Resumo:

Crystallization is achieved in amorphous Ge2Sb2Te5 films upon irradiation with a single femtosecond laser pulse. Transmission electron microscopy images evidence the morphology of the crystallized spot which depends on the fluence of the ferntosecond laser pulse. Fine crystalline grains are induced at low fluence, and the coarse crystalline grains are obtained at high fluence. At the damage fluence, ablation of the films occurs. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The single-layer and multilayer Sb-rich AgInSbTe films were irradiated by a single femtosecond laser pulse with the duration of 120 fs. The morphological feature resulting from the laser irradiation have been investigated by scanning electron microscopy and atom force microscopy. For the single-layer film, the center of the irradiated spot is a dark depression and the border is a bright protrusion; however, for the multilayer film, the center morphology changes from a depression to a protrusion as the energy increases. The crystallization threshold fluence of the single-layer and the multilayer films is 46.36 mJ/cm(2), 63.74 mJ/cm(2), respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The morphology of materials resulting from laser irradiation of the single-layer and the multilayer amorphous Ge2Sb2Te5 films using 120 fs pulses at 800 nm was observed using scanning electron microscopy and atomic force microscopy. For the single-layer film, the center of the irradiated spot is depression and the border is protrusion, however, for the multilayer film, the center morphology changes from a depression to a protrusion as the increase of the energy. The crystallization threshold fluence of the single-layer and the multilayer film is 22 and 23 mJ/cm(2), respectively. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel azo dye containing isoxazole ring and beta-diketone derivative (TIAD) and its two nickel (II) complexes (Ni (II)-ETIAD and Ni (II)-HTIAD) were synthesized in order to obtain a blue-violet light absorption and better thermal stability as a promising organic storage material for next generation of high density digital versatile disc-recordable (HD-DVD-R) systems that uses a high numerical aperture of 0.85 at 405 nm wavelength. Their structures were confirmed on the basis of elemental analysis, MS, FT-IR, UV-Vis and magnetic data. Their solubility in 2,2,3,3-tetrafluoro-1-propanol (TFP) and absorption properties of thin film were measured. The difference of absorption maximum from the complexes to their ligands was discussed. In addition, the TG analysis of the complexes was also determined, and their thermal stability was evaluated. (C) 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Formation of bumps in chalcogenide phase change thin films during the laser writing process is theoretically and experimentally investigated. The process involves basically fast heating and quenching stages. Circular bumps are formed after cooling, and the shape and size of the bumps depend on various parameters such as temperatures, laser power, beam size, laser pulse duration, etc. In extreme cases, holes are formed at the apex of the bumps. To understand the bumps and their formation is of great interest for data storage. In the present work, a theoretical model is established for the formation process, and the geometric characters of the formed bumps can be analytically and quantitatively evaluated from various parameters involved in the formation. Simulations based on the analytic solution are carried out taking Ag8In14Sb55Te23 as an example. The results are verified with experimental observations of the bumps. (C) 2008 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An injection-locking excimer laser beam with a pulse duration of 25 ns is focused on the surface of a polymide film. The laser beam that passes through the etching film is shorter than the original one. By optimizing the thickness of the film and the beam power density, a pulse with a 3-ns pulse duration can be obtained using this switch technology.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A single-longitudinal-mode (SLM) laser-diode pumped Nd: YAG laser with adjustable pulse width is developed by using the techniques of pre-lasing and changing polarization of birefingent crystal. The Q-switching voltage is triggered by the peak of the pre-lasing pulse to achieve the higher stability of output pulse energy. The output energy of more than 1 mJ is obtained with output energy stability of 3% (rms) at 100 Hz. The pulse-width can be adjusted from 30 ns to 300 ns by changing the Q-switching voltage. The probability of putting out single-longitudinal-mode pulses is almost 100%. The laser can be run over four hours continually without mode hopping.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

实验采用三倍频Nd:YAG(波长355nm,脉宽8ns,频率30Hz)脉冲激光器作为抽运光源,在ZnO纳米粉末(直径~100nm)中发现了类似激光现象.并用环形腔理论模拟了ZnO的颗粒密度对平均自由程的影响,从理论上证明在纳秒级激光器的抽运下,ZnO纳米粉末也可以发射激光.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel acousto-optic switch operation by a simple laser-diode pumped acousto-optic, Q-switched, ytterbium-doped, double-clad fiber laser is reported. Stable compressed Q-switched sub-40 ns pulses with a beam quality factor (M-2 = 2) are achieved at the repetition rate of 1-50 kHz. Q-switched pulses of similar to 20 mu J pulse energy and 35 as pulse width are obtained at the repetition rate of 50 kHz. Finally, a reasonable explanation of the novel Q-switched operation is presented. (c) 2007 Optical Society of America.