868 resultados para welding metallurgy
Resumo:
Includes "Suggested reading."
Resumo:
We present a brief résumé of the history of solidification research and key factors affecting the solidification of fusion welds. There is a general agreement of the basic solidification theory, albeit differing - even confusing - nomenclatures do exist, and Cases 2 and 3 (the Chalmers' basic boundary conditions for solidification, categorized by Savage as Cases) are variably emphasized. Model Frame, a tool helping to model the continuum of fusion weld solidification from start to end, is proposed. It incorporates the general solidification models, of which the pertinent ones are selected for the actual modeling. The basic models are the main solidification Cases 1…4. These discrete Cases are joined with Sub-Cases: models of Pfann, Flemings and others, bringing needed Sub-Case variables into the model. Model Frame depicts a grain growing from the weld interface to its centerline. Besides modeling, the Model Frame supports education and academic debate. The new mathematical modeling techniques will extend its use into multi-dimensional modeling, introducing new variables and increasing the modeling accuracy. We propose a model: melting/solidification-model (M/S-model) - predicting the solute profile at the start of the solidification of a fusion weld. This Case 3-based Sub-Case takes into account the melting stage, the solute back-diffusion in the solid, and the growth rate acceleration typical to fusion welds. We propose - based on works of Rutter & Chalmers, David & Vitek and our experimental results on copper - that NEGS-EGS-transition is not associated only with cellular-dendritic-transition. Solidification is studied experimentally on pure and doped copper with welding speed range from 0 to 200 cm/min, with one test at 3000 cm/min. Found were only planar and cellular structures, no dendrites - columnar or equiaxed. Cell sub structures: rows of cubic elements we call "cubelettes", "cell-bands" and "micro-cells", as well as an anomalous crack morphology "crack-eye", were detected, as well as microscopic hot crack nucleus we call "grain-lag cracks", caused by a grain slightly lagging behind its neighbors in arrival to the weld centerline. Varestraint test and R-test revealed a change of crack morphologies from centerline cracks to grainand cell boundary cracks with an increasing welding speed. High speed made the cracks invisible to bare eye and hardly detectable with light microscope, while electron microscope often revealed networks of fine micro-cracks.
Resumo:
Työn teoriaosassa käsitellään ruostumattomia teräksiä ja terästen metallurgiaan vaikuttavia tekijöitä yleisesti, sekä terästen hitsattavuutta. Hitsauksesta teoriassa käydään läpi laser- ja kaasukaarihitsausta ja hitsin metallurgiaan vaikuttavia tekijöitä. Kokeellisessa osassa paneudutaan kahdeksan eri ruostumattoman teräksen hitsien metallurgiaan ja metallurgiassa tapahtuviin muutoksiin hitsausparametrien mukaan. Koemateriaaleina on neljä austeniittista ruostumatonta terästä, 201, 301LN, 316L ja 254 SMO, kaksi austeniittis-ferriittistä ruostumatonta terästä, 2101 LDX ja 2205, sekä kaksi ferriittistä ruostumatonta terästä, 430 ja 1.4003. Hitsien mikrorakenteen tutkimisessa käytettiin sekä valomikroskooppia sekä joissain tapauksissa pyyhkäisyelektronimikroskooppia. Lisäksi työn kokeellisessa osassa paneuduttiin hitsien metallografisiin syövytystekniikoihin. Kokeiden perusteella voidaan sanoa, että hitsin metallurgia riippuu hitsauksen aikaisesta lämpösyklistä ja hitsausparametreilla voidaan vaikuttaa tämän lämpösyklin muotoon. Austeniittis-ferriittisillä teräksillä hitsauksen aikaisesta lämpösyklistä riippuu pitkälti hitsin austeniitti-ferriitti-suhde. Ferriittisillä teräksillä lämpösyklin muoto vaikuttaa hitsiin muodostuvan martensiitin kovuuteen ja määrään sekä rakenteen hienojakoisuuteen. Austeniittisilla teräksillä lämpösyklinmuodon vaikutus riippuu pitkälti teräksen seostusasteesta ja seosaineista. Austeniittisilla teräksillä kokeissa havaittuja muutoksia, parametrien muutosten mukaan oli muun muassa suotautumisen voimakkuuden
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
"Metallurgy and Ceramics."
Resumo:
Selected unclassified reports, supplementing those abstracted in TID-3059, which were available in TISE files on July 1, 1956, on welding and brazing of materials of interest to nuclear technology, such as Al, Be, Hf, Mo, Th, Ti, Zr, stainless steels, high-temperature alloys, pressure vessels, and heat exchangers, are annotated. Author, subject, and report number indexes are included. 127 references.
Resumo:
The aim of this study was to analyze the shear bond strength between commercially pure titanium, with and without laser welding, after airbone-particle abrasion (Al2O3) and 2 indirect composites. Sixty-four specimens were cast and divided into 2 groups with and without laser welding. Each group was divided in 4 subgroups, related to Al2O3 grain size: A - 250 µm; B - 180 µm; C- 110 µm; and D - 50 µm. Composite rings were formed around the rods and light polymerized using UniXS unit. Specimens were invested and their shear bond strength at failure was measured with a universal testing machine at a crosshead speed of 2.0 mm/min. Statistical analysis was carried out with ANOVA and Tukey's test (α=0.05). The highest bond strength means were recorded in 250 µm group without laser welding. The lowest shear bond strength means were recorded in 50 µm group with laser welding. Statistically significant differences (p<0.05) were found between all groups. In conclusion, airborne particle abrasion yielded significantly lower bond strength as the Al2O3 particle size decreased. Shear bond strength decreased in the laser welded specimens.
Resumo:
Welded equipment for cryogenic applications is utilized in chemical, petrochemical, and metallurgical industries. One material suitable for cryogenic application is austenitic stainless steel, which usually doesn`t present ductile/brittle transition temperature, except in the weld metal, where the presence of ferrite and micro inclusions can promote a brittle failure, either by ferrite cleavage or dimple nucleation and growth, respectively. A 25-mm- (1-in.-) thick AISI 304 stainless steel base metal was welded with the SAW process using a 308L solid wire and two kinds of fluxes and constant voltage power sources with two types of electrical outputs: direct current electrode positive and balanced square wave alternating current. The welded joints were analyzed by chemical composition, microstructure characterization, room temperature mechanical properties, and CVN impact test at -100 degrees C (-73 degrees F). Results showed that an increase of chromium and nickel content was observed in all weld beads compared to base metal. The chromium and nickel equivalents ratio for the weld beads were always higher for welding with square wave AC for the two types of fluxes than for direct current. The modification in the Cr(eq)/Ni(eq) ratio changes the delta ferrite morphology and, consequently, modifies the weld bead toughness at lower temperatures. The oxygen content can also affect the toughness in the weld bead. The highest absorbed energy in a CVN impact test was obtained for the welding condition with square wave AC electrical output and neutral flux, followed by DC(+) electrical output and neutral flux, and square wave AC electrical output and alloyed flux.
Resumo:
Duplex and superduplex stainless steels present superior mechanical and corrosion properties when compared to usual stainless steels. This superiority is based on chemical composition when in a balanced microstructure (approximately 50% of ferrite). During welding, changes may occur in both, the chemical composition and volume fraction of phases in the material, which may generate the presence of intermetallic phases and, as a consequence, modify the mechanical and corrosion properties of this group of stainless steels. The objective of this work is to apply ASTM A923- Practice A to verify the presence of intermetallic phases in welded joints of UNS 32750 su-perduplex stainless steel. Tubes of UNS 32750, with external diameters of 18 and 44 mm and a thickness of 1.5 mm, were welded using orbital GTAW, with filler metal 25Cr-10Ni-4Mo and a diameter of 0.8 mm. The metal-based and welded joints were characterized by optical and scanning electron microscopy. The results showed that there was no precipitation of the intermetallic phase, such as sigma phase, detected by ASTM A923, but the HAZ of the two tubes studied presented small regions with chromium nitrides, which can also change the properties of welded joins.
Resumo:
Freeform fabrication methods allow the direct formation of parts built layer by layer, under the control of a CAD drawing. Most of these methods form parts in thermoplastic or thermoset polymers, but there would be many applications for freeform fabrication of fully functional metal or ceramic parts. We describe here the freeforming of sinterable aluminium alloys. In addition, the building approach allows different materials to be positioned within a monolithic part for an optimal combination of properties. This is illustrated here with the formation of an aluminium gear with a metal-matrix composite wear surface. (C) 1999 Kluwer Academic Publishers.
Resumo:
Objective: This study aimed at investigating the influence of the porous titanium (Ti) structure on the osteogenic cell behaviour. Materials and methods: Porous Ti discs were fabricated by the powder metallurgy process with the pore size typically between 50 and 400 mm and a porosity of 60%. Osteogenic cells obtained from human alveolar bone were cultured until subconfluence and subcultured on dense Ti (control) and porous Ti for periods of up to 17 days. Results: Cultures grown on porous Ti exhibited increased cell proliferation and total protein content, and lower levels of alkaline phosphatase (ALP) activity than on dense Ti. In general, gene expression of osteoblastic markers-runt-related transcription factor 2, collagen type I, alkaline phosphatase, bone morphogenetic protein-7, and osteocalcin was lower at day 7 and higher at day 17 in cultures grown on porous Ti compared with dense Ti, a finding consistent with the enhanced growth rate for such cultures. The amount of mineralized matrix was greater on porous Ti compared with the dense one. Conclusion: These results indicate that the porous Ti is an appropriate substrate for osteogenic cell adhesion, proliferation, and production of a mineralized matrix. Because of the three-dimensional environment it provides, porous Ti should be considered an advantageous substrate for promoting desirable implant surface-bone interactions.
Resumo:
The Las Canadas caldera is a nested collapse caldera formed by the successive migration and collapse of shallow magmatic chambers. Among the pyroclastic products of this caldera are phonolitic fallout deposits that crop out in the caldera wall and on the extracaldera slopes. These deposits exhibit an uninterrupted facies gradation from nonwelded to lava-like and record continuous volcanic deposition. Densely welded and lava-like facies result from the extreme attenuation and complete homogenization of juvenile clasts that destroy original clast outlines and any evidence of fallout deposition. Agglutination contributes significantly to the final degree of flattening observed in the welded facies. After deposition, rheomorphic flowage occurs. Emplacement temperatures for one of the welding sequences are calculated from magmatic temperatures and a model of tephra cooling during fallout. Results are 486 degreesC for the nonwelded facies and 740 degreesC for the moderately welded facies. For the same welding sequence, a cooling time between 25 and 54 days is estimated from published experimental and computational data as the possible duration of welding and rheomorphism. Following deposition and agglutination, the lava-like pyroclastic facies had the rheological properties of viscous lavas and flowed down the outer slopes away from the caldera. Some lava-like masses detached from proximal areas to more distal regions. During deposition, the eruptive style evolved from Plinian fallout to fountain-fed spatter deposition. This evolution was accompanied by a decrease in explosive power and a lower height of the eruptive column, which produce higher emplacement temperatures and more effective heat retention of pyroclasts.
Resumo:
This article describes work performed on the assessment of the levels of airborne ultrafine particles emitted in two welding processes metal-active gas (MAG) of carbon steel and friction-stir welding (FSW) of aluminium in terms of deposited area in alveolar tract of the lung using a nanoparticle surface area monitor analyser. The obtained results showed the dependence from process parameters on emitted ultrafine particles and clearly demonstrated the presence of ultrafine particles, when compared with background levels. The obtained results showed that the process that results on the lower levels of alveolar-deposited surface area is FSW, unlike MAG. Nevertheless, all the tested processes resulted in important doses of ultrafine particles that are to be deposited in the human lung of exposed workers.
Resumo:
The aim of this study is to assess the levels of airborne ultrafine particles emitted in welding processes (tungsten inert gas [TIG], metal active gas [MAG] of carbon steel, and friction stir welding [FSW] of aluminum) in terms of deposited area in pulmonary alveolar tract using a nanoparticle surface area monitor (NSAM) analyzer. The obtained results showed the dependence of process parameters on emitted ultrafine particles and demonstrated the presence of ultrafine particles compared to background levels. Data indicated that the process that resulted in the lowest levels of alveolar deposited surface area (ADSA) was FSW, followed by TIG and MAG. However, all tested processes resulted in significant concentrations of ultrafine particles being deposited in humans lungs of exposed workers.
Resumo:
This study is focused on the characterization of particles emitted in the metal active gas welding of carbon steel using mixture of Ar + CO2, and intends to analyze which are the main process parameters that influence the emission itself. It was found that the amount of emitted particles (measured by particle number and alveolar deposited surface area) are clearly dependent on the distance to the welding front and also on the main welding parameters, namely the current intensity and heat input in the welding process. The emission of airborne fine particles seems to increase with the current intensity as fume-formation rate does. When comparing the tested gas mixtures, higher emissions are observed for more oxidant mixtures, that is, mixtures with higher CO2 content, which result in higher arc stability. These mixtures originate higher concentrations of fine particles (as measured by number of particles by cm 3 of air) and higher values of alveolar deposited surface area of particles, thus resulting in a more severe worker's exposure.