Composite sapphire/Ti:sapphire crystals for high-power laser application were grown by the hydrothermal method. The results of the X-ray rocking curve analysis indicate high crystalline quality of the surface Al2O3 material. The strong bonding between the overgrown Al2O3 and seed Ti:Al2O3 crystals is indispensable for withstanding high thermal stresses produced by intense optical pumping. The optical loss at the boundary of the composite crystal is considerably low, indicating the lack of scattering centers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Cerium-doped lutetium pyrosilicate crystal, Ce:Lu2Si2O7 (Ce:LPS), was grown by the Czochralski method. The segregation coefficient of Ce3+ ion was studied by the ICP-AES method. X-ray diffraction analysis showed that the structure of Ce:LPS crystal was monoclinic symmetry with space group of C2/m. Perfect cleavage planes (110) and imperfect cleavage planes (001) were observed by optical microscope. The reasons why it is difficult to grow crack-free crystals were studied. After optimized growth parameters, a Ce:LPS crystal with dimension of Phi 25 x 30 mm was grown, which is colorless, high optical quality, cracking-free and no inclusions. The transmittance of Ce:LPS crystal from 380 to 800 nm is over 82% and there is no observable absorption. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Homoepitaxial ZnO films have been grown via liquid-phase epitaxy (LPE) on (000 1) oriented ZnO substrates. X-ray rocking curve revealed the high quality of the ZnO films with a FWHM of 40 arc sec. Films of thickness about 20 gm were gown in the temperature range 700-720 degrees C. The growth rate of ZnO films was estimated to be 0.3 mu m h(-1). Atomic force microscope analysis showed that the surface roughness of ZnO films was very low, which further confirmed the high crystallinity of ZnO films. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
gamma-LiAlO2 single crystal was successfully grown by Czochralski method. The crystal quality was characterized by X-ray rocking curve and chemical etching. The effects of air-annealing and vapor transport equilibration (VTE) on the crystal quality, etch pits and absorption spectra of LiAlO2 were also investigated in detail. The results show that the as-grown crystal has very high quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec. Dislocation density in the middle part of the crystal is as low as about 3.0 x 10(3) cm(-2). The VTE-treated slice has larger FWHM value, etch pits density and absorption coefficient as compared with those of untreated and air-annealed slices, which indicates that the crystal quality became inferior after VTE treatment. (C) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Aluminum nitride (AlN) films were prepared on gamma-LiAlO2 substrates by radio frequency (rf) magnetron sputtering. The influence of substrate temperature (T-s) and nitrogen (N-2) concentration on film growth was investigated. The X-ray diffraction (XRD) results reveal that highly c-axis oriented AlN films can be obtained in the temperature range from room temperature (RT) to 300 degrees C. A smoother surface and a crystalline quality decrease with increasing N-2 concentration have been observed by XRD and atomic force microscopy (AFM) for the films deposited at lower substrate temperature. On the contrary, the degradation of the surface smoothness and the higher crystalline quality can be observed for the films deposited at a higher substrate temperature with N-2-rich ambient. The growth mechanism which leads to different crystalline quality of the films is discussed. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
In this work. an alpha-Al2O3:C crystal was directly grown by the temperature gradient technique (TGT) using Al2O3 and graphite powders as the raw materials. The optical, optically stimulated luminescence (OSL) properties and dosimetric characteristics of as-grown crystal were investigated. As-grown alpha-Al2O3:C crystal shows strong absorption band at 205, 230 and 256 nm. Three-dimensional thermoluminescence (TL) emission spectrum of the crystal shows a single emission peak at similar to 415 nm. The OSL decay curve can be fitted to two exponentials, the faster component and the slower component. The OSL response of the crystal shows a linear-sublinear-saturation characteristic. As-grown alpha-Al2O3:C crystal shows excellent linearity in the dose range from 5 x 10(-6) to 50 Gy. For doses higher than the saturation dose (100 Gy). the OSL sensitivity decreases as the dose increases. Crown Copyright (C) 2008 Published by Elsevier B.V. All rights reserved.
Resumo:
Vascular endothelial growth factor (VEGF) plays an important role in normal and pathological angiogenesis. VEGF receptors (VEGFRs, including VEGFR-1, VEGFR-2, and VEGFR-3) and neuropilins (NRPs, including NRP-1 and NRF-2) are high-affinity receptors for V
Resumo:
It has been demonstrated that growth hormone (GH) transgenic fish often posses a trait for fast growth. Here, we investigated the growth of F-4 'all-fish' GH transgenic carp Cyprinus carpio and their serum GH levels for a year. The results showed that F-4 all-fish GH transgenic carp were significantly larger in body mass (c. two-fold, P < 0 center dot 001) and body length (c. 1 center dot 3 fold, P < 0 center dot 001), compared with the non-transgenic group. The discrepancy of serum GH levels between the transgenic carp group and control group is 54 fold, when the water temperature was 12-34 degrees C. When the water temperature decreased to 3 center dot 5 degrees C in January, the discrepancy was 256 fold. The serum GH level of the transgenic group was relatively constant, while that of control varied greatly based on month and water temperature. The changes of growth rates between the transgenic group and the control group were similar for a year. Taken together, the results indicated that F-4 all-fish GH transgenic carp had not only higher and constant serum GH levels but also a significant fast-growing effect, compared with the control. To our knowledge, this is the first report on a one-year investigation of growth trait and serum growth hormone level in F-4 all-fish GH transgenic carp.
Resumo:
There were large losses of exotic species Elodea nuttallii during summer in eutrophic lakes of the middle and lower reaches of the Yanatze River, China. To investigate the main causes, the heat tolerance of E. nuttallii was studied and compared with that of native species Ceratopkyllum demersum by using an aquaria system in the laboratory. Under 4500 lx light intensity and 12-h L/12-h D cycle, E. nuttallii cultured in 1/5 Hoaglands solution at 39 degrees C showed a positive growth rate during the first 15 days, and the growth rate was higher than that at 35 degrees C. But after 15 days, the growth rates became negative for those cultured both at 39 and 35 degrees C. However, the growth rate was positive for more than 20 days for those cultured at 25 degrees C. Under the same conditions, the growth rate, productivity and chlorophyll content of E. nuttallii were significantly higher than that of C. demersum. Heat tolerance of E. nuttallii was also stronger than that of C. demersum. The optimal temperature for the growth of the two plants depended on the experimental period: both plants grew at an optimal rate at higher temperature if the experimental period was short; nevertheless the plants achieved optimal growth at a lower temperature if the experiment was conducted for a longer period. At the same light intensity, the heat tolerance of C. demersum in tap water with sediment was markedly stronger than that of E. nuttallii at 39 degrees C. Average growth rate of C. demersum was 4.5 times higher than that of E. nuttallii within 25 days. The positive growth period lasted for less than 25 days for E. nuttallii and for more than 25 days for C. demersum. When they were cultured in 1/5 Hoaglands solution and in tap water with sediment, the growth rate of C. demersum increased from 0.4 to 79.4 mg/d.g fresh weight (FW) within 20 days. E. nuttallii increased from 8.3 to 24.4 mg/d-g FW within 20 days. Both grew better in tap water with sediment than in 1/5 Hoaglands solution. The results demonstrated that the nutritional status of the water other than the high temperature affected the heat tolerance of E. nuttallii during summer. E. nuttallii has great ecological safe risk in China.
Resumo:
The influence of bicarbonate (HCO3-) on Microcystis aeruginosa FACHB 905 was assessed in this study. Growth curves, chlorophyll a fluorescence and ultrastructure were measured at two HCO3- concentrations, 2.3 mM and 12.4 mM. A treatment of sodium chloride (NaCl) was also conducted alongside to establish the influence level of sodium. It was found that upon treatment with elevated HCO3- concentrations of 2.3 mM and 12.4 mM, cell densities were 13% and 27% (respectively) higher than controls. In photosynthetic performance, elevated HCO3- concentration initially stimulated Fv/Fm at the prophase of culture and then subsequently inhibited it. The inhibition of 2.3mM was higher than that of 12.4mM HCO3-. The maximum relative electron transport rate (ETRmax) exhibited inhibition at elevated HCO3- concentrations. DI0/CS was decreased at 2.3 mM and increased at 12.4mM. In the case of both treatments. ABS/CSI TR0/CS, ET0/CS, RC/CS0 and RC/CSm were decreased by elevated HCO3- concentrations, which indicated damage to photosynthetic apparati and an inactivation of a fraction of reaction centers. This point was also proven by ultrastructural photos. High HCO3--exposed cells lost the characteristic photosynthetic membrane arrangement compared with the control and high salinity treated samples. At the 2.3mM concentration of HCO3-. damage to photosynthetic apparati caused decreased photosynthetic activity. These findings suggested that elevated HCO3- concentration stimulated the growth and photosynthesis of M. aeruginosa FACHB 905 in a short time. Exposure to high HCO3- concentrations for a longer period of time will damage photosynthetic apparatus. In addition, the ultrastructure indicated that elevated HCO3--concentration lead to photosynthetic apparati damage. In our experiment, it was observed that the inhibition effect of 2.3mM HCO3- was higher than that of 12.4mM HCO3-. We hypothesized that M. aeruginosa FACHB 905 induced a protective mechanism under high concentrations of HCO3-.
Resumo:
Potamogeton crispus is a cosmopolitan aquatic species and is widely used as a pioneer species for vegetation restoration of eutrophic lakes. However, many restoration projects applying P. crispus turions have not been successful. Earlier studies focused on effects of light and temperature on turion germination. The purpose of this study was to determine whether sediment anoxia and light interactively affected the turion germination and early growth of P. crispus. Anoxic conditions in the experiment were produced by adding sucrose to the sediment. The germination rate of the turions was 68-73% lower in the highly anoxic condition treatment than in the control. Medium light intensity (10% of natural light at the water surface) was more favorable for germination under slightly anoxic conditions than either low or high light intensity. The growth of newly-formed sprouts was also significantly inhibited by sediment anoxia. Photosynthesis and shoot biomass were reduced under sediment anoxia, whereas total chlorophyll content, root biomass, and soluble protein content were highest in the low anoxic condition treatment. Medium light improved net photosynthesis and biomass production of the sprouts. We conclude that turion germination and sprout growth can be significantly inhibited by sediment anoxia. Medium light intensity may alleviate this inhibition by anoxia, but light has little effect when sediment anoxia is severe. For the purposes of vegetation restoration, more attention should be paid to the role of sediment anoxia, and it is necessary to improve sediment and light conditions for turion germination and early growth of P. crispus in eutrophic lakes. These results will contribute to a more complete understanding of turion germination dynamics of P. crispus and will be useful for future restoration programs.
Resumo:
The effects of temperature and light on the growth and geosmin production of Lyngbya kuetzingii were determined. Of the three temperatures tested, 10, 25 and 35A degrees C, the maximal geosmin concentration and geosmin productivity were yielded at 10A degrees C, while the highest chl a production was observed at 25A degrees C. In the studies on light intensity, the maximal geosmin concentration and geosmin productivity were observed at 10 mu mol m(-2) s(-1), while the highest chl a production was at 20 mu mol m(-2) s(-1). It was suggested that more geosmin was synthesized with lower chl a demand. Meanwhile, the relative amounts of extra- and intracellular geosmin were investigated. Under optimum growth conditions (20 mu mol m(-2) s(-1), 25A degrees C; BG-11 medium), the amounts of extracellular geosmin increased as the growth progressed and reached the maximum in the stationary phase, while the intracellular geosmin reached its maximum value in the late exponential phase, and then began to decline. However, under the low temperature (10A degrees C) or light (10 mu mol m(-2) s(-1)) conditions, more intracellular geosmin was synthesized and mainly accumulated in the cells. The proportions of extracellular geosmin were high, to 33.33 and 32.27%, respectively, during the stationary phase at 35A degrees C and 20 mu mol m(-2) s(-1). It was indicated that low temperature or light could stimulate geosmin production and favor the accumulation of geosmin in cells, while more intracellular geosmin may be released into the medium at higher temperatures or optimum light intensity.