Resumo:
A new type of sulfonated clay (clay-SO3H) was prepared by the ion exchange method with the sulfanilic acid as the surfactant agent. The grafted amount of sulfanilic acid in clay-SO3H was 51.8 mequiv. (100 g)(-1), which was measured by thermogravimetric analysis (TGA). Sulfonated poly(ether ether ketone) (SPEEK)/clay-SO3H hybrid membranes which composed of SPEEK and different weight contents of clay-SO3H, were prepared by a solution casting and evaporation method. For comparison, the SPEEK/clay hybrid membranes were produced with the same method.
Resumo:
A novel method to tune surface wettability rapidly and reversibly has been developed by ion exchange of the counterions at the surface of a multilayer film assembled via electrostatic interaction.
Resumo:
We propose a simple but efficient, rapid, and quantitative ion-responsive micelle system based on counter-anion exchange of a surfactant with an imidazolium unit. The ion-exchange reaction results in the amphiphilic-to-hydrophobic transition of the imidazolium salt, leading to the destruction of the micelles, which has been successfully applied to control led release and emulsification.
Resumo:
We report a general method for incorporation of nanoparticles into polyelectrolyte multilayer (PEM) thin films by utilizing the excess charges and associated counterions present in the PEMs. Silver ions were introduced directly into multilayers assembled from poly(diallyldimethylammonium chloride) (PDDA) and poly(styrene sulfonate) (PSS), (PDDA/PSS)(n), by a rapid ion exchange process, which were then converted into silver nanoparticles via in situ reduction to create composite thin films. The size and the content of the nanoparticles in the film call be tuned by adjusting the ionic strength in the polyelectrolyte solutions used for the assembly. Spatial control over the distribution of the nanoparticles in the PEM was achieved via the use of multilayer heterostructure containing PDDA/PSS bilayer blocks assembled at different salt concentrations. Because excess charges and counterions are always present in any PEM, this approach can be applied to fabricate a wide variety of composite thin Films based on electrostatic self-assembly.
Resumo:
Counterions present at the surface of polyelectrolyte multilayers (PEMs) were utilized for modulation of surface wettability via ion exchange. The PEM film was dipped in aqueous solutions of different anions, respectively, and the water contact angle of the surface varied from about 10 degrees to 120 degrees, depending on the hydration characteristics of the anion. The ion exchange mechanism was verified by X-ray photoelectron spectroscopy. The process was rapid and reversible. Ionic strength of the polyelectrolyte solution used for preparing the PEMs was found to be crucial to the surface wetting properties and the reversibility and kinetics of the process, and the effects were correlated to the surface density of the excess charge and counterion. This work provides a general, facile and rapid approach of surface property modulation.
Resumo:
The organic-inorganic hybrid, PSS-silica composite material was developed for the immobilization of tris(2,2'-bipyridyl)ruthenium(II) (Ru(bpy)(3)(2+)) on glassy carbon electrode via ion-exchange (PSS stands for poly(sodium 4-styrene-sulfonate)). The electrochemiluminescence (ECL) and electrochemistry of Ru(bpy)(3)(2-) immobilized in the composite thin films have been investigated with tripropylamine (TPA) as the coreactant. The immobilized Ru(bpy)(3)(2-) underwent a surface process. The modified electrode was used for the ECL detection of TPA and showed high sensitivity. Detection limit was 0,1 mumol L-1 for TPA (S/N = 3) with a linear range from 0.5 mumol L-1 to 5 mmol L-1 (R = 0.998), Moreover, the resulting modified electrode was stable over six months and the good stability may be due to the strong interaction between Ru(bpy)(3)(2-) and the high ion-exchange able PSS-silica composite films on GCE. Compared with other materials. the PSS-silica composite films containing incorporated Ru(bpy)(3)(2-) showed improved sensitivity and long-term stability, Thus, such composite thin film can be a promising material for the construction of ECL sensor.
Resumo:
The lipid layer membranes were fabricated on the glassy carbon electrode (GC) and demonstrated to be bilayer lipid membranes by impedance spectroscopy. The formation of incorporated poly L-glutamate bilayer lipid membrane was achieved. The ion channel behavior of the incorporated poly L-glutamate membrane was determined. When the stimulus calcium cations were added into the electrolyte, the ion channel was opened immediately and exhibited distinct channel current. Otherwise, the ion channel was closed. The cyclic voltammogram at the GC electrode coated with incorporated poly L-glutamate DMPC film response to calcium ion is very fast compared with that at the GC electrode coated only with DMPC film. Ion channel current is not dependent on the time but on the concentration of calcium. The mechanism of the ion channel formation was investigated.
Resumo:
The stability constants of M-L binary system and M-L-L' (M = La3+ similar to Yb3+, Y3+ and Ca2+; L= DL-malic aicd, L' = L-hydroxyproline) ternary system were determined by pH-(0)-tentiometric method under the simulating physiological condition(37 degrees C, I=0.15 mol/L NaCl). The complex species MpLqLr'H-s(abbr as pqrs) in the sytems were ascertained by program COMPLEX. The results show that there are three species(1101, 1100 and 1200) in M-L binary system and one species(1010) in M-L' binary system. In addition to the above four species, a new species, 1112 was found in the M-L-L' ternary system, which is the only species of mixed ligands. Rare earth ions form more stable complexes than calcium ion does and the stability differences between their complexes in the ternary system are less than that in the binary system. The distributions of all the species in La-L-L' ternary system vs pH are discussed.
Resumo:
For nearly three decades, organogermanium compounds have become increasingly of interest owing to their extensive physiological and pharmaceutical activity. In this paper, two new high performance ion chromatographic methods for separation and determination of three kinds of organogermanium compounds beta-carboxyethylgermanium sesquioxide (I), beta-(alpha-methyl)-carboxyethylgermanium sesquioxide (II) and d-(beta-carboxyethyl)germanium hydroxide (III) were proposed. A Dionex DX-300 ion chromatograph equipped with a Dionex FED-II pulsed electrochemical detector (conductivity mode), and a Dionex AI-450 chromatography workstation was employed. The separation was achieved by using ion-exchange or ion-exclusion mechanism. The detection limits(S/N=3, expressed as germanium) for the three compounds were all below sub- mu g/mL level. The methods have been applied to the analysis of tonic oral drinks, and the average recoveries for the three compounds range from 95 - 108%. The results obtained were in agreement with those of hydride generation atomic fluorescence spectrometry (HG-AFS).
Resumo:
The hetero atom substituted aluminophosphate molecular sieves Me-VPI-5(Me = Mgt Ti, Sn, Si) were synthesized hydrothermally. Rare earth ions are originally doped into these microporous materials by aqueous solution ion exchange procedures. The phase transitions of the microporous materials are investigated by high-temperature and high-pressure experimental techniques. The influence of the phase transitions on the rare earth ions' spectral structures is discussed, With the increase of temperature, Eu(II)Mg-VPI-5 is converted into Eu(II)Mg-AIPO(4)-8, then into tridymite phase. The pressure has a notable influence on Eu(II) ion's spectral structures. The spectral structures have changed regularly with the increase of pressure.
Resumo:
Separation of the acidic compounds in the ion-exchange capillary electrochromatograph (IE-CEC) with strong anion-exchange packing as the stationary phase was studied. It was observed that the electroosmotic flow (EOF) in strong anion-exchange CEC moderately changed with increase of the eluent ionic strength and decrease of the eluent pH, but the acetonitrile concentration in the eluent had almost no effect on the EOF. The EOF in Strong anion-exchange CEC with eluent of low pH value was much larger than that in RP-CEC with Spherisorb-ODS as the stationary phase. The retention of acidic compounds on the strong anion-exchange packing was relatively weak due to only partial ionization of them, and both chromatographic and electrophoretic processes contributed to separation. It was observed that the retention values of acidic compounds decreased with the increase of phosphate buffer and acetonitrile concentration in the eluent as well as the decrease of the applied voltage, and even the acidic compounds could elute before the void time. These factors also made an important contribution to the separation selectivity for tested acidic compounds, which could be separated rapidly with high column efficiency of more than 220 000 plates/m under the optimized separation conditions. (C) 2000 Elsevier Science BN. All rights reserved.
Resumo:
Separation of small peptides on ion-exchange capillary electrochromatography (IE-CEC) with strong cation-exchange packing (SCX) as stationary phase was investigated. It was observed that the number of theoretical plates for small peptides varied from 240 000 to 460 000/m, and the relative standard deviation for t(0) and the migration time of peptides were less than 0.57% and 0.27%, respectively for ten consecutive runs. Unusually high column efficiency has been explained by the capillary electrophoretic stacking and chromatofocusing phenomena during the injection and separation of positively charged peptides. The sample buffer concentration had a marked effect on the column efficiency and peak area of the retained peptides. The influences of the buffer concentration and pH value as well as the applied voltage on the separation were investigated. It has been shown that the electrostatic interaction between the positively charged peptides and the SCX stationary phase played a very important role in IE-CEC, which provided the different separation selectivity from those in the capillary electrophoresis and reversed-phase liquid chromatography. A fast separation of ten peptides in less than 3.5 min on IE-CEC by adoption of the highly applied voltage was demonstrated. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
采用AgNO3和KNO3混和熔盐作为离子交换源,在K9玻璃上制备了跑道形波导谐振腔滤波器。利用ASE宽带光源和光谱仪对器件特性进行了测试,得到的该滤波器自由光谱范围为0.176nm。对比对Cr=4dB和3dB带宽δλ=0.13nm来说,耦合系数和传输损耗分别为κ=0.9和α=3.2dB/cm。测试了环形腔的热光调相特性,在16℃的变化范围内实现了2π的相移。通过分析,波导材料的热光系数约为1.49×10^-5/C。该滤波器不仅可用于滤波、传感等领域,而且也可与其它波导结构相结合实现新的功能。
Resumo:
介绍了采用光刻离子交换工艺制作平面交叉型微透镜阵列的方法。利用积分形式的光线方程式讨论了平面交叉型微透镜的近轴光学特性,研究了微透镜的光线轨迹方程式和一些重要的近轴成像特性,利用ABCD定理得到了平面交叉型微透镜像距、焦距、像高、横向放大率和主平面位置的数学表达式,焦距的理论计算结果和实验数据吻合得很好。
Resumo:
对离子交换波导制备过程中掺铒磷酸盐玻璃表面的侵蚀问题进行了研究,分析了产生侵蚀的原因,提出镀K9玻璃薄膜的方法,对掺铒磷酸盐玻璃表面进行保护.采用光学显微镜和原子力显微镜对波导表面特性进行了表征。同时对平板波导的光学特性进行了测试.研究表明K9玻璃薄膜不仅能够对掺铒磷酸盐玻璃起到保护作用,同时允许交换离子透过进入磷酸盐玻璃形成波导层.