162 resultados para LD pump


Relevância:

20.00% 20.00%

Publicador:

Resumo:

An asymmetric MOSFET-C band-pass filter(BPF)with on chip charge pump auto-tuning is presented.It is implemented in UMC (United Manufacturing Corporation)0.18μm CMOS process technology. The filter system with auto-tuning uses a master-slave technique for continuous tuning in which the charge pump OUtputs 2.663 V, much higher than the power supply voltage, to improve the linearity of the filter. The main filter with third order low-pass and second order high-pass properties is an asymmetric band-pass filter with bandwidth of 2.730-5.340 MHz. The in-band third order harmonic input intercept point(HP3) is 16.621 dBm,wim 50 Ω as the source impedance. The input referred noise iS about 47.455μVrms. The main filter dissipates 3.528 mW while the auto-tuning system dissipates 2.412 mW from a 1.8 V power supply. The filter with the auto-tuning system occupies 0.592 mm~2 and it can be utilized in GPS (global positioning system)and Bluetooth systems.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The intensity-dependent two-photon absorption and nonlinear refraction coefficients of GaP optical crystal at 800 nm were measured with time-resolved femtosecond pump-probe technique. A nonlinear refraction coefficient of 1.7*10^(-17) m2/W and a two-photon absorption coefficient of 1.5*10^(-12) m/W of GaP crystal were obtained at a pump intensity of 3.5*10^(12) W/m2. The nonlinear refraction coefficient saturates at 3.5*10^(12) W/m2, while the two-photon absorption coefficient keeps linear increase at 6*10^(12) W/m2. Furthermore, fifth-order nonlinear refraction of the GaP optical crystal was revealed to occur above pump intensity of 3.5*10^(12) W/m2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports on the design, fabrication, and performance of an integrated electro-absorptive modulated laser based on butt-joint configuration for 10Gbit/s application. This paper mainly aims at two aspects. One is to improve the optical coupling between the laser and modulator; another is to increase the bandwidth of such devices by reducing the capacitance parameter of the modulator. The integrated devices exhibit high static and dynamic characteristics. Typical threshold current is 15mA,with some value as low as 8mA. Output power at 100mA is more than 10mW. The extinction characteristics,modulation bandwidth, and electrical return loss are measured. 3dB bandwidth more than 10GHz is monitored.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

介绍了抽运腔在半导体侧面抽运固体激光头中的应用.运用光线追迹的方法,从理论上分析了抽运腔对抽运光在晶体中的吸收效率和相对强度分布的影响,然后对无抽运腔、有抽运腔、抽运腔内表面经过镀金处理、抽运腔内表面经过抛光和镀金处理四种情况进行了实验研究.从理论模拟和实验结果中可以看出,抽运腔及其内表面的处理质量对激光头输入输出性能有很大的影响.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

介绍了一种二极管侧面泵浦激光头的新结构,用Nd:YAG晶体作为工作物质,将此结构下激光头的输入输出性能与传统结构下的输入输出性能进行了比较。此外利用这种新结构,对一种新型晶体Nd:GdVO4进行了实验,获得了连续1064nm的激光输出42.6W,最大光光效率为23.7%。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

介绍了一种二极管侧面泵浦的Nd:YAG连续激光器,采用了简单、实用的侧面泵浦结构,获得37.9W的连续1064 nm的激光多模输出;斜效率为31.5%,光效率为23.7%。文中还对该泵浦头的热透镜效应作了测试。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report an LD side-pumped continuous-wave passive mode-locked Nd:YAG laser with a Z-type folded cavity based on a semiconductor saturable absorber mirror (SESAM). The average output power 2.95 W of mode-locked laser with electro-optical conversion efficiency of 1.3% and high beam quality (M-x(2) = 1.25 and M-y(2) = 1.22) is achieved. The repetition rate of mode-locked pulse of 88 MHz with pulse energy of 34 nJ is obtained.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A packed-bed electroosmotic pump (EOP) was constructed and evaluated. The EOP consisted of three capillary columns packed in parallel, a gas-releasing device, Pt electrodes and a high-voltage power supply. The EOP could generate output pressure above 5.0 MPa and constant flow rate in the range of nl/min to a few mul/min for pure water, pure methanol, 2 mM potassium dihydrogenphosphate buffer, the buffer-methanol mixture and the pure water-methanol mixture at applied potentials less than 20 W The composition of solvent before/after pumping was quantitatively determined by using a gas chromatograph equipped with both flame ionization detector and thermal conductivity detector. It was found that there were no apparent changes in composition and relative concentrations after pumping process for a methanol-ethanol-acetonitrile mixture and a methanol-water mixture. Theoretical aspect of the EOP was discussed in detail. An capillary HPLC system consisting of the EOP, an injection valve, a 15 cm x 320 mum i.d., 5 mum Spherigel C(18) stainless steel analytical column, and an on-column UV detector was connected to evaluate the performance of the EOP. A comparative study was also carried out with a mechanical capillary HPLC pump on the same system. The results demonstrated that the reproducibility of flow rate and the pulsation-free flow property of the EOP are superior to that of mechanical pump in capillary HPLC application. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An electroosmotic pump (EOP) capable of generating pressure above 3 MPa and mul/min flow rate with reverse phase mobile phases of HPLC was constructed and evaluated. The pump consisted of three parallel connected fused silica capillary columns (25 cm x 320 mum I.D.) packed with 2 mum silica materials, hollow electrodes, a high voltage DC power supply, and. a liquid pressure transducer. The EOP was applied in a capillary liquid chromatographic system for mobile phase delivery instead of a mechanical pump. Standard samples containing thiourea, naphthalene, anthracene, phenanthrene and acetonitrile were separated on a 15 cm x 320 mum I.D. 5 mum Chromasil C-18 packed capillary column with acetonitrile/water as mobile phase. (C) 2003 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The multi-photon dissociative photoionization dynamics of CF3I has been studied with femtosecond two-color pump-probe time-of-flight mass spectra at a pump pulse of 265 nm and a probe pulse of 398 nn. This enables the A band and 5ppi(3)7ssigma((2)Pi(1/2)) Rydberg state to be accessed with the pump beam. The observed fast and slow decay components of CF3+ and I+ reflect the fast repulsive A band and some higher lying ion-pair states may be responsible for the decay of the 5ppi(3)7ssigma((2)Pi(1/2)) Rydberg state. The results provide information on the different multi-photon pathways producing these ions and the de-excitation mechanism of the 5ppi(3)7ssigma((2)Pi(1/2)) Rydberg state. (C) 2003 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Various analytical physical models are presented to extract the photodissociation dynamics information from the data obtained in the femtosecond pump-probe experiment. The single- and double-component models are employed to explain the single- and double-channel dissociation of parent molecules. Another single-component model for fragment dissociation or deexcitation is also presented. All cases are explanatorily demonstrated on the pump-probe experimental data.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work reports on the design and performance evaluation of a miniature direct methanol fuel cell(DMFC)integrated with an electro_osmotic(EO)pump for methanol delivery.Electro-osmotic pumps require minimal parasitic power while boasting no moving parts and simple fuel cell integration.Here ,aneletro-osmotic pump is realized from a commercially available porous glass frit.We characterize a custom-fabricated DMFC with a free convection cathode and coupled to an extennal electro-osmotic pump operated at applied potentials of 4.0,7.0,and 10V.Maximum gross power density of our free convection DMFC(operated at 50°)is 55 mW/cm2 using 4.0 mol/L concentration methanol solution supplied by the EO pump.Experimental results show that electro-osmotic pumps can deliver 2.0,4.0 and 8.0mol/L methanol/water mixtures to DMFCs while utilizing ~5.0% of the fuel cell power.Furthermore ,we discuss pertinent design considerations when using electro-osmotic pumps with DMFCs and areas of further study.