894 resultados para ring opening polymerization
Resumo:
Blends of the poly(ether sulfone) derived from 4,4'-biphenol and 4,4'-dichlorodiphenylsulfone (Radel-R(TM)) with its homologous macrocyclic oligomers show greatly lowered melt viscosities relative to that of the parent polymer, potentially enabling more facile production and fabrication of fiber-reinforced composite materials. The macrocycles can then undergo entropically driven ring-opening polymerization in situ. The required blends can be obtained easily in one step, by carrying out polycondensations at concentrations lower than those usually used for polymer synthesis.
Resumo:
An amorphous, catechol-based analogue of PEEK ("o-PEEK") has been prepared by a classical step-growth polymerization reaction between catechol and 4,4'-difluorobenzophenone and shown to be readily soluble in a range of organic solvents. Copolymers with p-PEEK have been investigated, including an amorphous 50: 50 composition and a semicrystalline though still organic-soluble material comprising 70% p-PEEK. o-PEEK has also been obtained by entropy-driven ring-opening polymerization of the macrocyclic oligomers (MCO's) formed by cyclo-condensation of catechol with 4,4'-difluorobenzophenone under pseudo-high-dilution conditions. The principal products of this latter reaction were the cyclic dimer 3a (20 wt %), cyclic trimer 3b (16%) cyclic tetramer 3c (14%), cyclic pentamer 3d (13%) and cyclic hexamer 3e (12%). Macrocycles 3a-c were isolated as pure compounds by gradient column chromatography, and the structures of the cyclic dimer 3a and cyclic tetramer 3c were analyzed by single-crystal X-ray diffraction. A mixture of MCO's, 3, of similar composition, was obtained by cyclodepolymerization of high molar mass o-PEEK in dilute soluion.
Resumo:
A homologous series of macrocyclic oligoamides has been prepared in high yield by reaction of isophthaloyl chloride with m-phenylenediamine under pseudo-high-dilution conditions. The products were characterized by infrared and H-1 NMR spectroscopies, matrix assisted laser desorption-ionization time-of-flight mass spectrometry, and gel permeation chromatography (GPC). A series of linear oligomers was prepared for comparison. The macrocycles ranged in size from the cyclic trimer up to at least the cyclic nonamer (90 ring atoms). The same homologous series of macrocyclic oligomers was prepared in high yield by the cyclodepolymerization of poly(m-phenylene isophthalamide) (Nomex). Cyclodepolymerization was best achieved by treating a 1% w/v solution of the polymer in dimethyl sulfoxide containing calcium chloride or lithium chloride with 3-4 mol % of sodium hydride or the sodium salt of benzanilide at 150 degreesC for 70 h. Treatment of a concentrated solution of the macrocyclic oligomers (25% w/v) with 4 mol % of sodium hydride or the sodium salt of benzanilide in a solution of lithium chloride in dimethyl sulfoxide at 170 degreesC for 6 h resulted in efficient entropically driven ring-opening polymerizations to give poly(m-phenylene isophthalamide), characterized by infrared and H-1 NMR spectroscopies and by GPC. The molecular weights obtained were comparable with those of the commercial polymer.
Resumo:
Highly strained macrocyclic ether-ketones obtained by nickel-catalyzed cyclization of linear precursor oligomers undergo ring-opening polyinerization via ether exchange in the presence of nucleophilic initiators such as fluoride or phenoxide anions. Strain enthapies of these macrocycles, from DSC analyses of their exothermic ring-opening polymerization are in the range 50-90 kJ mol(-1). Melt-phase polymerization generally affords slightly cross-linked materials, but solution-phase polymerization at high macrocycle concentrations gives fully soluble, high molar mass polymers with inherent viscosities of up to 1.78 dL g(-1). Sequence-analysis of the resulting polymers by C-13 NMR shows that alternating or random monomer sequences may be obtained, depending on whether one or both aromatic rings adjacent to the ether linkages are activated toward nucleophilic attack.
Resumo:
Polymerizable macrocyclic biarylene-ether-ketones and biarylene-ether-sulfones are accessible from linear, bis(chloro)-terminated oligomers via nickel-catalyzed, intramolecular coupling under pseudo-high-dilution conditions. Single-crystal X-ray analyses of the resulting cyclo-oligomers reveal extremely distorted and highly strained geometries, with 4,4 '-biphenylene units showing deviations of up to 70 degrees from linearity.
Resumo:
Spontaneous ring-opening polymerization of macrocyclic aromatic thioether ketones [-1,4-SC6H4CO-C6H4-](n) (n = 3 and 4), in which the thioether linkages are para to the ketone, occurs during rapid, transient heating to 480degreesC, to afford a soluble, semi-crystalline poly(thioether ketone) of high molar mass (eta(inh) > 1.0 dL . g(-1)). Corresponding macrocyclic ether ketone, and a macrocyclic thioether ether ketone in which the thioether linkage is para to the ether rather than to the ketone, show no evidence of polymerization under analogous conditions.
Resumo:
Uncatalyzed, ring-opening polymerization of individual macrocyclic poly(arylene thioether ketone)s (1-4) and mixtures (5) under dynamic heating conditions has been demonstrated for the first time. High-molecular-weight, film-forming products were obtained after heating of the macrocycles up to 480 degreesC, with a heating rate of 10-20 degreesC /min. Depending on the macrocyclic structure and heat treatment conditions, the polymers obtained were amorphous or semicrystalline, soluble or slightly crosslinked. NMR analyses of the soluble polymers revealed their linear, highly regular structure. According to NMR, DSC, and TGA studies, the polymers obtained do not contain any residual macrocycles. The polymers with thio-p-arylene moieties in the main chain were thermally stabile. The catalyzed ring opening polymerization of 5 carried out in diphenyl sulfone solution is also reported for comparison. Using quantum mechanical calculations of the ring opening of macrocycles, a reaction mechanism is suggested. Preparation of nanosized poly(thioether ketone) fibrils by a replication method is described.
Resumo:
Blends of PEEK with macrocyclic thioether-ketones show initial melt-viscosities reduced by more than an order of magnitude relative to the polymer itself, enabling more facile processing and fabrication. On raising the temperature of the melt, however, the macrocycle undergoes spontaneous, entropically-driven ring-opening polymerization (ED-ROP), so that the properties of the final polymer should not, in principle, be compromised by the presence of low-MW macrocyclic material.
Resumo:
The kinetics and mechanisms of ring opening polymerization and copolymerizntion of different cyclic ethers were studied using mainly a cationic system of iinitiation. BF30Et2/ethanediol. The cyclic ethers reacted differently showing that ring strain and basicity are the main driving forces in cationic ring opening polymerizaion. In most cases it was found that the degree of polymerization is controlled kinetically via terminations with the counterion and the monomers, and that the contribution of each type of reaction to the overall termination differs markedly. The Gel permeation chromatography studies showed that the molecular weight distribution of the samples of polyoxetanes were bimodal. This was in accordance with previous work establishing that the cyclic tetramer is found in much higher proportions than any of the other cyclic oligomers. However the molecular weight distribution of the copolymers made from oxetane and THF or from oxetane and oxepane were shown to be unimodal. These observations could be explained by a change in the structure of the growing end involved in the cationic polymerization. In addition crown ethers like dibenzo-crown-6 and compounds such as veratrole are believed to stabilise the propagating end and promote the formation of living polymers from oxetane.
Resumo:
The kinetics and mechanisms of the ring-opening polymerization of oxetane were studied using cationic and coordinated anionic catalysts. The cationic initiators used were BF30Et2!/ethanol, BF30Et2!/ethanediol and BF30Et2/propantriol. Kinetic determinations with the BF30Et2/diol system indicated that a 1: 1 BF3:0H ratio gave the maximum rate of polymerization and this ratio was employed to detenmne the overall rates of polymerization. An overall second-order dependence was obtained when the system involved ethanediol or propantriol as co-catalyst and a 3/2-order dependence with ethanol, in each case the monomer gave a first-order relationship. This suggested that two mechanisms accounted for the cationic polymerization. These mechanisms were investigated and further evidence for these was obtained from the study of the complex formation of BF30Et2 and the co-catalysts by 1H NMR. Molecular weight studies (using size-exclusion chromatography) indicated that the hydroxyl ion acted as a chain transfer reagent when the [OH] > [BF3]. A linear relationship was observed when the number average molecular weight was plotted against [oxetane] at constant [BF3:0H], and similarly a linear dependency was observed on the BF3:0H 1:1 adduct at constant oxetane concentration. Copolymerization of oxetane and THF was carried out using BF30Et2/ethanol system. The reactivity ratios were calculated as rOXT = 1.2 ± 0.30 and rTHF = 0.14 ± 0.03. These copolymers were random copolymers with no evidence of oligomer formation. The coordinated anionic catalyst, porphinato-aluminium chloride [(TPP)AICl], was used to produce a living polymerization of oxetane. An overall third-order kinetics was obtained, with a second-order with respect to the [(TPP)AICl] and a first-order with respect to the [oxetane] and a mechanism was postulated using these results. The stereochemistry of [(TPP)AlCl] catalyst was investigated using cyclohexene and cyclopentene oxide monomers, using extensive 1H NMR, 2-D COSY and decoupling NMR techniques it was concluded that [(TPP)AlCl] gave rise to stereoregular polymers.
Resumo:
The activation-deactivation pseudo-equilibrium coefficient Qt and constant K0 (=Qt x PaT1,t = ([A1]x[Ox])/([T1]x[T])) as well as the factor of activation (PaT1,t) and rate constants of elementary steps reactions that govern the increase of Mn with conversion in controlled cationic ring-opening polymerization of oxetane (Ox) in 1,4-dioxane (1,4-D) and in tetrahydropyran (THP) (i.e. cyclic ethers which have no homopolymerizability (T)) were determined using terminal-model kinetics. We show analytically that the dynamic behavior of the two growing species (A1 and T1) competing for the same resources (Ox and T) follows a Lotka-Volterra model of predator-prey interactions. © 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Nucleobase-functionalized polymers are widely used in the fields of supramolecular chemistry and self-assembly, and their development for biomedical applications is also an area of interest. They are usually synthesized by tedious multistep procedures. In this study, we assess adenine as an organoinitiator/ organocatalyst for the ring-opening polymerization of lactide. L-Lactide can be quantitatively polymerized in the presence of adenine. Reaction conditions involving short reaction times and relatively low temperatures enable the access to adenine end-capped polylactide in a simple one-step procedure, in bulk, without additional catalyst. DFT calculations show that the polymerization occurs via hydrogen bond catalysis. The mechanism involves (i) a hydrogen bond between the NH9 of adenine and the carbonyl moiety of lactide, leading to an electron deficient carbon atom, and (ii) a second hydrogen bond between the N3 of adenine and the NH2 of a second adenine molecule, followed by a nucleophilic attack of the latter activated amine on the former electron deficient carbon on the monomer. For longer reaction times and higher temperatures, macrocyclic species are formed, and a mechanism involving the imidazole ring of adenine is proposed based on literature studies. Depending on the reaction conditions, adenine can thus be considered as an organoinitiator or an organocatalyst for the ring-opening polymerization of lactide.
Resumo:
Nucleobase-functionalized polymers are widely used in the fields of supramolecular chemistry and self-assembly, and their development for biomedical applications is also an area of interest. They are usually synthesized by tedious multistep procedures. In this study, we assess adenine as an organoinitiator/organocatalyst for the ring-opening polymerization of lactide. L-Lactide can be quantitatively polymerized in the presence of adenine. Reaction conditions involving short reaction times and relatively low temperatures enable the access to adenine end-capped polylactide in a simple one-step procedure, in bulk, without additional catalyst. DFT calculations show that the polymerization occurs via hydrogen bond catalysis. The mechanism involves (i) a hydrogen bond between the NH9 of adenine and the carbonyl moiety of lactide, leading to an electron deficient carbon atom, and (ii) a second hydrogen bond between the N3 of adenine and the NH2 of a second adenine molecule, followed by a nucleophilic attack of the latter activated amine on the former electron deficient carbon on the monomer. For longer reaction times and higher temperatures, macrocyclic species are formed, and a mechanism involving the imidazole ring of adenine is proposed based on literature studies. Depending on the reaction conditions, adenine can thus be considered as an organoinitiator or an organocatalyst for the ring-opening polymerization of lactide.