(1-x)PbF2-(x)CdF2 solid solutions (with 0.1 less than or equal to x less than or equal to 0.5) were obtained by hyper-quenching the melt. Structural characteristics have been studied by X-ray diffraction (XRD) and extended X-ray absorption fine structure (EXAFS). A cubic solid solution was obtained in which the lattice parameter decreases with increasing CdF2 content. High anionic disorder was evidenced from EXAFS investigations, whereas cations remain in the FCC arrangement. Pb L-3-edge EXAFS results illustrate clearly the occurrence of CdxPb1-xF2 mixed crystals by the introduction of Cd atoms in the second Pb coordination shell. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Glasses and glass-ceramics have been obtained in oxyfluoride systems involving lead and cadmium fluorides and one of the well-known glass former oxides SiO2, B2O3 and TeO2. Vitreous domains were established and a wide range of compositions including high heavy metal contents lead to stable glasses. Amorphous structures have been studied by short-range order spectroscopy techniques (Raman scattering and x-ray absorption) and molecular basic structures have been identified. Besides the usual oxides, the role of glass former could also be proposed for cadmium ions. Special attention has been paid for crystallization process. Cubic lead fluoride, cubic lead tellurite, tetragonal tellurium oxide and a solid solution of the type Pb1-xCdxF2 are obtained as crystallization products depending on the composition and temperature of heat treatments. Pb1-xCdxF2 solid solutions are well known superionic materials and obtaining this solid solution as a crystal phase could be very interesting for applications concerning ionic electrical conduction properties. The addition of rare earth ions led to the control of the crystallization process. In the presence of the nucleating ion only the cubic form beta-PbF2 was identified. Rare earth ions are present in the crystal phase and crystal-like spectroscopic properties were observed suggesting interesting applications for these perfectly transparent glass ceramics in photonics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In Lead-cadmium fluorogermanate glasses (PbF2-CdF 2-PbGeO3) the addition of metal fluorides to the base PbGeO3 glass leads to a decrease of the glass transition temperature (Tg) and to an enhancement of the ionic conductivity properties. Based on different spectroscopic techniques (19F NMR, Ge K-edge X-ryas absorption and Raman scattering) an heterogeneous glass structure is proposed at the molecular scale, which can be described by fluoride rich regions permeating the metagermanate chains. The temperature dependence of the 19F NMR lineshapes and relaxation times exhibits the qualitative and quantitative features associated with the high fluoride mobility in these systems. Eu 3+ emission and vibronic spectra are used to follow the crystallization process leading to transparent glass ceramics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A study to measure the heavy metal pollution level in the sediment of coastal and offshore area indicates that high concentration of heavy metals were found around Manora channel and eastern coast of Karachi. In comparison with coastal areas, relatively low concentration of heavy metals was recorded in the offshore area. The result shows that sewage and industrial wastes are the main source of heavy metal pollution in the coastal area. The concentration of heavy metals in the sediments is as follows: Chromium 10.4-33.69, nickel 13.3-47.6, lead 10.0-39.04, cadmium 0.08-0.21, zinc 7.4-73.2 and copper 9.44-18.56 mg/kg. In the offshore areas strong correlation was observed between copper and organic carbon, and calcium carbonate and cadmium. In the shore area such correlation has been recorded among nickel, chromium, zinc, and chromium and copper. The Karachi. coast is viewed as moderately polluted when compared to other continental coastal areas.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In order to assess the toxicity of heavy metals on the early development of Meretrix meretrix, the effects of mercury (Hg), cadmium (Cd) and lead (Pb) on embryogenesis, survival, growth and metamorphosis of larvae were investigated. The EC50 for embryogenesis was 5.4 mu g l(-1) for Hg, 1014 mu g l(-1) for Cd and 297 mu g l(-1) for Pb, respectively. The 96 h LC50 for D-shaped larvae was 14.0 mu g l(-1) for Hg, 68 mu g l(-1) for Cd and 353 mu g l(-1) for Pb, respectively. Growth was significantly retarded at 18.5 mu g l(-1) (0.1 mu M) for Hg, 104 mu g l(-1) (1 mu M) for Cd and 197 mu g l(-1) (1 mu M) for Pb, respectively. The EC50 for metamorphosis, similar to 48 h LC50, was higher than 96 h LC50. Our results indicate that the early development of M. meretrix is highly sensitive to heavy metals and can be used as a test organism for ecotoxicology bioassays in temperate and subtropical regions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Blue, green, red, and near-infrared upconversion luminescence in the wavelength region of 480-740 nm in Pr3+/Yb3+-codoped lead-cadmium-germanate glass under 980 nm diode laser excitation, is presented. Upconversion emission peaks around 485, 530, 610, 645, and 725 nm which were ascribed to the P-3(0)-H-3(J) (J = 4, 5, and 6), and P-3(0)-F-3(J) (J = 2, 3, and 4), transitions, respectively, were observed. The population of the praseodymium upper P-3(0) emitting level was accomplished through a combination of ground-state absorption of Yb3+ ions at the F-2(7/2), energy-transfer Yb3+(2F(5/2))-Pr3+(H-3(4)), and excited-state absorption of Pr3+ ions provoking the (1)G(4)-P-3(0) transition. The dependence of the upconversion luminescence upon the Yb3+-concentration and diode laser power, is also examined, in order to subsidize the proposed upconversion excitation mechanism. (C) 2004 Elsevier B,V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Glass structure and fluorine motion dynamics are investigated in lead-cadmium fluorgermanate glasses by means of differential scanning calorimetry, Raman scattering, x-ray absorption (EXAFS), electrical conductivity (EC), and F-19 nuclear magnetic resonance (NMR) techniques. Glasses with composition 60PbGeO(3)-xPbF(2)-yCdF(2) (in mol %), with x+y=40 and x=10, 20, 30, 40, are studied. Addition of metal fluorides to the base PbGeO3 glass leads to a decrease of the glass transition temperature (T-g) and to an enhancement of the ionic conductivity properties. Raman and EXAFS data analysis suggest that metagermanate chains form the basic structural feature of these glasses. The NMR study leads to the conclusion that the F-F distances are similar to those found in pure crystalline phases. Experimental results suggest the existence of a heterogeneous glass structure at the molecular scale, which can be described by fluorine rich regions permeating the metagermanate chains. The temperature dependence of the NMR line shapes and relaxation times exhibits the qualitative and quantitative features associated with the high fluorine mobility in these systems. (C) 2004 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Blue, green, red, and near-infrared upconversion luminescence in the wavelength region of 480 - 740 nm in Pr3+/Yb3+-codoped lead-cadmium-germanate glass under 980 nm diode laser excitation, is presented. Upconversion emission peaks around 485, 530, 610, 645, and 725 nm which were ascribed to the 3P0 - 3HJ (J=4, 5, and 6), and 3P0 - 3FJ (J=2, and 3,4), transitions, respectively, were observed. The population of the praseodymium upper 3P0 emitting level was accomplished through a combination of ground-state absorption of Yb3+ ions at the 2F7/2, energy-transfer Yb3+(2F 5/2) Pr3+(3H4), and excited-state absorption of Pr3+ ions provoking the 1G4 - 3P0 transition. The dependence of the upconversion luminescence upon the Yb3+-concentration and diode laser power, is also examined, in order to subsidize the proposed upconversion excitation mechanism.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this report we investigate the optical properties and energy-transfer upconversion luminescence of Ho3+- and Tb3+/Yb 3+-codoped PbGeO3-PbF2-CdF2 glass-ceramic under infrared excitation. In Ho3+/Yb 3+-codoped sample, green(545 nm), red(652 nm), and near-infrared(754 nm) upconversion luminescence corresponding to the 4S 2(5F4) → 5I8, 5F5 → 5I8, and 4S2(5F4) → 5I 7, respectively, was readly observed. Blue(490 nm) signals assigned to the 5F2,3 → 5I8 transition was also detected. In the Tb3+/Yb3+ system, bright UV-visible emission around 384, 415, 438, 473-490, 545, 587, and 623 nm, identified as due to the 5D3(5G6) → 7FJ(J=6,5,4) and 5D4→ 7FJ(J=6,5,4,3) transitions, was measured. The comparison of the upconversion process in glass ceramic and its glassy precursor revealed that the former samples present much higher upconversion efficiencies. The dependence of the upconversion emission upon pump power, and doping contents was also examined. The results indicate that successive energy-transfer between ytterbium and holmium ions and cooperative energy-transfer between ytterbium and terbium ions followed by excited-state absorption are the dominant upconversion excitation mechanisms herein involved. The viability of using the samples for three-dimensional solid-state color displays is also discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The general purpose of this study is to investigate the degree of heavy metal accumulation in hard and soft tissue of sea urchin, and determining these tissues as the most suitable bioindicator for lead and cadmium in the environment of the sampling stations. The way of doing this assessment was MOOPAM. Samples were prepared and classified according to sea urchin organ (soft tissue, hard tissue, Tube feet, Test, Lantern Structure and spines) and then lead and cadmium were measured in them. Result of this study shows that hard tissue is a better index of lead and cadmium than soft tissue. The result of bioaccumulation of lead in the related tissue was found to be in the following order: Soft tissue=21, hard tissue=28.1, Test=20.8, Lantern Structure=20.5 and spines=23.9. The result of bioaccumulation of cadmium in the related tissue was found to be in the following order: Soft tissue=9. 7, hard tissue=5.01, Test=4.2, Lantern Structure=4.06 and spines=5.53.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lead-Cadmium fluorosilicate stable glasses were prepared and the vitreous domain region determined in the composition diagram. Characteristic temperatures were obtained from thermal analysis and the structural studies performed illustrate clearly the role played by lead atoms in the glasses crystallization behavior and the glass-forming ability of cadmium atoms. The occurrence of either a cubic lead fluoride or a lead-cadmium fluoride solid solution in crystallizing samples was found to be dependent on Er3+ doping. The optically active ions were found to concentrate in the crystalline phase and in fact play the role of nucleating agent as suggested from X-ray diffraction and EXAFS measurements. (C) 2002 Elsevier B.V. Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)