290 resultados para GA2O3 NANOWIRES
Resumo:
Transparent Ni2+-doped MgO-Al2O3-Ga2O3-SiO2-TiO2 glass ceramics were fabricated. The precipitated nanocrystal phase in the glass ceramics was identified by X-ray diffraction and transmission electron microscope. Broadband near-infrared emission centered at 1220 nm with full width at half maximum of about 240 nm and lifetime of about 250 mu s was observed with 980 nm excitation. The longer wavelength emission compared with Ni2+-doped MgAl2O4 crystal was attributed to the low crystal field occupied by Ni2+ in the glass ceramics. The present Ni2+-doped transparent glass ceramics may have potential applications in broadband optical amplifiers. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Tin oxide doped beta-Ga2O3 single crystals are recognized as transparent conductive oxides (TCOs) materials. They have a larger band gap (4.8 eV) than any other TCOs, thus can be transparent in UV region. This property shows that they have the potential to make the optoelectronic device used in even shorter wavelength than usual TCOs. beta-Ga2O3 single crystals doped with different Sn4+ concentrations were grown by the floating zone technique. Their optical properties and electrical conductivities were systematically studied. It has been found that their conductivities and optical properties were influenced by the Sn4+ concentrations and annealing. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
为获得与GaN薄膜晶格失配小的衬底材料,报道了利用气相传输平衡技术(VTE)在(100)β-Ga2O3单晶衬底上制备高度[001]取向LiGaO2薄膜的方法。经过X射线衍射分析表明得到的薄膜是由单相LiGaO2组成。利用扫描电镜(SEM)观察表面形貌,发现经气相传输平衡技术处理得到的薄膜表面形貌主要受温度的影响,表面晶粒尺寸随温度上升而增大。而X射线衍射测试表明随着温度上升,所得到的薄膜也从多晶向单晶化转变。在经过退火处理后,通过观察吸收谱发现LiGaO2薄膜中产生色心,并且色心的种类与温度有关。表明可以
Resumo:
由于与GaN晶格失配小(约1.4%),γ-LiAlO2单晶有望成为GaN外延衬底材料。本文首先使用提拉法生长出了尺寸达φ45×50mm^3的γ-LiAlO2单晶,然后采用Ga2O3作为掺杂剂,仍用提拉法生长出了三种不同掺镓浓度的LiAl1-xGaxO2(x=0.1,0.2,0.3)晶体,并用X射线粉末衍射(XRPD)分别对晶体及坩锅中剩余的熔体的成份进行了表征。结果表明LiAl1-xGaxO2(x=0,0.1,0.2,0.3)晶体归属于γ-LiAlO2结晶结构,Ga^3+离子部分地取代Al^3+离子,发生
Resumo:
The magnetic behavior of Mn-doped beta-Ga2O3 is Studied from first-principles calculations within the generalized gradient approximation method. Calculations show that ferromagnetic ordering is always favorable for configurations in which two Mn ions substitute either tetrahedral or octahedral sites, and the ferromagnetic ground state is also sometimes favorable for configurations where one Mn ion substitutes a tetrahedral site and another Mn ion substitutes an octahedral site. However, the configurations of the latter case are less stable than those of the former. (c) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
On the basis of the density functional theory (DFT) within local density approximations (LDA) approach, we calculate the band gaps for different size SnO2 quantum wire (QWs) and quantum dots (QDs). A model is proposed to passivate the surface atoms of SnO2 QWs and QDs. We find that the band gap increases between QWs and bulk evolve as Delta E-g(wire) = 1.74/d(1.20) as the effective diameter d decreases, while being Delta E-g(dot) = 2.84/d(1.26) for the QDs. Though the similar to d(1.2) scale is significantly different from similar to d(2) of the effective mass result, the ratio of band gap increases between SnO2 QWs and QDs is 0.609, very close to the effective mass prediction. We also confirm, although the LDS calculations underestimate the band gap, that they give the trend of band gap shift as much as that obtained by the hybrid functional (PBE0) with a rational mixing of 25% Fock exchange and 75% of the conventional Perdew-Burke-Ernzerhof (PBE) exchange functional for the SnO2 QWs and QDs. The relative deviation of the LDA calculated band gap difference Lambda E-g compared with the corresponding PBE0 results is only within 5%. Additionally, it is found the states of valence band maximum (VBM) and conduction band minimum (CBM) of SnO2 QWs or QDs have a mostly p- and s-like envelope function symmetry, respectively, from both LDA and PBE0 calculations.
Resumo:
ZnMgO hexagonal-nanotowers/films grown on m-plane sapphire substrates were successfully synthesized using a vertical low-pressure metal organic chemical vapour deposition system. The structural and optical properties of the as-obtained products were characterized using various techniques. They were grown along the non-polar [1 0 (1) over bar 0] direction and possessed wurtzite structure. The ZnMgO hexagonal-nanotowers were about 200 nm in diameter at the bottom and 120 nm in length. Photoluminescence and Raman spectra show that the products have good crystal quality with few oxygen vacancies. With Mg incorporation, multiple-phonon scattering becomes weak and broad, and the intensities of all observed vibrational modes decrease. The ultraviolet near band edge emission shows a clear blueshift (as much as 100 meV) and broadening compared with that of pure ZnO products.
Resumo:
Hexagonal nanopillars with a single InGaAs/GaAs quantum well (QW) were fabricated on a GaAs (111) B substrate by selective-area metal-organic vapor phase epitaxy. The standard deviations in diameter and height of the nanopillars are about 2% and 5%, respectively. Zincblende structure and rotation twins were identified in both the GaAs and the InGaAs layers by electron diffraction. The excitation-power-density-dependent micro-photoluminescence (mu-PL) of the nanopillars was measured at 4.2, 50, 100 and 150 K. It was shown that, with increasing excitation power density, the mu-PL peak's positions shift to a higher energy, and their intensity and width increase, which were rationalized using a model that includes the effects of piezoelectricity, photon-screening and band-filling. It was also revealed that the rotation twins significantly reduce the diffusion length of the carriers in the nanopillars, compared to that in the regular semiconductors.
Resumo:
ZnO nanoflowers are synthesized on AIN films by solution method. The synthesized nanoflowers are composed of nanorods, which are pyramidal and grow from a central point, thus forming structures that are flower-shaped as a whole. The nanoflowers have two typical morphologies: plate-like and bush-like. The XRD spectrum corresponds to the side planes of the ZnO nanorods made up of the nanoflowers. The micro-Raman spectrum of the ZnO nanoflowers exhibits the E-2 (high) mode and the second order multiple-phonon mode. The photoluminescence spectrum of the ZnO nanoflowers exhibits ultraviolet emission centred at 375 nm and a broad green emission centred at 526 nm.
Resumo:
Nanostructured hexagonal InN overlayers were heteroepitaxially deposited on vertically oriented c-axis GaN nanorods by metal-organic chemical vapor deposition. InN overlayers grown in radial directions are featured by a nonpolar heteroepitaxial growth mode on GaN nanorods, showing a great difference from the conventional InN growth on (0001) c-plane GaN template. The surface of InN overlayers is mainly composed of several specific facets with lower crystallographic indices. The orientation relationship between InN and GaN lattices is found to be [0001](InN) parallel to [0001](GaN) and [1100](InN)parallel to[1100](GaN). A strong photoluminescence of InN nanostructures is observed. (C) 2009 American Institute of Physics. [DOI 10.1063/1.3177347]
Resumo:
We report the synthesis and characterization of Zn-doped InN nanorods by metal-organic chemical vapor deposition. Electron microscopy images show that the InN nanorods are single-crystalline structures and vertically well-aligned. Energy-dispersive X-ray spectroscopy analyses suggest that Zn ions are distributed nonhomogenously in InN nanorods. Simulations based on diffusion model show that the doping concentration along the radial direction of InN nanorod is bowl-like from the exterior to the interior, the doping concentration decreases, and Such dopant distribution result in a bimodal EDXS spectrum of Zn across the nanorod. The study of the mechanism of doping effect is useful for the design of InN-based nanometer devices. Also, high-quality Zn-doped InN nanorods will be very attractive as building blocks for nano-optoelectronic devices.'
Resumo:
We report on the fabrication of the nanowires with InGaAs/GaAs heterostructures on the GaAs(111) B substrate using selective-area metal organic vapor phase epitaxy. Fabry-Perot microcavity modes were observed in the nanowires with perfect end facets dispersed onto the silicon substrate and not observed in the free-standing nanowires. We find that the calculated group refractive indices only considering the material dispersion do not agree with the experimentally determined values although this method was used by some researchers. The calculated group refractive indices considering both the material dispersion and the waveguide dispersion agree with the experimentally determined values well. We also find that Fabry-Perot microcavity modes are not observable in the nanowires with the width less than about 180 nm, which is mainly caused by their poor reflectivity at the end facets due to their weak confinement to the optical field. (C) 2009 Optical Society of America
Resumo:
Using first-principles molecular dynamics simulations, the displacement threshold energy and defect configurations are determined in SiC nanotubes. The simulation results reveal that a rich variety of defect structures (vacancies, Stone-Wales defects and antisite defects) are formed with threshold energies from 11 to 64 eV. The threshold energy shows an anisotropic behavior and exhibits a dramatic decrease with decreasing tube diameter. The electronic structure can be altered by the defects formed by irradiation, which suggests that the electron irradiation may be a way to use defect engineering to tailor electronic properties of SiC nanotubes.
Resumo:
The origin of ferromagnetism in d(0) semiconductors is studied using first-principles methods with ZnO as a prototype material. We show that the presence of spontaneous magnetization in nitrides and oxides with sufficient holes is an intrinsic property of these first-row d(0) semiconductors and can be attributed to the localized nature of the 2p states of O and N. We find that acceptor doping, especially doping at the anion site, can enhance the ferromagnetism with much smaller threshold hole concentrations. The quantum confinement effect also reduces the critical hole concentration to induce ferromagnetism in ZnO nanowires. The characteristic nonmonotonic spin couplings in these systems are explained in terms of the band coupling model.
Resumo:
Size self-scaling effect in stacked InAs/In0.52Al0.48As nanowires on InP substrates is revealed, i.e., the base width and height of the InAs nanowires have clear proportional dependence on thickness of the InAlAs spacer layer used in different samples. The photoluminescence wavelength from different samples, which varies between 1.3 and 1.9 mum, is also found closely correlated to the size self-scaling effect. This phenomenon can be well explained in the context of formation mechanism and growth features of the InAs/InAlAs nanowire arrays. The finding illustrates a degree of freedom to control the structural and optical properties of strained self-organized nanostructures. (C) 2004 American Institute of Physics.