279 resultados para Deposition temperatures


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The glancing angle deposition (GLAD) technique was used to deposit ZnS films by electron beam evaporation method. The cross sectional scanning electron microscopy (SEM) image illustrated a highly orientated microstructure composed of slanted column. The atomic force microscopy (APM) analysis indicated that incident flux angle had significant effects on the nodule size and surface roughness. Under identical nominal thickness, the actual thickness of the GLAD films is related to the incident flux angle. The refractive index and in-plane birefringence of the GLAD ZnS films were discussed, and the maximum bireffingence Delta n = 0.036 was obtained at incident flux angle of alpha = 80 degrees. Therefore, the glancing angle deposition technique is a promising way to create a columnar structure with enhanced birefringent property. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 thin films were prepared on BK7 glass substrates by electron beam evaporation deposition method. The influence of deposition rate varying from 1.2 to 6.3 nm s(-1) on surface morphology and other properties of ZrO2 films were examined. With increasing deposition rate, the surface defect density increased. The decrease in half width at full maximum in X-ray diffraction pattern with deposition rate indicates an increase in crystal dimension with increasing deposition rate. Electron beam deposited ZrO2 films are known to be inhomogeneous. From the change of the peak transmittance value, it can be deduced that the inhomogeneity of ZrO2 films strengthened gradually with increasing deposition rate. The type of surface defects changed from nodules to craters when the deposition rate was high enough.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Glancing angle deposition is a novel method to prepare graded index coatings. By using this method and physical vapour deposition, ZrO2 is used to engineer graded index filter on BK7 glass substrate. Controlling the deposition rate and the periodic oscillation of oblique angle of deposited material, a 10-period graded index ZrO2 filter with high reflection near 532 nm and high transmittance at wavelength 1064 nm is fabricated. The causes of difference between the theoretical and experimental results are discussed in detail. The material properties and electron gun nonlinearity are possibly the main origins of the difference, which result in the variations in both thickness control and deposition rate of the Elm material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

HfO2 Elms are deposited on BK7 glass substrates by electron beam evaporation. The influences of annealing between 100 degrees C and 400 degrees C on residual stresses and structures of HfO2 films are studied. It is found that little differences of spectra, residual stresses and structures are obtained after annealing at lower temperatures. After annealing at higher temperatures, the spectra shift to short wavelength, the residual stress increases with the increasing annealing temperature. At the same time, the crystallite size increases and interplanar distance decreases. The variations of optical spectra and residual stress correspond to the evolutions of structures induced by annealing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 thin films are prepared on fused silica with conventional electron beam evaporation deposition. After annealed at different temperatures for 4h, the spectra and XRD patterns of the TiO2 thin film are obtained. Weak absorption of coatings is measured by the surface thermal lensing technique, and laser-induced damage threshold (LIDT) is determined. It is found that with the increasing annealing temperature, the transmittance of TiO2 films decreases. Especially when coatings are annealed at high temperature over 1173K, the optical loss is very serious. Weak absorption detection indicates that the absorption of coatings decreases firstly and then increases, and the absorption and defects play major roles in the LIDT of TiO2 thin films.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 films deposited by electron beam evaporation with glancing angle deposition (GLAD) technique were reported. The influence of flux angle on the surface morphology and the microstructure was investigated by scanning electron microscopy. The GLAD TiO2 films are anisotropy with highly orientated nanostructure of the slanted columns. With the increase of flux angle, refractive index and packing density decrease. This is caused by the shadowing effect dominating film growth. The anisotropic structure of TiO2 films results in optical birefringence, which reaches its maximum at the flux angle alpha = 65 degrees. The maximum birefringence of GLAD TiO2 films is higher than that of common bulk materials. It is suggested that glancing angle deposition may offer an effective method to obtain tailorable refractive index and birefringence in a large continuous range. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Single layers and antireflection films were deposited by electron beam evaporation, ion assisted deposition and interrupted ion assisted deposition, respectively. Antireflection film of quite high laser damage threshold (18J/cm(2)) deposited by interrupted ion assisted deposition were got. The electric field distribution, weak absorption, and residual stress of films and their relations to damage threshold were investigated. It was shown that the laser induced damage threshold of film was the result of competition of disadvantages and advantages, and interrupted ion assisted deposition was one of the valuable methods for preparing high laser induced damage threshold films. (c) 2007 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 thin films were prepared by electron beam evaporation at different oxygen partial pressures. The influences of oxygen partial pressure on structure and related properties of ZrO2 thin films were studied. Transmittance, thermal absorption, structure and residual stress of ZrO2 thin films were measured by spectrophotometer, surface thermal lensing technique (STL), X-ray diffraction and optical interferometer, respectively. The results showed that the structure and related properties varied progressively with the increase of oxygen partial pressure. The refractive indices and the packing densities of the thin films decreased when the oxygen partial pressure increased. The tetragonal phase fraction in the thin films decreased gradually as oxygen partial pressure increased. The residual stress of film deposited at base pressure was high compressive stress, the value decreased with the increase of oxygen partial pressure, and the residual stress became tensile with the further increase of oxygen pressure, which was corresponding to the evolution of packing densities and variation of interplanar distances. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZrO2 films were prepared by electron beam evaporation with glancing angle deposition (GLAD) technique. The as-deposition and annealed ZrO2 films are all amorphous, different from that deposited at normal incidence. Due to the shadowing effect, a highly orientated structure composed of slanted columns formed, and the obtained films became the mixture of slanted columns and voids. The relationship among the effective refractive index, packing density and flux incident angle was investigated. The refractive index and packing density of ZrO2 films decrease with the increase of the incident angle. The in-plane birefringence of GLAD ZrO2 films was calculated. At the packing density of 0.576, the maximum birefringence is 0.037. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

采用热舟蒸发方法沉积了氟化镁(MgF2)材料的单层膜,沉积温度从200℃上升到350℃,间隔为50℃。测量了样品的透射率和反射率光谱曲线,进行了表面粗糙度的标定,并在此基础上进行了光学损耗及散射损耗的计算。同时对355nm波长处的激光诱导损伤阈值进行了测量。结果表明:随着沉积温度的升高,光学损耗增加;在短波长范围散射损耗在光学损耗中所占比例很小,光学损耗的增加主要由吸收损耗引起;在355nm波长处的损伤阈值变化与吸收损耗的变化趋势相关,损伤机制主要是吸收起主导作用。样品的微缺陷密度也是影响损伤阈值的一个重要因素,损伤阈值随缺陷密度的增加而降低。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hot pressing (HP) at higher sintering temperature has been a traditional and prevalent technique for the fabrication of alpha-SiAlON. In order to prepare translucent SiAlON more easily, LiF was used as a non-oxide sintering additive to lower the sintering temperature to <= 1650 degrees C. As a result, all of the samples possessed a good hardness and fracture toughness. At the same time, the lower temperature sintered samples showed a higher optical transmittance in the range of 2.5-5.5 mu m wavelength (0.5 mm in thickness). The maximum infrared transmission reached 68% at a wavelength of 3.3 mu m. The present work shows that the sintering process has a strong effect on microstructure and property of alpha-SiAlON. To be exact, a lower sintering temperature and longer holding time can produce some fully-developed microstrcture, which is beneficial for the optical transmittance. (C) 2008 The Ceramic Society of Japan. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Antireflection coatings at the center wavelength of 1053 nm were prepared on BK7 glasses by electron-beam evaporation deposition (EBD) and ion beam assisted deposition (IBAD). Parts of the two kinds of samples were post-treated with oxygen plasma at the environment temperature after deposition. Absorption at 1064 nm was characterized based on surface thermal lensing (STL) technique. The laser-induced damage threshold (LIDT) was measured by a 1064-nm Nd:YAG laser with a pulse width of 38 ps. Leica-DMRXE Microscope was applied to gain damage morphologies of samples. The results revealed that oxygen post-treatment could lower the absorption and increase the damage thresholds for both kinds of as-grown samples. However, the improving effects are not the same. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nb2O5 sculptured thin. films deposited by electron beam evaporation with glancing angle deposition were prepared. Nb2O5 sculptured thin. films with tilted columns are optical anisotropy. XRD, SEM, UV-vis-NIR spectra are employed to characterize the microstructure and optical properties. The maximum of birefringence (Delta n) is up to 0.045 at alpha = 70 degrees with packing density of 0.487. With increasing the deposition angle, refractive index and packing density of Nb2O5 STF are decreasing. The relationship among deposition parameter, microstructure and optical properties was investigated in detail. (C) 2008 Elsevier B. V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

TiO2 single layers and TiO2/SiO2 high reflectors (HR) are prepared by electron beam evaporation at different TiO2 deposition rates. It is found that the changes of properties of TiO2 films with the increase of rate, such as the increase of refractive index and extinction coefficient and the decrease of physical thickness, lead to the spectrum shift and reflectivity bandwidth broadening of HR together with the increase of absorption and decrease of laser-induced damage threshold. The damages are found of different morphologies: a shallow pit to a seriously delaminated and deep crater, and the different amorphous-to-anatase-to-rutile phase transition processes detected by Raman study. The frequency shift of Raman vibration mode correlates with the strain in. film. Energy dispersive X-ray analysis reveals that impurities and non-stoichiometric defects are two absorption initiations resulting to the laser-induced transformation. (C) 2008 Elsevier B. V. All rights reserved.