciation to Dr. Tieying Yang and Prof. Huanhua Wang (Beijing Synchrotron Radiation Facility, Institute of High Energy Physics, Chinese Academy of Sciences) for XRD measurements and helpful discussions.
Resumo:
By in situ monitoring structural changes with the reflection spectrometer during the colloidal crystallization, we present direct experimental evidence of liquid-bcc-fcc phase transition in crystallization of charged colloidal particles, as a manifestation of the Ostwald's step rule. In addition, the lifetime of the bcc metastable structure in this system decreases significantly with increasing particle volume fraction, offering a possible explanation for "exceptions" to the step rule.
Resumo:
提出关联参照模型和随位错位置变化的柔性位移边界条件,提供了一个在固定位移边界条件下位错穿越边界的方法。应用三维分子动力学方法研究了体心立方(BCC)金属晶体钼理解尖发射位错的力学行为。
Resumo:
A correlative reference model for computer molecular dynamics simulations is proposed. Based on this model, a flexible displacement boundary scheme is introduced and the dislocations emitted from a crack tip can continuously pass through the border of the inner discrete atomic region and pile up at the outer continuum region. The effect of the emitted dislocations within the plastic zone on the inner atomistic region can be clearly demonstrated. The simulations for a molybdinum crystal show that a full dislocation in a bcc crystal is dissociated into three partial dislocations and interaction between the crack and the emitted dislocations results in gradual decrease of the local stress intensity factor.
Resumo:
We reported that work softening takes place during room-temperature rolling of nanocrystalline Ni at an equivalent strain of around 0.30. The work softening corresponds to a strain-induced phase transformation from a face-centered cubic (fcc) to a body-centered cubic (bcc) lattice. The hardness decreases with increasing volume fraction of the bcc phase. When the deformed samples are annealed at 423 K, a hardening of the samples takes place. This hardening by annealing can be attributed to a variety of factors including the recovery transformation from the bcc to the fcc phase, grain boundary relaxation, and retardation of dislocation gliding by microtwins.
Resumo:
Colloidal crystals formed by two types of polystyrene particles of different sizes (94 and 141 nm) at various number ratios (94:141 nm) are studied. Experiments showed that the formation time of crystals lengthens as the number ratio of the two components approaches 1:1. The dependence of the mean interparticle distance (D-0), crystal structure and alloy structure on the number ratio of the two types of particles was Studied by means of Kossel diffraction technique and reflection spectra. The results showed that as the number ratio decreased, the mean interparticle distance (D-0) became larger. And the colloidal crystal in binary mixtures is more preferably to form the bcc structure. This study found that binary systems form the substitutional solid solution (sss)-type alloy structure in all cases except when the number ratio of two types of particles is 5:1, which results instead in the superlattice structure. (C) 2008 Elsevier Inc. All rights reserved.
Resumo:
Based on detailed x-ray diffraction and transmission electron microscopy we have found body-centered-cubic (bcc) Ni upon room-temperature rolling of nanocrystalline (nc) face-centered-cubic (fcc) Ni. The bcc phase forms via the Kurdjumov-Sachs (KS) martensitic transformation mechanism when the von Mises equivalent strain exceeds similar to 0.3, much higher than accessible in tensile testing. The fcc and bcc phases keep either the KS or the Nishiyama-Wasserman orientation relationship. Our results provide insights into the deformation physics in nc Ni, namely, the fcc-to-bcc phase transformation can also accommodate plasticity at large plastic strains. (C) 2008 American Institute of Physics.
Resumo:
Based on the embedded atom method (EAM) proposed by Daw and Baskes and Johnson's model, this paper constructs a new N-body potential for bcc crystal Mo. The procedure of constructing the new N-body potential can be applied to other metals. The dislocation emission from a crack tip has been simulated successfully using molecular dynamics method, the result is in good agreement with the elastic solution.
Resumo:
Zr-based bulk metallic glass matrix composites with the composition of Zr56.2Ti13.8Nb5.0Cu6.9Ni5.6Be12.(5) were synthesized by the copper-mould suction casting and the Bridgman solidification. The composite, containing a well-developed flowery beta-Zr dendritic phase, was obtained by the Bridgman solidification with the withdrawal velocity of 0.8 mm/s and the temperature gradient of 45 K/mm, and the ultimate strength of 2050 MPa and fracture plastic strain of 14.6% of the composite were achieved, which was mainly interpreted by the homogeneous dispersion of bcc beta-Zr phase in the glass matrix. Crown Copyright (C) 2008 Published by Elsevier B.V. All rights reserved.
Resumo:
比较研究了鲫鱼异倍体细胞系(CAB-80)、团头鲂尾鳍细胞系(BCC)、大鳞副泥鳅雌核发育单倍体胚胎细胞系(PHG)、草鱼胚胎细胞系(GCE)、草鱼尾鳍细胞系(GCRF-2)、草鱼肾细胞系(GCK-84)及其四个克隆对草鱼呼肠孤病毒(GCRV)的敏感性。证实了这些细胞(PHG除外)在不同程度上对GCRV敏感,其中以GCK-84的敏感性最强。这表明,在体外培养条件下,GCRV并无严格的种族特异性。用经GCK-84传代的病毒感染草鱼种,能复制出典型的出血病症状。用GCK-84检测了病毒在GCK-84、GCRF
Resumo:
Fe films with the different thicknesses were grown on c(4x4) reconstructed GaAs (001) surfaces at low temperature by molecular-beam epitaxy. Well-ordered bcc structural Fe epitaxial films are confirmed by x-ray diffraction patterns and high-resolution cross-sectional transmission electron microscopy images. A large lattice expansion perpendicular to the surface in Fe film is observed. In-plane uniaxial magnetic anisotropy is determined by the difference between magnetizing energy along [110] and [110] directions, and the constant of interfacial uniaxial magnetic anisotropy is calculated to be 1.02x10(-4) J m(-2). We also find that magnetic anisotropy is not obviously influenced after in situ annealing, but in-plane strain is completely changed.
Resumo:
In this article, we give the electronic structure and optical transition matrix elements of coupled quantum dots (QDs) arranged as different cubic lattices: simple cubic (sc), body-centered cubic (bcc), and face-centered cubic (fcc) superlattices. The results indicate that electron and hole energies of bcc, sc, and fcc superlattices are the lowest, the highest, and the middle, respectively, for the same subband under the same QD density or under the same superlattice constant. For a fixed QD density, the confinement effects in sc, fcc, and bcc superlattices are the strongest, the middle, and the weakest, respectively. There are only one, two, and four confined energy bands, with energies lower than the potential barrier for sc, bcc, and fcc QD superlattices, respectively. The results have great significance for researching and making semiconductor quantum dot devices. (C) 1998 American Institute of Physics. [S0021-8979(98)02119-7]
Resumo:
本论文首先研究了Ni、Zr分别对Ti-V-Cr固溶体储氢合金中Cr和Ti部分取代的影响,得到了性能良好的Ti0.17Zr0.08V0.35Cr0.10Ni030基质合金。在此基础上进一步研究了入甄、B、Fe、Co、Al元素的添加或取代对基质合金的结构及电化学性能的影响。采用XRD、ICP、SEM一EDX、XPS、EIS、线性极化和阳极极化等表征手段对Ti一V-Cr固溶体储氢合金的结构及电化学性能进行分析和表征,主要结果如下:①Ti一V-Cr合金自身在碱性电解液中几乎无电化学活性。当用Ni部分取代Cr后,合金中出现具有电化学活性的第二相,其电化学性能得到有效地改善和提高。②Ti0.25-xZr_xV0.35Cr0.1Ni0.3(x=0.05-0.15)合金主要是由bcc相和c14Laves相组成。随Zr含量从0.05增加到0.08,合金电极的放电容量和倍率放电能力增加;当x继续从0.08增加到0.15时,其变化较小。合金电极的电荷转移电阻随x增加而降低,当x在0.08到0.15之间变化时,电荷转移电阻变化也比较小。表明电荷转移电阻的大小与合金的电化学性能密切相关。③经过50次充、放电循环后,Tio.17zr"sV时scrol0Ni03。合金电极在303K和313K的放电容量能保持在90%以上;在70℃时的放电容量仍能达到275mA扮g。根据不同温度时的交换电流密度,计算了Ti。,17Zr008V时SCr川0Ni030合金电极表面电化学反应的表观活化能,其值约为50kJ/mol。④通过Nln、B、Fe、C。、AI对Tio.17zroosvo35Crol0Nio3。合金基质的添加与取代的研究,得到了具有高容量的储氢合金。其中Tio.17Zr008Vo35Cro.10Ni020Mnol。合金室温最高放电容量达到390n1A扮g;在253一343K的温度范围内,Tiol7Zr08V035Cr0JONioz5Mnoos合金具有高的放电容量,其容量在167一298mA树g之间变化,但是这些合金的稳定性有待进一步的提高。⑤合金充、放电过程中,晶格的扭曲和膨胀、Zr和V的溶解使得合金结构发生变化;合金的严重粉化及表面致密氧化膜的形成,是导致Ti一V-Cr合金电化学性能的衰减的主要原因。