Synthesis and characterization of PLZT (9/65/35) by the Pechini method and partial oxalate


Autoria(s): Cerqueira, M.; Nasar, R. S.; Leite, E. R.; Longo, Elson; Varela, José Arana
Contribuinte(s)

Universidade Estadual Paulista (UNESP)

Data(s)

20/05/2014

20/05/2014

01/05/1998

Resumo

ZrTiO4 (ZT), obtained by the Pechini method, was used as precursor for obtaining PLZT (lead lanthanum zirconium titanate). An aqueous solution of oxalic acid was prepared with particles of ZT, Pb(NO3)(2) and La2O3. After the PbC2O4 and La2O3 precipitate on ZT particles, the materials were calcined and X-ray diffraction (XRD) showed the cubic phase of PLZT. This material was sintered, in two steps, and a density of about 8.0 g/cm(3) was obtained. After the second sintering the XRD pattern showed the occurrence of tetragonal and rhombohedral phases. This was caused by a stoichiometric deviation and the material showed a high optical transparency. (C) 1998 Elsevier B.V. B.V. All rights reserved.

Formato

166-171

Identificador

http://dx.doi.org/10.1016/S0167-577X(97)00240-1

Materials Letters. Amsterdam: Elsevier B.V., v. 35, n. 3-4, p. 166-171, 1998.

0167-577X

http://hdl.handle.net/11449/31339

10.1016/S0167-577X(97)00240-1

WOS:000074363500006

Idioma(s)

eng

Publicador

Elsevier B.V.

Relação

Materials Letters

Direitos

closedAccess

Palavras-Chave #synthesis #Pechini process #zirconium titanate #ZrTiO4 #Pb containing ZrTiO4 (PLZT)
Tipo

info:eu-repo/semantics/article