467 resultados para FLUORESCENCE-SPECTRA
Resumo:
A V:YAG single crystal was grown by the temperature gradient technique (TGT) with graphite-heating elements. The as-grown crystal has different colorations of light green and yellow brown in different parts. Distribution of vanadium in three samples with different colorations was determined by inductively coupled plasma-mass spectrometry. From the absorption spectrum of the yellow-brown part with peaks at 370, 820 and 1320nm, we can deduce that the reducing atmosphere of carbon diffused from the heating elements can increase the concentration of tetrahedral V3+ ions and induce F color centers. All three samples exhibited light-green color after annealing in vacuum or H-2 atmospheres. In the vacuum annealing process, the V3+ ions in tetrahedral positions were enhanced through two methods: one method is the exchanging of octahedral V3+ and tetrahedral Al3+ ions in neighboring sites under thermal excitation, the other is that F color centers were thoroughly eliminated and the escaped free electrons could be captured by V ions with higher valance states to further improve the concentration of tetrahedral V3+ ions. Besides the two mechanisms, the H-2 annealing process greatly improved the V-tetra(3+) ions through the reduction effect of H-2. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
用提拉法生长了掺铬、钕的钆镓石榴石(Cr^4+,Nd^3+:GGG)自调Q激光品体。报道了室温下的吸收光谱和荧光光谱特性。分析了Cr离子浓度对光谱性质的影响。比较了Cr^4+:GGG,Nd^3+:GGG和(Cr^4+,Nd^3+):GGG晶体吸收光谱的关系。测量了(Cr^4+,Nd^3+):GGG晶体和Nd^3+:GGG晶体的荧光寿命,它们分别是33μs和250μs。实验表明,(Cr^4+,Nd^3+):GGG晶体是一种非常有潜力的自调Q激光晶体,可以实现大功率激光器的小型化和全固态化。
Resumo:
用提拉法成功地生长了6mol%的高浓度掺铒铌酸锂晶体。测量了晶体的两个非偏振方向(X和Z)以及两个偏振方向(π和δ)的吸收光谱。高浓度掺铒铌酸锂晶体的吸收系数高,有利于提高泵浦效率。根据所测的吸收光谱用Judd-Ofelt理论拟合出了Er^3+离子的强度参数Ωλ。所得的均方差结果显示偏振拟合的误差要小于非偏振拟合。利用偏振吸收数据计算了各能级跃迁的自发辐射跃迁几率(AJJ’)、辐射寿命(τ)、荧光分支比(β)和积分发射截面(σp)等参数,对计算结果进行了讨论并与其他文献的报道结果进行了比较。
Resumo:
We report on photoreduction of Ag+ in aluminoborate glasses induced by irradiation of a femtosecond laser. Novel fluorescence was observed in the femtosecond laser irradiated glass when excited by a 365 nm ultraviolet lamp. Optical absorption, emission, and electron spin resonance spectra of the glass samples demonstrated that after the laser irradiation, portions of silver ions near the focused part of the laser beam inside the glass were reduced to silver atoms, which resulted in the formation of the characteristic fluorescence. The observed phenomenon may have promising applications in the fabrication of functional optical devices.
Resumo:
In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
For the first time, a quaternary doping system of Er3+, Yb3+, Ce3+, Na+:CaF2 single crystal was demonstrated to have high fluorescence yield in the eye-safe 1.5 mu m region under 980 nm laser diode pumping, with relatively broad and flat gain curves. A simplified model was established to illustrate the effect of Ce3+ on the branching ratio for the Er3+4I11/2 -> I-4(13/2) transition. With 0.2-at.% Er3+ and 2.0-at.% Ce3+ in the quaternary-doped CaF2 crystal, the branching ratio was estimated to be improved more than 40 times by the deactivating effect of Ce3+ on the Er3+ 4I11/2 level. The quaternary-doped CaF2, system shows great potential to achieve high laser performance in the 1.5 mu m region. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法生长Y3Al5O12(YAG)晶体和Yb3+掺杂原子数分数分别为5%, 10%, 15%, 20%, 25%, 50%和100%的Yb∶Y3Al5O12(Yb∶YAG)晶体。系统表征和分析了Yb3+掺杂浓度对拉曼光谱的影响。随着Yb3+掺杂浓度的增加,晶体的振动模式没有明显的变化,晶体结构没有改变;在370 cm-1和785 cm-1附近,振动吸收峰的半峰全宽逐渐增大。分析得出,Yb3+掺杂浓度对晶体的晶格、对称性、荧光寿命均有影响,从而可能影响到晶体的光谱和激光性能。
Resumo:
The 10at% Yb-YAP crystal has been grown by the Czochralski method. The absorption and emission spectra and fluorescence lifetime of Yb:YAP crystal at room temperature were studied. There is a strong absorption band centered at 959 nm and the absorption cross-section of 1.51 × 10-20 cm2. The emission cross-section at 1040 nm is 0.6 × 10-20 cm2 and the fluorescence lifetime is about 1.2 ms. The effects of O2-annealing on the spectral properties were studied. The spectroscopic properties strongly depended on the axis direction and b axis was the best direction for laser output. The spectrum parameters of Yb:YAP and Yb:YAG crystal were compared.}
Resumo:
gamma-LiAlO2 single crystal was successfully grown by Czochralski method. The crystal quality was characterized by X-ray rocking curve and chemical etching. The effects of air-annealing and vapor transport equilibration (VTE) on the crystal quality, etch pits and absorption spectra of LiAlO2 were also investigated in detail. The results show that the as-grown crystal has very high quality with the full width at half maximum (FWHM) of 17.7-22.6 arcsec. Dislocation density in the middle part of the crystal is as low as about 3.0 x 10(3) cm(-2). The VTE-treated slice has larger FWHM value, etch pits density and absorption coefficient as compared with those of untreated and air-annealed slices, which indicates that the crystal quality became inferior after VTE treatment. (C) 2008 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Ytterbium-doped calcium pyroniobate single crystal has been grown for the first time. Spectral properties of Yb: Ca2Nb2O7 were investigated by emission and absorption spectra. Its cooperative luminescence and fluorescence lifetime were also studied. Yb ions in Ca2Nb2O7 showed very broad absorption and emission bandwidth and relatively large absorption and emission cross-sections. Along with other optical properties, this Yb-doped crystal would be a potential self-frequency doubling femtosecond laser gain material. (C) 2007 Published by Elsevier B.V.
Resumo:
采用丘克拉斯基(Czochralski)技术生长了掺铥硅酸镥(Tm∶Lu2SiO5,Tm∶LSO)晶体;测量了LSO晶体在室温下的非偏振吸收光谱和非偏振荧光光谱;利用窄得-奥菲特(Judd-Ofelt)理论计算了Tm∶LSO晶体的窄得-奥菲特强度参数、振子强度、自发辐射概率、辐射寿命、积分吸收截面和积分发射截面.Tm∶LSO晶体的强度参数为Ω2=9.1355×10-20cm2,Ω4=8.4103×10-20cm2,Ω6=1.5908×10-20cm2;Tm∶LSO晶体在1.9μm附近有明显的发射峰(3F4→3H6跃迁),相应的辐射寿命为2.03 ms,积分发射截面为5.81×10-18cm2,半峰全宽(FWHM)为250 nm.用Tm∶LSO晶体在77 K温度下实现了激光运转.利用792 nm的激光二极管(LD)作为抽运源,获得中心波长为1960 nm的激光输出,抽运阈值为2.13 kW/cm2.
Resumo:
The electronic structures and absorption spectra for the perfect PbMoO4 crystal and the crystal containing lead vacancy V-Pb(2-) with lattice structure optimized are calculated using density functional theory code CASTEP. The calculated absorption spectra of the PbMoO4 crystal containing V-Pb(2-) exhibit three absorption bands peaking at 2.0 eV (620 nm), 3.0 eV (413 run) and 3.3 eV (375 nm), which are in good agreement with experimental values. The theory predicts that the 390 nm, 430 nm and 580 run absorption bands are related to the existence of V-Pb(2-) in the PbMoO4 crystal.
Resumo:
The Ho:YAP crystal is grown by the Czochralski technique. The room-temperature polarized absorption spectra of Ho:YAP crystal was measured on a c-cut sample with 1 at% holmium. According to the obtained Judd-Ofelt intensity parameters Omega(2) = 1.42 x 10(-20) cm(2), Omega(4) = 2.92 x 10(-20) cm(2), and Omega(6) = 1.71 x 10(-20) cm(2), this paper calculated the fluorescence lifetime to be 6 ms for I-5(7) -> I-5(8) transition, and the integrated emission cross section to be 2.24 x 10(-18) cm(2). It investigates the room-temperature Ho:YAP laser end-pumped by a 1.91-mu m Tm:YLF laser. The maximum output power was 4.1 W when the incident 1.91-mu m pump power was 14.4W. The slope efficiency is 40.8%, corresponding to an optical-to-optical conversion efficiency of 28.4%. The Ho:YAP output wavelength was centred at 2118 nm with full width at half maximum of about 0.8 nm.
Resumo:
National Nature Science Foundation of China (Grant No. 60607015)