High-quality compressively strained In0.63Ga0.37As/InP quantum wells with different well widths (1-11 nm) have been grown coherently on InP substrates using a home-made gas source molecular beam epitaxy (GSMBE) system. The indium composition in the wells of the sample was determined by means of high-resolution X-ray diffraction and its computer simulation. it is found that the exciton transition energies determined by photoluminescence (PL) at 10 K are in good agreement with those calculated using a deformation potential model. Sharp and intense peaks for each well can be well resolved in the 10 K PL spectra. For wells narrower than 4 nm, the line width of the PL peaks are smaller than the theoretical values of the line-width broadening due to 1 hit interface fluctuation, showing that the interface fluctuation of our sample is within 1 ML. For wells of 7 and 9 nm, the PL peak widths are as low as 4.5 meV.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An asymmetrically coupled (GaAs/AlAs/GaAs/AlAs)/GaAs (001) double-well supperlattice is studied by HRDCD (high resolution double-crystal X-ray diffractometry). The intensity of satellite peaks is modulated by wave packet of different sublayers. In the course of simulation, the satellite peaks in the vicinity of the node points of wave packet are very informative for precise determination of sublayer thickness and for improving accuracy.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Low-temperature photoluminescence and excitation spectra from InAs monolayer quantum structures, grown on (311)A, (311)B, and (100) GaAs substrates, are investigated, The structures were grown simultaneously by conventional molecular-beam epitaxy (MBE), The experimental results show that the quality of InAs monolayer on (311)B GaAs substrate is obviously better in crystal quality than those on the two other oriented GaAs substrates. In addition, the transition peaks of the InAs layer grown on (311) GaAs substrates shift to higher energy with respect to that from the InAs layer grown on (100) GaAs substrate.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The electronic states and optical transition properties of three semiconductor wires Si? GaAs, and ZnSe are studied by the empirical pseudopotential homojunction model. The energy levels, wave functions, optical transition matrix elements, and lifetimes are obtained for wires of square cross section with width from 2 to 5 (root 2a/2), where a is the lattice constant. It is found that these three kinds of wires have different quantum confinement properties. For Si wires, the energy gap is pseudodirect, and the wave function of the electronic ground state consists mainly of four bulk Delta states. The optical transition matrix elements are much smaller than that of a direct transition, and increase with decreasing wire width. Where the width of wire is 7.7 Angstrom, the Si wire changes from an indirect energy gap to a direct energy gap due to mixing of the bulk Gamma(15) state. For GaAs wires. the energy gap is also pseudodirect in the width range considered, but the optical transition matrix elements are larger than those of Si wires by two orders of magnitude for the same width. However, there is no transfer to a direct energy gap as the wire width decreases. For ZnSe wires, the energy gap is always direct, and the optical transition matrix elements are comparable to those of the direct energy gap bulk semiconductors. They decrease with decreasing wire width due to mixing of the bulk Gamma(1) state with other states. All quantum confinement properties are discussed and explained by our theoretical model and the semiconductor energy band structures derived. The calculated lifetimes of the Si wire, and the positions of photoluminescence peaks, are in good agreement with experimental results.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The photoluminescence (PL) properties of ZnSe films grown by hot wall epitaxy are reported. The PL spectra show clear neutral donor-bound exciton peak; donor acceptor pair (DAP) peak, conduction band to acceptor (CA) peak, and their phonon replicas until fourth order. The conduction band to acceptor peak and it's phonon replicas exist until room temperature. From the ratio of PL intensities of DAP and CA peaks and their replicas, we obtain the Huang-Rhys factor S = 0.58, in agreement with other experiments for acceptor-bound exciton transitions. From the temperature dependence of PL intensities we derive the activation energy of thermal quenching process for the DAP transitions as about 7 meV.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The one-dimensional energy bands and corresponding conductivities of a T-shaped quantum-dot superlattice are studied in various cases: different periods, with potential barriers between dots, and in transverse electric fields. It is found that the conductivity of the superlattices has a similar energy relation to the conductance of a single quantum dot, but vanishes in the energy gap region. The energy band of a superlattice with periodically modulated conducting width in the perpendicular magnetic field is calculated for comparison with magneto-transport experiments. It is found that due to the edge state effect the electron has strong quantum transport features. The energy gaps change with the width of the channel, corresponding to the deep peaks in the conductance curve. This method of calculating the energy bands of quantum-dot superlattices is applicable to complex geometric structures without substantial difficulty. (C) 1997 American Institute of Physics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this work we investigate the structural properties of symmetrically strained (GaIn)As/GaAs/Ga(PAs)/GaAs superlattices by means of x-ray diffraction, reciprocal-space mapping, and x-ray reflectivity. The multilayers were grown by metalorganic vapor-phase epitaxy on (001) GaAs substrates intentionally off-oriented towards one of the nearest [110] directions. High-resolution triple-crystal reciprocal-space maps recorded for different azimuth angles in the vicinity of the (004) Bragg diffraction clearly show a double periodicity of the x-ray peak intensity that can be ascribed to a lateral and a vertical periodicity occurring parallel and perpendicular to the growth surface. Moreover, from the intensity modulation of the satellite peaks, a lateral-strain gradient within the epilayer unit cell is found, varying from a tensile to a compressive strain. Thus, the substrate off-orientation promotes a lateral modulation of the layer thickness (ordered interface roughness) and of the lattice strain, giving rise to laterally ordered macrosteps. In this respect, contour maps of the specular reflected beam in the vicinity of the (000) reciprocal lattice point were recorded in order to inspect the vertical and lateral interface roughness correlation, A semiquantitative analysis of our results shows that the interface morphology and roughness is greatly influenced by the off-orientation angle and the lateral strain distribution. Two mean spatial wavelengths can be determined, one corresponding exactly to the macrostep periodicity and the other indicating a further interface waviness along the macrosteps. The same spatial periodicities were found on the surface by atomic-force-microscopy images confirming the x-ray results and revealing a strong vertical correlation of the interfaces up to the outer surface.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We have measured low-temperature photoluminescence (PL) and absorption spectra of In0.2Ga0.8As/GaAs multiple quantum wells (MQW's) under hydrostatic pressures up to 8 GPa. In PL, only a single peak is observed below 4.9 GPa corresponding to the n = 1 heavy-hole (HH) exciton in the InxGa1-xAs wells. Above 4.9 GPa, new PL lines related to X-like conduction band states appear. They are assigned to the type-II transition from the X(Z) states in GaAs to the HH subband of the InxGa1-xAs wells and to the zero-phonon line and LO-phonon replica of the type-I transition involving the X(XY) valleys of the wells. In addition to absorption peaks corresponding to direct exciton transitions in the wells, a new strong absorption feature is apparent in spectra for pressures between 4.5 and 5.5 GPa. This absorption is attributed to the pseudodirect transition between the HH subband and the X, state of the wells. This gives clear evidence for an enhanced strength of indirect optical transitions due to the breakdown of translational invariance in MQW structures. From experimental level splittings we determine the valence band offset and the shear deformation potential for X states in the In0.2Ga0.8As layer.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Using a home-made gas-source molecular beam epitaxy system, high quality InGaAs quantum wells with different well widths lattice-matched to a (001) InP substrate have been obtained. Sharp and intense peaks for each well can be well resolved in the PL spectra for the sample. For well widths larger than similar to 60 Angstrom, the exciton energies are in good agreement with those of calculation. For wells narrower than 40 Angstrom, our line widths are below the theoretical values of line width broadening due to one monolayer interface fluctuation, showing that the interface fluctuation of our sample is within one monolayer.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An (A1As/GaAs/A1As/A1GaAs)/GaAs(001) double-barrier superlattice grown by molecular beam epitaxy (MBE) is studied by combining synchrotron radiation and double-crystal x-ray diffraction (DCD). The intensity of satellite peaks is modulated by the wave function of each sublayer in one superlattice period. Simulated by the x-ray dynamical diffraction theory, it is discovered that the intensity of the satellite peaks situated near the modulating wave node point of each sublayer is very sensitive to the variation of the layer structural parameters, The accurate layer thickness of each sublayer is obtained with an error less than 1 Angstrom. Furthermore, x-ray kinematical diffraction theory is used to explain the modulation phenomenon. (C) 1996 American Institute of Physics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

By using the mass-analyzed low energy dual ion beam deposition technique, a high quality epitaxial, insulating cerium dioxide thin film with a thickness of about 2000 Angstrom, has been grown on a silicon (111) substrate. The component species, cerium and oxygen, are homogeneous in depth, and have the correct stoichiometry for CeO2. X-ray double-crystal diffraction shows that the full width at half maximum of the (222) and (111) peaks of the film are less than 23 and 32 s, respectively, confirming that the film is a perfect single crystal. (C) 1995 American Institute of Physics.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Growth interruption-induced microroughness is studied by photoluminescence (PL) of single quantum wells with different well widths and interruption times. Analysis of the peak splitting in the PL spectra shows that the adjacent peak splittings correspond to well width differences smaller than one monolayer. The number of split peaks increases with increasing well width, saturating when the well width exceeds 11 monolayers. This trend correlates well with the decrease in the lateral dimension of the exciton, which corresponds roughly to the minimum optically sampled area of the interface. For a given quantum well, a plot of the normalized integrated intensities of the split PL peaks versus the well width fluctuation is well described by a Gaussian distribution with an average fluctuation smaller than one monolayer. These results are consistent with the microroughness model.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Recent infrared spectroscpic observations of local vibrational mode absorptions have revealed a number of photosensitive centers in semi-insulating GaAs. They include (OVAs) center which has three modes at 730 cm(-1) (A), 715 cm(-1) (B), and 714 cm(-1) (C), respectively, a suggested NH center related to a line at 983 cm(-1) (X(1)), and centers related to hydrogen, such as (H-O) or (H-N) bonds, corresponding to a group of peaks in the region of 2900-3500 cm(-1). The photosensitivity of various local vibration centers was observed to have similar time dependence under near-infrared illumination and was suggested to be due to their charge-state interconversion. Mainly described in this work is the effect of the 1.25-eV illumination. It is confirmed that this photoinduced kinetic process results from both electron capture and hole capture, which are closely related to the photoionization behavior and metastability of the EL2 center.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The LO phonon modes in the barrier layers of a GaInAs/AlInAs multiple quantum well structure are investigated by resonance Raman scattering (RRS), the excitation laser photon energy tuned to resonate with the above barrier interband transition energy. The resonance enhancement of LO phonon peaks are shown to be caused by Frohlich electron-phonon interaction. The pressure-dependent profiles for both AlAs-like (LO(2) mode) and InAs-like (LO(1) mode) Raman peak intensities are well fitted by the Gaussian lineshape. The shift between these two profiles can be explained by the outgoing RRS mechanism, providing information on the pressure-induced shift of the excitonic transition energy. The amplitude ratios of the two profiles are close to 1, showing a well defined two-mode behavior and the nearly equal polarizability for Al-As and In-As bonds in AlInAs alloy.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We present photoluminescence studies on highly dense two-dimensional electron gases in selectively Si delta-doped GaAs/In0.18Ga0.82As/Al0.25Ga0.75As quantum wells (N(s) = 4.24 x 10(12) cm-2). Five well-resolved photoluminescence lines centered at 1.4194, 1.4506, 1.4609, 1.4695 and 1.4808 eV were observed, which are attributed to the subband excition emission. The subband separations clearly exhibit the feature of a typical quantum well with triangle and square potential. These very intensive and sharp luminescence peaks with linewidths of 2.2 to 3.5 meV indicate the high quality of the structures. Their dependence on the excitation intensity and temperatures are also discussed.