330 resultados para EPITAXIALLY GROWN CRYSTALS
Resumo:
ZnO films were grown on (0 0 0 1) LiNbO3 substrates by metal organic chemical vapor deposition (MOCVD). Annealing of ZnO films was performed in air for I h at 800 degrees C. The effects of annealing on the structural and optical properties of ZnO thin films on LiNbO3 substrates were investigated using X-ray diffraction (XRD), atomic force microscopy (AFM) and photoluminescence (PL) measurements. XRD patterns and AFM showed that the as-grown and the annealed ZnO films grown on LiNbO3 substrates had c-axis preferential orientation, the crystallinity of the ZnO films grown on LiNbO3 Substrates was improved, and the grain size increased by annealing. The PL spectra showed that the intensity of the UV near-band-edge peak was increased after annealing, while the intensity of visible peak (deep-level emission) decreased. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Composite sapphire/Ti:sapphire crystals for high-power laser application were grown by the hydrothermal method. The results of the X-ray rocking curve analysis indicate high crystalline quality of the surface Al2O3 material. The strong bonding between the overgrown Al2O3 and seed Ti:Al2O3 crystals is indispensable for withstanding high thermal stresses produced by intense optical pumping. The optical loss at the boundary of the composite crystal is considerably low, indicating the lack of scattering centers. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Large ruby with the size of circle divide75 x 45 mm was grown by temperature gradient technique for the first time. Absorption spectrum was carried out in the range of 190-800 nm by spectrophotometer, and the concentration spatial distribution of Cr3+ in ruby was calculated from the absorption coefficient that based on the Beer-Lambert's Law. Cr3+ ions gradually increase alone both the growth axis and the radial direction. The shape and ingredient of the inclusions were measured by means of Leitz ride field microscopy and scanning electron microscopy. Lane photos and X-ray omega scan show the good quality of as grown ruby. The optimized growth conditions were pointed out based on the observation. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
水热法生长了复合钛宝石(Al2O3/Ti:Al2O3)激光晶体.对外层Al2O3X射线ω扫描表明其晶体质量很高.外层生长的Al2O3和内部的钛宝石激光棒结合牢固、紧密,因而能适应高强度泵浦所带来的激光介质内部的热应力.复合激光晶体界面层带来的光损耗很小.就我们所知,这是首次用水热法生长复合激光晶体.
Resumo:
Optical properties were investigated of ZnO thin films grown oil (100) gamma-LiAlO2 (LAO) substrates by pulsed laser deposition method. C-axis oriented ZnO film was grown oil (100) LAO substrate at the substrate temperature of 550 degrees C. The transmittances of the films were over 85%. Peaks attributed to excitons were seen in the absorption spectra, indicating that the thin films have high crystallinity. Photoluminescence spectra were observed at room temperature; the peak at 550 urn is ascribed to oxygen vacancies in the ZnO films caused by the diffusion of Li from the substrate into the film during deposition. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法成功生长了纯LaAlO3和掺铈的LaAlO3单晶体,测试了它们的远红外吸收谱,紫外吸收谱,荧光谱,根据吸收光谱确定了晶体中Ce^3+的能级结构,利用这一能级结构模型较好地解释了Ce:LaAlO3晶体的荧光光谱。
Resumo:
We found that Ce3+:Lu2Si2O7 single crystals could be excited at 800 nm by using a femtosecond Ti:sapphire laser. The emission spectra of Ce3+:Lu2Si2O7 crystals were the same for one-photon excitation at 267 nm as for excitation at 800 nm. The emission intensity of Ce3+: Lu2Si2O7 crystals was found to depend on the cube of the laser power at 800 nm, consistent with simultaneous absorption of three 800 nm photons. The measured value of the three-photon absorption cross section is sigma'(3) = 2.44 x 10(-77) cm(6) s(2). (c) 2006 Optical Society of America.
Resumo:
Blue frequency-upconversion fluorescence emission has been observed in Ce3+-doped Gd2SiO5 single crystals, pumped with 120-fs 800 nm IR laser pulses. The observed fluorescence emission peaks at about 440nm is due to 5d -> 4f transition of Ce3+ ions. The intensity dependence of the blue fluorescence emission on the IR excitation laser power obeys the cubic law, demonstrating three-photon absorption process. Analysis suggested that three-photon simultaneous absorption induced population inversion should be the predominant frequency upconversion mechanism. (c) 2006 Optical Society of America.
Resumo:
The effects of Na+ doping level on the thermal conductivities, absorption and emission spectra, and fluorescence lifetimes of Yb3+ ,Na+ :CaF2 crystals were systematically studied. Sites structure, covalent force, and crystal field strength of Yb3+ :CaF2 crystals were markedly varied by codoping Na+ as charge compensator. The 2.0at% Yb3+ and 3.0at% Na+-codoped CaF2 crystal was demonstrated to operate in diode-pumped passively mode-locking scheme. Transform-limited 1 ps laser pulses were obtained, showing the crystal capable of producing ultra-short laser pulses. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Large-sized (similar to 2 inch, 50.8 mm) gamma-UA102 single crystal has been grown by conventional Czochralski (Cz) method, but the crystal ha's a milky, dendriform center. The samples taken from transparent and milky parts were ground and examined by X-ray diffraction. All diffraction peaks could be indexed in gamma-LiAlO2. The crystal quality was characterized by X-ray rocking curve. The full-width at half-maximum (FWHM) values are 116.9 and 132.0 arcsec for transparent and milky parts, respectively. The vapor transport equilibrium (VTE) technique was introduced to modify the crystal quality. After 1000 degrees C/48 h, 1100 degrees C/48 h, 1200 degrees C/48 h VTE processes, the FWHM values dropped to 44.2 and 55.2 arcsec for transparent and milky part, respectively. The optical transmission of transparent part was greatly enhanced from 85% to 90%, and transmission of milky part from 75% to 80% in the range of 190 similar to 1900 nm at room temperature. When the VTE temperature was raised to 1300 degrees C, the sample cracked and FWHM values of transparent and milky parts were increased to 55.2 and 80.9 arcsec, respectively. By combining Cz technique with VTE technique, large-sized and high quality gamma-LiAlO2 crystal can be obtained.
Resumo:
Sapphire crystals, 140 mm in diameter and 90 turn in height, have been grown by temperature gradient techniques (TGT). The growth direction of the boule was fixed by means of Lane X-ray diffraction. A prominent 204 nm absorption band in TGT-Al2O3. which does not appear in single crystals grown by Czochralski method has been studied. Analysis further substantiates the F-center model of this band. Two relatively weaker bands absorbing at 232 nm and 254 nm were ascribed to F+ centers. F-type centers concentration was determined using Smakula's equation. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A V:YAG single crystal was grown by the temperature gradient technique (TGT) with graphite-heating elements. The as-grown crystal has different colorations of light green and yellow brown in different parts. Distribution of vanadium in three samples with different colorations was determined by inductively coupled plasma-mass spectrometry. From the absorption spectrum of the yellow-brown part with peaks at 370, 820 and 1320nm, we can deduce that the reducing atmosphere of carbon diffused from the heating elements can increase the concentration of tetrahedral V3+ ions and induce F color centers. All three samples exhibited light-green color after annealing in vacuum or H-2 atmospheres. In the vacuum annealing process, the V3+ ions in tetrahedral positions were enhanced through two methods: one method is the exchanging of octahedral V3+ and tetrahedral Al3+ ions in neighboring sites under thermal excitation, the other is that F color centers were thoroughly eliminated and the escaped free electrons could be captured by V ions with higher valance states to further improve the concentration of tetrahedral V3+ ions. Besides the two mechanisms, the H-2 annealing process greatly improved the V-tetra(3+) ions through the reduction effect of H-2. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法生长了Yb^3+掺杂量分别为5.4at%,16.3at%,27.1at%,53.6at%和100at%的Yb:Y3Al5O12晶体.系统地表征和分析了Yb^3+掺杂量对晶体吸收光谱和荧光光谱的影响.随着Yb^3+掺杂量的增加,各峰值吸收系数呈线性增加的趋势.应用Smakula公式计算了各吸收峰对应的振荡强度,并分析了Yb^3+掺杂量对振荡强度的影响.当Yb^3+掺杂量增加到27.1at%时观察到了荧光猝灭现象;当Yb^3+掺杂量增加到53.6at%时,荧光光谱的线形发生了很大的变化。
Resumo:
About Phi 45 mm LiAlO2 single crystal was grown by Czochralski (Cz) technique. However, the full-width at half-maximum (FWHM) value was high to 116.9 arcsec. After three vapor transport equilibration (VTE) processes, we can obtain high-quality LiAlO2 slice with the FWHM value of 44.2 arcsec. ZnO films were fabricated on as-grown slices and after-VTE ones by pulsed laser deposition (PLD). It was found that ZnO films on the two slices have similar crystallinity, optical transmittance and optical band gap at room temperature. These results not only show that LAO substrate is suitable for ZnO growth, but also prove that the crystal quality of LAO substrate slightly affects the structural and optical properties of ZnO film.
Resumo:
温度梯度法(temperature gradient technique,TGT)生长的Al2O3晶体因石墨发热体在高温时的挥发和原料中过渡性金属离子的存在,在不同部位呈现不同颜色,一般上部为浅红色,尾部为浅黄绿色.将TGT法生长的Al2O3晶体(Ф110×80mm^3)依次经过高温氧化气氛、高温还原气氛脱碳、去色退火实验,即“两步法”退火实验,晶体变成无色、透明.经测试,Al2O3晶体的完整性、光学透过率和光学均匀性均有显著提高.