We fabricated the interdiffused organic photovoltaic devices, which composed of poly (2-methoxy-5-(2'-ethylhexyloxy)-1, 4-phenylenevinylene) (MEH-PPV) and buckminsterfullerene (C-60), by annealing treatment. After annealing, C60 diffused into the MEH-PPV layer, in consequence, MEH-PPV/C-60 interfacial area was increased and their interface became closer proximity. The results lead to reduce reverse-bias saturation current (J(s)), and increase the open-circuit voltage (V-OC) and the short-circuit current (J(SC)).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the effects of thermal annealing before and after cathode deposition on poly(3-hexylthiophene)(P3HT)/[6,6]-phenyl C61-butyric acid methyl ester (PCBM) blend photovoltaic cells with different cathode buffer layers. The introduction of cathode buffer layer such as lithium fluoride (LiF) and calcium oxide (CaO) in pre-annealing cells can increase the open-circuit voltage (V-oc) and the power conversion efficiency (PCE). Post thermal annealing after cathode deposition further enhanced the PCE of the cells with LiF/Al cathode.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microstructure and mechanical properties of beta-nucleated iPP before and after being annealed at different temperatures (90-160 degrees C) have been analyzed, Annealing induced different degrees of variation in fracture toughness of beta-nucleated iPP samples. namely, slight enhancement at relatively low annealing temperatures (< 110 degrees C) and great improvement at moderate temperatures (120-130 degrees C), whereas dramatic deterioration at relatively high temperatures ( > 140 degrees C) has been observed. The variation of fracture toughness of beta-nucleated iPP is observed to be dependent on the content of beta-NA. Experiments, including scanning electronic microscope (SEM), wide-angle X-ray diffraction (WAXD), differential scanning calorimetry (DSC), small-angle X-ray scattering (SAXS), and dynamic mechanical analysis (DMA), are performed to study the variations of microstructures as well as the toughening mechanism of the beta-nucleated iPP after being annealed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Needle-like single crystals of poly(3-octylthiophene) (P3OT) have been prepared by tetrahydrofuran-vapor annealing. The morphology and structure of the crystals were characterized with optical microscopy, scanning electron microscopy, atomic force microscopy, transmission electron microscopy, and wide-angle X-ray diffraction. It is observed that the P3OT molecules are packed with the backbones parallel to the length axis of the crystal and the alkyl side chains perpendicular to the substrate. The field effect transistor based on the P3OT single crystal exhibited a charge carrier mobility of 1.54 x 10(-4) cm(2)/(Vs) and on/off current ratio of 37, and the molecular orientation of the crystal is ascribed to account for the device performance. The time-dependent morphological evolution demonstrated that the crystals underwent Ostwald ripening when annealed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three-dimensional Au nanorod and An nanoparticle nanostructured materials were prepared by layer-by-layer self-assembly. The plasmonic properties of the An nanorod and An nanoparticle self-assembled nanostructured materials (abbreviated as AuNR and AuNP SANMs) are tunable by the controlled self-assenibly process. The effect of thermal annealing at 180 and 500 degrees C to the morphologies, plasmonic properties and surface-enhanced Raman scattering (SERS) responses of these SANMs were investigated. According to the experimental results, these properties correlate with the structure of the SANMs.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the effect of thermal annealing before and after cathode deposition on the stability of polymer light-emitting diodes (PLEDs) based on green fluorescent polyfluorene derivative. The annealed PLEDs exhibit improved charge transport and red-shift emission compared to the as-fabricated device. The stability of the PLEDs is largely enhanced by post-annealing before and after Ca deposition, which is attributed to the enhanced charge transport and the intimate contact between the cathode and the emissive layer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structural evolution of high-density polyethylene subjected to uniaxial tensile deformation was investigated as a function of strain and after annealing at different temperatures using a scanning synchrotron small-angle X-ray scattering (SAXS) technique. The results confirm that in the course of tensile deformation intralamellar block slips were activated at small deformations followed by a stress-induced fragmentation and recrystallization process yielding thinner lamellae with their normal parallel to the stretching direction. The original sheared lamellae underwent severe internal deformation so that they were even less stable than the newly developed thinner lamellae. Accordingly, annealing results in a melting of the original crystallites even at moderate strains where the stress-induced fragmentation and recrystallization just sets in and generates a distinctly different form of lamellar stacks aligned along the drawing direction. It was found that the lamellae newly formed during stretching at moderate strains remain stable at lower temperature. Only at a very high annealing temperature of 120 degrees C can they be melted, leading to an isotropic distribution of the lamellar structure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Deuterated polyethylene tracer molecules with small amount of branches (12 C2H5- branches per 1000 backbone carbon atoms) were blended with a hydrogenated polyethylene matrix to form a homogenous mixture. The conformational evolution of the deuterated chains in a stretched semi-cry stall me film was observed via online small angle neutron scattering measurements during annealing at high temperatures close to the melting point. Because the sample was annealed at a temperature closely below its melting point, the crystalline lamellae were only partially molten and the system could not fully relax. The global chain dimensions were preserved during annealing. Recrystallization of released polymeric chain segments allows for local phase separation thus driving the deuterated chain segments into the confining interlamellar amorphous layers giving rise to an interesting intra-molecular clustering effect of the long deuterated chain. This clustering is deduced from characteristic small angle neutron scattering patterns. The confined phase separation has its origin in primarily the small amount of the branches on the deuterated polymers which impede the crystallization of the deuterated chain segments.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Self-assembly thin films of symmetric triblock copolymer after annealing and quenching were examined by an effective Monte Carlo simulation method. The defects in the ordered lamellae of the thin films after quenching, which were dependent on the initialization of copolymer melts, are removed in the thin films after annealing. The mean-square gyration radius and end-to-end distance of copolymer chains in the thin films after annealing are smaller than those in the thin films after quenching because of the complete relaxation of polymer during annealing. We also find that the density of A block in the region near to the surface is higher than that in the interior of the thin films. As a result, it is different from the thin films of symmetric A(n)B(n) diblock copolymer, in which surface ordering forms before the interior, that ordering phenomena occurs first in the interior region in the thin films of symmetric A(n)B(m)A(n). triblocl copolymer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The surface morphology evolution of three thin polystyrene (PS)/polymethyl methacrylate (PMMA) blend films (<70 nm) on SiOx substrates upon annealing were investigated by atomic force microscopy (AFM) and some interesting phenomena were observed. All the spin-coated PS/PMMA blend films were not in thermodynamic equilibrium. For the 67.1 and the 27.2 nm PS/PMMA blend films, owing to the low mobility of the PMMA-rich phase layer at substrate surfaces and interfacial stabilization caused by long-range van der Waals forces of the substrates, the long-lived metastable surface morphologies (the foam-like and the bicontinuous morphologies) were first observed. For the two-dimensional ultrathin PS/PMMA blend film (16.3 nm), the discrete domains of the PS-rich phases upon the PMMA-rich phase layer formed and the secondary phase separation occurred after a longer annealing time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two series of tensile tests with constant crosshead speeds (ranging from 5 to 200 mm/min) and tensile relaxation tests (at strains from 0.03 to 0.09) were performed on low-density polyethylene in the subyield region of deformations at room temperature. Mechanical tests were carried out on nonannealed specimens and on samples annealed for 24 h at the temperatures T = 50, 60, 70, 80, and 100 degreesC. Constitutive equations were derived for the time-dependent response of semicrystalline polymers at isothermal deformations with small strains. A polymer is treated as an equivalent heterogeneous network of chains bridged by temporary junctions (entanglements, physical crosslinks, and lamellar blocks). The network is thought of as an ensemble of mesoregions linked with each other. The viscoelastic behavior of a polymer is modeled as a thermally induced rearrangement of strands (separation of active strands from temporary junctions and merging of dangling strands with the network). The viscoplastic response reflects sliding of junctions in the network with respect to their reference positions driven by macrostrains. Stress-strain relations involve five material constants that were found by fitting the observations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystalline-phase transition in polyamide-66/montmorillonite nanocomposites before melting was investigated by in situ X-ray diffraction and is reported for the first time in this work. The phase-transition temperature in the nanocomposites was 170 degreesC, 20 degreesC lower than that in polyamide-66. The lower phase-transition temperature of the nanocomposites could be attributed to the gamma-phase-favorable environment caused by silicate layers. Meanwhile, the addition of silicate layers changed the crystal structure of the polyamide-66 matrix and influenced the phase-transition behavior.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of nanodispersed clay on the alpha crystalline structure of polyamide 6 (PA6) was examined in-situ with X-ray diffraction (XRD) between room temperature and melting. In pure PA6 upon annealing the alpha crystalline phase was substituted by an unstable pseudohexagonal phase at 150degreesC, then it transformed into a new stable crystalline structure - high temperature alpha' phase above the transition temperature. However, in PA6/clay nanocomposite (PA6CN), the alpha phase did not present crystalline phase transition on heating. The increase in the annealing temperature only led to continuous intensity variation. The different behaviors were caused by the confined spaces formed by silicate layers, which constrained the mobility of the polymer chains in-between.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Full Paper: A study has been made on the annealing of nylon-1010 under high pressures. Heat treatment of melt-crystallized nylon-1010 was performed at 250degreesC for 30 min in the pressure range 0.7 similar to 2.5 GPa. It was found that the triclinic crystals of virgin nylon-1010 were retained at pressures less than 1.0 GPa or larger than 1.2 GPa. The X-ray diffraction intensity of (100) planes decreased with increasing pressure. The diffraction peaks shifted slightly to higher angles (2theta) relative to the virgin nylon-1010, indicating dense packing of polymer chains at high pressures. The highest melting temperature was 208degreesC for the sample annealed at 1.5 GPa. No extended-chain crystals were formed under the experimental conditions. Crosslinking occurred in the pressure range 1.0 similar to 1.2 GPa. The structure of the crosslinked samples was characterized by means of infrared spectroscopy and X-ray photoelectron spectroscopy. It is concluded that a mechanism of crosslinking via carbodiimide can explain the nature of crosslinking of nylon-1010 annealed at high pressures. The remarkable changes of the structure of annealed nylon-1010 are also discussed in this article.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we study the effects of electrical annealing at different voltages on the performance of organic light-emitting diodes. The light-emitting diodes studied here are single-layer devices based on a conjugated dendrimer doped with 2-(4-biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxadiazole as the emissive layer. We find that these devices can be annealed electrically by applying a voltage. This process reduces the turn-on voltage and enhances the brightness and efficiency. We obtained an external electroluminescence quantum efficiency of 0.07% photon/electron and a brightness of 2900 cd m(-2) after 12.4 V electrical annealing, which are about 6 times and 9 times higher than un-annealing devices, respectively. The improved luminance and efficiency are attributed to the presence of a space charge field near the electrodes caused by charging of traps.