58 resultados para yeast-to-hypha transition
Resumo:
We have investigated the effect of Shear flow on the formation of rill.-shaped ABA triblock copolymer (P4VP(43)-b-PS260-b-P4VP(43)) micelles. The results reveal that Shear flow Plays an important role in the formation of the rings Both ring size and its, distribution are found to be dependent sensitively on the stirring rate. Sizable rings are more likely to be formed at moderate stirring rate, Interestingly, the ring formation mechanism is also dependent oil the Shear flow. Copolymers are likely to form rings via end-to-end cylinder connection at low stirring rates, whereas they tend to form rings via the pathway of the rod-sphere-vesicle-ring it high stirring rates.
Resumo:
A new biocompatible film based on chitosan and poly(L-glutamic acid) (CS/PGA), created by alternate deposition of CS and PGA, was investigated. FT-IR spectroscopy, UV-vis spectroscopy and QCM were used to analyze the build-up process. The growth of CS and PGA deposition are both exponential to the deposition steps at first. After about 9 (CS/PGA) depositions, the exponential to linear transition takes place. QCM measurements combined with UV-vis spectra revealed the increase in the multilayer film growth at different pH (4.4, 5.0 and 5.5). The build-up of the multilayer stops after a few depositions at pH = 6.5. A muscle myoblast cell (C2C12) assay showed that (CS/PGA)(n) multilayer films obviously promote C2C12 attachment and growth.
Resumo:
We have studied the lamellar orientation in thin films of a model diblock copolymer, symmetric poly(styrene)-b-poly(L-lactide) (PS-PLLA), in the melt state on supported silicon wafer surface. In this system, while the PLLA block prefers to wet the polymer/substrate interface, the polymer/air as well as polymer/polymer interface is neutral for both blocks due to the similar surface energies of PS and PLLA in melt state. Our results demonstrate that the interplay of the interfaces during phase separation results in a series of structures before approaching the equilibrium state. Lamellar orientation of thin films with different initial film thicknesses at different annealing stages has been investigated using atomic force microscopy (AFM), transmission electronic microscopy (TEM), and X-ray photoelectron spectroscopy (XPS). It is found that in the early stage (annealing time t < 10 min), the polymer/substrate interface dominates the structure evolution, leading to a parallel lamellar structure with holes or islands formed depending on the initial film thickness. Later on, the neutral air interface becomes important and leads to a transition of lamellar orientation from parallel to perpendicular. It is interesting to see that for films with thickness h > 2L, where L is the bulk lamellar period, the lamellar orientation transition can occur independently in different parallel lamellar domains due to the neutrality of polymer/polymer interface.
Resumo:
The phase transition behavior of a thermotropic liquid crystalline poly(aryl ether ketone) synthesized by nucleophilic substitution reactions of 4,4'-biphenol (BP), and chlorohydroquinone (CH) with 1,4-bis(4-fluorobenzoyl)benzene (BF) has been investigated by differential scanning calorimetry (DSC) and wide angle X-ray diffraction (WAXD). The copolymer exhibits multiple first order phase transitions, which are associated with crystal-to-smectic liquid crystal transition and smectic liquid crystal-to-isotropic transition. When the cooling rate is low (<10
Resumo:
The shear-induced spiral-like morphology of a main-chain thermotropic liquid crystalline poly(aryl ether ketone) is observed and characterized by means of polarizing light microscopy, atomic force microscopy, transmission electron microscopy and electron diffraction techniques. The spiral-like texture is formed during shearing in the temperature range of liquid crystalline to isotropic transition (335-340 degreesC), and dispersed discontinuously in the mosaic matrix. Electron diffraction results indicate that the spiral exhibits orthorhombic lateral packing of the crystals and homeotropic alignment of the molecules. The spiral formation process and possible affecting factors are discussed.
Resumo:
The fracture behavior of ABS materials with a particle diameter of 110 nm and of 330 nm was studied using instrumented Charpy impact tests. The effects of rubber content and temperature on fracture behavior, deformation mode, stable crack extension, plastic zone size, J-integral value, and crack opening displacement were investigated. In the case of a particle size of 110 nm, the material was found to break in a brittle manner, and the dominant crack mechanism was unstable crack propagation. Fracture toughness increases with increasing rubber content. In the case of a particle size of 330 nm, brittle-to-tough transition was observed. The J-integral value first increases with rubber content, then levels off after the rubber content is greater than 16 wt %. The J-integral value of a particle diameter of 330 nm was found to be much greater than that of 110 nm. The J-integral value of both series first increased with increasing temperature until reaching the maximum value, after which it decreased with further increasing temperature. The conclusion is that a particle diameter of 330 nm is more efficient than that of 110 nm in toughening, but for both series the effectiveness of rubber modification decreases with increasing temperatures higher than 40 degreesC because of intrinsic craze formation in the SAN matrix at temperatures near the glass transition of SAN. (C) 2000 John Wiley & Sons, Inc.
Resumo:
A poly(methyloctadecylsilane) oligomer was synthesized by a typical Wurtz coupling reaction. Upon cooling, three transitions were observed at temperatures of 39.9, 37.5 and 33.9 degreesC at a rate of 2.5 degreesC/min in differential scanning calorimetry (DSC). The first transition, with enthalpy change of 0.47 kT/mol and supercooling of 0.2 degreesC, was characteristic of the conformational change in the Si-Si backbone into an all-trans conformation, which was detected by temperature-dependent Fourier transform infrared (FT-FR) spectroscopy. The second and the third transitions with large supercooling were identified as the formation of two-dimensional hexagonal crystal packing and three-dimensional two-chain orthorhombic crystal packing, respectively. The crystal structure was determined by the combination of WAXD and transmission electron microscopy (TEM) experiments. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
Formulas for decomposing of complex crystals to a sum of binary crystals are described and applied to the study of bond covalency in La1-xSrxFeO3 (0.0 less than or equal to x less than or equal to 0.9) and Ca1-xSrxMnO3 (0.0 less than or equal to x less than or equal to 0.5). The bond valence is treated by bond-valence sums scheme. The results indicate that, for both compounds, with the increasing doping level, the bond covalency and bond valence show the same trend, namely, larger bond covalency corresponds to higher bond valence. For La1-xSrxFeO3, with the increase of doping level, the bond covalency of La-O, Ca-O decreases in the orthorhombic (0.0 less than or equal to x less than or equal to 0.2) and rhombohedral (0.4 less than or equal to x less than or equal to 0.7) systems, then increases slightly for the cubic (0.8 less than or equal to x less than or equal to 0.9) system, but that of Fe-O increases for all crystal systems. A sharp decrease in bond covalency was observed where the crystal changes from orthorhombic to rhombohedral, while a smooth trend was seen for the rhombohedral-to-cubic transition. On the other hand, for orthorhombic Ca1-xSrxMnO3, the bond covalency of Ca-O, Sr-O, and Mn-O (4-coordinate site) decreases with the increasing doping level, that of Mn-O (2-coordinate site) increases.
Resumo:
The novel poly(aryl ether ketone)s were synthesized by nucleophilic substitution reactions of 4,4'-difluorobenzophenone with 4,4'-biphenyldiol and chlorohydroquinone. As expected, the copolymers have lower melting transitions than the biphenyldiol-based homopoly(aryl ether ketone) because of the copolymerization effect of the crystal-disrupting monomer chlorohydroquinone. Copolymers containing 50 and 70% biphenyldiol show two first-order transitions which are associated with the crystal-to-liquid crystal transition and the liquid crystal-to-isotropic transition.
Resumo:
Tension-tension fatigue tests were conducted on unnotched injection moulded poly(phenylene ether ketone) (PEK-C) specimens with two stress ratios, R. The fatigue behaviour of this material is described. The S-N curves (S = alternating stress, N = number of cycles to failure) for different R values have the same general shape, but the curve for bigger R is shifted to long cycles. A fatigue lifetime inversion is observed from constructed S-N curves. Examinations of failure surfaces and analyses of the fatigue data reveal that the fatigue failure mechanism of the material studied is crack growth dominated. But the manner of the fatigue crack initiation and propagation depends on the maximum cyclic stress applied. At higher stresses, the fatigue crack originates at the corner of the specimen and propagates inward; at lower stresses, the fatigue crack nucleates at an internal flaw of the specimen and propagates outward. The fatigue lifetime inversion corresponds to the transition of crack initiation and propagation from one mode to the other. Copyright (C) 1996 Elsevier Science Ltd.
Resumo:
Poly-o-methylaniline (poly-o-toluidine) was doped by some protonic acids. It was found that the acidity, molecular size and oxidizing ability of protonic acids affected the doping level and conductivity of polymer obtained to some extent. The organic acid
Resumo:
A mass of geological, geophysical and geochemical data and information from the Okinawa Trough area are collected for comprehensive research in the study area from East China to Okinawa Trough and then to Ryukyu Island Are region. According to the seismic tomography result (P and S wave) and the processing result of free-air and Bouguer gravity anomaly and magnetic anomaly data in the study area, the comprehensive interpretation is carried out. The Moho depth distribution of the study area is obtained by the inversion calculation based on gravity data using the Harmonious Series method. The crust properties are analyzed. Meantime, some Cenozoic basalt data from Kuandian (NE China), Hannuoba (North China), Minxi (South China), Penghu Islands (Taiwan Strait), Okinawa Trough and Japan Island Arc regions are chosen to make the comparison research on element- isotopes. The result indicates that the lithosphere thickness in the Okinawa Trough area has obviously decreased, where a Low -velocity layer of upper-mantle has reached the Moho interface and the metasometized asthenosphere has formed. The research result on element- isotopes shows that the characteristic of the crust in the Okinawa Trough area is different from that in East China area and the Ryukyu Island Arc area. It is considered that the crust in the Okinawa Trough area belongs to the transition type, which is quite similar to the feature of the oceanic crust.
Resumo:
Indexes of sediment grain size, sedimentation rates, geochemical composition, heavy minerals, benthic foraminiferal fauna, indicator species of the Kuroshio Current, paleo-SST and carbonate dissolution of core E017 conformably suggest a great marine environmental change occurring at about 10.1-9.2 cal. kaBP in the southern Okinawa Trough, which may correspond to the strengthening of the Kuroshio Warm Current and re-entering the Okinawa Trough through the sea area off northeast Taiwan. The invasion of Kuroshio current has experienced a process of gradual strengthening and then weakening, and its intensity became more fluctuation during the last 5000 years. Compared to the transition of sediment grain size, geochemical composition and heavy minerals, the foraminiferal faunas show a 900-year lag, which may indicate that the invasion of Kuroshio Current and the consequent sea surface and deep-water environmental changes is a gradual process, and fauna has an obvious lag compared to environment altering. The carbonate dissolution of the Okinawa Trough has had an apparent strengthening since 9.2 cal. kaBP, and reached a maximum in the late 3000 years, which may be caused by the deep-water environmental changes due to the invasion of Kuroshio Current.