Resumo:
Nanostructured PbS with different morphologies and particle sizes have been prepared through a polyol process. Narrow size distribution for star-shaped, octahedral, tetradecanehedral, and cubic products were achieved by slowly introducing the source materials using a peristaltic pump in the presence of poly(vinylpyrrolidone) (PVP) as additive. Systematic variation of the kinetic factors, including the additive, the reaction temperature, the duration time, the ratio of source materials, the Sulfur sources, and the Pb(Ac)(2)center dot 3H(2)O concentration, reveals that the morphology depends mainly on the supersaturation degree of the free sulfur ions released from thiourea under elevated temperature.
Resumo:
The m-plane GaN films grown on LiAlO2(100) by metal-organic chemical vapor deposition exhibit anisotropic crystallographic properties. The Williamson-Hall plots point out they are due to the different tilts and lateral correlation lengths of mosaic blocks parallel and perpendicular to GaN[0001] in the growth plane. The symmetric and asymmetric reciprocal space maps reveal the strain of m-plane GaN to be biaxial in-plane compress epsilon(xx)=-0.79% and epsilon(zz)=-0.14% with an out-of-plane dilatation epsilon(yy)=0.38%. This anisotropic strain further separates the energy levels of top valence band at Gamma point. The energy splitting as 37 meV as well as in-plane polarization anisotropy for transitions are found by the polarized photoluminescence spectra at room temperature. (c) 2008 American Institute of Physics.
Resumo:
The crystalline, surface, and optical properties of the (10 (1) over bar(3) over bar) semipolar GaN directly grown on m-plane sapphire substrates by hydride vapor phase epitaxy (HVPE) were investigated. It was found that the increase of V/III ratio led to high quality (10 (1) over bar(3) over bar) oriented GaN epilayers with a morphology that may have been produced by step-flow growth and with minor evidence of anisotropic crystalline structure. After etching in the mixed acids, the inclined pyramids dominated the GaN surface with a density of 2 X 10(5) cm(-2), revealing the N-polarity characteristic. In the low-temperature PL spectra, weak BSF-related emission at 3.44eV could be observed as a shoulder of donor-bound exciton lines for the epilayer at high V/III ratio, which was indicative of obvious reduction of BSFs density. In comparison with other defect related emissions, a different quenching behavior was found for the 3.29 eV emission, characterized by the temperature-dependent PL measurement. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Sapphire substrates were nano-patterned by inductive coupled plasma etching process. Nonpolar a-plane GaN films were grown on planar and nano-patterned r-plane sapphire substrates by metal organic chemical vapor deposition. The anisotropic characteristic and the crystalline quality of the a-plane GaN films were studied through XRD rocking curves. The cross section and surface morphologies of the a-plane GaN films were studied using SEM and AFM measurements, respectively. The crystal quality and surface flatness of the nonpolar a-plane GaN were greatly improved through the usage of the nano-patterned r-plane sapphire substrates. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
National Natural Science Foundation of China 60836002 10674130 60521001;Major State Basic Research of China 2007CB924903;Chinese Academy of Sciences KJCX2.YW.W09-1
Resumo:
We presented a series of symmetric double crystal X-ray diffraction (DCXD) measurements, (0 0 4), (2 2 0) and (2 - 2 0) diffraction, to investigate the strain relaxation in an InAs film grown on a GaAs(0 0 1) substrate. The strain tensor and rotation tensor were calculated according to the DCXD results. It is found that the misfit strain is relaxed nearly completely and the strain relaxation caused a triclinic deformation in the epilayer. The lattice parameter along the [1 1 0] direction is a little longer than that along the [1 - 1 0] direction. Furthermore, a significant tilt, 0.2 degrees, towards the [1 1 0] direction while a very slight one: 0.002 degrees, towards [1 - 1 0] direction were discussed. This anisotropic strain relaxation is attributed to the asymmetric distribution of misfit dislocations, which is also indicated by the variation of the full-width at half-maximum (FWHM) of (0 0 4) diffraction along four azimuth angles. (C) 1998 Elsevier Science B.V. All rights reserved.