238 resultados para Hybrid organic-inorganic mesoporous materials
Resumo:
The effect of template phase on the structures of as-synthesized silica nanoparticles with fragile DDAB vesicles as templates is reported. It is found that the template phase plays a critical role in the growth process of silica: the unstable DDAB vesicles in liquid-crystalline phase often lead to the formation of mesostructured solid spheres, and the rather stable DDAB vesicles in gel phase lead to the formation of hollow spheres with less mesostructures.
Resumo:
Conductive hybrids were prepared in a water/ethanol solution via the Solgel process from an inorganic sol containing carboxyl groups and water-borne conductive polyaniline (cPANI). The inorganic sol was prepared by the hydrolysis and condensation of methyltriethoxysilane with the condensed product of maleic anhydride and aminopropyltriethoxysilane as a catalyst, for which the carboxyl counterion along the cPANI backbone acted as an electrostatic-interaction moiety. The existence of this electrostatic interaction could improve the compatibility of the two components and contribute to the homogeneous dispersion of cPANI in the silica phase. The electrostaticinteraction hybrids displayed a conductivity percolation threshold as low as 1.1 wt % polyaniline in an emeraldine base, showing 2 orders of magnitude higher electrical conductivity than that without electrostatic interactions. The electrostatic-interaction hybrids also showed good water resistance; the electrical conductivity with a cPANI loading of 16 wt % underwent a slight change after 14 days of soaking in water.
Resumo:
A mesostructured cellular foam (MCF) with three-dimensional (313) disordered strutlike structure is prepared by using triblock copolymer (poly(styrene-b-butadiene-b-styrene), SBS, M-W = 140K) as template under strong acid conditions. It is the first report to use triblock copolymer with both hydrophobic head and tail groups instead of hydrophilic head and hydrophobic tail copolymers to synthesize siliceous mesostructured cellular foams. The resulted materials have high pore volume (0.92 cm(3)/g) and relatively narrow pore size distributions with a large pore size of 7.9 nm, which will allow for the fixation of large active complexes, reduce diffusional restriction of reactants and enable reactions involving bulky molecules to take place, especially.
Resumo:
The samples of as-synthesized siliceous MCM-41, extracted MCM-41, amorphous silica particles and silica xerogels were heat treated from room temperature to 1000degreesC. Their photoluminescence (PL) spectra at room temperature excited by 254nm and 365nm ultraviolet light (UV) were investigated and compared. Excited by 254nm UV the MCM-41 samples do not display PL but amorphous silica particles and silica xerogels show PL, which changes with the heat treatment conditions for the samples. However, when excited by 365nm UV the PL spectra for the MCM-41 and the amorphous samples are similar. The carbon impurity and E' center mechanisms can be ruled out as the origin of PL in siliceous MCM-41 under UV excitation. The PL of MCM-41 series samples probably originates from oxygen-related defect center like dropSi-O-. according to the present work.
Resumo:
Organo-functionalized MCM-41 containing non-covalently linked 1,10-phenanthroline (denoted as Phen-MCM-41) was synthesized by template-directed co-condensation of tetraethoxysilane and the modified phenanthroline (denoted as Phen-Si). XRD, FTIR, UV/VIS spectroscopy as well as luminescence spectroscopy were employed to characterize Phen-MCM-41. No disintegration or loss of the Phen-Si during the solvent extraction procedure could be observed. When monitored by the ligand absorption wavelength (272 nm), the undoped MCM-41 produces a broad band emission centered at 450 run, whereas europium (III) doped Phen-MCM-41 displays the emission of the Eu3+, i.e., D-5(0) --> F-7(J) (J = 0, 1, 2, 3, 4) transition lines due to the energy transfer from the ligands to Eu3+ as well as a broad band emission centered at 442 nm.
Resumo:
Two novel dibenzo-18-crown-6 sodium isopolytungstates, [(DB18C6)(CH3OH)Na](2)W(6)O(19)(.)DB18C6(.)H(2)O 1 and [(DB18C6)(DMF)(2)Na](4)W(10)O(32)(.)2DMF(.)2H(2)O 2, have been synthesized in mixed methanol and acetonitrile solvents and characterized by elemental analysis, TGA, IR and single crystal X-ray diffraction. The compound 1 crystallizes in the monoclinic space group C2/c with a = 23.182(8), b = 19.527(2), c = 18.737(3) Angstrom, beta = 115.15(2)degrees, V = 7678(3) Angstrom(3), Z = 4, and R1(wR2) = 0.0611(0.1504). The compound 2 crystallizes in the monoclinic space group P21/n with a = 16.516(2), b = 22.325(6), c = 20.425(7) Angstrom, beta = 91.78(2)degrees, V = 7528(3) Angstrom(3), Z = 2, and R1(wR2) = 0.0397(0.0773). The compound 1 exhibits a novel organic-inorganic sandwich-type structure, in which the crown ether-sodium complexes are coordinated to the terminal oxygen atoms of W6O192-. In compound 2, all Na+ ions are thoroughly enveloped into the organic moieties of crown ether and DMF molecules and are connected with the 'naked' polyanions W10O324- via the electrostatic attraction.
Resumo:
In this article, we report on an approach of using an emulsion polymerized polymer in preparing organic-inorganic nanocomposites through a sol-gel technique. By mixing a polymer emulsion with prehydrolyzed tetraethoxysilane transparent poly(butyl methacrylate)/SiO2, nanocomposites were prepared as shown by TEM. AFM, FTIR, and XPS results show that there is a strong interaction between polymer latex particles and the SiO2 network. Comparison of the emulsion method with a traditional solution method shows that nanocomposites can be prepared by both methods, but there is some difference in their morphology and properties.
Resumo:
An amperometric tyrosinase enzyme electrode for the determination of phenols was developed by a simple and effective immobilization method using sol-gel techniques. A grafting copolymer was introduced into sol-gel solution and the composition of the resultant organic-inorganic composite material was optimized, the tyrosinase retained its activity in the sol-gel thin film and its response to several phenol compounds was determined at 0 mV vs. Ag/AgCl (sat. KCI). The dependences of the current response on pH, oxygen level and temperature were studied, and the stability of the biosensor was also evaluated. The sensitivity of the biosensor for catechol, phenol and p-cresol was 59.6, 23.1 and 39.4 muA/mM, respectively. The enzyme electrode maintained 73% of its original activity after intermittent use for three weeks when storing in a dry state at 4 degreesC. (C) 2000 Elsevier Science S.A. All rights reserved.