98 resultados para nature and quantum of damages


Relevância:

100.00% 100.00%

Publicador:

Resumo:

We introduce the concept of the Loschmidt echo (LE) to the space of the reduced density matrix of spin and fermionic systems to study the density matrix LEs (DMLEs) of the one-dimensional extended Hubbard model and the transverse field Ising model. Our results show that the DMLEs are remarkably influenced by the criticality of the system, and the method is a convenient way to study quantum phase transitions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report the growth of hexagonal ZnO nanorods and nanoflowers on GaN-based LED epiwafer using a solution deposition method. We also discuss the mechanisms of epitaxial nucleation and of the growth of ZnO nanorods and nanoflowers. A GaN-based LED epiwafer was first deposited on a sapphire substrate by MOCVD with no electrode being fabricated on it. Vertically aligned ZnO nanorods with an average height of similar to 2.4 mu m were then grown on the LED epiwafer, and nanoflowers were synthesized on the nanorods. The growth orientation of the nanorods was perpendicular to the surface, and the synthesized nanoflowers were composed of nanorods. The micro-Raman spectra of the ZnO nanorods and nanoflowers are similar and both exhibit the E-2 (high) mode and the second-order multiple-phonon mode. The photoluminescence spectrum of ZnO nanostructures exhibits ultraviolet emission centred at about 380 nm and a broad and enhanced green emission centred at about 526 nm. The green emission of the ZnO nanostructures combined with the emission of InGaN quantum wells provides a valuable method to improve the colour rendering index (CRI) of LEDs.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Deep level defects in as-grown and annealed n-type and semi-insulating InP have been studied. After annealing in phosphorus ambient, a large quantity of deep level defects were generated in both n-type and semi-insulating InP materials. In contrast, few deep level defects exist in InP after annealing in iron phosphide ambient. The generation of deep level defects has direct relation with in-diffusion of iron and phosphorus in the annealing process. The in-diffused phosphorus and iron atoms occupy indium sites in the lattice, resulting in the formation of P anti-site defects and iron deep acceptors, respectively. T e results indicate that iron atoms fully occupy indium sites and suppress the formation of indium vacancy and P anti-site, etc., whereas indium vacancies and P anti-site defects. are formed after annealing in phosphor-us ambient. The nature of the deep level defects in InP has been studied based on the results.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Zinc oxide flower-like bunches were directly synthesized on indium-doped tin oxide (ITO) glass substrates through a simple chemical bath deposition process. By adjusting precursor concentration, other morphologies ( spindles and rods) were also obtained. All of them are hexagonal and single crystalline in nature and grow along the [ 0001] crystallographic direction. The possible growth mechanisms for these nano- and microcrystals were proposed. It was revealed that both the inherent highly anisotropic structure of ZnO and the precursor concentration play crucial roles in determining final morphologies of the products. In addition, vibrational properties of ZnO crystals with different morphologies were investigated by Raman spectroscopy.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The growth of SiC epilayers on C-face (0 0 0 1) sapphire (alpha-Al2O3) has been performed using CVD method. We found that the quality of SiC epilayers has been improved through the nitridation of substrates by exposing them to ammonia ambient, as compared to growth on bare sapphire substrates. The single crystallinity of these layers was verified by XRD and double crystal XRD measurements. Atomic force microscopy was used to evaluate the surface morphology. Infrared reflectivity and Raman scattering measurement were carried out to investigate the phonon modes in the grown SiC. Detailed Raman analysis identified the 6H nature of the as-grown SiC films. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fourth-order spatial interference of entangled photon pairs generated in the process of spontaneous parametric down-conversion pumped by a femtosecond pulse laser has been performed for the first time. In theory, it takes into account the transverse correlation between the two photons and is used to calculate the dependence of the visibility of the interference pattern obtained in Young's double-slit experiment. In this experiment, a short focal length tens and two narrow band interference filters were adopted to eliminate the effects of the broadband pump laser and improve the visibility of the interference pattern under the condition of nearly collinear light and degenerate phase matching.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Indium antisite defect In-P-related photoluminescence has been observed in Fe-diffused semi-insulating (SI) InP. Compared to annealed undoped or Fe-predoped SI InP, there are fewer defects in SI InP obtained by long-duration, high-temperature Fe diffusion. The suppression of the formation of point defects in Fe-diffused SI InP can be explained in terms of the complete occupation by Fe at indium vacancy. The In-P defect is enhanced by the indium interstitial that is caused by the kick out of In and the substitution at the indium site of Fe in the diffusion process. Through these Fe-diffusion results, the nature of the defects in annealed undoped SI InP is better understood. (C) 2002 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Self-assembled Ge islands were grown on Si (1 0 0) substrate by Si2H6-Ge molecular beam epitaxy. Subjected to a chemical etching, it is found that the size and shape (i.e. ratio of height to base width) of Ge islands change with etching time. In addition, the photoluminescence from the etched Ge islands shifted to the higher energy side compared to that of the as-deposited Ge islands. Our results demonstrated that chemical etching can be a way to change the size and shape of the as-deposited islands as well as their luminescence property. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have studied the growth of GaInNAs/GaAs quantum well (QW) by molecular beam epitaxy using a DC plasma as the N sourer. The N concentration was independent of the As pressure and the In concentration, but inversely proportional to the growth rate. It was almost independent of T, over the range of 400-500 degreesC, but dropped rapidly when T-g exceeded 500 degreesC. Thermally-activated N surface segregation is considered to account for the strong falloff of the N concentration. As increasing N concentration, the steep absorption edge of the photovoltage spectra of GaInNAs/GaAs QW became gentle, the full-width at half-maximum of the photoluminescence (PL) peal; increased rapidly, and a so-called S-shaped temperature dependence of PL peak energy showed up. All these were attributed to the increasing localized state as N concentration. Ion-induced damage was one of the origins of the localized state. A rapid thermal annealing procedure could effectively remote the localized state. (C) 2001 Elsevier Science D.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Molecular beam epitaxy-grown self-assembled In(Ga)As/GaAs and InAs/InAlAs/InP quantum dots (QDs) and quantum wires (QWRs) have been studied. By adjusting growth conditions, surprising alignment. preferential elongation, and pronounced sequential coalescence of dots and wires under specific condition are realized. The lateral ordering of QDs and the vertical anti-correlation of QWRs are theoretically discussed. Room-temperature (RT) continuous-wave (CW) lasing at the wavelength of 960 nm with output power of 3.6 W from both uncoated facets is achieved fi-om vertical coupled InAs/GaAs QDs ensemble. The RT threshold current density is 218 A/cm(2). A RT CW output power of 0.6 W/facet ensures at least 3570 h lasing (only drops 0.83 dB). (C) 2001 Elsevier Science B.V, All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Systematic study of molecular beam epitaxy-grown self-assembled In(Ga)As/GaAs, In-AlAs/AlGaAs/GaAs, and InAs/InAlAs/InP quantum dots (QDs) is demonstrated. By adjusting growth conditions, surprising alignment, preferential elongation, and pronounced sequential coalescence of dots under the specific condition are realized. Room-temperature (RT) continuous-wave (CW) lasing at the wavelength of 960 nm with output power of 1 W is achieved from vertical coupled InAs/GaAs QDs ensemble. The RT threshold current density is 218 A/cm(2). An RT CW output power of 0.53 W ensures at least 3 000 h lasing (only drops 0.83 db). This is one of the best results ever reported.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Eu2+-doped ZnS nanoparticles with an average size of around 3 nm were prepared, and an emission band around 530 nm was observed. By heating in air at 150 degrees C, this emission decreased, while the typical sharp line emission of Eu3+ increased. This suggests that the emission around 530 nm is from intraion transition of Eu2+: In bulk ZnS:Eu2+, no intraion transition of Eu2+ was observed because the excited states of Eu2+ are degenerate with the continuum of the ZnS conduction band. We show that the band gap in ZnS:Eu2+ nanoparticles opens up due to quantum confinement, such that the conduction band of ZnS is higher than the first excited state of Eu2+, thus enabling the intraion transition of Eu2+ to occur.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The formation of triangular-shaped dot-like (TD) structures grown by molecular beam epitaxy on GaAs (311)A substrates patterned with square- and triangular-shaped holes is compared. On substrates patterned with square-shaped holes, TD structures are formed via the pinch-off of two symmetrically arranged {111} planes which develop freely in the regions between the holes on the original substrate surface, while the (111)A sidewalls of the as-etched holes develop a rough morphology during growth. The evolution of the rough ( 1 1 1)A sidewalls is eliminated on substrates patterned with triangular shaped holes resulting in similar TD structures with highly improved uniformity over the entire pattern. Spectrally and spatially resolved cathodoluminescence spectroscopy reveals the lateral variation of the quantum-well confinement energy in the TD structures generating distinct lateral energy barriers between the top portion and the nearby smooth regions with efficient radiative recombination. Formation of TD structures provides a new approach Do fabricate three-dimensionally confined nanostructures in a controlled manner.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Two strong photoluminescence (PL) bands in the spectral range of 550-900 nm have been observed at room temperature from a series of a-SiOx:H films fabricated by plasma-enhanced chemical vapor deposition (PECVD) technique. One is composed of a main band in the red-light region and a shoulder; the other is located at about 850 nm, only found after 1170 degrees C annealing in N-2 atmosphere. In conjunction with infrared (IR) and micro-Raman spectra, it is thought that the two PL bands are associated with a-Si clusters in the SiOx network and nanocrystalline silicon in SiO2, respectively.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

CdS nanoparticies were prepared in air and their stability by air annealing was studied. A small change in crystal structure and particle size was observed by air annealing, but a rapid reduction in fluorescence was found. Through investigation, it is revealed that it is the surface change or reconstruction rather than the variation of the size or structure that decreases the fluorescence. The emission of the particles consists with two peaks which are dependent on the excitation energy. The two peaks are considered to be arisen from "two" different sizes of nanoparticles and may be explained in terms of selectively excited photoluminescence. Finally we discuss why the discrete state of nanoparticles are able to be resolved in the photoluminescence excitation spectrum, but could not be differentiated in the absorption spectrum.