180 resultados para atomic force spectroscopy
Resumo:
A new technique was developed for characterisation of stainless steel to intergramilar stress corrosion cracking by atomic force microscopy. The technique proved to be effective in sensitisation identification of AISI 304 stainless steel and might be promising in sensitisation identification of other stainless steels. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
We obtained a low density of coupled InAs/GaAs quantum dots (QDs) with an emission wavelength of around 1.3 mu m at room temperature. Atomic force microscopy and transmission electronic microscopy reveal that the dot size difference and the lateral displacement between the two dots are related to the spacer thickness. Spectroscopy of the coupled QD ensembles is considerably influenced by the spacer thickness.
Resumo:
For the InAs/GaAs quantum-dot system, the evolution of the wetting layer (WL) with the InAs deposition thickness has been studied by reflectance difference spectroscopy (RDS) in combination with atomic force microscopy and photoluminescence. One transition related to the light hole in the WL has been observed clearly in RDS, from which its transition energy and in-plane optical anisotropy (OA) are determined. The evolution of WL with the InAs dot formation and ripening has been discussed. In addition, the remarkable changes in OA at the onsets of the dot formation and ripening have been observed, implying the mode transitions of atom transport between the WL and the dots.
Resumo:
In this work, we have adopted reflectance difference spectroscopy to study the evolution of InAs layer grown at different temperatures in GaAs matrix. Associated with the two- to three-dimensional growth transition of InAs layer, the transition energies and the in-plane optical anisotropy of InAs wetting layer exhibit abrupt changes. This provides a new way to decide the critical thickness h(c) for the growth transition. The obtained h(c)s are compared with those determined by atomic force microscope measurement, and discrepancy is found at high temperatures. The origin of the difference is clarified and the variations in hc with temperature are further discussed. (C) 2010 American Institute of Physics. [doi:10.1063/1.3494043]
Resumo:
Several methods have been used for the measurement of the electronic decay constant (beta) of organic molecules. However, each of them has some disadvantages. For the first time, electrochemical impedance spectroscopy (EIS) was used to obtain the 18 value by measuring the tunneling resistance through alkanedithiols. The tunneling resistance through alkanedithiols increases exponentially with the molecular length in terms of the mechanism of coherent nonresonant tunneling. beta was 0.51 +/- 0.01 per carbon.
Resumo:
Aiming at understanding how a liquid film on a substrate affects the atomic force microscopic image in experiments, we present an analytical representation of the shape of liquid surface under van der Waals interaction induced by a non-contact probe tip. The analytical expression shows good consistence with the corresponding numerical results. According to the expression, we find that the vertical scale of the liquid dome is mainly governed by a combination of van der Waals force, surface tension and probe tip radius, and is weekly related to gravity. However, its horizontal extension is determined by the capillary length.
Resumo:
Mn ions were implanted to n-type Si(0 0 1) single crystal by low-energy ion beam deposition technique with an energy of 1000 eV and a dose of 7.5 x 10^{17} cm^{-2}. The samples were held at room temperature and at 300degreesC during implantation. Auger electron spectroscopy depth profiles of samples indicate that the Mn ions reach deeper in the sample implanted at 300degreesC than in the sample implanted at room temperature. X-ray diffraction measurements show that the structure of the sample implanted at room temperature is amorphous while that of the sample implanted at 300degreesC is crystallized. There are no new phases found except silicon both in the two samples. Atomic force microscopy images of samples indicate that the sample implanted at 300degreesC has island-like humps that cover the sample surface while there is no such kind of characteristic in the sample implanted at room temperature. The magnetic properties of samples were investigated by alternating gradient magnetometer (AGM). The sample implanted at 300degreesC shows ferromagnetic behavior at room temperature.
Resumo:
Gadolinium oxide thin films have been prepared on silicon (100) substrates with a low-energy dual ion-beam epitaxial technique. Substrate temperature was an important factor to affect the crystal structures and textures in an ion energy range of 100-500 eV. The films had a monoclinic Gd2O3 structure with preferred orientation ((4) over bar 02) at low substrate temperatures. When the substrate temperature was increased, the orientation turned to (202), and finally, the cubic structure appeared at the substrate temperature of 700 degreesC, which disagreed with the previous report because of the ion energy. The AES studies found that Gadolinium oxide shared Gd2O3 structures, although there were a lot of oxygen deficiencies in the films, and the XPS results confirmed this. AFM was also used to investigate the surface images of the samples. Finally, the electrical properties were presented. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Spin-coated films of nickel 1,6,10,15,19,24,28,33-octa-iso-pentyloxy-2,3-naphthalocyanine complex were obtained and characterized by UV-vis absorption spectroscopy. A linear relationship between the absorbance and solution concentration was observed. Low concentration solutions could afford smooth and homogeneous film surfaces as indicated by atomic force microscopy. The film structure was studied by small angle X-ray diffraction. The films were used for NO2 sensing experiments. The results indicate that the elevation of sensing temperature can shorten the response time and increase recovery ratio and response magnitude of the sensing films. High NO2 concentration can also shorten response time. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Two kinds of silanes, 3-glycidoxypropyltrimethoxysilane (GLYMO) and 3-trimethoxysililpropylmethacrylate (TMSPM), were used to prepare ormosil waveguide films by the sol-gel method. Thirty percent Ti(OBu)(4) and 70% silane were contained in the precursor sets. The properties of films were measured by scanning electron microscopy (SEM), Fourier transform infrared spectroscopy (FTIR), UV/VIS/NIR spectrophotometer (UV-vis), atomic force microscopy (AFM), m-line and scattering-detection method. The films from GLYMO and TMSPM precursors exhibit similar thickness (2.58 mu m for GLYMO, 2.51 mu m for TMSPM) and refractive index (1.5438 for GLYMO, 1.5392 for TMSPM, lambda=632.8 nm), but the film from TMSPM precursor has higher propagation loss (1.024 dB/cm, lambda=632.8 nm) than the film prepared from GLYMO (0.569 dB/cm, lambda=632.8 nm). Furthermore, the film prepared from TMSPM is easy to be opaque and cracks during coating whereas the same phenomenon was not found for the film prepared with GLYMO. It is confirmed that GLYMO is a better precursor than TMSPM for waveguide film preparation. (C) 2005 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
Sol-gel derived TiO2/SiO2/ormosil hybrid planar waveguides have been deposited on soda-lime glass slides and silicon substrates, films were heat treated at 150 degreesC for 2 h or dried at room temperature. Different amounts of water were added to sols to study their impacts on microstructures and optical properties of films. The samples were characterized by m-line spectroscopy, Fourier transform infrared spectroscopy (FT-IR), UV/VIS/NIR spectrophotometer (UV-vis), atomic force microscopy (AFM), thermal analysis instrument and scattering-detection method. The refractive index was found to have the largest value at the molar ratio H2O/OR = 1 in sol (OR means -OCH3, -OC2H5 and -OC4H9 in the sol), whereas the thickest film appears at H2O/OR = 1/2. The rms surface roughness of all the films is lower than 1.1 nm, and increases with the increase of water content in sol. Higher water content leads to higher attenuation of film. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
abstract = {TiO2/ormosil planar waveguide was prepared by sol-gel method at low thermal treatment temperature ( less than or equal 200°C). Scanning electron microscope, FT-IR spectrometer, spectrophotometer, atomic force microscopy, thermal analyzer, and dark m-line spectroscopy were used with the method of scattering-detection to investigate optical and structural properties. High optical quality waveguide film was obtained. The propagation loss of film was 0.569 dB/cm at a wavelength of 632.8 nm.
Resumo:
The influence of mechanical polishing, chemo-mechanical polishing (CMP), as well as CMP and subsequent chemical etching on the properties of sapphire substrate surfaces has been studied. The sapphire substrates have been investigated by means of polarizing microscopy, atomic force microscopy (AFM). X-ray diffraction rocking curves (XRCs) and micro-Raman spectroscopy. The results show that CMP with subsequent chemically etching yields the best-quality sapphire substrate surfaces. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Morphological defects in beta-barium borate (beta-BBO) thin films grown on Sr2+ -doped alpha-BBO substrates by liquid phase epitaxy (LPE) technique were studied by scanning electron micrograph (SEM), atomic force microscopy (AFM) and optical spectroscopy. The present results indicate that the main defects exit in beta-BBO thin films are microcracks and hollow structure. The formation of microcrack is due to the lattice mismatch and the difference of thermal expansion coefficients between substrate and film. The hollow structure might be caused during the combination of islands, which formed in the initial stage. (C) 2006 Elsevier GmbH. All rights reserved.
Resumo:
Nonpolar a-plane (1120) ZnO thin films have been fabricated on gamma-LiAlO2 (302) substrates via the low-pressure metal-organic chemical vapor deposition. An obvious intensity variation of the E-2 mode in the Raman spectra indicates that there exhibits in-plane optical anisotropy in the a-plane ZnO thin films. Highly-oriented uniform grains of rectangular shape can be seen from the atomic force microscopy images, which mean that the lateral growth rate of the thin films is also anisotropic. It is demonstrated experimentally that a buffer layer deposited at a low temperature (200 degrees C) can improve the structural and optical properties of the epilayer to a large extent. (c) 2007 Elsevier B.V. All rights reserved.