206 resultados para Diffusive gradients in thin films


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Because of its high energy density direct current(dc)thermal plasmas are widely accepted as a processing medium which facilitates high processing rates high fluxes of radical species the potential for smaller jnstallations a wide choice of reactants and high quench rates[1].A broad range of industrial processing methods have been developed based on dc plasma technology. However,nonstationary features limited new applications of dc plasma in advanced processing, where reliability£¬reproducibility and precise controllability are required£. These challenges call for better understanding of the arc and jet behavior over a wide range of generating parameters and a comprehensive control of every aspect of lhe plasma processing.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, a serial of Bi3.4Yb0.6Ti3-xVxO12 (BYTV) thin film with different V5+ contents were deposited on Pt/Ti/SiO2/Si substrates by chemical solution deposition (CSD). The crystallized phase and electrical properties of the films were investigated using X-ray diffraction, polarization hysteresis loops, leakage current-voltage, and fatigue test. From our experimental results, it can be found that the ferroelectric properties can be improved greatly using V5+-doped in Bi3.4Yb0.6Ti3O12 (BYT) thin film, compared with the reported BYT thin film. The remanent polarization was enhanced and excellent leakage current characteristic with 10(-11)A at the bias voltage of 4V, which is much lower than the BYT thin film or some reported bismuth layer-structure ferroelectric films. Fatigue test shows that the fabricated films have good anti-fatigue characteristic after 10(10) switching cycles. (c) 2008 Published by Elsevier B.V.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

W-doped Fe2O3 films have been fabricated on polycrystalline alumina substrates by the RF magnetron sputtering method, and effects of annealing temperature on the NO2 sensing properties have been examined. The crystal structure of the obtained film changed from Fe3O4 to α-Fe2O3 after annealing at temperatures of 500 to 500°C in air. An increase in the annealing temperature increased the particle size, resulting in a decrease in the NO2-gas sensitivity. These results suggest that the NO2 sensitivity of W-doped Fe2O3 film depends on the particle size.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The morphologies and structures for the thin film of blend systems consisting of two asymmetric polystyrene-block-polybutadiene (SB) diblock copolymers induced by annealing in the vapor of different solvents, namely, cyclohexane, benzene, and heptane, which have different selectivity or preferential affinity for a certain block, were investigated by tapping mode atomic force microscopy (AFM) and transmission electron microscopy (TEM). The results revealed that even a slight preferential affinity of good solvent for one block would strongly alter the morphology of the blend thin film.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report single mode and multimodes lasing emission from conjugated polymer poly[2-methoxy-5-(2-ethylhexyloxy)-1,4-phenylenevinylene] (MEH-PPV) doped polystyrene ( PS) thin films with surface ripples. Surface ripples were formed by water vapour-induced phase separation. A single mode lasing emission at 606 nm with a line-width of less than 0.4 nm was obtained. The laser threshold was as low as 3.5 mu J pulse(-1). The side mode suppression ratio was 5.76 dB. The periodic changes of the refraction index in the MEH-PPV : PS blending film due to the phase separation should be attributed to the lasing actions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The fabrication of organic semiconductor thin films is extremely important in organic electronic devices. This tutorial review-which should particularly appeal to chemists and physicists interested in organic thin-film growth, organic electronic devices and organic semiconductor materials-summarizes the method of weak epitaxy growth (WEG) and its application in the fabrication of high quality organic semiconductor thin films.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The structural evolution of a single-layer latex film during annealing was studied via grazing incidence ultrasmall-angle X-ray scattering (GIUSAXS) and atomic force microscopy (AFM). The latex particles were composed of a low-T-g (-54 degrees C) core (n-butylacrylate, 30 wt %) and a high-T-g (41 degrees C) shell (t-butylacrylate, 70 wt %) and had an overall diameter of about 500 nm. GIUSAXS data indicate that the q(y) scan at q(z) = 0.27 nm(-1) (out-of-plane scan) contains information about both the structure factor and the form factor. The GIUSAXS data on latex films annealed at various temperatures ranging from room temperature to 140 degrees C indicate that the structure of the latex thin film beneath the surface changed significantly. The evolution of the out-of-plane scan plot reveals the surface reconstruction of the film. Furthermore, we also followed the time-dependent behavior of structural evolution when the latex film was annealed at a relatively low temperature (60 degrees C) where restructuring within the film can be followed that cannot be detected by AFM, which detects only surface morphology.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The transition of lamellar crystal orientation from flat-on to edge-on in ultrathin films of polystyrene-b-poly(ethylene oxide) (PS-b-PEO) via solvent vapor (toluene) treatment Was investigated. When the as-prepared film was treated in saturated solvent vapor, breakout crystals could form quickly, and then they transformed from square single crystals (flat-on lamellae) to dendrites and finally to nanowire crystals (edge-on lamellae). Initially, heterogeneous nucleation tit the polymer/substrate interface dominated the structure evolution, leading to flat-on lamellar crystals orientation. And the transition from faceted habits to dendrites indicated a transition of underlying mechanism from nucleation-controlled to diffusion-limited growth. As the solvent molecules gradually diffused into the polymer/substrate interface, it will subsequently weaken the polymer-substrate interaction.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A series of binary SB blend samples with various overall volume fraction of PS (Phi(PS)) and different discrete distribution of the block length (denoted as d(PS) or d(PB)) were prepared by mixing various asymmetric poly(styrene)-block-poly(butadiene) (SB) block copolymers with a symmetric SB block copolymer. The influences of the external solvent field, composition, and the block length distribution on the morphologies of the blends in the thin films were investigated by atomic force microscopy (AFM) and transmission electron microscopy (TEM). The experimental results revealed that after solvent annealing, the interface of the blend thin films depended mainly on the cooperative effects of the annealing solvent and the inherently interfacial curvature of the blends. Upon exposure to the saturated vapor of cyclohexane, which has preferential affinity for the PB block, a "threshold" of Phi(PS) (approximate 0.635-0.707) was found. Below such threshold, the influence of the annealing solvent played an important role on the interfacial curvature of the blend thin film.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tb3+-doped LiYF4 films were deposited on quartz glass by a simple sol-gel method. X-ray diffraction (XRD), atomic force microscopy (AFM), field emission scanning electron microscopy (FESEM), photoluminescence spectra, and lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 300 degrees C and fully crystallized at 400 degrees C. AFM and FESEM images of singly coated LiY0.95Tb0.05F4 annealed at 400 degrees C indicated that the film is uniform and crack-free films with average grain size of 90 nm, root mean square roughness of 11 nm and thickness of 120 nm. The doped Tb3+ ions showed its characteristic emission in crystalline LiYF4 films, i.e., D-5(3), F--7(4)J (J = 6, 5, 4, 3) emissions. The optimum doping concentration of the Tb3+ was determined to be 5.0 mol% of Y3+ in LiYF4 films.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Through electrostatic layer-by-layer (LbL) assembly, negatively charged calf thymus double stranded DNA (CTds-DNA), and positively charged Zr4+ ions were alternately deposited on gold substrate modified with chemisorbed cysteamine. Thus-prepared three-dimensional DNA networks were characterized by surface plasmon resonance (SPR) spectroscopy, X-ray photoelectron spectroscopy (XPS) and infrared reflection-absorption spectroscopy (IR-RAS). SPR spectroscopy indicates that the effective thickness of DNA monolayer in the (DNA/Zr4+), bilayer was 1.5 +/- 0.1 nm, which corresponds to the surface coverage of 79% of its full packed monolayer. At the same time, a linear increase of film thickness with increasing number of layers was also confirmed by SPR characterizations. The data of XPS and IR-RAS show that Zr4+ ions interact with both the phosphate groups and nitrogenous bases of DNA and load into the framework of DNA. Furthermore, the interactions between this composite film and heme protein cytochrome c (Cyt c) were investigated by SPR spectroscopy and electrochemistry.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Through electrostatic layer-by-layer (LbL) assembly, negatively charged calf thymus double stranded DNA (CTds-DNA), and positively charged Zr4+ ions were alternately deposited on gold substrate modified with chemisorbed cysteamine. Thus-prepared three-dimensional DNA networks were characterized by surface plasmon resonance (SPR) spectroscopy, X-ray photoelectron spectroscopy (XPS) and infrared reflection-absorption spectroscopy (IR-RAS). SPR spectroscopy indicates that the effective thickness of DNA monolayer in the (DNA/Zr4+), bilayer was 1.5 +/- 0.1 nm, which corresponds to the surface coverage of 79% of its full packed monolayer. At the same time, a linear increase of film thickness with increasing number of layers was also confirmed by SPR characterizations. The data of XPS and IR-RAS show that Zr4+ ions interact with both the phosphate groups and nitrogenous bases of DNA and load into the framework of DNA. Furthermore, the interactions between this composite film and heme protein cytochrome c (Cyt c) were investigated by SPR spectroscopy and electrochemistry. Compared with the adsorption of Cyt c on DNA monolayer, this composite multilayer film can obviously enhance the amount of immobilized Cyt c confirmed by SPR reflectivity-incident angle (R-theta) curves.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Self-assembly thin films of symmetric triblock copolymer after annealing and quenching were examined by an effective Monte Carlo simulation method. The defects in the ordered lamellae of the thin films after quenching, which were dependent on the initialization of copolymer melts, are removed in the thin films after annealing. The mean-square gyration radius and end-to-end distance of copolymer chains in the thin films after annealing are smaller than those in the thin films after quenching because of the complete relaxation of polymer during annealing. We also find that the density of A block in the region near to the surface is higher than that in the interior of the thin films. As a result, it is different from the thin films of symmetric A(n)B(n) diblock copolymer, in which surface ordering forms before the interior, that ordering phenomena occurs first in the interior region in the thin films of symmetric A(n)B(m)A(n). triblocl copolymer.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Binary symmetric diblock copolymer blends, that is, low-molecular-weight poly(styrene-block-methyl methacrylate) (PS-b-PMMA) and high-molecular-weight poly(styrene-block-methacrylate) (PS-b-PMA), self-assemble on silicon substrates to form structures with highly ordered nanoholes in thin films. As a result of the chemically similar structure of the PMA and the PMMA block, the PMMA chain penetrates through the large PMA block that absorbs preferentially on the polar silicon substrate. This results in the formation of nanoholes in the PS continuous matrix.