3 resultados para ACID PRODUCTION
em CaltechTHESIS
Resumo:
Part I: Synthesis of L-Amino Acid Oxidase by a Serine- or Glycine-Requiring Strain of Neurospora
Wild-type cultures of Neurospora crassa growing on minimal medium contain low levels of L-amino acid oxidase, tyrosinase, and nicotinarnide adenine dinucleotide glycohydrase (NADase). The enzymes are derepressed by starvation and by a number of other conditions which are inhibitory to growth. L-amino acid oxidase is, in addition, induced by growth on amino acids. A mutant which produces large quantities of both L-amino acid oxidase and NADase when growing on minimal medium was investigated. Constitutive synthesis of L-amino acid oxidase was shown to be inherited as a single gene, called P110, which is separable from constitutive synthesis of NADase. P110 maps near the centromere on linkage group IV.
L-amino acid oxidase produced constitutively by P110 was partially purified and compared to partially purified L-amino acid oxidase produced by derepressed wild-type cultures. The enzymes are identical with respect to thermostability and molecular weight as judged by gel filtration.
The mutant P110 was shown to be an incompletely blocked auxotroph which requires serine or glycine. None of the enzymes involved in the synthesis of serine from 3-phosphoglyceric acid or glyceric acid was found to be deficient in the mutant, however. An investigation of the free intracellular amino acid pools of P110 indicated that the mutant is deficient in serine, glycine, and alanine, and accumulates threonine and homoserine.
The relationship between the amino acid requirement of P110 and its synthesis of L-amino acid oxidase is discussed.
Part II: Studies Concerning Multiple Electrophoretic Forms of Tyrosinase in Neurospora
Supernumerary bands shown by some crude tyrosinase preparations in paper electrophoresis were investigated. Genetic analysis indicated that the location of the extra bands is determined by the particular T allele present. The presence of supernumerary bands varies with the method used to derepress tyrosinase production, and with the duration of derepression. The extra bands are unstable and may convert to the major electrophoretic band, suggesting that they result from modification of a single protein. Attempts to isolate the supernumerary bands by continuous flow paper electrophoresis or density gradient zonal electrophoresis were unsuccessful.
Resumo:
New and promising treatments for coronary heart disease are enabled by vascular scaffolds made of poly(L-lactic acid) (PLLA), as demonstrated by Abbott Vascular’s bioresorbable vascular scaffold. PLLA is a semicrystalline polymer whose degree of crystallinity and crystalline microstructure depend on the thermal and deformation history during processing. In turn, the semicrystalline morphology determines scaffold strength and biodegradation time. However, spatially-resolved information about the resulting material structure (crystallinity and crystal orientation) is needed to interpret in vivo observations.
The first manufacturing step of the scaffold is tube expansion in a process similar to injection blow molding. Spatial uniformity of the tube microstructure is essential for the consistent production and performance of the final scaffold. For implantation into the artery, solid-state deformation below the glass transition temperature is imposed on a laser-cut subassembly to crimp it into a small diameter. Regions of localized strain during crimping are implicated in deployment behavior.
To examine the semicrystalline microstructure development of the scaffold, we employed complementary techniques of scanning electron and polarized light microscopy, wide-angle X-ray scattering, and X-ray microdiffraction. These techniques enabled us to assess the microstructure at the micro and nano length scale. The results show that the expanded tube is very uniform in the azimuthal and axial directions and that radial variations are more pronounced. The crimping step dramatically changes the microstructure of the subassembly by imposing extreme elongation and compression. Spatial information on the degree and direction of chain orientation from X-ray microdiffraction data gives insight into the mechanism by which the PLLA dissipates the stresses during crimping, without fracture. Finally, analysis of the microstructure after deployment shows that it is inherited from the crimping step and contributes to the scaffold’s successful implantation in vivo.
Resumo:
Terephthalic acid (PTA) is one of the monomers used for the synthesis of the polyester, polyethylene terephthalate (PET), that is used for the large-scale manufacture of synthetic fibers and plastic bottles. PTA is largely produced from the liquid-phase oxidation of petroleum-derived p-xylene (PX). However, there are now ongoing worldwide efforts exploring alternative routes for producing PTA from renewable, biomass resources.
In this thesis, I present a new route to PTA starting from the biomass-derived platform chemical, 5-hydroxymethylfurfural (HMF). This route utilizes new, selective Diels-Alder-dehydration reactions involving ethylene and is advantageous over the previously proposed Diels-Alder-dehydration route to PTA from HMF via 2,5-dimethylfuran (DMF) since the H2 reduction of HMF to DMF is avoided. Specifically, oxidized derivatives of HMF are reacted as is, or after etherification-esterification with methanol, with ethylene over solid Lewis acid catalysts that do not contain strong Brønsted acids in order to synthesize intermediates of PTA and its equally important diester, dimethyl terephthalate (DMT). The partially oxidized HMF, 5-(hydroxymethyl)furoic acid (HMFA) is reacted with high pressure ethylene over a pure-silica molecular sieve catalyst containing framework tin (Sn-Beta) to produce the Diels-Alder-dehydration product, 4-(hydroxymethyl)benzoic acid (HMBA), with ~30% selectivity at ~20% yield. If HMFA is protected with methanol to form methyl 5-(methoxymethyl)furan-2-carboxylate (MMFC), MMFC can react with ethylene in the presence of a pure-silica molecular sieve containing framework zirconium (Zr-Beta) to produce methyl 4-(methoxymethyl)benzenecarboxylate (MMBC) with >70% selectivity at >20% yield. HMBA and MMBC can then be oxidized to produce PTA and DMT, respectively. When Lewis acid containing mesoporous silica (MCM-41) and amorphous silica, or Brønsted acid containing zeolites (Al-Beta), are used as catalysts, a significant decrease in selectivity/yield of the Diels-Alder-dehydration product is observed.
An investigation to elucidate the reaction network and side products in the conversion of MMFC to MMBC was performed, and the main side products are found to be methyl 4-formylcyclohexa-1,3-diene-1-carboxylate and the ethylene Diels-Alder adduct of this cyclohexadiene. These products presumably form by a different dehydration pathway of the MMFC/ethylene Diels-Alder adduct and should be included when determining the overall selectivity to PTA or DMT since, like MMBC, these compounds are precursors to PTA or DMT.
Fundamental physical and chemical information on the ethylene Diels-Alder-dehydration reactions catalyzed by the Lewis acid-containing molecular sieves was obtained. Madon-Boudart experiments using Zr-Beta as catalyst show that the reaction rates are limited by chemical kinetics only (physical transport limitations are not present), all the Zr4+ centers are incorporated into the framework of the molecular sieve, and the whole molecular sieve crystal is accessible for catalysis. Apparent activation energies using Zr-Beta are low, suggesting that the overall activation energy of the system may be determined by a collection of terms and is not the true activation energy of a single chemical step.